CN104131149A - Annealing device for stainless steel wires - Google Patents
Annealing device for stainless steel wires Download PDFInfo
- Publication number
- CN104131149A CN104131149A CN201410380364.7A CN201410380364A CN104131149A CN 104131149 A CN104131149 A CN 104131149A CN 201410380364 A CN201410380364 A CN 201410380364A CN 104131149 A CN104131149 A CN 104131149A
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- steel wire
- annealing
- metal tube
- annealing device
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to an annealing device for stainless steel wires. The annealing device disclosed by the invention comprises a heating area, a plurality of metal tubes, combustion areas and a hydrogen tank, wherein the plurality of metal tubes pass through the heating area, and are used for passing stainless steel wires; the combustion area is arranged at the outlet of each metal tube; and the hydrogen tank is connected with the combustion area of each metal tube, and used for providing hydrogen for the combustion area of each metal tube. The annealing device disclosed by the invention has the following beneficial effects that through adding the protective combustion of hydrogen, the oxidized traces of stainless steel wires subjected to annealing are eliminated, so that the surfaces of the stainless steel wires subjected to annealing are bright, a protective layer is formed on each surface, and the elongation and tensile strength of the stainless steel wires subjected to annealing are improved.
Description
Technical field
The invention belongs to metalworking technology field, be specifically related to a kind of Stainless Steel Wire annealing device.
Background technology
Stainless Steel Wire needs annealed processing.Unrelieved stress after stainless steel processing is as eliminated not in time the cracking that often causes steel.There is residualinternal stress in the process wire after drawing, must annealed technique eliminate internal stress, to play, prevents cracking, eliminates the effect of work hardening, is beneficial to continue processing.
Because the annealing process of Stainless Steel Wire can, to Stainless Steel Wire surface generation oxygenizement, although can alleviate oxidative phenomena by applying annealing liquid and epithelium liquid, can not be eliminated the evidence of oxide of the Stainless Steel Wire after annealing completely.
Summary of the invention
The problems referred to above that exist for existing Stainless Steel Wire annealing process, now provide a kind of Stainless Steel Wire annealing device that is intended to the evidence of oxide of the Stainless Steel Wire after elimination annealing.
For achieving the above object, the present invention has adopted following technical scheme:
A Stainless Steel Wire annealing device, wherein, comprising:
Heating zone;
A plurality of metal tubes, by described heating zone, with so that Stainless Steel Wire walk wherein;
Combustion zone, is arranged at each metal tube exit;
Hydrogen gas tank, connects the combustion zone of metal tube described in each, in order to the combustion zone to metal tube described in each, provides hydrogen.
Another aspect of the present invention, a plurality of described metal tubes exit is provided with wrap-up.
Another aspect of the present invention, is provided with cooling zone between a plurality of described metal tube exits and described wrap-up.
Another aspect of the present invention, is provided with annealing liquid bath between described cooling zone and described wrap-up, in order to the Stainless Steel Wire after annealing, applies annealing liquid.
Another aspect of the present invention, is provided with epithelium liquid bath between described annealing liquid bath and described wrap-up, in order to apply epithelium liquid to described Stainless Steel Wire.
Another aspect of the present invention, is provided with unwinding device in a plurality of described metal tubes ingress.
Another aspect of the present invention, is provided with pickling tub between a plurality of described metal tube ingress and described unwinding device, in order to treat the Stainless Steel Wire of annealing, carries out pickling.
Another aspect of the present invention, is provided with preheating zone between a plurality of described metal tube ingress and described pickling tub, in order to treat the Stainless Steel Wire of annealing, carries out preheating.
The present invention has obtained following beneficial effect: the evidence of oxide of having eliminated the Stainless Steel Wire after annealing by increasing the protectiveness burning of hydrogen; Stainless Steel Wire surface-brightening after making to anneal; and form protective layer, and improve unit elongation and the tensile strength of the Stainless Steel Wire after annealing.
Accompanying drawing explanation
Fig. 1 is the structural representation of a kind of Stainless Steel Wire annealing device of the present invention.
Embodiment
Below in conjunction with the drawings and specific embodiments, the invention will be further described, but not as limiting to the invention.
