CN103373036A - Temporary bonding method and bonding apparatus - Google Patents

Temporary bonding method and bonding apparatus Download PDF

Info

Publication number
CN103373036A
CN103373036A CN2012102016202A CN201210201620A CN103373036A CN 103373036 A CN103373036 A CN 103373036A CN 2012102016202 A CN2012102016202 A CN 2012102016202A CN 201210201620 A CN201210201620 A CN 201210201620A CN 103373036 A CN103373036 A CN 103373036A
Authority
CN
China
Prior art keywords
glass
glass protection
carrying tablet
carrying
sheet
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012102016202A
Other languages
Chinese (zh)
Other versions
CN103373036B (en
Inventor
黄文翰
陈柏宏
桂武俊
洪庆振
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mirle Automation Corp
Original Assignee
Mirle Automation Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mirle Automation Corp filed Critical Mirle Automation Corp
Publication of CN103373036A publication Critical patent/CN103373036A/en
Application granted granted Critical
Publication of CN103373036B publication Critical patent/CN103373036B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a temporary attaching method, which is applied to the manufacturing process of a touch display screen and comprises the steps of attaching a plurality of glass protection sheets on a glass bearing sheet, carrying out a touch sensing layer forming manufacturing process aiming at the glass protection sheets to form a touch sensing layer on each glass protection sheet, and taking down the glass protection sheets from the glass bearing sheet. The invention not only can effectively solve the problem of insufficient strength of the glass protection sheet after cutting, but also can achieve the effect of batch production, thereby shortening the processing time consumed by directly forming the touch sensing layer on the glass protection sheet of the touch display screen.

Description

Temporary applying method and abutted equipment thereof
Technical field
The present invention relates to a kind of temporary applying method and abutted equipment thereof, particularly relate to a kind of being applied on the touch control display screen processing procedure a plurality of glass protection sheets are temporarily fitted in temporary applying method and the abutted equipment thereof on the glass carrying tablet.
Background technology
In general, touch control display screen utilizes vacuum abutted mode to finish the applying of glass protection sheet and touch-control sensing sheet usually.But because above-mentioned applying flow process must be utilized artificial or mechanical arm carries out picking and placeing of glass protection sheet and touch-control sensing sheet, therefore will bring time-consuming applying flow process of taking a lot of work.In addition; use is fitted in the shortcoming that the integral thickness of the touch control display screen that the designing institute on the glass protection sheet brings increases with the touch-control sensing sheet; the trend that also is unfavorable for the touch control display screen slimming, thus directly the touch-control sensing layer is formed on the glass protection sheet of touch control display screen design in response to and give birth to.
In order to meet the glass pieces dimensional requirement of present touch control display screen processing procedure; the above-mentioned design that directly the touch-control sensing layer is formed on the glass protection sheet needs first after large stretch of glass protection sheet forms the touch-control sensing layer; recycling cutting processing procedure is to cut out the small pieces glass protection sheet of the size that meets touch control display screen; yet the small pieces glass protection sheet with touch-control sensing layer that it cuts out often has the problem of undercapacity.On the other hand, if change use first small pieces glass protection sheet is carried out structure-reinforced after more sequentially the small pieces glass protection sheet after reinforcement form the design of touch-control sensing layer, then can cause again the time-consuming problem of taking a lot of work of overall process.
Summary of the invention
The invention provides a kind of temporary applying method; it is applied on the touch control display screen processing procedure; described temporary applying method is included in a plurality of glass protection sheets of fitting on the glass carrying tablet, carries out a touch-control sensing formable layer processing procedure to form a touch-control sensing layer at each glass protection sheet for described a plurality of glass protection sheets, reaches and takes off described a plurality of glass protection sheet from described glass carrying tablet.
