CN103408810A - 一种液压缸用密封垫及其制备方法 - Google Patents

一种液压缸用密封垫及其制备方法 Download PDF

Info

Publication number
CN103408810A
CN103408810A CN2013102733360A CN201310273336A CN103408810A CN 103408810 A CN103408810 A CN 103408810A CN 2013102733360 A CN2013102733360 A CN 2013102733360A CN 201310273336 A CN201310273336 A CN 201310273336A CN 103408810 A CN103408810 A CN 103408810A
Authority
CN
China
Prior art keywords
add
rubber
wollastonite
preparation
under
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102733360A
Other languages
English (en)
Inventor
张开会
陶庭鸿
张火生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUHU YINHONG HYDRAULIC COMPONENTS CO Ltd
Original Assignee
WUHU YINHONG HYDRAULIC COMPONENTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUHU YINHONG HYDRAULIC COMPONENTS CO Ltd filed Critical WUHU YINHONG HYDRAULIC COMPONENTS CO Ltd
Priority to CN2013102733360A priority Critical patent/CN103408810A/zh
Publication of CN103408810A publication Critical patent/CN103408810A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种液压缸用密封垫及其制备方法,其由丁腈橡胶、氯醇橡胶、POM、聚异丁烯、2,4-二氯过氧化苯甲酰、2.2'-二硫化二苯骈噻、癸二酸二辛酯、甲基丙烯酸正丁酯、微晶石蜡、改性硅灰石、纳米海泡石、硫酸钙晶须等原料制成。本发明在丁腈橡胶、氯醇橡胶共混的基础上,又加入了POM、聚异丁烯,可以改善橡胶的耐油、耐温、耐磨性以及抗压强度等性能,还添加了改性的硅灰石粉,可以明显改善硅灰石在橡胶中的分散性,提高密封材料的机械强度、耐油性、耐磨性以及耐高温性等性能。

