CN103512935A - 一种测试涂层电化学性能的电解池 - Google Patents

一种测试涂层电化学性能的电解池 Download PDF

Info

Publication number
CN103512935A
CN103512935A CN201210205553.1A CN201210205553A CN103512935A CN 103512935 A CN103512935 A CN 103512935A CN 201210205553 A CN201210205553 A CN 201210205553A CN 103512935 A CN103512935 A CN 103512935A
Authority
CN
China
Prior art keywords
electrode
cover plate
base
electrolytic cell
auxiliary electrode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201210205553.1A
Other languages
English (en)
Other versions
CN103512935B (zh
Inventor
徐承明
王永明
张宇
肖宇
陈义庆
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Angang Steel Co Ltd
Original Assignee
Angang Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Angang Steel Co Ltd filed Critical Angang Steel Co Ltd
Priority to CN201210205553.1A priority Critical patent/CN103512935B/zh
Publication of CN103512935A publication Critical patent/CN103512935A/zh
Application granted granted Critical
Publication of CN103512935B publication Critical patent/CN103512935B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供一种测试涂层电化学性能的电解池,它是由盖板、底座、一端带螺纹的圆筒、工作电极套件和辅助电极组成,盖板中央开有一个大圆孔,并在大圆孔两边开有两个小圆孔,大圆孔内径开有螺纹与工作电极套件的螺纹相配合,两个小圆孔分别安装辅助电极导电极棒和参比电极棒,辅助电极安装在底座的内部中央的圆形槽内。本发明的优点及效果在于,结构简单,组装方便,只需更换工作电极即可进行一组新的电化学测试,不仅可以测试普通的平板试样,还可以检测表面形态相对复杂的不同尺寸的试样;另外本发明主体部件全部采用绝缘塑料制成,有效避免腐蚀的发生,并提高装置的使用寿命。

