Prior art keywords
powder
alumina
insulating adhesive
zinc oxide
silicon sol
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410535422.9A
Other languages
English (en)
Other versions
CN104327749A (zh
Inventor
不公告发明人
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Huacheng New Materials Co., Ltd.
Original Assignee
HEFEI TINGSUO ENVIRONMENTAL PROTECTION MATERIALS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HEFEI TINGSUO ENVIRONMENTAL PROTECTION MATERIALS Co Ltd filed Critical HEFEI TINGSUO ENVIRONMENTAL PROTECTION MATERIALS Co Ltd
Priority to CN201410535422.9A priority Critical patent/CN104327749B/zh
Publication of CN104327749A publication Critical patent/CN104327749A/zh
Application granted granted Critical
Publication of CN104327749B publication Critical patent/CN104327749B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Adhesives Or Adhesive Processes (AREA)
  • Laminated Bodies (AREA)

Abstract

本发明公开了一种绝缘粘结剂及其制作方法,其组成原料为:硅溶胶75-80、硅丙乳液30-35、矾土细粉40-50、氧化铝粉末10-12、玻璃纤维4-5、甲基三甲基硅烷6-9、氧化锌粉末3-4、聚乙烯蜡4-5、对苯二甲酸酯1-2、对羟基苯磺酸0.3-0.4、钛酸正丁酯5-6、聚乙烯吡咯烷酮2-3和水80-90;本发明采用硅溶胶、硅丙乳液为原料,粘性大,加入矾土细粉、氧化铝粉末和氧化锌粉末,使得粘结剂中的结构多层复合,结构巧妙,使其具备较强的抗干扰能力,同时具有绝缘和抗干扰能力,适用于各种干扰环境。

Description

绝缘粘结剂及其制作方法
技术领域
本发明属于建筑建材技术领域,具体涉及一种绝缘粘结剂及其制作方法。
背景技术
随着人类对环境保护和身体健康的日益重视,绿色环保粘结剂得到越来越广泛的使用,大多采用天然原材料,资源丰富,价格低,可再生;大多数胶黏剂的组份中含石油的衍生化工产品,随着石油资源日益减少,寻找石油替代品成为必然;人们的环保意识增强,对影响环境质量的有毒有害气体、废水等污染物的排放提出了严格的要求。
发明内容
本发明的目的在于提供一种绝缘粘结剂及其制作方法。
本发明采用如下技术方案:
绝缘粘结剂,其组成原料的重量份为:硅溶胶75-80、硅丙乳液30-35、矾土细粉40-50、氧化铝粉末10-12、玻璃纤维4-5、甲基三甲基硅烷6-9、氧化锌粉末3-4、聚乙烯蜡4-5、对苯二甲酸酯1-2、对羟基苯磺酸0.3-0.4、钛酸正丁酯5-6、聚乙烯吡咯烷酮2-3和水80-90。
绝缘粘结剂,其组成原料的重量份为:
硅溶胶78、硅丙乳液32、矾土细粉45、氧化铝粉末11、玻璃纤维4.5、甲基三甲基硅烷8、氧化锌粉末3.5、聚乙烯蜡4.5、对苯二甲酸酯1.5、对羟基苯磺酸0.3、钛酸正丁酯5.5、聚乙烯吡咯烷酮2.5和水85。
绝缘粘结剂的制作方法,包括以下步骤:
(1)按组成原料的重量份称取各原料,先将硅溶胶和硅丙乳液混合均匀,向其中加入矾土细粉、氧化铝粉末、氧化锌粉末,混合加热至70-80℃,30-40分钟后冷却,备用;
(2)称取玻璃纤维,先用15%氢氧化钠溶液浸泡2-3h,滤过烘干,然后加入聚乙烯蜡、对苯二甲酸酯、对羟基苯磺酸和适量的水,调节Ph至中性,加热至45-50℃,搅拌均匀备用;
(3)合并步骤(1)、(2)的备用料,然后加入其它剩余组成原料,加热至85-95℃搅拌30-60min,降温至45℃以下出料。
本发明的有益效果:
本发明采用硅溶胶、硅丙乳液为原料,粘性大,加入矾土细粉、氧化铝粉末和氧化锌粉末,使得粘结剂中的结构多层复合,结构巧妙,使其具备较强的抗干扰能力,同时具有绝缘和抗干扰能力,适用于各种干扰环境。
具体实施方式
实施例1:绝缘粘结剂,其组成原料的重量份(kg)为:硅溶胶78、硅丙乳液32、矾土细粉45、氧化铝粉末11、玻璃纤维4.5、甲基三甲基硅烷8、氧化锌粉末3.5、聚乙烯蜡4.5、对苯二甲酸酯1.5、对羟基苯磺酸0.3、钛酸正丁酯5.5、聚乙烯吡咯烷酮2.5和水85。
绝缘粘结剂的制作方法,包括以下步骤:
(1)按组成原料的重量份称取各原料,先将硅溶胶和硅丙乳液混合均匀,向其中加入矾土细粉、氧化铝粉末、氧化锌粉末,混合加热至75℃,35分钟后冷却,备用;
(2)称取玻璃纤维,先用15%氢氧化钠溶液浸泡2-3h,滤过烘干,然后加入聚乙烯蜡、对苯二甲酸酯、对羟基苯磺酸和适量的水,调节Ph至中性,加热至45-50℃,搅拌均匀备用;
(3)合并步骤(1)、(2)的备用料,然后加入其它剩余组成原料,加热至90℃搅拌45min,降温至45℃以下出料。
上述制得的粘结剂的性能指标:滴度:53滴/分钟,干燥速度32-35分钟;粘合强度:15-17Kgf/10cm楞;抗压强度640-650Kgf。

