CN103963957B - 一种玻璃低温防雾方法 - Google Patents
一种玻璃低温防雾方法 Download PDFInfo
- Publication number
- CN103963957B CN103963957B CN201410165935.5A CN201410165935A CN103963957B CN 103963957 B CN103963957 B CN 103963957B CN 201410165935 A CN201410165935 A CN 201410165935A CN 103963957 B CN103963957 B CN 103963957B
- Authority
- CN
- China
- Prior art keywords
- glass plate
- double
- antifogging glass
- sided tape
- broadside
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明是一种玻璃板低温防雾方法,该方法的步骤是:加工防雾玻璃板;粘贴双面胶条;粘接防雾玻璃板;涂抹玻璃板胶。本方法是通过在普通玻璃板上粘接防雾玻璃板,利用双面胶的厚度和玻璃板胶的密封粘接作用在普通玻璃板和防雾玻璃板之间形成了一个封闭的空气腔,使外界的低温不易传递到防雾玻璃板的内表面,从而保持了防雾玻璃板的表面温度,进而防止了雾气的产生。该方法加工的装置提高了玻璃板与外界的隔温能力,使内表面的玻璃板不受外界低温的影响,提高了内表面玻璃板的温度,从而减少了内表面雾气的产生。
Description
技术领域
本发明是一种玻璃低温防雾方法,用于玻璃板低温下内部防雾。
背景技术
飞机飞行过程中在高空会遇到外界温度低于0℃的情况,这时由于在内部的玻璃板上会凝集水珠,形成雾气,影响了驾驶员的视线。
发明内容
本发明下是针对上述情况而设计提供了一种玻璃低温防雾方法,其目的是在低温环境下防止玻璃板产生雾气。
本发明的技术解决方案是:
该种玻璃板低温防雾方法的步骤是:
第一步、加工防雾玻璃板
防雾玻璃板(2)的厚度m=2mm~4mm,防雾玻璃板(2)的长度L1等于被防雾玻璃板(1)的长度,防雾玻璃板(2)的宽度L2等于被防雾玻璃板(1)的宽度;
第二步、粘贴双面胶条
双面胶条由两个长边双面胶条(3)和两个宽边双面胶条(4)组成,长边双面胶条(3)和宽边双面胶条(4)的宽度b=10mm~20mm,长边双面胶条(3)和宽边双面胶条(4)的厚度t=20mm~30mm;
先将两个长边双面胶(3)粘接到被防雾玻璃板(1)的长边上,长边双面胶(3)的外边缘和被防雾玻璃板(1)的长边边缘的距离a=10mm~20mm,长边双面胶(3)的两端与被防雾玻璃板(1)的宽边边缘之间留出的距离为a+b,然后将两个宽边双面胶(4)粘接到防雾玻璃板(1)的宽边上,宽边双面胶条(4)的外边缘和被防雾玻璃板(1)的宽边边缘的距离也是a,宽边双面胶条(4)的两端与被防雾玻璃板(1)的长边边缘之间留出的距离也是a,所述长边双面胶条(3)的长度L3=L1-2a-2b,宽边双面胶条(4)的长度L4=L2-2a;
第三步、粘接防雾玻璃板
将防雾玻璃板(2)的长边与被防雾玻璃板(1)的长边对齐,将防雾玻璃板(2)的宽边与被防雾玻璃板(1)的宽边对齐,然后将防雾玻璃板(2)粘接在长边双面胶条(3)和宽边双面胶条(4)上;
第四步、涂抹玻璃胶
在防雾玻璃板(2)、被防雾玻璃板(1)的侧面和与两者侧面平齐的长边双面胶(3)和宽边双面胶(4)的侧面涂抹酸性玻璃胶,玻璃胶胶接后自然干燥24小时以上,使防雾玻璃板(2)、被防雾玻璃板(1)之间形成的空腔与外界空气保持隔绝。