Description

一种测试涂层电化学性能的电解池
技术领域
本发明涉及电化学分析测试用的配套设备,尤其涉及一种涂层电化学测试用的电解池。
背景技术
金属板材或金属表面涂层的电化学腐蚀测试实验通常都使用电解池。现有的电化学测试用电解池一般都是由工作电极、辅助电极、参比电极、盐桥和电解液容器等几个主要部件组成的,而在结构上根据测试样品的形状和大小的不同又可分为平板式电解池、多孔烧瓶(腐蚀)电解池和泰特式电解池等类型。例如:美国Princeton Appied Research公司生产的电解池有Flat Cell Kit Model K0235、Corrosion Cell Kit Model K0047及Tait Cell Kit Model K0307等。
常用的金属表面涂层电化学检测电解池主要有平板式和泰特式两种电解池,这两种电解池在测试实验中,作为工作电极的涂层试样放在底部硬板与套筒的下管口之间或直接固定在底板中心部位开设的小圆孔上,这种电解池的缺点是不容易组装,每次实验更换不同试样时,都需要将整个装置拆开,组装不方便,而且更换时间较长;此外,工作电极的窗口较小,并且是固定不可变更的,而在实际测试工作中,除了要测试正常涂层的腐蚀性能等失效状态外,有时还要测试涂层板在成型后失效模式,例如:冲压变形或弯折变形,要求对表面形貌比较复杂的连续涂层试验样板进行综合评测,现有的电解池的工作电极由于尺寸单一、固定,需要不断变换测试的部位,才能适应这种测试需要,而且测试试验也不能准确反映整个试样膜层的耐腐蚀性能。
发明内容
本发明的目的是提供一种测试涂层电化学性能的电解池,该电解池能够测试表面形状相对复杂的涂层试样,并且组装十分方便。
本发明的特点在于它是由盖板、底座、一端带螺纹的圆筒、工作电极套件和辅助电极组成,圆筒与底座通过螺纹配合,盖板盖在圆筒上,盖板中央开有一个大圆孔,在大圆孔两边分别开有两个小圆孔,大圆孔内径有螺纹与工作电极套件的螺纹相配合,两个小圆孔分别安装辅助电极导电极棒和参比电极棒,辅助电极安装在底座的内部中央的圆形槽内。
本发明的具体结构有,工作电极套件是由导电极棒、电极座、样板压盖、密封垫圈组成。电极座上的螺纹与盖板中央的大圆孔的内螺纹相配合,电极棒安装在电极座中心孔中,样板压盖通过螺纹与电极座下端连接,并与密封垫圈配合,使样板的非测试部位密封、绝缘,根据测试样板面积的不同,工作电极可制作成由大到小的一系列尺寸,即电极座与盖板连接部位配合的尺寸不变,通过改变样板压盖与电极座的配合尺寸实现工作电极尺寸的改变。
本发明的具体结构还有,底座的内口开有螺纹与圆筒带螺纹端相配合,为了保证密封防止电解液渗漏,底座与圆筒连接部位添加适当密封材料或垫圈,在底座的内部中央开有的圆形槽,槽内放置辅助电极,槽的旁边开有用于固定电极导电极棒的的立孔和侧孔,侧孔上部装有固定螺钉、内部装有导电连接片用以连接辅助电极与电极导电极棒。
本发明的优点及效果在于,结构简单,组装方便,只需更换工作电极即可进行一组新的电化学测试,不仅可以测试普通的平板试样,还可以检测表面形态相对复杂的不同尺寸的试样;另外本发明主体部件全部采用绝缘塑料制成,有效避免腐蚀的发生,并提高装置的使用寿命。
附图说明
附图是本发明的装配示意图。
具体实施方式
下面结合附图对本发明的具体实施例做详细说明。
如图所示,本发明是由盖板7、底座10、一端带螺纹的圆筒8、工作电极套件和辅助电极9组成,圆筒8与底座10通过螺纹配合,盖板7盖在圆筒上,盖板中央开有一个大圆孔,并在大圆孔两边开有两个小圆孔,大圆孔内径开有螺纹与工作电极套件的螺纹相配合,两个小圆孔分别安装辅助电极导电极棒1和参比电极棒6,辅助电极9安装在底座10的内部中央的圆形槽内;
工作电极套件是由电极座2、导电极棒3、样板压盖5和密封垫圈13组成,样板压盖5与电极座2通过螺纹连接并与密封垫圈13配合使测试样板4的非测试部位密封、绝缘,根据测试样板面积的不同,通过改变样板压盖5与电极座2的配合尺寸实现工作电极尺寸的改变,即可将工作电极的样板压盖5与电极座2的配合螺纹直径分别制作成大、中、小三个尺寸,例如:50mm、30mm和15mm。
底座10的圆形槽旁边侧孔12的上部装有固定螺钉15,通过侧孔内的连接片13连接和固定辅助电极9与电极导电极棒1,底座10内径开有螺纹与圆筒8有螺纹的一端相配合;
试验时,根据测试样板4的大小将样板放入适当的工作电极套件内,将密封垫圈17放入压盖5内,旋紧备用;将辅助电极9放入底座10的圆形槽内,并将辅助电极导电极棒1插入底座的立孔14和侧孔12中,通过连接片13用螺钉15将辅助电极导电极棒1和辅助电极9连接、固定;将圆筒8有螺纹一端与底座10的配合螺纹旋转拧紧,为了保证密封可在连接部位加入密封材料或垫圈11;将参比电极6固定在盖板7上的小圆孔内,将工作电极套件的底座2与盖板7的大圆孔螺纹连接并通过旋转调节高度,使参比电极6上的盐桥16与测试样板4保持合适的距离(3mm~5mm),组装完后备用;向圆筒内倒入电解液,将组装好的盖板安放到圆筒上并调成水平,组装完毕后将各电极连接到测试设备的电路中即可进行电化学检测。

Claims (3)

1.一种测试涂层电化学性能的电解池,其特征在于它是由盖板、底座、一端带螺纹的圆筒、工作电极套件和辅助电极组成,圆筒与底座通过螺纹配合,盖板盖在圆筒上,盖板中央开有一个大圆孔,并在大圆孔两边开有两个小圆孔,大圆孔内径开有螺纹与工作电极套件的螺纹相配合,两个小圆孔分别安装辅助电极导电极棒和参比电极棒,辅助电极安装在底座的内部中央的圆形槽内。
2.根据权利要求1所述的一种测试涂层电化学性能的电解池,其特征在于,所述的工作电极套件是由导电极棒、电极座、样板压盖、密封垫圈组成,电极座上的螺纹与盖板中央的大圆孔内螺纹相配合,电极棒安装在电极座中心孔中,样板压盖通过螺纹与电极座下端连接,并与密封垫圈配合。
3.根据权利要求1所述的一种测试涂层电化学性能的电解池,其特征在于,所述底座内部中央圆形槽的旁边开有用于固定电极导电极棒的的立孔和侧孔,侧孔上部装有固定螺钉、内部装有导电连接片,固定螺钉及导电连接片连接辅助电极与电极导电极棒。
CN201210205553.1A 2012-06-20 2012-06-20 一种测试涂层电化学性能的电解池 Active CN103512935B (zh)