Claims (3)

1.一种绝缘粘结剂,其特征在于其组成原料的重量份为:
硅溶胶75-80、硅丙乳液30-35、矾土细粉40-50、氧化铝粉末10-12、玻璃纤维4-5、甲基三甲基硅烷6-9、氧化锌粉末3-4、聚乙烯蜡4-5、对苯二甲酸酯1-2、对羟基苯磺酸0.3-0.4、钛酸正丁酯5-6、聚乙烯吡咯烷酮2-3和水80-90。
2.根据权利要求1所述的绝缘粘结剂,其特征在于其组成原料的重量份为:
硅溶胶78、硅丙乳液32、矾土细粉45、氧化铝粉末11、玻璃纤维4.5、甲基三甲基硅烷8、氧化锌粉末3.5、聚乙烯蜡4.5、对苯二甲酸酯1.5、对羟基苯磺酸0.3、钛酸正丁酯5.5、聚乙烯吡咯烷酮2.5和水85。
3.一种如权利要求1所述的绝缘粘结剂的制作方法,其特征在于包括以下步骤:
(1)按组成原料的重量份称取各原料,先将硅溶胶和硅丙乳液混合均匀,向其中加入矾土细粉、氧化铝粉末、氧化锌粉末,混合加热至70-80℃,30-40分钟后冷却,备用;
(2)称取玻璃纤维,先用15%氢氧化钠溶液浸泡2-3h,滤过烘干,然后加入聚乙烯蜡、对苯二甲酸酯、对羟基苯磺酸和适量的水,调节pH至中性,加热至45-50℃,搅拌均匀备用;
(3)合并步骤(1)、(2)的备用料,然后加入其它剩余组成原料,加热至85-95℃搅拌30-60min,降温至45℃以下出料。
CN201410535422.9A 2014-10-13 2014-10-13 绝缘粘结剂及其制作方法 Active CN104327749B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410535422.9A CN104327749B (zh) 2014-10-13 2014-10-13 绝缘粘结剂及其制作方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410535422.9A CN104327749B (zh) 2014-10-13 2014-10-13 绝缘粘结剂及其制作方法

Publications (2)

Publication Number Publication Date
CN104327749A CN104327749A (zh) 2015-02-04
CN104327749B true CN104327749B (zh) 2016-06-01

Family

ID=52402563

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410535422.9A Active CN104327749B (zh) 2014-10-13 2014-10-13 绝缘粘结剂及其制作方法

Country Status (1)

Country Link
CN (1) CN104327749B (zh)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106007631B (zh) * 2016-05-17 2019-04-16 重庆固安捷实业有限公司 一种发泡混凝土锚固增强剂

