CN104149509A - Coating method taking photographic developable coatings as spraying covering jig - Google Patents

Coating method taking photographic developable coatings as spraying covering jig Download PDF

Info

Publication number
CN104149509A
CN104149509A CN201410392630.8A CN201410392630A CN104149509A CN 104149509 A CN104149509 A CN 104149509A CN 201410392630 A CN201410392630 A CN 201410392630A CN 104149509 A CN104149509 A CN 104149509A
Authority
CN
China
Prior art keywords
coating
sensitization
move back
target
film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410392630.8A
Other languages
Chinese (zh)
Other versions
CN104149509B (en
Inventor
潘奇
孙俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU AORU PLASTIC Co Ltd
Original Assignee
SUZHOU AORU PLASTIC Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU AORU PLASTIC Co Ltd filed Critical SUZHOU AORU PLASTIC Co Ltd
Priority to CN201410392630.8A priority Critical patent/CN104149509B/en
Publication of CN104149509A publication Critical patent/CN104149509A/en
Application granted granted Critical
Publication of CN104149509B publication Critical patent/CN104149509B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a coating method taking photographic developable coatings as a spraying covering jig. The photographic developable film-stripping coatings are used as the covering jig to cover the material surface, target coatings are sprayed on the whole surface, and after the film-stripping coatings are removed, a target pattern is left. The method is free from the restriction of the shape of a printing surface and the structure and position of a spraying pattern, and spraying of any pattern can be carried out on any irregular surface; after the photographic developable film-stripping coatings are covered with other coatings, the adhesive force difference exists and is utilized, and therefore synchronous removal of the photographic developable film-stripping coatings and the other coatings covering the photographic developable film-stripping coatings is achieved. The process is simple, and the economic benefits are large.

