CN103495381A CN201310387335.9A CN201310387335A CN103495381A CN 103495381 A CN103495381 A CN 103495381A CN 201310387335 A CN201310387335 A CN 201310387335A CN 103495381 A CN103495381 A CN 103495381A
Authority
CN
China
Prior art keywords
activated carbon
hour
attapulgite
modified
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310387335.9A
Other languages
English (en)
Inventor
陈登宇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bengbu Phoenix International Co Ltd
Original Assignee
Bengbu Phoenix International Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bengbu Phoenix International Co Ltd filed Critical Bengbu Phoenix International Co Ltd
Priority to CN201310387335.9A priority Critical patent/CN103495381A/zh
Publication of CN103495381A publication Critical patent/CN103495381A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Solid-Sorbent Or Filter-Aiding Compositions (AREA)

Abstract

一种改性活性炭基汽油脱硫剂,由下列重量份的原料制成:活性炭100-120、重质碳酸钙12-14、硫酸铈1.4-2.8、氯化铁5-6、改性凹凸棒土8-10、水适量。本发明使用了硫酸铈、氯化铁等氧化剂与重质碳酸钙结合使用,能有效脱除汽油中的噻吩及其衍生物,本发明原料易得,工艺简单,成本低,适合工业化生产,无有害物质生成,具有良好的应用前景。

Description

一种改性活性炭基汽油脱硫剂及其制备方法
技术领域
本发明涉及一种非金属矿的改性方法,尤其涉及一种改性活性炭基汽油脱硫剂及其制备方法。
背景技术
随着科技的发展,现代化工业的逐步建设,各种化学品被开发利用,给人们生活带来了便利,同时由于化学品产生了对环境和人体有害的物质,也成了人们不得不面对的问题。
目前空气中的污染物主要是工业燃料燃烧产生的气体、汽车尾气、生产中产生的有毒有害气体。水污染主要是工业生产排放的污水里含有大量有毒物质,还有人们生活中的污水产生很多有害物质。人们生活中也有很多时候需要脱除毒素,比如空调过滤网上有很多细菌、毒素,新装修的间有甲醛等有害物质,都需要脱除毒素。目前都脱除毒素经常用到吸附剂,主要有硅胶、活性氧化铝、活性炭、分子筛等,另外还有针对某种组分选择性吸附而研制的吸附材料。但是这些吸附剂大多吸附能力有限,需要针对不同的要求研究不同的吸附剂,发挥最好的作用。同时,寻找新的原料,以增强吸附效果,节约成本。
发明内容
本发明的目的在于提供一种改性活性炭基汽油脱硫剂及其制备方法。
本发明的技术方案如下:
一种改性活性炭基汽油脱硫剂,其特征在于由下列重量份的原料制成:活性炭100-120、重质碳酸钙12-14、硫酸铈1.4-2.8、氯化铁5-6、改性凹凸棒土8-10、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、碳酸钠3-4、铝矾土5-6、硼化钒1-2、玉石粉3-4、硫酸亚铁1-2、硫酸钛14-18、活性炭12-14、麦饭石2-3、氧化镧1-2、氧化铬3-4、吗啉1-2、水适量;将凹凸棒土、铝矾土、玉石粉、活性炭送入煅烧炉中,在850-870℃下煅烧4-5小时,取出,再放入适量水中研磨,调节研磨液PH值为4-5,研磨1-2小时,得到100-150目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200-300目浆料,喷雾干燥,即得。
所述改性活性炭基汽油脱硫剂的制备方法,其特征在于包括以下步骤:将重质碳酸钙送入煅烧炉中在900-950℃下煅烧3-4小时,取出与硫酸铈、氯化铁混合,加入适量水,加热至80-90℃,调节研磨液PH值为4-5,研磨得200-300目浆料,再加入活性炭、改性凹凸棒土一并研磨2-3小时,调节研磨液PH值为中性,喷雾干燥后,送入300-340℃热处理炉中处理2-3小时,即得。
分发明的有益效果
本发明使用了硫酸铈、氯化铁等氧化剂与重质碳酸钙结合使用,能有效脱除汽油中的噻吩及其衍生物,本发明原料易得,工艺简单,成本低,适合工业化生产,无有害物质生成,具有良好的应用前景。
具体实施方式
一种改性活性炭基汽油脱硫剂,由下列重量份(公斤)的原料制成:活性炭110、重质碳酸钙13、硫酸铈2、氯化铁5、改性凹凸棒土9、水适量;
所述改性凹凸棒土由以下重量份(公斤)的原料制成:凹凸棒土110、碳酸钠3、铝矾土5、硼化钒1、玉石粉3、硫酸亚铁1、硫酸钛15、活性炭13、麦饭石2、氧化镧1、氧化铬3、吗啉1、水适量;将凹凸棒土、铝矾土、玉石粉、活性炭送入煅烧炉中,在860℃下煅烧4小时,取出,再放入适量水中研磨,调节研磨液PH值为4,研磨1小时,得到100目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200目浆料,喷雾干燥,即得。
所述改性活性炭基汽油脱硫剂的制备方法,包括以下步骤:将重质碳酸钙送入煅烧炉中在920℃下煅烧3小时,取出与硫酸铈、氯化铁混合,加入适量水,加热至85℃,调节研磨液PH值为4,研磨得200目浆料,再加入活性炭、改性凹凸棒土一并研磨2小时,调节研磨液PH值为中性,喷雾干燥后,送入320℃热处理炉中处理2.5小时,即得。
经测定,其碘值1538mg/g,亚甲基蓝吸附值26.5mL/0.1g。

