CN104277593A - Net flavor easily constructed oily color concentrate and production method thereof - Google Patents

Net flavor easily constructed oily color concentrate and production method thereof Download PDF

Info

Publication number
CN104277593A
CN104277593A CN201310291326.XA CN201310291326A CN104277593A CN 104277593 A CN104277593 A CN 104277593A CN 201310291326 A CN201310291326 A CN 201310291326A CN 104277593 A CN104277593 A CN 104277593A
Authority
CN
China
Prior art keywords
toner
easily constructed
color concentrate
oily
clean taste
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310291326.XA
Other languages
Chinese (zh)
Inventor
孙军
周琼辉
王磊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHENGDU ZHANCHEN CHEMICAL Co Ltd
QINGDAO FUCHEN CHEMICAL CO Ltd
Shanghai Fuchen Chemical Co Ltd
Beijing Zhanchen Chemical Co Ltd
Zhanchen Paint Group Co Ltd
Original Assignee
CHENGDU ZHANCHEN CHEMICAL Co Ltd
QINGDAO FUCHEN CHEMICAL CO Ltd
Shanghai Fuchen Chemical Co Ltd
Beijing Zhanchen Chemical Co Ltd
Zhanchen Paint Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHENGDU ZHANCHEN CHEMICAL Co Ltd, QINGDAO FUCHEN CHEMICAL CO Ltd, Shanghai Fuchen Chemical Co Ltd, Beijing Zhanchen Chemical Co Ltd, Zhanchen Paint Group Co Ltd filed Critical CHENGDU ZHANCHEN CHEMICAL Co Ltd
Priority to CN201310291326.XA priority Critical patent/CN104277593A/en
Publication of CN104277593A publication Critical patent/CN104277593A/en
Pending legal-status Critical Current

Abstract

The invention provides net flavor easily constructed oily color concentrate for an oily wood lacquer coloring and wiping process and a production method of the color concentrate. The net flavor easily constructed oily color concentrate comprises the following raw materials in percentage by weight: a net flavor solvent, toner and a flatting agent, wherein the net flavor solvent adopts a product with the model of Augeo191 in the NCM limited company; the toner adopts toner Y-20 or toner R-35 or toner B-20 in Ming Hui in Jiangsu province; and the flatting agent can adopt a product with the model of BYK333 in BYK. The net flavor easily constructed oily color concentrate disclosed by the invention has basic performances of the traditional oily color concentrate and is environment-friendly and odorless, multiple construction process operations such as erasing, brushing and spraying can be adopted, and the color types, color degree and color brightness can be selected according to pigments. The oily color concentrate is suitable for bottom coloring and finish padding of various oil systems. The defect that the oily color concentrate is fast in volatilization and only can be sprayed is overcome, and the problem that water-based color concentrate is high in permeability and is easy in floating is solved.