本发明的有益效果是在普通玻璃板和防雾玻璃板之间形成了一个封闭的空气腔,使外界的低温不易传递到防雾玻璃板的内表面,从而保持了防雾玻璃板的表面温度,进而防止了雾气的产生。
附图说明
图1是本发明技术方案的结构示意图
图2是本发明技术方案中铺贴长边双面胶(3)和宽边双面胶(4)的示意图
具体实施方式
下面结构实施例对本发明技术方案做进一步详细说明
参见图1、2所示,该种玻璃板低温防雾方法的步骤是:
第一步、加工防雾玻璃板
防雾玻璃板2的厚度m=2mm~4mm,防雾玻璃板2的长度L1等于被防雾玻璃板1的长度,防雾玻璃板2的宽度L2等于被防雾玻璃板1的宽度;
第二步、粘贴双面胶条
双面胶条由两个长边双面胶条3和两个宽边双面胶条4组成,长边双面胶条3和宽边双面胶条4的宽度b=10mm~20mm,长边双面胶条3和宽边双面胶条4的厚度t=20mm~30mm;
先将两个长边双面胶3粘接到被防雾玻璃板1的长边上,长边双面胶3的外边缘和被防雾玻璃板1的长边边缘的距离a=10mm~20mm,长边双面胶3的两端与被防雾玻璃板1的宽边边缘之间留出的距离为a+b,然后将两个宽边双面胶4粘接到防雾玻璃板1的宽边上,宽边双面胶条4的外边缘和被防雾玻璃板1的宽边边缘的距离也是a,宽边双面胶条4的两端与被防雾玻璃板1的长边边缘之间留出的距离也是a,所述长边双面胶条3的长度L3=L1-2a-2b,宽边双面胶条4的长度L4=L2-2a;
第三步、粘接防雾玻璃板
将防雾玻璃板2的长边与被防雾玻璃板1的长边对齐,将防雾玻璃板2的宽边与被防雾玻璃板1的宽边对齐,然后将防雾玻璃板2粘接在长边双面胶条3和宽边双面胶条4上;
第四步、涂抹玻璃胶
在防雾玻璃板2、被防雾玻璃板1的侧面和与两者侧面平齐的长边双面胶3和宽边双面胶4的侧面涂抹酸性玻璃胶,玻璃胶胶接后自然干燥24小时以上,使防雾玻璃板2、被防雾玻璃板1之间形成的空腔与外界空气保持隔绝。
本发明是通过在普通玻璃板上粘接防雾玻璃板,利用双面胶的厚度和玻璃板胶的密封粘接作用在普通玻璃板和防雾玻璃板之间形成了一个封闭的空气腔,使外界的低温不易传递到防雾玻璃板的内表面,从而保持了防雾玻璃板的表面温度,进而防止了雾气的产生。
Claims (1)
1.一种玻璃板低温防雾方法,其特征在于:该方法的步骤是:
第一步、加工防雾玻璃板
防雾玻璃板(2)的厚度m=2mm~4mm,防雾玻璃板(2)的长度L1等于被防雾玻璃板(1)的长度,防雾玻璃板(2)的宽度L2等于被防雾玻璃板(1)的宽度;
第二步、粘贴双面胶条
双面胶条由两个长边双面胶条(3)和两个宽边双面胶条(4)组成,长边双面胶条(3)和宽边双面胶条(4)的宽度b=10mm~20mm,长边双面胶条(3)和宽边双面胶条(4)的厚度t=20mm~30mm;
先将两个长边双面胶条(3)粘接到被防雾玻璃板(1)的长边上,长边双面胶条(3)的外边缘和被防雾玻璃板(1)的长边边缘的距离a=10mm~20mm,长边双面胶条(3)的两端与被防雾玻璃板(1)的宽边边缘之间留出的距离为a+b,然后将两个宽边双面胶条(4)粘接到防雾玻璃板(1)的宽边上,宽边双面胶条(4)的外边缘和被防雾玻璃板(1)的宽边边缘的距离也是a,宽边双面胶条(4)的两端与被防雾玻璃板(1)的长边边缘之间留出的距离也是a,所述长边双面胶条(3)的长度L3=L1-2a-2b,宽边双面胶条(4)的长度L4=L2-2a;
第三步、粘接防雾玻璃板
将防雾玻璃板(2)的长边与被防雾玻璃板(1)的长边对齐,将防雾玻璃板(2)的宽边与被防雾玻璃板(1)的宽边对齐,然后将防雾玻璃板(2)粘接在长边双面胶条(3)和宽边双面胶条(4)上;
第四步、涂抹玻璃胶
在防雾玻璃板(2)、被防雾玻璃板(1)的侧面和与两者侧面平齐的长边双面胶条(3)和宽边双面胶条(4)的侧面涂抹酸性玻璃胶,玻璃胶胶接后自然干燥24小时以上,使防雾玻璃板(2)、被防雾玻璃板(1)之间形成的空腔与外界空气保持隔绝。