CN104084144A - 一种壳聚糖参与煤渣改性的加强型氨吸附剂 - Google Patents
一种壳聚糖参与煤渣改性的加强型氨吸附剂 Download PDFInfo
- Publication number
- CN104084144A CN104084144A CN201410358638.2A CN201410358638A CN104084144A CN 104084144 A CN104084144 A CN 104084144A CN 201410358638 A CN201410358638 A CN 201410358638A CN 104084144 A CN104084144 A CN 104084144A
- Authority
- CN
- China
- Prior art keywords
- ammonia adsorbent
- cinder
- chitosan
- reinforced
- modification
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明的目的是提供一种壳聚糖参与煤渣改性的加强型氨吸附剂,为实现上述目的,本发明采用的技术方案如下:将燃煤炉渣粉碎,取一定量炉渣粉,用水冲洗数次,去除可溶性杂质,在104℃下干燥4h,然后将固体物质和壳聚糖按照一定的比例混合均匀,加入一定量的1-5mol/L的氢氧化钠溶液,振荡一定时间后用水冲洗至中性,在104℃条件下干燥1-4h后,即为该加强型氨吸附剂。
Description
技术领域
本发明涉及氨吸附领域,具体涉及一种壳聚糖参与煤渣改性的加强型氨吸附剂。
背景技术
氨,无机化合物,常温下为气体,无色有刺激性恶臭的气体,易溶于水,氨溶于水时,氨分子跟水分子通过氢键结合成一水合氨,一水合氨能小部分电离成氨离子和氢氧根离子,故氨水显弱碱性,能灼伤皮肤、眼睛、呼吸器官的粘膜,人吸入过多,能引起肺肿胀,以致死亡。
由于城市污水及工业废水的大量产生,以及尾气排放,造成环境越来越恶化。情况的日益严重,致使治理工作势在必行。
吸附法是处理废水和废气中有害和难降解污染物的一种重要的物化方法, 活性炭是最常用的吸附材料, 但由于原料缺乏、成本较高、再生困难等原因使其应用受到限制。以工业和农业废弃物为原料, 制备和开发廉价、高效吸附材料取代活性炭是吸附材料研究的重要方向。
发明内容
本发明的目的是提供一种壳聚糖参与煤渣改性的加强型氨吸附剂,以克服现有技术存在的原料缺乏,成本高的缺点。为实现上述目的,本发明采用的技术方案如下:
将燃煤炉渣粉碎,取一定量炉渣粉,用水冲洗数次,去除可溶性杂质,在104℃下干燥4h,然后将固体物质和壳聚糖按照一定的比例混合均匀,加入一定量的1-5mol/L的氢氧化钠溶液,振荡一定时间后用水冲洗至中性,在104℃条件下干燥1-4h后,即为该加强型氨吸附剂。
在本发明具有以下显著特点:
(1) 发明所述加强型氨吸附剂,原料来源广泛,价格低廉;
(2) 发明所述加强型氨吸附剂制备方法简单,吸附率高;
(3) 发明所述加强型氨吸附剂性能稳定,寿命长,可以长期保存使用。
具体实施方式:
实施例1:
将燃煤炉渣粉碎,称取100 g 粉煤灰,用水冲洗数次,去除可溶性杂质,在104℃下干燥4h,然后将固体物质和壳聚糖按照质量比4:1混合均匀,加入300ml浓度为1mol/L的氢氧化钠溶液,振荡1h后用水冲洗至中性,在104℃条件下干燥1h后,即为该加强型氨吸附剂。
实施例2:
将燃煤炉渣粉碎,称取100 g 粉煤灰,用水冲洗数次,去除可溶性杂质,在104℃下干燥4h,然后将固体物质和壳聚糖按照质量比3:1混合均匀,加入300ml浓度为2mol/L的氢氧化钠溶液,振荡2h后用水冲洗至中性,在104℃条件下干燥1h后,即为该加强型氨吸附剂。
实施例3:
将燃煤炉渣粉碎,称取100 g 粉煤灰,用水冲洗数次,去除可溶性杂质,在104℃下干燥4h,然后将固体物质和壳聚糖按照质量比2:1混合均匀,加入300ml浓度为5mol/L的氢氧化钠溶液,振荡3h后用水冲洗至中性,在104℃条件下干燥1h后,即为该加强型氨吸附剂。
Claims (1)
1.本发明公开了一种壳聚糖参与煤渣改性的加强型氨吸附剂,为实现上述目的,本发明采用的技术方案如下:
将燃煤炉渣粉碎,取一定量炉渣粉,用水冲洗数次,去除可溶性杂质,在104℃下干燥4h,然后将固体物质和壳聚糖按照一定的比例混合均匀,加入一定量的1-5mol/L的氢氧化钠溶液,振荡一定时间后用水冲洗至中性,在104℃条件下干燥1-4h后,即为该加强型氨吸附剂。