Summary of the invention
A kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface that the object of the invention is to overcome the deficiency of above-mentioned prior art and provide.
The present invention solves the technical scheme that prior art problem adopts: a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface, and it comprises the following steps:
S1, plastic shell surface pretreatment;
Vacuum plating or spraying are carried out in plastic shell surface, so that plastic shell surface presents bright gloss;
S2, plastic shell surface preparation;
In the surface of plastic shell, choose and need the bright face of processing position, and install a suitable fixture, do not need the bright face of processing position so that block, and then, the bright face position of needs processing is corroded or etching or cure process;
S3, the processing of spraying paint;
To the processing of spraying paint of the position after excessive erosion or etching or cure process, so that it forms needed cloudy surface;
S4, clamper for disassembling;
After above-mentioned formed cloudy surface curing molding, clamper for disassembling, the bright mist consubstantiality processing in surface of plastic shell is disposed.
Below above technical scheme is further elaborated:
Preferably, step S2 comprises the following steps:
S21, prefabricated one with the suitable fixture of plastic shell, and to make the position that this fixture contacts with plastic shell be flexible glue material;
S22, by prefabricated grip device on plastic shell, so that block the bright face position that does not need processing;
S23, surface to plastic shell, need the bright face position of processing to corrode or etching or cure process;
S24, the position after excessive erosion or etching or cure process and described fixture are cleaned, in order to the follow-up processing of spraying paint.
Preferably, step S3 sprays paint in processing, and the material that sprays paint used is any one in UV paint, PU paint, additive color UV paint, UV finish paint.
Preferably, after step S4, also comprise:
After the dismounting of S5, fixture, clean to dismantled fixture and through bright, the plastic shell of cloudy surface processing.
The invention has the beneficial effects as follows:
One, a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface provided by the present invention, make also can realize on the surface of plastic shell the effect of bright mist consubstantiality, they can be according to user's needs, at the plastic shell jet surface that need to be processed into cloudy surface photo-curing paint or baking of varnish etc. variable concentrations or different classes of, make the different parts of plastic shell present as required different colors and different glossiness, meet popular demand.
Two, the present invention, by realize bright mist consubstantiality effect on plastic shell surface, realizes bright mist consubstantiality effect with respect to traditional surface at metal shell, because of the superiority of material, also makes production cost of the present invention lower.
Three, a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface provided by the present invention, especially can be applicable to being applied to the processing of the side surface of plastic cellphone shell center being carried out to bright and cloudy surface, and machining accuracy is high, glossiness is good, and in the specific implementation, processing technology is simple, swift and convenient to operate, can adapt to production demand, enhance productivity, in the speed production cycle, improve greatly production capacity, therefore, very welcome of meeting of the present invention, can effectively be popularized.
Four, the present invention is only not limited to the processing processing of the surface of plastic cellphone shell center being carried out to bright and cloudy surface, it also can carry out to the surface of mobile phone battery cover, Mobile phone decoration, panel computer shell, camera case etc. the processing processing of bright and cloudy surface, it is every plastic cement material housing, the present invention is all applicable, thereby, the present invention is applied widely, and the present invention must have good market popularization value.
Detailed description of the invention
Describe technical scheme of the present invention in detail below with reference to drawings and the specific embodiments, so as clearer, understand invention essence of the present invention intuitively.
Fig. 1 is the flow chart of steps that the present invention realizes the Treatment technique for processing of the bright mist consubstantiality in plastic shell surface; Fig. 2 is the flow chart of step S2 in Fig. 1;
Shown in Fig. 1 and Fig. 2, a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface provided by the present invention is mainly the processing of the surface of plastic shell being carried out to bright and cloudy surface, makes its different parts present the gloss of different colours or different brightness;
Specifically, a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface provided by the present invention, it comprises the following steps:
S1, plastic shell surface pretreatment;
Vacuum plating or spraying are carried out in plastic shell surface, so that plastic shell surface presents bright gloss;
S2, plastic shell surface preparation;
In the surface of plastic shell, choose and need the bright face of processing position, and install a suitable fixture, do not need the bright face of processing position so that block, and then, the bright face position of needs processing is corroded or etching or cure process, in this step, corrode or the object of etching or cure process is for strengthening in subsequent technique, the adhesive force of the material that sprays paint.
S3, the processing of spraying paint;
To the processing of spraying paint of the position after excessive erosion or etching or cure process, so that it forms needed cloudy surface;
S4, clamper for disassembling;
After above-mentioned formed cloudy surface curing molding, clamper for disassembling, the bright mist consubstantiality processing in surface of plastic shell is disposed.
It should be noted that, above-mentioned steps S2 comprises the following steps:
S21, prefabricated one with the suitable fixture of plastic shell, and to make the position that this fixture contacts with plastic shell be flexible glue material;
It is emphasized that, in process because of pre-treatment, plastic shell surface is processed and is presented bright gloss by plating or spraying coating process, so, adaptive fixture in step S21, position that it contacts with plastic shell surface adopts flexible glue material, and flexible glue has certain flexibility, its object be in case bright gloss position because contacting by scratch or weighing wounded.
