CN104324814A - Low-grade copper mine flotation agent and preparation method thereof - Google Patents
Low-grade copper mine flotation agent and preparation method thereof Download PDFInfo
- Publication number
- CN104324814A CN104324814A CN201410506800.0A CN201410506800A CN104324814A CN 104324814 A CN104324814 A CN 104324814A CN 201410506800 A CN201410506800 A CN 201410506800A CN 104324814 A CN104324814 A CN 104324814A
- Authority
- CN
- China
- Prior art keywords
- parts
- flotation agent
- activator
- copper
- good
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a low-grade copper mine flotation agent, which is prepared with the following materials in part by weight: 25 to 30 parts of 208 dithiophosphate, 12 to 14 parts of ethyl isopropylxanthogenic formate, 9 to 12 parts of ammonium dibutyl dithiophosphate, 2 to 3 parts of dihenylethyl phenol polyoxyethylene ether, 1 to 2 parts of polyethyleneglycol monooleate, 3 to 4 parts of triethylene tetramine, 5 to 7 parts of menthol, 5 to 8 parts of phytic acid, 2 to 3 parts of calcium oxide, 2 to 4 parts of soda and 4 to 5 parts of activator. The foam of the flotation agent is stable, the flocculation effect is good, the flotation agent has good collecting capability within the pH range between 7 and 10, the capability of copper collection is high, yield is high, the selectivity of the agent is good, and the grade of copper is high; becauase the activator contains components such as fumed silica, dispersion is stable, moreover, permeability is good, activation is good, the duration of the activation effect is long, and the yield and grade of copper can be increased.
Description
Technical field
The present invention relates to mineral flotation agent field, particularly a kind of Treating Low-grade Copper Ores flotation agent and preparation method thereof.
Background technology
At present, China selects smelting copper mineral raw material mainly chalcopyrite, vitreous copper, bornite, malachite etc.By selecting and smelting technology condition, Copper Ores is marked three natural types with the ratio of cupric oxide and copper sulfide.I.e. sulfide ore, is less than 10% containing cupric oxide; Oxidized ore, is greater than 30% containing cupric oxide; Mixed ore, containing cupric oxide 10% ~ 30%.
The collecting agent occupying leading position in current copper ore floatation technique is the floating agent such as xanthates, thiophosphate and mercaptan, thiamines ester, xanthate, black powder ester, xanthate, but in the ore dressing of reality, the many requirements that can not reach design of result, often occur that copper, sulphur content are from undesirable, the phenomenon that in copper concentrate product, sulfur-bearing exceeds standard; Also have the productive rate of copper low, the copper concentrate rate of recovery is on the low side, causes the waste of mining deposits.
Summary of the invention
The object of this invention is to provide a kind of Treating Low-grade Copper Ores flotation agent and preparation method thereof, this flotation agent has pH strong adaptability, and collecting performance is good, selective good, the advantage that activation effect is good.
Technical scheme of the present invention is as follows:
A kind of Treating Low-grade Copper Ores flotation agent, is characterized in that being made up of the raw material of following weight portion: 208 black powder 25-30, isopropyl xanthogen ethyl formate 12-14, butyl ammonium aerofloat 9-12, Diphenethyl multiple phenol polyethenoxy ether 2-3, polyoxyethylene oleic acid ester 1-2, triethylene tetramine 3-4, menthol 5-7, phytic acid 5-8, calcium oxide 2-3, soda 2-4, activator 4-5;
Described activator is made up of the raw material of following weight portion: gas-phase silica 2-4, SIMMONDSIA CHINENSIS SEED OIL 2-3, butyl hydroxybenzoate 2-3, silane resin acceptor kh-550 1-2, penetrant t 2-3, disecoctylmaleate sodium sulfonate 2-3, isocyanates 4-6, CuSO
44-7, sodium hydrogen phosphate 4-6, water 40-50; Its preparation method is mixed by each raw material, is heated to 60-65 DEG C, turns lower stirring 40-50 minute, to obtain final product at 2000-2500.
The preparation method of described Treating Low-grade Copper Ores flotation agent, it is characterized in that: by other composition mixing except activator, at 40-50 DEG C, under 7000-9000 rev/min, stir 10-15 minute, add activator again, stir under 5000-7000 rev/min 20-30 minute and get final product.
Beneficial effect of the present invention
Flotation agent foam stabilization of the present invention, solidifying wadding is effective, within the scope of pH7-10, all have good collecting ability, and strong to copper collecting ability, productive rate is high, and medicament is selective good, copper of high grade; Activator of the present invention contains the compositions such as gas-phase silica, stably dispersing, and good penetrability, and reactivity is good, and the activation effect duration is long, can improve productive rate and the grade of copper.
Detailed description of the invention
A kind of Treating Low-grade Copper Ores flotation agent, is made up of the raw material of following weight portion (kilogram): 208 black powder 28, isopropyl xanthogen ethyl formate 13, butyl ammonium aerofloat 11, Diphenethyl multiple phenol polyethenoxy ether 2.5, polyoxyethylene oleic acid ester 1.5, triethylene tetramine 3.5, menthol 6, phytic acid 7, calcium oxide 2.5, soda 3, activator 4.5;
Described activator is made up of the raw material of following weight portion (kilogram): gas-phase silica 3, SIMMONDSIA CHINENSIS SEED OIL 2.5, butyl hydroxybenzoate 2.5, silane resin acceptor kh-550 1.5, penetrant t 2.5, disecoctylmaleate sodium sulfonate 2.5, isocyanates 5, CuSO
46, sodium hydrogen phosphate 5, water 45; Its preparation method is mixed by each raw material, is heated to 63 DEG C, 2300 turns of lower stirrings 45 minutes, to obtain final product.
The preparation method of described Treating Low-grade Copper Ores flotation agent is: by other composition mixing except activator, at 45 DEG C, stir 13 minutes, then add activator under 8000 revs/min, stir 25 minutes and get final product under 6000 revs/min.
The flotation agent of the present embodiment is used for Treating Low-grade Copper Ores flotation, and copper productive rate reaches 3.6%, and copper grade reaches 15.4%, and copper recovery reaches 90.5%.
Claims (2)
1. a Treating Low-grade Copper Ores flotation agent, is characterized in that being made up of the raw material of following weight portion: 208 black powder 25-30, isopropyl xanthogen ethyl formate 12-14, butyl ammonium aerofloat 9-12, Diphenethyl multiple phenol polyethenoxy ether 2-3, polyoxyethylene oleic acid ester 1-2, triethylene tetramine 3-4, menthol 5-7, phytic acid 5-8, calcium oxide 2-3, soda 2-4, activator 4-5;
Described activator is made up of the raw material of following weight portion: gas-phase silica 2-4, SIMMONDSIA CHINENSIS SEED OIL 2-3, butyl hydroxybenzoate 2-3, silane resin acceptor kh-550 1-2, penetrant t 2-3, disecoctylmaleate sodium sulfonate 2-3, isocyanates 4-6, CuSO
44-7, sodium hydrogen phosphate 4-6, water 40-50; Its preparation method is mixed by each raw material, is heated to 60-65 DEG C, turns lower stirring 40-50 minute, to obtain final product at 2000-2500.
2. the preparation method of Treating Low-grade Copper Ores flotation agent according to claim 1, it is characterized in that: by other composition mixing except activator, at 40-50 DEG C, under 7000-9000 rev/min, stir 10-15 minute, add activator again, stir under 5000-7000 rev/min 20-30 minute and get final product.