Described glass carrying tablet comprises carrying master slice and a carrier sheet; can comprise and form a plurality of accommodating holes on the position of the corresponding described a plurality of glass protection sheets of described carrier sheet, described carrier sheet is fitted on the described carrying master slice in the fit step of described a plurality of glass protection sheets of described glass carrying tablet, and with the coplanar mode of described carrier sheet each glass protection sheet is fitted in respectively in the corresponding accommodating holes.
Form described a plurality of accommodating holes and can comprise that in the locational step of the corresponding described a plurality of glass protection sheets of described carrier sheet using a water cutter to cut processing procedure forms described a plurality of accommodating holes with the position at the corresponding described a plurality of glass protection sheets of described carrier sheet.
Described glass carrying tablet can comprise carrying master slice and an a plurality of carrier sheet; can be included in each carrier sheet and form an accommodating holes, described a plurality of carrier sheets are fitted on the described carrying master slice in the fit step of a plurality of glass protection sheets of described glass carrying tablet, reach each glass protection sheet to be fitted in respectively in the corresponding accommodating holes with the corresponding coplanar mode of carrier sheet.
The step that forms described accommodating holes at each carrier sheet can comprise that use one water cutter cutting processing procedure is to form described accommodating holes at each carrier sheet.
Step at the described a plurality of glass protection sheets of described glass carrying tablet applying can comprise a plurality of storage tanks of formation on the position of the corresponding described a plurality of glass protection sheets of described glass carrying tablet, and with the coplanar mode of described glass carrying tablet each glass protection sheet is fitted in respectively in the corresponding storage tank.
Form described a plurality of storage tank and can comprise that in the locational step of the corresponding described a plurality of glass protection sheets of described glass carrying tablet use one sandblast processing procedure forms described a plurality of storage tanks with the position at the corresponding described a plurality of glass protection sheets of described glass carrying tablet.
The present invention also provides a kind of abutted equipment, and it is applied on the touch control display screen processing procedure a plurality of glass protection sheets to be fitted on the glass carrying tablet being used for, and described abutted equipment comprises that a carrying board, a mechanical taking arm and solidify lamp tube device.Described carrying board has a carrying tablet platform and a screening glass platform, and described carrying tablet platform is used for carrying described glass carrying tablet, and described screening glass platform is used for carrying described a plurality of glass protection sheet.Described mechanical taking arm is arranged on the described carrying board movably, is used for respectively described a plurality of glass protection sheets being transported to described carrying tablet platform to be fitted on the described glass carrying tablet from described screening glass platform.Described curing lamp tube device is arranged on the described mechanical taking arm; be used for when described mechanical taking arm is fitted in described a plurality of glass protection sheets on the described glass carrying tablet respectively; shine described a plurality of glass protection sheet, so that described a plurality of glass protection sheet is fixed on the described glass carrying tablet.
Described glass carrying tablet can comprise carrying master slice and a carrier sheet; described carrier sheet is fitted on the described carrying master slice and in the position of the described a plurality of glass protection sheets of correspondence and forms a plurality of accommodating holes; described abutted equipment can also comprise a location altimeter; described positioning height meter is arranged on the described mechanical taking arm, described positioning height meter be used for controlling described mechanical taking arm with each glass protection sheet to be fitted in respectively in the corresponding accommodating holes with the coplanar mode of described carrier sheet.
Described glass carrying tablet can comprise carrying master slice and an a plurality of carrier sheet; each carrier sheet is fitted on the described carrying master slice and forms an accommodating holes; described abutted equipment can also comprise a location altimeter; described positioning height meter is arranged on the described mechanical taking arm, described positioning height meter be used for controlling described mechanical taking arm with each glass protection sheet to be fitted in respectively in the corresponding accommodating holes with the corresponding coplanar mode of carrier sheet.
Can form a plurality of storage tanks on the described glass carrying tablet; described abutted equipment can also comprise a location altimeter; described positioning height meter is arranged on the described mechanical taking arm, described positioning height meter be used for controlling described mechanical taking arm with each glass protection sheet to be fitted in respectively in the corresponding storage tank with the coplanar mode of described glass carrying tablet.