Claims (2)

1.一种改性活性炭基汽油脱硫剂,其特征在于由下列重量份的原料制成:活性炭100-120、重质碳酸钙12-14、硫酸铈1.4-2.8、氯化铁5-6、改性凹凸棒土8-10、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、碳酸钠3-4、铝矾土5-6、硼化钒1-2、玉石粉3-4、硫酸亚铁1-2、硫酸钛14-18、活性炭12-14、麦饭石2-3、氧化镧1-2、氧化铬3-4、吗啉1-2、水适量;将凹凸棒土、铝矾土、玉石粉、活性炭送入煅烧炉中,在850-870℃下煅烧4-5小时,取出,再放入适量水中研磨,调节研磨液PH值为4-5,研磨1-2小时,得到100-150目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200-300目浆料,喷雾干燥,即得。
2.根据权利要求1所述改性活性炭基汽油脱硫剂的制备方法,其特征在于包括以下步骤:将重质碳酸钙送入煅烧炉中在900-950℃下煅烧3-4小时,取出与硫酸铈、氯化铁混合,加入适量水,加热至80-90℃,调节研磨液PH值为4-5,研磨得200-300目浆料,再加入活性炭、改性凹凸棒土一并研磨2-3小时,调节研磨液PH值为中性,喷雾干燥后,送入300-340℃热处理炉中处理2-3小时,即得。
CN201310387335.9A 2013-08-30 2013-08-30 一种改性活性炭基汽油脱硫剂及其制备方法 Pending CN103495381A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310387335.9A CN103495381A (zh) 2013-08-30 2013-08-30 一种改性活性炭基汽油脱硫剂及其制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310387335.9A CN103495381A (zh) 2013-08-30 2013-08-30 一种改性活性炭基汽油脱硫剂及其制备方法

Publications (1)

Publication Number Publication Date
CN103495381A true CN103495381A (zh) 2014-01-08

Family

ID=49860693

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310387335.9A Pending CN103495381A (zh) 2013-08-30 2013-08-30 一种改性活性炭基汽油脱硫剂及其制备方法

Country Status (1)

Country Link
CN (1) CN103495381A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108212093A (zh) * 2018-03-28 2018-06-29 山东佳星环保科技有限公司 一种基于石墨烯的脱硫吸附剂
CN110152602A (zh) * 2018-04-12 2019-08-23 济南开发区星火科学技术研究院 一种用于汽油的脱硫吸附剂