Description

一种液压缸用密封垫及其制备方法
技术领域
本发明涉及一种密封垫及其制备方法,具体涉及一种液压缸用密封垫及其制备方法。 
背景技术
密封垫是液压缸的一个重要组成部分,用来防止工作介质的泄露及外界灰尘和异物的侵入。密封垫的综合性能,是衡量液压系统好坏的重要指标。然而现有的密封垫密封性能不理想、耐磨性较差、强度低、耐老化差、耐油性差等缺陷,已远不能满足现实要求,容易造成膨胀、老化龟裂、漏油等现象,从而导致液压装置无法正常工作,因此急需开发一种高性能密封垫。 
发明内容
本发明的目的在于针对现有技术的不足,提供一种高强度、耐油性好、耐磨性好、低压缩永久变形的液压缸用密封垫及其制备方法,以满足液压缸的工作需求。 
本发明采用的技术方案如下: 
一种液压缸用密封垫,由以下重量份的原料制成:丁腈橡胶(CR322) 60-70、氯醇橡胶(H45)15-25、POM 10-15、聚异丁烯 8-12、2,4-二氯过氧化苯甲酰 2-3、2.2'-二硫化二苯骈噻1-2、癸二酸二辛酯3-5、甲基丙烯酸正丁酯4-6、微晶石蜡 5-8、改性硅灰石 10-15、纳米海泡石5-10、硫酸钙晶须4-8、氧化锌2-3、氧化镁1-2、炭黑N339 10-15、二甲基二巯基乙酸异辛酯锡1-2、二硫化四甲基秋兰姆2-3、防老剂OD 1-2、防老剂NBC 2-3、抗氧剂1010 1-2、抗氧剂168 1-2。 
所述的改性硅灰石制备方法如下: 
a.取干燥后的硅灰石粉碎至15μm以下,投入分散釜中,加入硅灰石量2-4倍的去离子水,搅拌下再加入2-3%的聚丙烯酸钠、1-2%的磷酸三钙、2-3%的椰油酸单乙醇酰胺、1-2%的稻壳灰、3-4%的有机膨润土,2000-3000rpm高速分散20-30min,经砂磨机研磨成浆料,待用; 
b.取相当于硅灰石量20-30%的纳米硅溶胶加入搅拌机内,搅拌下加入0.5-1%的四异丙基二(二辛基亚磷酸酰氧基)钛酸酯、3-4%的纳米碳、1-2%的纳米氮化铝、 2-3%的氧化镨和1-2%的月桂醇硫酸钠,50-60℃搅拌分散30-40min,冷却后待用;
c.将上述预处理后的硅溶胶与步骤(a)制得的浆料混合均匀,加入5-8%的苯丙乳液、1-2%的丙二醇苯醚和2-3%的十二碳醇酯,搅拌30-50min,过滤,烘干,粉碎研细,过200-300目筛即可。
一种液压缸用密封垫的制备方法,包括以下步骤:取POM、聚异丁烯、纳米海泡石、氧化镁在混炼机中于40-50℃下混炼4-8min,排料,放置24-36h后按比例与丁腈橡胶、氯醇橡胶、改性硅灰石 、硫酸钙晶须、微晶石蜡加入混炼机中,在50-60℃下混炼5-10min;将混炼好的胶料加入开炼机中,再加入其余原料在85-95℃下炼胶3-6min,薄通5-8次后下片;将胶片用平板硫化机在15-20MPa压力下压制成型,然后进行两次硫化处理,第一次硫化的硫化温度控制在175-185℃,硫化时间为4-7min,第二次硫化在烘箱中进行,硫化温度为200-220℃,硫化时间为2-4h,修边、检验、包装,即得成品。 
本发明的有益效果: 
本发明在丁腈橡胶、氯醇橡胶共混的基础上,又加入了POM、聚异丁烯,可以改善橡胶的耐油、耐温、耐磨性以及抗压强度等性能,还添加了改性的硅灰石粉,可以明显改善硅灰石在橡胶中的分散性,提高密封材料的机械强度、耐油性、耐磨性以及耐高温性等性能。本发明生产出来的密封垫综合性能优异,密封效果好,高耐油,化学稳定性好,抗腐蚀性好,在酸,碱,油等介质中能长期工作,不易膨胀、龟裂;还具有良好的压缩回弹性、耐高温性、耐老化、耐磨性等优点,经久耐用。 
具体实施方式
一种液压缸用密封垫,由以下重量(kg)的原料制成:丁腈橡胶(CR322) 64、氯醇橡胶(H45)165、POM 12、聚异丁烯 10、2,4-二氯过氧化苯甲酰 2、2.2'-二硫化二苯骈噻1.5、癸二酸二辛酯4、甲基丙烯酸正丁酯5、微晶石蜡 6、改性硅灰石 12、纳米海泡石8、硫酸钙晶须6、氧化锌2、氧化镁1.5、炭黑N339 15、二甲基二巯基乙酸异辛酯锡1.5、二硫化四甲基秋兰姆2、防老剂OD 2、防老剂NBC 2、抗氧剂1010 2、抗氧剂168 1。 
所述的改性硅灰石制备方法如下: 
a.取干燥后的硅灰石粉碎至15μm以下,投入分散釜中,加入硅灰石量3倍 的去离子水,搅拌下再加入3%的聚丙烯酸钠、1.5%的磷酸三钙、2%的椰油酸单乙醇酰胺、1%的稻壳灰、3%的有机膨润土,2000rpm高速分散30min,经砂磨机研磨成浆料,待用;
b.取相当于硅灰石量20%的纳米硅溶胶加入搅拌机内,搅拌下加入0.6%的四异丙基二(二辛基亚磷酸酰氧基)钛酸酯、3%的纳米碳、2%的纳米氮化铝、3%的氧化镨和1.5%的月桂醇硫酸钠,60℃搅拌分散30min,冷却后待用; 
c.将上述预处理后的硅溶胶与步骤(a)制得的浆料混合均匀,加入6%的苯丙乳液、1.5%的丙二醇苯醚和2%的十二碳醇酯,搅拌40min,过滤,烘干,粉碎研细,过300目筛即可。 
一种液压缸用密封垫的制备方法,包括以下步骤:取POM、聚异丁烯、纳米海泡石、氧化镁在混炼机中于45℃下混炼6min,排料,放置36h后按比例与丁腈橡胶、氯醇橡胶、改性硅灰石 、硫酸钙晶须、微晶石蜡加入混炼机中,在60℃下混炼5min;将混炼好的胶料加入开炼机中,再加入其余原料在90℃下炼胶4min,薄通6次后下片;将胶片用平板硫化机在16MPa压力下压制成型,然后进行两次硫化处理,第一次硫化的硫化温度为175℃,硫化时间为6min,第二次硫化在烘箱中进行,硫化温度为215℃,硫化时间为3h,修边、检验、包装,即得成品。 
本发明的密封垫性能检测如下所示: 
Figure BDA0000344464751

