CN103601861A - 一种低硬度橡胶垫圈 - Google Patents
一种低硬度橡胶垫圈 Download PDFInfo
- Publication number
- CN103601861A CN103601861A CN201310515327.8A CN201310515327A CN103601861A CN 103601861 A CN103601861 A CN 103601861A CN 201310515327 A CN201310515327 A CN 201310515327A CN 103601861 A CN103601861 A CN 103601861A
- Authority
- CN
- China
- Prior art keywords
- parts
- low
- fluorubber
- hardness
- magnesium oxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种低硬度橡胶垫圈,包括下列组分,氟橡胶125份,丙烯腈14份,氧化镁2份,氧化锌2份,纳米碳酸钙2份,硬脂酸2份,甲苯二异氰酯7份,氧化镁18份,氢氧化钙4份,氟蜡1份,炭黑6份,氯化石蜡17份,聚丙烯23份,十二烷基苯8份。在保持较好物理机械性的同时,可得到低硬度氟橡胶。采用本发明所述的配方可大大节约企业的生产资源,降低企业的生产成本,具有良好的加工流动性,可以方便对其进行加工,制成各种氟橡胶制品,如骨架油封、垫片、膜片、胶管和O形圈等;该氟橡胶制品具有优异的耐化学性能,且低温柔韧性也较好。
Description
技术领域
本发明涉及一种化工产品,尤其是一种低硬度橡胶垫圈。
背景技术
氟橡胶应用最广泛的是汽车领域,在汽车零部件上,可作为发动机燃料软管、加油软管、燃料泵、空调装置O形圈,及喷射装置,动力活塞、气门杆、曲轴、空调压缩机的密封材料,氟橡胶骨架油封应用已经渗透到各个领域,使用条件也是千变万化,需要在恶劣环境下仍具有高稳定性和长寿命。例如一些活性介质等极端环境下,氟橡胶要求足具有苛刻的化学稳定性。因此氟橡胶的应用配方也一直在拓宽。现如今,氟橡胶已经是工业产业中不可缺少的材料之一,随着科学技术的发展,生产生活中所探索接触领域的不断拓展,其应用范围会越来越广泛。
发明内容
本发明要解决的技术问题是提供一种高强度铸件修复胶粘剂。
为解决上述技术问题,本发明的低硬度橡胶垫圈,包括下列组分,氟橡胶125份,丙烯腈14份,氧化镁2份,氧化锌2份,纳米碳酸钙2份,硬脂酸2份,甲苯二异氰酯7份,氧化镁18份,氢氧化钙4份,氟蜡1份,炭黑6份,氯化石蜡17份,聚丙烯23份,十二烷基苯8份。
所述橡胶垫圈还包括过氧化二异丙苯5份。
所述橡胶垫圈还包括硅氧烷2份。
本发明的有益效果为:在保持较好物理机械性的同时,可得到低硬度氟橡胶。采用本发明所述的配方可大大节约企业的生产资源,降低企业的生产成本,具有良好的加工流动性,可以方便对其进行加工,制成各种氟橡胶制品,如骨架油封、垫片、膜片、胶管和O 形圈等;该氟橡胶制品具有优异的耐化学性能,且低温柔韧性也较好。
具体实施方式
实施例1
本发明的低硬度橡胶垫圈,包括下列组分,氟橡胶125份,丙烯腈14份,氧化镁2份,氧化锌2份,纳米碳酸钙2份,硬脂酸2份,甲苯二异氰酯7份,氧化镁18份,氢氧化钙4份,氟蜡1份,炭黑6份,氯化石蜡17份,聚丙烯23份,十二烷基苯8份。所述橡胶垫圈还包括过氧化二异丙苯5份。
实施例2
本发明的低硬度橡胶垫圈,包括下列组分,氟橡胶125份,丙烯腈14份,氧化镁2份,氧化锌2份,纳米碳酸钙2份,硬脂酸2份,甲苯二异氰酯7份,氧化镁18份,氢氧化钙4份,氟蜡1份,炭黑6份,氯化石蜡17份,聚丙烯23份,十二烷基苯8份。所述橡胶垫圈还包括过氧化二异丙苯5份。所述橡胶垫圈还包括硅氧烷2份。
实施例3
本发明的低硬度橡胶垫圈,包括下列组分,氟橡胶125份,丙烯腈14份,氧化镁2份,氧化锌2份,纳米碳酸钙2份,硬脂酸2份,甲苯二异氰酯7份,氧化镁18份,氢氧化钙4份,氟蜡1份,炭黑6份,氯化石蜡17份,聚丙烯23份,十二烷基苯8份。
以上所述,仅是对本发明的较佳实施例而已,并非对本发明做其他形式的限制,任何熟悉本专业的技术人员可能利用上述揭示的技术内容加以变更或改型为同等变化的等效实施例。凡是未脱离本发明方案内容,依据本发明的技术实质对以上实施例所做的任何简单修改、等同变化与改型,均落在本发明的保护范围内。
Claims (3)
1.一种低硬度橡胶垫圈,其特征在于:包括下列组分,氟橡胶125份,丙烯腈14份,氧化镁2份,氧化锌2份,纳米碳酸钙2份,硬脂酸2份,甲苯二异氰酯7份,氧化镁18份,氢氧化钙4份,氟蜡1份,炭黑6份,氯化石蜡17份,聚丙烯23份,十二烷基苯8份。
2.按照权利要求1所述的低硬度橡胶垫圈,其特征在于:所述橡胶垫圈还包括过氧化二异丙苯5份。
3.按照权利要求2所述的低硬度橡胶垫圈,其特征在于:所述橡胶垫圈还包括硅氧烷2份。