Described curing lamp tube device can comprise four ultraviolet curing fluorescent tubes; be used for when described mechanical taking arm is fitted in each glass protection sheet on the described glass carrying tablet, shining respectively four corners of each glass protection sheet, so that each glass protection sheet is fixed on the described glass carrying tablet in the mode of 4 curing.
According to technique scheme; the present invention has following advantages and beneficial effect at least compared to prior art: see through a plurality of glass protection sheets and temporarily fit on the glass carrying tablet design with the moulding of carrying out the touch-control sensing layer; the present invention not only can solve the problem of glass protection sheet undercapacity after cutting effectively; also can reach simultaneously the effect that batch is produced, the touch-control sensing layer directly is being formed at the required processing procedure time of expending on the glass protection sheet thereby shorten significantly touch control display screen.
Description of drawings
Fig. 1 is the top view of the abutted equipment that proposes according to one preferred embodiment of the present invention;
Fig. 2 uses the abutted equipment of Fig. 1 to carry out the flow chart of temporary applying method provided by the present invention;
Fig. 3 is that the glass carrying tablet of a plurality of glass protection sheets of being fitted with of Fig. 1 is along the generalized section of hatching A-A ';
Fig. 4 fits in schematic perspective view on the glass carrying tablet for another preferred embodiment proposes according to the present invention a plurality of glass protection sheets;
Fig. 5 is that the glass carrying tablet of Fig. 4 is along the generalized section of hatching B-B ';
Fig. 6 is fitted with the schematic perspective view of glass protection sheet for the glass carrying tablet that another preferred embodiment proposes according to the present invention; And
Fig. 7 is fitted with the schematic perspective view of glass protection sheet for the glass carrying tablet that another preferred embodiment proposes according to the present invention.
Wherein, description of reference numerals is as follows:
10 abutted equipments, 12 glass protection sheets
13 cementing layers, 16 carrying boards
18 mechanical taking arms 20 solidify lamp tube device
22 carrying tablet platforms, 24 screening glass platforms
26 ultraviolet curing fluorescent tubes, 28 carrying master slices
30,30 ' carrier sheet, 32 accommodating holes
34 positioning height meters, 36 storage tanks
14,14 ', 14 ", glass carrying tablet
14”’
Step 200,202,204
The specific embodiment
See also Fig. 1, it is the top view of the abutted equipment 10 that proposes according to one embodiment of the invention.As shown in Figure 1; abutted equipment 10 is used for a plurality of glass protection sheets 12 are fitted on the glass carrying tablet 14; so that the follow-up processing procedure at glass protection sheet 12 formation touch-control sensing layers of wanting to carry out can be finished by the mode that batch is produced; thereby shorten touch control display screen and the touch-control sensing layer is being formed directly into the required processing procedure time of expending on the glass protection sheet; wherein in order to guarantee that further glass protection sheet 12 can have enough structural strengths, glass protection sheet 12 can preferably carry out first structure-reinforced before being fitted on the glass carrying tablet 14.Abutted equipment 10 comprises a carrying board 16, a mechanical taking arm 18, and one solidifies lamp tube device 20.Carrying board 16 has a carrying tablet platform 22 and a screening glass platform 24, and carrying tablet platform 22 is used for bearing glass carrying tablet 14, and 24 on screening glass platform is to carry respectively a plurality of glass protection sheets 12.As for the relevant bearer design of carrying tablet platform 22 with screening glass platform 24; it is common in the prior art; for example screening glass platform 24 can utilize the vacuum suction mode to adsorb glass protection sheet 12, and 22 on carrying tablet platform is can utilize vacuum suction mode and flexible thimble supporting way with bearing glass carrying tablet 14 thereon.
