CN103450591A - Anti-static rubber belt for escalator and preparation method thereof - Google Patents

Anti-static rubber belt for escalator and preparation method thereof Download PDF

Info

Publication number
CN103450591A
CN103450591A CN201310369553XA CN201310369553A CN103450591A CN 103450591 A CN103450591 A CN 103450591A CN 201310369553X A CN201310369553X A CN 201310369553XA CN 201310369553 A CN201310369553 A CN 201310369553A CN 103450591 A CN103450591 A CN 103450591A
Authority
CN
China
Prior art keywords
parts
escalator
rubber belt
preparation
silicon carbide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201310369553XA
Other languages
Chinese (zh)
Inventor
平利中
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wujiang Junda Elevator Parts Co Ltd
Original Assignee
Wujiang Junda Elevator Parts Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wujiang Junda Elevator Parts Co Ltd filed Critical Wujiang Junda Elevator Parts Co Ltd
Priority to CN201310369553XA priority Critical patent/CN103450591A/en
Publication of CN103450591A publication Critical patent/CN103450591A/en
Withdrawn legal-status Critical Current

Abstract

The invention discloses an anti-static rubber belt for an escalator and a preparation method thereof. The anti-static rubber belt comprises the following materials in parts by weight: 20-40 parts of polyvinyl chloride, 20-30 parts of acrylic resin, 10-20 parts of benzene ketone peroxide, 10-15 parts of chlorosulfonated styrene, 20-30 parts of stearic acid, 10-20 parts of silicon carbide and 5-10 parts of brenstone. The preparation method comprises the following steps: melting the polyvinyl chloride and the acrylic resin at 130-140 DEG C; adding the benzene ketone peroxide, the chlorosulfonated styrene, the stearic acid, the silicon carbide and the brenstone to mill for 20-30 minutes at 90-120 DEG C. The surface resistivity of the anti-static rubber belt achieves 109 omega.m; the anti-static rubber belt has good antistatic properties, and good tensile property, and is suitable for being used as the rubber belt for the escalator; the breaking stress is about 178-182 N; the tensile strength is 8.8-9.3 kpa.

Description

Be used for antistatic rubber belt of escalator and preparation method thereof
Technical field
The present invention relates to the escalator field, relate in particular to antistatic rubber belt for escalator and preparation method thereof.
Background technology
Escalator is common in the ground such as megastore, relatively general lifting elevator, and it is slow that speed is wanted, and the both sides of escalator are provided with belt, drive the operation of elevator.General escalator belt is that rubber is made, and people, when taking advantage of escalator, usually use the belt on side, during as astasia, but produces static with the people sometimes on balata belt, and human body is worked the mischief.
Summary of the invention
For the deficiencies in the prior art, the invention provides a kind of belt of the antistatic rubber for escalator and preparation method thereof, there is the function of the generation of static electricity of preventing, the protection HUMAN HEALTH.
For the antistatic rubber belt of escalator, comprise the raw material of following weight part meter: polyvinyl chloride 20-40 part, acrylic resin 20-30 part, benzoyl peroxide ketone 10-20 part, chlorosulphonation vinylbenzene 10-15 part, stearic acid 20-30 part, silicon carbide 10-20 part, sulphur 5-10 part.
The preparation method who is used for the antistatic rubber belt of escalator, comprise the following steps: polyvinyl chloride and acrylic resin are 130-140 ℃ of melting, add benzoyl peroxide ketone, chlorosulphonation vinylbenzene, stearic acid, silicon carbide, sulphur, at 90-120 ℃ of refining glue 20-30min.
Surface resistivity of the present invention reaches 10 9Ω m, have good antistatic performance, and rupture stress is in the 178-182N left and right, and tensile strength, at 8.8-9.3kpa, has good tensile property, is suitable as the balata belt of escalator.
Embodiment
Below by specific embodiment, the present invention is further described in detail.
Embodiment 1
For the antistatic rubber belt of escalator, comprise the raw material of following weight part meter: 20 parts of polyvinyl chloride, 20 parts of acrylic resins, 10 parts of benzoyl peroxide ketones, 10 parts of chlorosulphonation vinylbenzene, 20 parts of stearic acid, 10 parts, silicon carbide, 5 parts, sulphur.
Its preparation method comprises the following steps: polyvinyl chloride and acrylic resin, 130 ℃ of meltings, add benzoyl peroxide ketone, chlorosulphonation vinylbenzene, stearic acid, silicon carbide, sulphur, at 90 ℃ of refining glue 20min.
Embodiment 2
For the antistatic rubber belt of escalator, comprise the raw material of following weight part meter: 40 parts of polyvinyl chloride, 30 parts of acrylic resins, 20 parts of benzoyl peroxide ketones, 15 parts of chlorosulphonation vinylbenzene, 30 parts of stearic acid, 20 parts, silicon carbide, 10 parts, sulphur.
Its preparation method comprises the following steps: polyvinyl chloride and acrylic resin, 140 ℃ of meltings, add benzoyl peroxide ketone, chlorosulphonation vinylbenzene, stearic acid, silicon carbide, sulphur, at 120 ℃ of refining glue 30min.
Embodiment 3
For the antistatic rubber belt of escalator, comprise the raw material of following weight part meter: 30 parts of polyvinyl chloride, 25 parts of acrylic resins, 15 parts of benzoyl peroxide ketones, 13 parts of chlorosulphonation vinylbenzene, 25 parts of stearic acid, 15 parts, silicon carbide, 8 parts, sulphur.
Its preparation method comprises the following steps: polyvinyl chloride and acrylic resin, 135 ℃ of meltings, add benzoyl peroxide ketone, chlorosulphonation vinylbenzene, stearic acid, silicon carbide, sulphur, at 110 ℃ of refining glue 25min.
The belt of embodiment 1-3 is carried out to performance test, and result is as follows:
? Embodiment 1 Embodiment 2 Embodiment 3
Surface resistivity Ω m 10 9 10 9 10 9
Rupture stress N 180 178 182
Tensile strength kpa 8.8 9 9.3
Surface resistivity of the present invention reaches 10 9Ω m, illustrate that antistatic rubber belt of the present invention has good antistatic performance, rupture stress is in the 178-182N left and right, and tensile strength is at 8.8-9.3kpa, illustrate that antistatic rubber belt of the present invention has good tensile property, is suitable as the balata belt of escalator.
In addition, the invention is not restricted to above-mentioned embodiment, as long as within not exceeding scope of the present invention, can take variety of way to implement the present invention.

Claims (2)

1. for the antistatic rubber belt of escalator, it is characterized in that comprising the raw material of following weight part meter: polyvinyl chloride 20-40 part, acrylic resin 20-30 part, benzoyl peroxide ketone 10-20 part, chlorosulphonation vinylbenzene 10-15 part, stearic acid 20-30 part, silicon carbide 10-20 part, sulphur 5-10 part.
2. the preparation method based on the belt of the antistatic rubber for escalator claimed in claim 1, it is characterized in that comprising the following steps: polyvinyl chloride and acrylic resin are 130-140 ℃ of melting, add benzoyl peroxide ketone, chlorosulphonation vinylbenzene, stearic acid, silicon carbide, sulphur, at 90-120 ℃ of refining glue 20-30min.
CN201310369553XA 2013-08-22 2013-08-22 Anti-static rubber belt for escalator and preparation method thereof Withdrawn CN103450591A (en)