As shown in Figure 1, the invention provides a kind of Stainless Steel Wire annealing device, wherein, comprising:
Heating zone 1, in order to operation that Stainless Steel Wire is annealed, heating zone can obtain heat by electrically heated, can fire-proof and thermal-insulation structure be set in heating zone around simultaneously, guarantees personal security;
A plurality of metal tubes 2, by heating zone, with so that Stainless Steel Wire walk wherein, by a plurality of metal tubes are set, can be simultaneously to the operation of annealing of many Stainless Steel Wires, thereby improved the working efficiency of Stainless Steel Wire annealing device;
Combustion zone 21, is arranged at the exit of each metal tube 2, in order to the Stainless Steel Wire in each metal tube 2, implements protectiveness burning;
Hydrogen gas tank 3; the combustion zone 21 that connects each metal tube 2; in order to the combustion zone 21 to each metal tube 2, provide hydrogen; usining hydrogen can be at Stainless Steel Wire surface formation protective membrane as the gas of protectiveness burning; make the Stainless Steel Wire surface-brightening after annealing, and improve unit elongation and the tensile strength of the Stainless Steel Wire after annealing.
In a kind of embodiment of the present invention, the exit of a plurality of metal tubes 2 can arrange wrap-up 4, in order to the Stainless Steel Wire to after annealing, carries out rolling.
In a kind of embodiment of the present invention, between the exit of a plurality of metal tubes 2 and wrap-up 4, cooling zone 5 can be set.Cooling zone 5 is carried out cooling in order to the Stainless Steel Wire to after annealing.
In a kind of embodiment of the present invention, between cooling zone 5 and wrap-up 4, be provided with annealing liquid bath 6, in order to the Stainless Steel Wire after annealing, apply annealing liquid.
In a kind of embodiment of the present invention, between annealing liquid bath 6 and wrap-up 5, be provided with epithelium liquid bath 7, in order to apply epithelium liquid to Stainless Steel Wire.
In a kind of embodiment of the present invention, in the ingress of a plurality of metal tubes 2, be provided with unwinding device 8.Unwinding device 8 is in order to unreel the Stainless Steel Wire after wire drawing, is that Stainless Steel Wire enters the annealing device operation of annealing.
In a kind of embodiment of the present invention, between the ingress of a plurality of metal tubes 2 and unwinding device 8, be provided with pickling tub 9, in order to treat the Stainless Steel Wire of annealing, carry out pickling.
In a kind of embodiment of the present invention, between the ingress of a plurality of metal tubes 2 and pickling tub 9, be provided with preheating zone 10, in order to treat the Stainless Steel Wire of annealing, carry out preheating.
The foregoing is only preferred embodiment of the present invention; not thereby limit embodiments of the present invention and protection domain; to those skilled in the art; should recognize that being equal to that all utilizations specification sheets of the present invention and diagramatic content done replace and the resulting scheme of apparent variation, all should be included in protection scope of the present invention.
Claims (8)
1. a Stainless Steel Wire annealing device, is characterized in that, comprising:
Heating zone;
A plurality of metal tubes, by described heating zone, with so that Stainless Steel Wire walk wherein;
Combustion zone, is arranged at each metal tube exit;
Hydrogen gas tank, connects the combustion zone of metal tube described in each, in order to the combustion zone to metal tube described in each, provides hydrogen.
2. Stainless Steel Wire annealing device as claimed in claim 1, is characterized in that, a plurality of described metal tubes exit is provided with wrap-up.
3. Stainless Steel Wire annealing device as claimed in claim 2, is characterized in that, between a plurality of described metal tube exits and described wrap-up, is provided with cooling zone.
4. Stainless Steel Wire annealing device as claimed in claim 3, is characterized in that, between described cooling zone and described wrap-up, is provided with annealing liquid bath, in order to the Stainless Steel Wire after annealing, applies annealing liquid.
5. Stainless Steel Wire annealing device as claimed in claim 4, is characterized in that, between described annealing liquid bath and described wrap-up, is provided with epithelium liquid bath, in order to apply epithelium liquid to described Stainless Steel Wire.
6. Stainless Steel Wire annealing device as claimed in claim 1, is characterized in that, a plurality of described metal tubes ingress is provided with unwinding device.
7. Stainless Steel Wire annealing device as claimed in claim 6, is characterized in that, between a plurality of described metal tube ingress and described unwinding device, is provided with pickling tub, in order to treat the Stainless Steel Wire of annealing, carries out pickling.
8. Stainless Steel Wire annealing device as claimed in claim 7, is characterized in that, between a plurality of described metal tube ingress and described pickling tub, is provided with preheating zone, in order to treat the Stainless Steel Wire of annealing, carries out preheating.