Machinery taking arm 18 is arranged on the carrying board 16 movably, is used for respectively a plurality of glass protection sheets 12 being transported to carrying tablet platform 22 to be fitted in (as shown in Figure 1) on the glass carrying tablet 14 from screening glass platform 24.Solidifying lamp tube device 20 is arranged on the mechanical taking arm 18; solidify the mode that lamp tube device 20 can utilize the light irradiation to solidify when mechanical taking arm 18 is fitted in glass protection sheet 12 on the glass carrying tablet 14, so that glass protection sheet 12 is fixed on the glass carrying tablet 14.For instance; in this embodiment; as shown in Figure 1; solidify lamp tube device 20 and can comprise four ultraviolet curing fluorescent tubes 26; four ultraviolet curing fluorescent tubes 26 are used for when glass protection sheet 12 is fitted on the glass carrying tablet 14; four corners of irradiation glass protection sheet 12 are so that glass protection sheet 12 is fixed on the glass carrying tablet 14 in the mode of 4 curing.
Then; please consult simultaneously Fig. 2 and Fig. 3; Fig. 2 uses the abutted equipment 10 of Fig. 1 to carry out the flow chart of temporary applying method provided by the present invention; Fig. 3 be the glass carrying tablet 14 of a plurality of glass protection sheets 12 of being fitted with of Fig. 1 along the generalized section of hatching A-A ', described temporary applying method comprises the following steps.
Step 200: use mechanical taking arm 18 respectively that a plurality of glass protection sheets 12 are flat from screening glass
Platform 24 is transported to carrying tablet platform 22 to be fitted on the glass carrying tablet 14;
Step 202: carry out a touch-control sensing formable layer processing procedure for a plurality of glass protection sheets 12, to form the touch-control sensing layer at each glass protection sheet 12;
Step 204: take off a plurality of glass protection sheets 12 from glass carrying tablet 14.
Below be elaborated for above-mentioned steps.At first; in step 200; machinery taking arm 18 can move to first the position of corresponding screening glass platform 24; so that a plurality of glass protection sheets 12 are transported on the carrying tablet platform 22 from screening glass platform 24 respectively; then utilization cementing layer 13 as shown in Figure 3 is to be fitted in a plurality of glass protection sheets 12 on the glass carrying tablet 14 respectively; wherein cementing layer 13 can be preferably by high temperature resistant (about 250 ℃); acid and alkali-resistance; the viscose material of high resistance shear stress strength (shear strength) and low peel strength (peeling strength) forms; the coating of cementing layer 13 then is to adopt the common processing procedure of sheet glass on fitting that be applied to, such as slit coating (slit coating) etc.Should be noted; from the above; for a plurality of glass protection sheets 12 can more firmly being fitted on the glass carrying tablet 14 and unlikely slip; abutted equipment 10 can utilize four corners of each the glass protection sheet 12 of four ultraviolet curing fluorescent tubes 26 irradiation that are arranged on the mechanical taking arm 18, makes each glass protection sheet 12 be fixed in effect on the glass carrying tablet 14 in the mode of 4 curing with performance.
Then can carry out a touch-control sensing formable layer processing procedure (step 202) for each the glass protection sheet 12 that is fitted on the glass carrying tablet 14; to form corresponding touch-control sensing layer at each glass protection sheet 12; whereby; can reach the purpose that batch is produced, the touch-control sensing layer is being formed directly into the required processing procedure time of expending on the glass protection sheet thereby shorten significantly touch control display screen.As in the moulding of touch-control sensing layer, it can use general common manufacture of semiconductor, and such as light blockage coating, exposure, development, etching etc., its relevant processing procedure explanation is common in the prior art, so repeat no more in this.
At last; finish after forming respectively the step of corresponding touch-control sensing layer on each glass protection sheet 12; the corresponding cementing layer 13 of each glass protection sheet 12 and its is separated; so that each glass protection sheet 12 can take off (step 204) from glass carrying tablet 14; wherein; the mode that employed glass protection sheet 12 separates with cementing layer 13 in this step can adopt general common dispergation processing procedure (such as the heating dispergation; the laser dispergation; chemistry dispergation etc.) finish; in addition; its also directly curved glass carrying tablet 14 so that produce between cementing layer 13 and the glass protection sheet 12 peel off, then glass protection sheet 12 successfully can be torn off from cementing layer 13.As for adopting which kind of dispergation mode, it is looked closely the viscose characteristic that actual process requirement and cementing layer 13 adopt and decides.