S22, by prefabricated grip device on plastic shell, so that block the bright face position that does not need processing;
S23, surface to plastic shell, need the bright face position of processing to corrode or etching or cure process;
S24, the position after excessive erosion or etching or cure process and described fixture are cleaned, in order to the follow-up processing of spraying paint.
And step S3 sprays paint in processing, the material that sprays paint used is any one in UV paint, PU paint, additive color UV paint, UV finish paint, and certainly, it also can be other photo-curing paint or baking of varnish etc., at this, does not do one by one and illustrates.
Further, after step S4, also comprise:
After the dismounting of S5, fixture, clean to dismantled fixture and through bright, the plastic shell of cloudy surface processing.
So, through after step S5 clean, on the one hand, described fixture is reusable, on the other hand, can pack through bright, the plastic shell of cloudy surface processing, uses as finished product.
By this, a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface provided by the present invention, make also can realize on the surface of plastic shell the effect of bright mist consubstantiality, they can be according to user's needs, at the plastic shell jet surface that need to be processed into cloudy surface photo-curing paint, baking of varnish etc. variable concentrations or different classes of, make the different parts of plastic shell present different colors or different glossiness, meet popular demand.
Meanwhile, the present invention is by realizing bright mist consubstantiality effect on plastic shell surface, realize bright mist consubstantiality effect with respect to traditional surface at metal shell, because of the superiority of material, also make production cost of the present invention lower, and the present invention especially can be applicable to being applied to the processing of the side surface of plastic cellphone casing being carried out to bright and cloudy surface, below will elaborate with embodiment mono-.
Embodiment mono-
The present embodiment provides a kind of surface to plastic cellphone shell center to carry out the processing processing of bright and cloudy surface;
Contrast Fig. 1 and Fig. 2, and with reference to shown in Fig. 3, Fig. 4 and Fig. 5; The middle part of Fig. 3 is the vertical structure generalized section of a mobile phone shell center 10, and both sides are to be fixed with suitable fixture 20, and the scheme of the present embodiment is to carry out cloudy surface processing in the surperficial middle part of mobile phone shell center 10.
The present embodiment in the specific implementation, first, carries out pre-treatment to the surface of mobile phone shell center 10, vacuum plating or spraying is carried out in the surface of mobile phone shell center 10, so that the surface of mobile phone shell center 10 presents bright gloss;
And then, prefabricated one with the suitable fixture 20 of mobile phone shell center 10, and the position that this fixture 20 is contacted with mobile phone shell center 10 is flexible glue 201 materials;
Then, prefabricated fixture 20 is installed on mobile phone shell center 10, so that block mobile phone shell center 10 dual-sides along the bright face position that does not need processing;
Again, to the surface of mobile phone shell center 10, need the bright face position of the centre of processing to corrode or etching or cure process;
Finally, the position after excessive erosion or etching or cure process and described fixture 20 are cleaned, in order to the processing of spraying paint of next technique.
Be that next processing technology is to the processing of spraying paint of the position after excessive erosion or etching or cure process, so that it forms needed cloudy surface 102;
Meanwhile, after above-mentioned formed cloudy surface 102 curing moldings, clamper for disassembling 20, the bright mist consubstantiality processing in surface of mobile phone shell center 10 is disposed, and after fixture 20 dismountings, clean to dismantled fixture 20 and through the mobile phone shell center 10 that bright 101, cloudy surface 102 process, on the one hand, the described fixture 20 after cleaning is reusable, on the other hand, bright 101 of process after clean, the mobile phone shell center 10 that cloudy surface 102 is processed can be packed, and use as finished product.
Through evidence, when a kind of Treatment technique for processing of realizing the bright mist consubstantiality in plastic shell surface provided by the present invention, when the side surface of plastic cellphone shell center 10 is carried out to the processing of bright 101 and cloudy surface 102, machining accuracy is high, glossiness is good, and in the specific implementation, processing technology is simple, swift and convenient to operate, make to adapt to production demand, enhance productivity, the speed production cycle, improve greatly production capacity, therefore, very welcome of meeting of the present invention, can effectively be popularized.
And the present invention is only not limited to the processing processing of the surface of plastic cellphone shell center 10 being carried out to bright 101 and cloudy surface 102, it also can carry out to the surface of mobile phone battery cover, Mobile phone decoration, panel computer shell, camera case etc. the processing processing of bright and cloudy surface, it is every plastic cement material housing, the present invention is all applicable, thereby, the present invention is applied widely, and the present invention must have good market popularization value.
The foregoing is only the preferred embodiments of the present invention; not thereby limit scope of patent protection of the present invention; every equivalent structure or conversion of equivalent flow process that utilizes description of the present invention and accompanying drawing content to do; or be directly or indirectly used in other relevant technical fields, be all in like manner included in scope of patent protection of the present invention.