CN103506074A - 一种消除有害物质的过渡金属改性活性炭及其制备方法 - Google Patents

一种消除有害物质的过渡金属改性活性炭及其制备方法 Download PDF

Info

Publication number
CN103506074A
CN103506074A CN201310387304.3A CN201310387304A CN103506074A CN 103506074 A CN103506074 A CN 103506074A CN 201310387304 A CN201310387304 A CN 201310387304A CN 103506074 A CN103506074 A CN 103506074A
Authority
CN
China
Prior art keywords
active carbon
water
parts
transition metal
clay
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310387304.3A
Other languages
English (en)
Inventor
陈登宇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bengbu Phoenix International Co Ltd
Original Assignee
Bengbu Phoenix International Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bengbu Phoenix International Co Ltd filed Critical Bengbu Phoenix International Co Ltd
Priority to CN201310387304.3A priority Critical patent/CN103506074A/zh
Publication of CN103506074A publication Critical patent/CN103506074A/zh
Pending legal-status Critical Current

Abstract

一种消除有害物质的过渡金属改性活性炭,由下列重量份的原料制成:活性炭100-120、硝酸铜3-4、硫酸亚铁铵12-13、粘土30-34、稻壳12-14、改性凹凸棒土8-10、水适量。本发明使用了硝酸铜、硫酸亚铁铵对活性炭进行改性,能催化氧化消除有害物质,而且效果持续时间长;还加入了粘土、稻壳,经煅烧形成了与活性炭不同的空隙,与活性炭配合使用,能容纳不同大小污染物;而且粘土和稻壳的成本低;适合室内空气、水净化,效果好,持续时间长。

Description

一种消除有害物质的过渡金属改性活性炭及其制备方法
技术领域
本发明涉及一种非金属矿的改性方法,尤其涉及一种消除有害物质的过渡金属改性活性炭及其制备方法。
背景技术
随着科技的发展,现代化工业的逐步建设,各种化学品被开发利用,给人们生活带来了便利,同时由于化学品产生了对环境和人体有害的物质,也成了人们不得不面对的问题。
目前空气中的污染物主要是工业燃料燃烧产生的气体、汽车尾气、生产中产生的有毒有害气体。水污染主要是工业生产排放的污水里含有大量有毒物质,还有人们生活中的污水产生很多有害物质。人们生活中也有很多时候需要脱除毒素,比如空调过滤网上有很多细菌、毒素,新装修的间有甲醛等有害物质,都需要脱除毒素。目前都脱除毒素经常用到吸附剂,主要有硅胶、活性氧化铝、活性炭、分子筛等,另外还有针对某种组分选择性吸附而研制的吸附材料。但是这些吸附剂大多吸附能力有限,需要针对不同的要求研究不同的吸附剂,发挥最好的作用。同时,寻找新的原料,以增强吸附效果,节约成本。
发明内容
本发明的目的在于提供一种消除有害物质的过渡金属改性活性炭及其制备方法。
本发明的技术方案如下:
一种消除有害物质的过渡金属改性活性炭,其特征在于由下列重量份的原料制成:活性炭100-120、硝酸铜3-4、硫酸亚铁铵12-13、粘土30-34、稻壳12-14、改性凹凸棒土8-10、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、碳酸钠3-4、氧化铝3-4、氧化镁3-4、硫酸钛14-18、白砂糖3-4、木质素磺酸钠2-3、玉石粉12-14、钼酸铵2-3、氧化铬3-4、吗啉1-2、水适量;将凹凸棒土、白砂糖、木质素磺酸钠、碳酸钠混合,加入适量水,练成泥状,送入煅烧炉中,在930-950℃下煅烧3-4小时,取出,与其它剩余成分一并加入适量水中,研磨,得到200-300目浆料,喷雾干燥,即得。
所述消除有害物质的过渡金属改性活性炭的制备方法,其特征在于包括以下步骤:将稻壳粉碎,与粘土混合,加水练成泥状,送入600-670℃煅烧炉中,煅烧1-2小时,取出粉碎,与硫酸亚铁铵、硝酸铜、活性炭一起加入适量水,加热至75-85℃,调研磨液PH值为4-5,研磨得到200-300目浆料,喷雾干燥,与改性凹凸棒土混合,送入热处理炉中在340-360℃下处理2-3小时,取出冷却即得。
分发明的有益效果
本发明使用了硝酸铜、硫酸亚铁铵对活性炭进行改性,能催化氧化消除有害物质,而且效果持续时间长;还加入了粘土、稻壳,经煅烧形成了与活性炭不同的空隙,与活性炭配合使用,能容纳不同大小污染物;而且粘土和稻壳的成本低;适合室内空气、水净化,效果好,持续时间长。
具体实施方式
一种消除有害物质的过渡金属改性活性炭,由下列重量份(公斤)的原料制成:活性炭110、硝酸铜3、硫酸亚铁铵12、粘土33、稻壳13、改性凹凸棒土9、水适量;
所述改性凹凸棒土由以下重量份(公斤)的原料制成:凹凸棒土110、碳酸钠3、氧化铝3、氧化镁4、硫酸钛16、白砂糖4、木质素磺酸钠3、玉石粉13、钼酸铵2、氧化铬4、吗啉2、水适量;将凹凸棒土、白砂糖、木质素磺酸钠、碳酸钠混合,加入适量水,练成泥状,送入煅烧炉中,在940℃下煅烧3小时,取出,与其它剩余成分一并加入适量水中,研磨,得到200目浆料,喷雾干燥,即得。
所述消除有害物质的过渡金属改性活性炭的制备方法,包括以下步骤:将稻壳粉碎,与粘土混合,加水练成泥状,送入640℃煅烧炉中,煅烧1小时,取出粉碎,与硫酸亚铁铵、硝酸铜、活性炭一起加入适量水,加热至80℃,调研磨液PH值为4,研磨得到200目浆料,喷雾干燥,与改性凹凸棒土混合,送入热处理炉中在350℃下处理2小时,取出冷却即得。
经测定,其碘值1544mg/g,亚甲基蓝吸附值26.7mL/0.1g。

Claims (2)

1.一种消除有害物质的过渡金属改性活性炭,其特征在于由下列重量份的原料制成:活性炭100-120、硝酸铜3-4、硫酸亚铁铵12-13、粘土30-34、稻壳12-14、改性凹凸棒土8-10、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、碳酸钠3-4、氧化铝3-4、氧化镁3-4、硫酸钛14-18、白砂糖3-4、木质素磺酸钠2-3、玉石粉12-14、钼酸铵2-3、氧化铬3-4、吗啉1-2、水适量;将凹凸棒土、白砂糖、木质素磺酸钠、碳酸钠混合,加入适量水,练成泥状,送入煅烧炉中,在930-950℃下煅烧3-4小时,取出,与其它剩余成分一并加入适量水中,研磨,得到200-300目浆料,喷雾干燥,即得。
2.根据权利要求1所述消除有害物质的过渡金属改性活性炭的制备方法,其特征在于包括以下步骤:将稻壳粉碎,与粘土混合,加水练成泥状,送入600-670℃煅烧炉中,煅烧1-2小时,取出粉碎,与硫酸亚铁铵、硝酸铜、活性炭一起加入适量水,加热至75-85℃,调研磨液PH值为4-5,研磨得到200-300目浆料,喷雾干燥,与改性凹凸棒土混合,送入热处理炉中在340-360℃下处理2-3小时,取出冷却即得。
CN201310387304.3A 2013-08-30 2013-08-30 一种消除有害物质的过渡金属改性活性炭及其制备方法 Pending CN103506074A (zh)