In sum; temporarily be fitted on the glass carrying tablet step with the moulding of carrying out the touch-control sensing layer by above-mentioned a plurality of glass protection sheets; the present invention not only can solve the problem of above-mentioned mentioned glass protection sheet undercapacity after cutting effectively; also can reach simultaneously the effect that batch is produced, the touch-control sensing layer is being formed directly into the required processing procedure time of expending on the glass protection sheet thereby shorten significantly touch control display screen.
It is worth mentioning that the design of glass carrying tablet can be not limited to above-described embodiment.For instance; please consult simultaneously Fig. 1, Fig. 4 and Fig. 5; Fig. 4 is fitted in schematic perspective view on the glass carrying tablet 14 ' for another preferred embodiment proposes according to the present invention a plurality of glass protection sheets 12; Fig. 5 is that the glass carrying tablet 14 ' of Fig. 4 is along the generalized section of hatching B-B '; mentioned assembly is numbered identical person in mentioned assembly and above-described embodiment in this embodiment; represent that it has similar function or relative structure, repeats no more in this.
Glass carrying tablet 14 ' comprises carrying master slice 28 and a carrier sheet 30; carrier sheet 30 is fitted on the carrying master slice 28 and in the position of a plurality of glass protection sheets 12 of correspondence and is formed with a plurality of accommodating holes 32; wherein accommodating holes 32 can preferably use water cutter cutting processing procedure and be formed on the carrier sheet 30, but not limit by this.In this embodiment; abutted equipment 10 can comprise also that a location altimeter 34(as shown in Figure 1); positioning height meter 34 is arranged on the mechanical taking arm 18; positioning height meter 34 is used for controlling mechanical taking arm 18, with glass protection sheet 12 to be fitted in the corresponding accommodating holes 32 (as shown in Figure 5) by cementing layer 13 with carrier sheet 30 coplanar modes.Thus; be fitted on the carrying master slice 28 and glass protection sheet 12 and the 30 coplanar designs of carrier sheet by the carrier sheet 30 with a plurality of accommodating holes 32; compared to glass carrying tablet 14; not only glass carrying tablet 14 ' can increase further in the locational pliability of the accommodating holes 32 of correspondence; to promote the flexible amplitude of glass carrying tablet 14 '; and then glass protection sheet 12 can be torn off more easily from cementing layer 13; simultaneously also can make follow-up touch-control sensing formable layer processing procedure (such as light blockage coating; exposure; develop; etching etc.) can carry out at smooth molding flat, thus the Forming Quality of lifting touch-control sensing layer.In addition, this design also can increase the structural strength in the zone of glass carrying tablet 14 ' beyond the position of the accommodating holes 32 of correspondence, to avoid glass carrying tablet 14 ' recurring structure deflection and have influence on the moulding quality of follow-up touch-control sensing layer in processing procedure transmission way.
In addition, the glass carrying tablet also can change employing only for having the monolithic carrying tablet of a plurality of storage tanks or having the design of a plurality of carrier sheets.At first; only be the design aspect of monolithic carrying tablet at the glass carrying tablet; for instance; see also Fig. 6; it is another preferred embodiment proposes according to the present invention a glass carrying tablet 14 " be fitted with the schematic perspective view of glass protection sheet 12; and mentioned assembly is numbered identical person in mentioned assembly and above-described embodiment in this embodiment, represents that it has similar function or relative structure, repeats no more in this.