Description

Clean taste easily construct oiliness look essence and production method
Technical field
The present invention relates to a kind of oiliness look essence, refer in particular to a kind of clean taste for oiliness wood lacquer coloring process easily construct oiliness look essence and production method.
Background technology
Look essence is wood furniture, Wood craft manufactures raw material conventional in process.Common oiliness look essence is all solvent type, and its production technology generally adopts alcohols, ester class or ether-ether class as solvent.Adopt the look essence of producing in this way and there is a large amount of hazardous solvents, pungency is very large, all brings larger harm to the healthy of workmen and environment.And the water-based look in market single-minded as be all that although compare environmental protection, application property is relatively poor using water or alcohol as solvent.
Summary of the invention
The object of this invention is to provide a kind of clean taste painted for oiliness wood lacquer easily construct oiliness look essence and production method, with overcome prior art exist above-mentioned defect.
The present invention design clean taste easily construct oiliness look essence, it is characterized in that, be made up of following composition and weight percent:
Clean taste solvent 65% ~ 75%,
Toner 25% ~ 35%,
Flow agent 0.01% ~ 0.1%
Described clean taste solvent is that one derives from renewable resources, has the product of low volatility, and the trade mark adopting jade of the He family Chemical Co., Ltd. is the product of Augeo191.Described toner adopts organic toner that heavy metal content is extremely low, can adopt the Y-20 toner of river Su Minghui or R-35 toner or B-20 toner.Described flow agent adopts the flow agent not containing VOC and solvent, and the trade mark of German Bi Ke company can be adopted to be the product of BYK333.Prepare clean taste easily to construct the method for oiliness look essence, it is characterized in that, comprise the steps:
(1) be first conventional physical mixed dissolving method, first add, then slowly add toner by environmentally friendly solvent, high-speed stirring is complete to dissolving,
(2) then with the filter-cloth filtering of 10 μm, qualified product is namely obtained.Wherein, in step (1), described high speed is 1500 ~ 2000rpm, and wherein, in step (2), described fineness is≤10 μm.Beneficial effect of the present invention: traditional oiliness look vital essence taste is large, pungency is strong, can only adopt the construction technology of spraying simultaneously, although and the smaller and environmental protection of water-based look essence smell, wiping properties is poor.The present invention adopts clean taste solvent, reaches tasteless effect, and simultaneously because rate of volatilization is low, obliterating, brushing, spraying all can operate.
Embodiment
Embodiment 1
The red essence of clean taste oiliness:
It is as follows that weight got by starting material:
Augeo191 70 kilograms,
Bright brightness R-35 toner 29.99 kilograms,
Flow agent BYK333 0.01 kilogram,
Amount to double centner
Preparation method:
(1) be first conventional physical mixed dissolving method, first add, then slowly add toner by clean taste solvent, high-speed stirring is complete to dissolving,
(2) then with the filter-cloth filtering of 10 μm, qualified product is namely obtained.
Detected result is as follows:
Solid content is 30%GB/T 1725-79(second method)
Outward appearance: red semi-fluid GB 1727-79.
Embodiment 2
The yellow essence of clean taste oiliness:
It is as follows that weight got by starting material:
Augeo191 64.95 kilograms,
Bright brightness Y-20 toner 35 kilograms,
Flow agent BYK333 0.05 kilogram,
Amount to double centner
Preparation method:
(1) be first conventional physical mixed dissolving method, first add, then slowly add toner by clean taste solvent, high-speed stirring is complete to dissolving,
(2) then with the filter-cloth filtering of 10 μm, qualified product is namely obtained.
Detected result is as follows:
Solid content is 30% GB/T 1725-79(second method)
Outward appearance: yellow semi-fluid GB 1727-79.
Embodiment 3
Clean taste black essence:
It is as follows that weight got by starting material:
Augeo191 74.9 kilograms,
Bright brightness B-20 toner 25 kilograms,
Flow agent BYK333 0.1 kilogram,
Amount to double centner
Preparation method:
(1) be first conventional physical mixed dissolving method, first add, then slowly add toner by clean taste solvent, high-speed stirring is complete to dissolving,
(2) then with the filter-cloth filtering of 10 μm, qualified product is namely obtained.
Detected result is as follows:
Solid content is 30% GB/T 1725-79(second method)
Outward appearance: black semi-fluid GB 1727-79.

Claims (5)

1. clean taste is easily constructed oiliness look essence, it is characterized in that, is made up of following composition and weight percent:
Clean taste solvent 65% ~ 75%,
Toner 25% ~ 35%,
Flow agent 0.01% ~ 0.1%.
2. clean taste according to claim 1 is easily constructed oiliness look essence, and it is characterized in that, described clean taste solvent is that one derives from renewable resources, has the product of low volatility, adopts the trade mark of jade of the He family Chemical Co., Ltd. to be the product of Augeo191.
3. clean taste according to claim 1 is easily constructed oiliness look essence, and it is characterized in that, described toner adopts organic toner that heavy metal content is extremely low, can adopt the Y-20 toner of river Su Minghui or R-35 toner or B-20 toner.
4. clean taste according to claim 1 is easily constructed oiliness look essence, and it is characterized in that, described flow agent adopts the flow agent containing VOC and solvent, and the trade mark of German Bi Ke company can be adopted to be the product of BYK333.
5. the clean taste of preparation according to any one of Claims 1 to 4 is easily constructed the method for oiliness look essence, it is characterized in that, comprises the steps:
(1) be first conventional physical mixed dissolving method, first add, then slowly add toner by environmentally friendly solvent, high-speed stirring is complete to dissolving,
(2) then with the filter-cloth filtering of 10 μm, qualified product is namely obtained.
Wherein, in step (1), described high speed is 1500 ~ 2000rpm,
Wherein, in step (2), described fineness is≤10 μm.
CN201310291326.XA 2013-07-12 2013-07-12 Net flavor easily constructed oily color concentrate and production method thereof Pending CN104277593A (en)