Claims (2)

1.一种液压缸用密封垫,其特征在于,由以下重量份的原料制成:丁腈橡胶(CR322) 60-70、氯醇橡胶(H45)15-25、POM 10-15、聚异丁烯 8-12、2,4-二氯过氧化苯甲酰 2-3、2.2'-二硫化二苯骈噻1-2、癸二酸二辛酯3-5、甲基丙烯酸正丁酯4-6、微晶石蜡 5-8、改性硅灰石 10-15、纳米海泡石5-10、硫酸钙晶须4-8、氧化锌2-3、氧化镁1-2、炭黑N339 10-15、二甲基二巯基乙酸异辛酯锡1-2、二硫化四甲基秋兰姆2-3、防老剂OD 1-2、防老剂NBC 2-3、抗氧剂1010 1-2、抗氧剂168 1-2;
     所述的改性硅灰石制备方法如下:
   a.取干燥后的硅灰石粉碎至15μm以下,投入分散釜中,加入硅灰石量2-4倍的去离子水,搅拌下再加入2-3%的聚丙烯酸钠、1-2%的磷酸三钙、2-3%的椰油酸单乙醇酰胺、1-2%的稻壳灰、3-4%的有机膨润土,2000-3000rpm高速分散20-30min,经砂磨机研磨成浆料,待用;
   b.取相当于硅灰石量20-30%的纳米硅溶胶加入搅拌机内,搅拌下加入0.5-1%的四异丙基二(二辛基亚磷酸酰氧基)钛酸酯、3-4%的纳米碳、1-2%的纳米氮化铝、2-3%的氧化镨和1-2%的月桂醇硫酸钠,50-60℃搅拌分散30-40min,冷却后待用;
   c.将上述预处理后的硅溶胶与步骤(a)制得的浆料混合均匀,加入5-8%的苯丙乳液、1-2%的丙二醇苯醚和2-3%的十二碳醇酯,搅拌30-50min,过滤,烘干,粉碎研细,过200-300目筛即可。
2.一种如权利要求1所述的液压缸用密封垫的制备方法,其特征在于包括以下步骤:取POM、聚异丁烯、纳米海泡石、氧化镁在混炼机中于40-50℃下混炼4-8min,排料,放置24-36h后按比例与丁腈橡胶、氯醇橡胶、改性硅灰石 、硫酸钙晶须、微晶石蜡加入混炼机中,在50-60℃下混炼5-10min;将混炼好的胶料加入开炼机中,再加入其余原料在85-95℃下炼胶3-6min,薄通5-8次后下片;将胶片用平板硫化机在15-20MPa压力下压制成型,然后进行两次硫化处理,第一次硫化的硫化温度控制在175-185℃,硫化时间为4-7min,第二次硫化在烘箱中进行,硫化温度为200-220℃,硫化时间为2-4h,修边、检验、包装,即得成品。
CN2013102733360A 2013-07-01 2013-07-01 一种液压缸用密封垫及其制备方法 Pending CN103408810A (zh)