This embodiment and above-described embodiment main difference part are the structural design of glass carrying tablet, as shown in Figure 6, glass carrying tablet 14 " on be formed with a plurality of storage tanks 36, wherein storage tank 36 can preferably use a sandblast processing procedure and be formed on glass carrying tablet 14 " on, but not limit by this.In this embodiment, positioning height meter 34 is used for controlling mechanical taking arm 18, with glass protection sheet 12 with glass carrying tablet 14 " coplanar mode is fitted in the corresponding storage tank 36 by cementing layer 13.Thus; be fitted in glass carrying tablet 14 by glass protection sheet 12 " storage tank 36 in and glass protection sheets 12 and glass carrying tablets 14 " coplanar design; compared to glass carrying tablet 14; not only the glass carrying tablet 14 " can increase further in the locational pliability of corresponding storage tank 36; to promote glass carrying tablet 14 " flexible amplitude; and then glass protection sheet 12 can be torn off more easily from cementing layer 13; simultaneously also can make the molding manufacture procedure of follow-up touch-control sensing layer (such as light blockage coating; exposure; develop; etching etc.) can carry out at smooth molding flat, thus the Forming Quality of lifting touch-control sensing layer.In addition, this design also can increase glass carrying tablet 14 " structural strength in zone beyond the position of corresponding storage tank 36, to avoid glass carrying tablet 14 " recurring structure deflection and have influence on the moulding quality of follow-up touch-control sensing layer in processing procedure transmission way.
In addition; the design aspect that has a plurality of carrier sheets at the glass carrying tablet; for instance; see also Fig. 7; it is another preferred embodiment proposes according to the present invention a glass carrying tablet 14 " ' be fitted with the schematic perspective view of glass protection sheet 12; and mentioned assembly is numbered identical person in mentioned assembly and above-described embodiment in this embodiment, represents that it has similar function or relative structure, repeats no more in this.Glass carrying tablet 14 " ' be the design of carrier sheet with glass carrying tablet 14 ' main difference part.Glass carrying tablet 14 " ' comprise and carry master slice 28 and a plurality of carrier sheet 30 ' that each carrier sheet 30 ' is fitted on the carrying master slice 28 and is formed with accommodating holes 32.As for other related description and the effect that produces thereof, it can be with reference to above-described embodiment by that analogy, so repeat no more in this.
The above is the preferred embodiments of the present invention only, is not limited to the present invention, and for a person skilled in the art, the present invention can have various modifications and variations.Within the spirit and principles in the present invention all, any modification of doing, be equal to replacement, improvement etc., all should be included within protection scope of the present invention.

Claims (12)

1. temporary applying method, it is applied to it is characterized in that on the touch control display screen processing procedure that described temporary applying method comprises:
At a plurality of glass protection sheets of glass carrying tablet applying;
Carry out a touch-control sensing formable layer processing procedure for described a plurality of glass protection sheets, to form a touch-control sensing layer at each glass protection sheet; And
Take off described a plurality of glass protection sheet from described glass carrying tablet.
2. temporary applying method as claimed in claim 1 is characterized in that, described glass carrying tablet comprises carrying master slice and a carrier sheet, comprises in the fit step of described a plurality of glass protection sheets of described glass carrying tablet:
Form a plurality of accommodating holes on the position of the corresponding described a plurality of glass protection sheets of described carrier sheet;
Described carrier sheet is fitted on the described carrying master slice; And
With the coplanar mode of described carrier sheet each glass protection sheet is fitted in respectively in the corresponding accommodating holes.
3. temporary applying method as claimed in claim 2 is characterized in that, forms described a plurality of accommodating holes and comprises in the locational step of the corresponding described a plurality of glass protection sheets of described carrier sheet:
Use water cutter cutting processing procedure to form described a plurality of accommodating holes with the position at the corresponding described a plurality of glass protection sheets of described carrier sheet.
4. temporary applying method as claimed in claim 1 is characterized in that, described glass carrying tablet comprises carrying master slice and an a plurality of carrier sheet, comprises in the fit step of a plurality of glass protection sheets of described glass carrying tablet:
Form an accommodating holes at each carrier sheet;
Described a plurality of carrier sheets are fitted on the described carrying master slice; And
With the corresponding coplanar mode of carrier sheet each glass protection sheet is fitted in respectively in the corresponding accommodating holes.