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2008093606A (ja) * 2006-10-13 2008-04-24 Kurita Water Ind Ltd 水中の溶存酸素除去方法及び装置並びに水中の溶存酸素除去触媒
CN101234341A (zh) * 2008-02-28 2008-08-06 上海交通大学 用于水处理的功能性聚合物-活性炭复合材料的制备方法

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2008093606A (ja) * 2006-10-13 2008-04-24 Kurita Water Ind Ltd 水中の溶存酸素除去方法及び装置並びに水中の溶存酸素除去触媒
CN101234341A (zh) * 2008-02-28 2008-08-06 上海交通大学 用于水处理的功能性聚合物-活性炭复合材料的制备方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108212093A (zh) * 2018-03-28 2018-06-29 山东佳星环保科技有限公司 一种基于石墨烯的脱硫吸附剂
CN110152602A (zh) * 2018-04-12 2019-08-23 济南开发区星火科学技术研究院 一种用于汽油的脱硫吸附剂

Similar Documents

Publication Publication Date Title
CN103495389B (zh) 一种改性秸秆活性炭水处理剂及其制备方法
CN103495385A (zh) 一种处理染料废水改性活性炭及其制备方法
CN103506086A (zh) 一种偶联改性活性炭吸附脱硫剂及其制备方法
CN103495390A (zh) 一种氧化锆改性活性炭去磷酸盐吸附剂及其制备方法
CN103506090A (zh) 一种改性活性炭水处理吸附剂及其制备方法
CN103495386A (zh) 一种低浓度有机废气的改性活性炭吸附剂及其制备方法
CN103495433A (zh) 一种改性活性炭催化剂及其制备方法
CN103495384A (zh) 一种改性活性炭空气净化吸附剂及其制备方法
CN103495394A (zh) 一种脱除有机污染物改性活性炭及其制备方法
CN103566903B (zh) 一种凹凸棒石粘土改性活性炭及其制备方法
CN103691394A (zh) 一种碱性改性活性炭脱硫剂及其制备方法
CN103521176A (zh) 一种改性活性炭硫化氢吸附剂及其制备方法
CN103495406A (zh) 一种白云石改性活性炭脱硫剂及其制备方法
CN103521178A (zh) 一种处理含酚废水的竹质改性活性炭吸附剂及其制备方法
CN103495392A (zh) 一种柠檬酸改性活性炭材料及其制备方法
CN103495380A (zh) 一种改性活性炭空气吸附剂及其制备方法
CN103551109A (zh) 一种板栗壳活性炭及其制备方法
CN103521195A (zh) 一种羟基氧化铁改性活性炭脱硫剂及其制备方法
CN103521194A (zh) 一种表面聚合物改性木炭吸附剂及其制备方法
CN103495407A (zh) 一种竹质改性活性炭脱硫吸附剂及其制备方法
CN103521184A (zh) 一种谷物壳改性活性炭吸附剂及其制备方法
CN103495404A (zh) 一种铜银改性活性炭吸附剂及其制备方法
CN103495393A (zh) 一种富氧改性木炭吸附脱硫剂及其制备方法
CN103752278A (zh) 一种去除汞的改性活性炭及其制备方法
CN103495382A (zh) 一种改性麦麸活性炭及其制备方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C53 Correction of patent of invention or patent application
CB02 Change of applicant information

Address after: 233000 Mount Huangshan Road, Bengbu high tech Zone, Anhui, No. 8028

Applicant after: ANHUI PHOENIX FILTER CO., LTD.

Address before: 233000 Mount Huangshan Road, Bengbu high tech Zone, Anhui, No. 8028

Applicant before: Bengbu Fenghuang Filters Co., Ltd.

COR Change of bibliographic data

Free format text: CORRECT: APPLICANT; FROM: BENGBU FENGHUANG FILTERS CO., LTD. TO: ANHUI PHOENIX INTERNATIONAL CO., LTD.

RJ01 Rejection of invention patent application after publication

Application publication date: 20140108

RJ01 Rejection of invention patent application after publication