Description

A kind ofly using the coating process of sensitization development coating as spray sheltering fixture
Technical field
The invention belongs to external coating technical field, relate in particular to a kind of coating process of sensitization development coating as spray sheltering fixture of usining.
Background technology
For the application of material irregular surface (as curvature changes inner sunken face sharply, outer convex surface, compound curved surface) ad-hoc location or specific pattern, sometimes can take to block spraying or bat printing mode.What is called is blocked spraying not needing the part of coating process to cover up with tool, takes shading fixture after application away, leaves the specific pattern of ad-hoc location.So-called bat printing, develops special-purpose bat printing head, and the mode of the similar chapter of impressing prints to material surface pattern.Above-mentioned technique is subject to many condition restriction.For blocking spraying, tool corresponding to pattern be (otherwise cannot guarantee the position relationship between tool) continuously; Tool must be very good with material laminating (otherwise edge has seepage, pattern edge can be jagged), but due to the certainly existing property of product manufacturing tolerance, therefore laminating be difficult to accomplish very good; Meticulous especially pattern (as fade effect) is not developed shading fixture, thereby cannot spray.When cannot realizing, spray can consider that bat printing mode constructs hiding.For bat printing, limited by shape, special for shape, the face of undertaking the printing of that systematicness is poor, often can not develop respond well bat printing head; Can not use the occasion of pad-transfer printing ink (for example, to adhesive force require very high) this technique can not use completely.
In addition, develop special-purpose bat printing head and spray sheltering fixture, cost is often very high, is also difficult to once success, for few in batches order, all inadvisable in time and economic benefit.
Summary of the invention
The object of the embodiment of the present invention is to provide a kind of and usings sensitization development coating as the spraying method of spray sheltering fixture, is intended to solve traditional coating process and has the face shape of being undertaken the printing of, and pattern form restriction, process is complicated, cost is high, the problem of deficiency in economic performance.
The embodiment of the present invention is to realize like this, using sensitization development coating as the spraying method of spray sheltering fixture, and this processing method technological process comprises that usining sensitization can develop and can move back coating and after moving back film, leave target pattern as shading fixture, spraying, spray that target coating is carried out in whole surface;
Described using sensitization and can develop and can move back coating and refer to sensitization can be developed and can be moved back coating material surface is all covered as shading fixture, then the part that by sensitization visualization way, needs painting is installed to coating displays, expose material surface, do not need to be coated with the part install to coating and still by sensitization, can develop and can move back coating and cover;
Described application target coating is carried out in whole surface refer to application target coating is carried out in whole surface.
Described moving back leaves target pattern after film and refers to after target paint solidification, product is dropped into and moved back in film liquid, the effective ion (or molecule) that promotes to move back in film liquid in ultrasonic oscillation mode passes molecular gap in target paint film, can develop and can move back coating and react (thicker for target coating surface particularly compact or paint thickness with sensitization, move back that film liquid active ingredient still can not be through paint film surface under ultrasonic concussion, available laser or mechanical system break after osculum again row drop into move back film liquid), sensitization can be developed a little less than the adhesive force that can move back coating and material will become extremely, and target coating and material directly adhere to, it is many that adhesive force is eager to excel, with certain pressure, material surface is sprayed again, material surface is had sensitization to develop can to move back the part of coating remove in the lump together with the target coating covering on it, leave the target pattern of target location, realize the application of complex pattern on irregular curved surface.
Further, described using sensitization and can develop and can move back coating as the face shape of not undertaken the printing of in shading fixture, need the restriction of application this body structure of pattern and position, on irregular surface, can carry out the application of arbitrary graphic pattern arbitrarily, need not develop tool of a high price or bat printing head, only need to make the corresponding film and just can complete, cost is low.
Further, described carries out in sensitization, can developing and can moving back coating by the rear construction of other coating coverings in application target coating to whole surface, produce and utilize the difference of adhesive force, sensitization can be developed and can be moved back subsidiary other coating that cover top of coating and synchronously remove.
Provided by the inventionly using sensitization development coating as the coating process of spray sheltering fixture, the face shape of not undertaken the printing of, needs the restriction of application this body structure of pattern and position, can carry out the application of arbitrary graphic pattern arbitrarily on irregular surface; Need not develop tool of a high price or bat printing head, only need to make the corresponding film and just can complete, reduce cost low; Sensitization can develop can move back coating by other coating, covered after construction, produce and utilize the difference of adhesive force, realized sensitization and can develop and can move back the subsidiary synchronous removing that covers other coating on it of coating.Using sensitization development coating as the coating process of spray sheltering fixture do not need to develop special-purpose bat printing head and tool, process is simple, cost is low, economic well-being of workers and staff is large.
Accompanying drawing explanation
Fig. 1 be the embodiment of the present invention provide using the process chart of sensitization development coating as the coating process of spray sheltering fixture;
Fig. 2 be the embodiment of the present invention provide using the process chart of sensitization development coating as the embodiment 1 of the coating process of spray sheltering fixture.
The specific embodiment
In order to make object of the present invention, technical scheme and advantage clearer, below in conjunction with embodiment, the present invention is further elaborated.Should be appreciated that specific embodiment described herein, only in order to explain the present invention, is not intended to limit the present invention.
Below in conjunction with drawings and the specific embodiments, application principle of the present invention is further described.
As shown in Figure 1, using sensitization development coating as the coating process of spray sheltering fixture, and this processing method technological process comprises that usining sensitization can develop and can move back coating as shading fixture S101, whole surface is carried out application target coating S102, left target pattern S103 after moving back film;
Described using sensitization and can develop and can move back coating and refer to sensitization can be developed and can be moved back coating material surface is all covered as shading fixture S101, then the part that by sensitization visualization way, needs painting is installed to coating displays, expose material surface, do not need to be coated with the part install to coating and still by sensitization, can develop and can move back coating and cover;
Described application target coating S102 is carried out in whole surface refer to application target coating is carried out in whole surface
Described moving back leaves target pattern S103 after film and refers to after target paint solidification, product is dropped into and moved back in film liquid, the effective ion (or molecule) that promotes to move back in film liquid in ultrasonic oscillation mode passes molecular gap in target paint film, can develop and can move back coating and react (thicker for target coating surface particularly compact or paint thickness with sensitization, move back that film liquid active ingredient still can not be through paint film surface under ultrasonic concussion, available laser or mechanical system break after osculum again row drop into move back film liquid), sensitization can be developed a little less than the adhesive force that can move back coating and material will become extremely, and target coating and material directly adhere to, it is many that adhesive force is eager to excel, with certain pressure, material surface is sprayed again, material surface is had sensitization to develop can to move back the part of coating remove in the lump together with the target coating covering on it, leave the target pattern of target location, realize the application of complex pattern on irregular curved surface.
Further, described using sensitization and can develop and can move back coating as the face shape of not undertaken the printing of in shading fixture S101, need the restriction of application this body structure of pattern and position, on irregular surface, can carry out the application of arbitrary graphic pattern arbitrarily, need not develop tool of a high price or bat printing head, only need to make the corresponding film and just can complete, cost is low.
Further, move back stay after film in target pattern S103 sensitization can develop can move back coating by other coating, covered after construction, produce and utilize the difference of adhesive force, sensitization can be developed and can be moved back subsidiary other coating that cover top of coating and synchronously remove.
As shown in Figure 2, embodiment 1 realizes like this, sample adopts certain large end of brand football boot injection moulding, transparent nylon material, in inner side, (contact a side with air cushion, the middle end) and carry out pattern decorative, this decorative processing method technological process comprises the full spraying in material surface S201, irradiation ink face some time length S202, shows corresponding image S203, application nylon processing water S204, application bi-component PU coating S205, ultrasonic concussion S206, sprays surperficial S207;
Described refers to alkali solubility sensitization invisible ink and sprays material surface is complete the surperficial full spraying S201 of material, is baked to bone dry when temperature 60 C;
Described irradiation ink face some time length S202 refers to UV light source (can produce wavelength is that 365NM is to the light source of the light of 410NM) and irradiates ink face some time length by the corresponding film;
The described corresponding image S203 that shows refers to dilute sodium carbonate solution spraying ink face, shows corresponding image, do not need by follow-up paint spraying to region now by sensitization, can be developed and can move back coating and all cover;
Described application nylon is processed water S204 and is referred to the processing of carrying out application nylon processing water at all surfaces;
Described application bi-component PU coating S205 refers at all surfaces and carries out application bi-component PU coating (nylon is had to the kind compared with strong adhesive force);
Described ultrasonic concussion S206 refers to after bi-component PU paint solidification and material is put in 1% to 10% sodium hydroxide solution, carries out ultrasonic concussion and processes 1-5 minute;
Described spray surface S207 refers to and utilizes giant spray material surface, spray pressure is 1-5KG, be coated with the sensitization part that can move back coating and PU coating of can developing and be eliminated, be only coated with the part of PU coating clear and complete stayed material surface, show the pattern of requirement.
Operation principle
As shown in Figure 1, a kind of using sensitization development coating as the coating process technological process of spray sheltering fixture comprise using sensitization can develop can move back coating as shading fixture S101, expose material surface S102, whole surface carried out leaving target pattern S104 after application target coating S103, spray; Described using sensitization and can develop and can move back coating and refer to that as shading fixture S101 adopting sensitization to develop can move back coating as shading fixture, utilize sensitization to develop can to move back coating material surface is all covered; The described material surface S102 that exposes refers to that by sensitization visualization way, needs being coated with to the part that installs to coating displays, and exposes material surface, by not needing to be coated with the part that installs to coating, by sensitization, can be developed and can be moved back coating and cover; Described application target coating S103 is carried out in whole surface refer to whole surface is carried out after application target coating, wait for target coating surface drying, target coating is dropped into and moved back in film liquid, move back effective ion (or molecule) in film liquid under promoting by ultrasonic oscillation mode, through molecular gap in target paint film, can develop and can move back coating and react with sensitization, sensitization can be developed a little less than the adhesive force that can move back coating and material will become extremely, and target coating and material directly adhere to, it is many that adhesive force is eager to excel; After described spray, leaving target pattern S104 refers to and utilizes certain pressure to spray material surface, to not need part to remove, in target location, leave target pattern, for target coating surface particularly compact, move back that film liquid active ingredient still can not be through paint film surface under ultrasonic concussion, available laser or mechanical system break osculum, also can not need part to remove, in target location, leave target pattern, realize the application of complex pattern on irregular curved surface.
The foregoing is only preferred embodiment of the present invention, not in order to limit the present invention, all any modifications of doing within the spirit and principles in the present invention, be equal to and replace and improvement etc., within all should being included in protection scope of the present invention.