5. temporary applying method as claimed in claim 4 is characterized in that, the step that forms described accommodating holes at each carrier sheet comprises:
Use water cutter cutting processing procedure to form described accommodating holes at each carrier sheet.
6. temporary applying method as claimed in claim 1 is characterized in that, comprises in the fit step of described a plurality of glass protection sheets of described glass carrying tablet:
Form a plurality of storage tanks on the position of the corresponding described a plurality of glass protection sheets of described glass carrying tablet; And with the coplanar mode of described glass carrying tablet each glass protection sheet is fitted in respectively in the corresponding storage tank.
7. temporary applying method as claimed in claim 1 is characterized in that, forms described a plurality of storage tank and comprises in the locational step of the corresponding described a plurality of glass protection sheets of described glass carrying tablet:
Use a sandblast processing procedure to form described a plurality of storage tanks with the position at the corresponding described a plurality of glass protection sheets of described glass carrying tablet.
8. abutted equipment, it is applied on the touch control display screen processing procedure a plurality of glass protection sheets to be fitted on the glass carrying tablet being used for, and it is characterized in that described abutted equipment comprises:
One carrying board, it has a carrying tablet platform and a screening glass platform, and described carrying tablet platform is used for carrying described glass carrying tablet, and described screening glass platform is used for carrying described a plurality of glass protection sheet;
One mechanical taking arm, it is arranged on the described carrying board movably, is used for respectively described a plurality of glass protection sheets being transported to described carrying tablet platform to be fitted on the described glass carrying tablet from described screening glass platform; And
One solidifies lamp tube device; it is arranged on the described mechanical taking arm; be used for when described mechanical taking arm is fitted in described a plurality of glass protection sheets on the described glass carrying tablet respectively, shining described a plurality of glass protection sheet, so that described a plurality of glass protection sheet is fixed on the described glass carrying tablet.
9. abutted equipment as claimed in claim 8; it is characterized in that; described glass carrying tablet comprises carrying master slice and a carrier sheet; described carrier sheet is fitted on the described carrying master slice and in the position of the described a plurality of glass protection sheets of correspondence and forms a plurality of accommodating holes; described abutted equipment also comprises a location altimeter; described positioning height meter is arranged on the described mechanical taking arm, described positioning height meter be used for controlling described mechanical taking arm with each glass protection sheet to be fitted in respectively in the corresponding accommodating holes with the coplanar mode of described carrier sheet.
10. abutted equipment as claimed in claim 8; it is characterized in that; described glass carrying tablet comprises carrying master slice and an a plurality of carrier sheet; each carrier sheet is fitted on the described carrying master slice and forms an accommodating holes; described abutted equipment also comprises a location altimeter; described positioning height meter is arranged on the described mechanical taking arm, described positioning height meter be used for controlling described mechanical taking arm with each glass protection sheet to be fitted in respectively in the corresponding accommodating holes with the corresponding coplanar mode of carrier sheet.
11. abutted equipment as claimed in claim 8; it is characterized in that; form a plurality of storage tanks on the described glass carrying tablet; described abutted equipment also comprises a location altimeter; described positioning height meter is arranged on the described mechanical taking arm, described positioning height meter be used for controlling described mechanical taking arm with each glass protection sheet to be fitted in respectively in the corresponding storage tank with the coplanar mode of described glass carrying tablet.
12. abutted equipment as claimed in claim 8; it is characterized in that; described curing lamp tube device comprises four ultraviolet curing fluorescent tubes; be used for when described mechanical taking arm is fitted in each glass protection sheet on the described glass carrying tablet, shining respectively four corners of each glass protection sheet, so that each glass protection sheet is fixed on the described glass carrying tablet in the mode of 4 curing.
CN201210201620.2A 2012-04-25 2012-06-18 Temporary bonding method and bonding apparatus Active CN103373036B (en)