Family Cites Families (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1249187C (zh) * 2002-08-31 2006-04-05 贾铭琳 聚苯乙烯保温板外墙外保温专用有机无机复合粘结剂
CN101426872B (zh) * 2007-02-15 2011-08-31 中国科学院过程工程研究所 耐高温无机复合粘结剂
CN102533130B (zh) * 2010-12-07 2013-10-02 上海务宝机电科技有限公司 防水自固化无机型导热胶泥
CN103173130B (zh) * 2013-03-23 2014-07-30 广东新展化工新材料有限公司 一种建筑用改性有机硅密封胶及其制备方法
CN103450816B (zh) * 2013-05-23 2014-08-06 荣氏新材料(湖北)股份有限公司 一种蛭石防火板专用胶

Also Published As

Publication number Publication date
CN104327749A (zh) 2015-02-04

Similar Documents

Publication Publication Date Title
CN103483963B (zh) 一种多功能批刮型单、双组分隔热保温涂料及其制备方法
CN103614037B (zh) 一种绿色环保建筑防水涂料
CN102229771A (zh) 一种硅藻土活性涂料及制备方法
CN102585617A (zh) 一种氟碳改性苯丙涂料及其制备方法
CN106519594A (zh) 一种用于纳米注塑的抗油污耐水解的pbt工程塑料组合物及其制备方法
CN103993508B (zh) 玻璃纤维棉、核级玻璃纤维空气过滤纸和制造核级玻璃纤维的空气过滤纸的方法
CN104327749B (zh) 绝缘粘结剂及其制作方法
CN106189921A (zh) 一种具有高粘结强度的poe封装胶膜用复合增粘剂及其应用
CN106753203A (zh) 一种脱酸型有机硅胶粘剂及其制备方法
CN103614017B (zh) 一种含有松香水的防水涂料
CN104327776B (zh) 抗氧化耐摩擦粘结剂及其制作方法
CN103897577B (zh) 玻璃涂料及其制备方法
CN107177305A (zh) 一种防火漆
CN102719146A (zh) 一种立体油墨
CN102163497B (zh) 高性能宽频电磁辐射吸波挤出橡塑磁片的制备方法及磁片
CN102911538A (zh) 一种高分子乳胶防水涂料
CN104326715B (zh) 一种快速固化粘结剂及其制作方法
CN102403410B (zh) 太阳能电池背板生产工艺
CN103589329A (zh) 一种新型镇流器用绝缘漆及其制备方法
CN107324688A (zh) 一种吸波透气环保装饰线条及其制备方法
CN101864235A (zh) 一种外墙涂料的制备方法
CN109216630A (zh) 一种高性能锂离子电池复合隔膜制作方法
CN101818025A (zh) 一种隔热防水涂料
CN105037765A (zh) 一种电容器用掺混纳米二硫化钼负载氧化石墨烯的聚酰亚胺高介电复合薄膜及其制备方法
CN205818580U (zh) 一种镀膜夹层玻璃

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20181126

Address after: 233010 Pioneering Building 316, Huineng Small and Micro Enterprises Pioneering Center, 1750 Shengli West Road, Yuhui District, Bengbu City, Anhui Province

Patentee after: Bengbu Dingrong Science and Technology Information Consulting Co., Ltd.

Address before: 230601 room 803, 25 West Wen Jin new town, jadeite Road, Hefei, Anhui

Patentee before: HEFEI TINGSUO ENVIRONMENTAL PROTECTION MATERIALS CO., LTD.

TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20190409

Address after: Room 107, Building No. 28, Hexili, Xiba, Chaoyang District, Beijing

Patentee after: Li Qiannan

Address before: 233010 Pioneering Building 316, Huineng Small and Micro Enterprises Pioneering Center, 1750 Shengli West Road, Yuhui District, Bengbu City, Anhui Province

Patentee before: Bengbu Dingrong Science and Technology Information Consulting Co., Ltd.

TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20190516

Address after: 528400 No.5 Card of Building B, 101 Gaoping Avenue, Sanjiao Town, Zhongshan City, Guangdong Province

Patentee after: Guangdong Huacheng New Materials Co., Ltd.

Address before: Room 107, Building No. 28, Hexili, Xiba, Chaoyang District, Beijing

Patentee before: Li Qiannan