Claims (4)

1. using the coating process of sensitization development coating as spray sheltering fixture for one kind, it is characterized in that, should using sensitization development coating as the coating process of spray sheltering fixture, comprise that usining sensitization can develop and can move back coating and block material surface, whole surface is carried out the spraying of target coating, left target pattern after moving back film as shading fixture; Specifically comprise:
Step 1, utilize sensitization to develop can to move back coating material surface is all covered, by sensitization visualization way, needs are coated with to the part install to coating and display, expose material surface, by not needing to be coated with the part that installs to coating, by sensitization, can develop and can move back coating and cover;
Step 2, carries out the spraying of target coating to whole surface;
Step 3, after target paint solidification, product is dropped into and moved back in film liquid, move back effective ion in film liquid or molecule under promoting by ultrasonic oscillation mode, through molecular gap in target paint film, can develop and can move back coating and react with sensitization, sensitization can be developed a little less than the adhesive force that can move back coating and material will become extremely, recycling pressure sprays material surface, and the part a little less than adhesive force is removed, and in target location, leaves target pattern.
2. as claimed in claim 1ly using sensitization development coating as the coating process of spray sheltering fixture, it is characterized in that, the sensitization of usining can be developed and can be moved back coating as the shading fixture of spraying.
3. as claimed in claim 1ly using the coating process of sensitization development coating as spray sheltering fixture, it is characterized in that, described move back film sensitization can develop can move back coating by other coating, covered after construction, produce and utilize the difference of adhesive force, sensitization can be developed and can be moved back subsidiary other coating that cover top of coating and synchronously remove.
4. as claimed in claim 1ly using the coating process of sensitization development coating as spray sheltering fixture, it is characterized in that, thicker for target coating surface particularly compact or paint thickness in step 3, move back that film liquid active ingredient still can not be through paint film surface under ultrasonic concussion, by laser or mechanical system, break osculum, in order to moving back film.
CN201410392630.8A 2014-08-12 2014-08-12 Coating method taking photographic developable film-stripping coatings as spraying covering jig Active CN104149509B (en)