CN103352370B - 羽绒防蛀护理剂及其制备方法 - Google Patents

羽绒防蛀护理剂及其制备方法 Download PDF

Info

Publication number
CN103352370B
CN103352370B CN201310271187.4A CN201310271187A CN103352370B CN 103352370 B CN103352370 B CN 103352370B CN 201310271187 A CN201310271187 A CN 201310271187A CN 103352370 B CN103352370 B CN 103352370B
Authority
CN
China
Prior art keywords
eider down
mothproof
preparation
care agent
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310271187.4A
Other languages
English (en)
Other versions
CN103352370A (zh
Inventor
陈后前
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Luan Wanzhi Intellectual Property Operations Co.,Ltd.
Original Assignee
ANHUI RUNFENG EIDERDOWN Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI RUNFENG EIDERDOWN Co Ltd filed Critical ANHUI RUNFENG EIDERDOWN Co Ltd
Priority to CN201310271187.4A priority Critical patent/CN103352370B/zh
Publication of CN103352370A publication Critical patent/CN103352370A/zh
Application granted granted Critical
Publication of CN103352370B publication Critical patent/CN103352370B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种羽绒防蛀护理剂,其特征在于由下列重量份的原料制成:钨酸铵2-3、月桂酸钠3-4、二氯苯醚菊脂1-2、硅烷偶联剂KH-550 2-3、抗氧剂1010 1-2、柔软剂3-4、水140。本发明杀菌作用强,对羽绒有较好的调理、护理作用、阻燃、防蛀,羽绒恢复原有的弹性和膨松状,保持原有的保暖性能。

Description

羽绒防蛀护理剂及其制备方法
技术领域
本发明属于洗涤护理用品,具体是一种羽绒防蛀护理剂及其制备方法。
背景技术
羽绒广泛用于制作羽绒服,但由于羽绒来自于动物,通常带有较多细菌,有腥味。用一般的洗涤用品,可以洗去脏物,但没有杀菌功能,且容易损伤羽绒,造成板结,不再具有原来的弹性和膨松感,保暖性能降低,因此,急需研究对羽绒有兼有洗涤、护理、除味、杀菌功能兼顾的护理与洗涤剂。
发明内容
本发明的目的是提供一种羽绒防蛀护理剂及其制备方法。
本发明的技术方案如下:
一种羽绒防蛀护理剂,其特征在于由下列重量份的原料制成:钨酸铵2-3、月桂酸钠3-4、二氯苯醚菊脂1-2、硅烷偶联剂KH-550 2-3、抗氧剂1010 1-2、柔软剂3-4、水140。
所述的软柔剂由下列重量份的原料组分制成:茶多酚0.2-0.3、过硫酸钠0.3-0.4、单硬脂酸甘油酯2.3-2.5、吗啉1-1.2、三乙醇胺油酸皂0.8-0.9、氨基硅油3.4-3.8、聚氧乙烯醚1.2-1.5、钛酸酯偶联剂TMC-TTS 1.2-1.5、柠檬酸2.0-2.4、二正辛基-4- 异噻唑啉-3- 酮0.3-0.5、水15-18;制备方法是将过硫酸钠加适量水溶解,滴加至其它剩余成分的混合物中,搅拌40-50分钟,然后升温至70-80℃,搅拌反应1-2小时即得。
所述的羽绒护理剂的制备方法,其特征在于将各原料成分混合,加热至90-98℃,高速分散搅拌反应1-2小时,即得。
本发明杀菌作用强,对羽绒有较好的调理、护理作用、阻燃、防蛀,羽绒恢复原有的弹性和膨松状,保持原有的保暖性能。
具体实施方式
一种羽绒防蛀护理剂,由下列重量份(公斤)的原料制成:钨酸铵3、月桂酸钠3、二氯苯醚菊脂1、硅烷偶联剂KH-550 3、抗氧剂1010 1、柔软剂3、水140。
所述的羽绒护理剂的制备方法,其特征在于将各原料成分混合,加热至90-98℃,高速分散搅拌反应1-2小时,即得。
所述的软柔剂由下列重量份(公斤)的原料组分制成:茶多酚0.2、过硫酸钠0.3、单硬脂酸甘油酯2.3、吗啉1、三乙醇胺油酸皂0.9、氨基硅油3.4、聚氧乙烯醚1.2、钛酸酯偶联剂TMC-TTS 1.2、柠檬酸2.0、二正辛基-4- 异噻唑啉-3- 酮0.3、水15;制备方法是将过硫酸钠加适量水溶解,滴加至其它剩余成分的混合物中,搅拌40-50分钟,然后升温至70-80℃,搅拌反应1-2小时即得。

Claims (2)

1.一种羽绒防蛀护理剂,其特征在于由下列重量份的原料制成:钨酸铵2-3、月桂酸钠3-4、二氯苯醚菊酯1-2、硅烷偶联剂KH-550 2-3、抗氧剂1010 1-2、柔软剂3-4、水140;
所述的柔软剂由下列重量份的原料组分制成:茶多酚0.2-0.3、过硫酸钠0.3-0.4、单硬脂酸甘油酯2.3-2.5、吗啉1-1.2、三乙醇胺油酸皂0.8-0.9、氨基硅油3.4-3.8、聚氧乙烯醚1.2-1.5、钛酸酯偶联剂TMC-TTS 1.2-1.5、柠檬酸2.0-2.4、2-正辛基-4- 异噻唑啉-3- 酮0.3-0.5、水15-18;制备方法是将过硫酸钠加适量水溶解,滴加至其它剩余成分的混合物中,搅拌40-50分钟,然后升温至70-80℃,搅拌反应1-2小时即得。
2.权利要求1所述的羽绒防蛀护理剂的制备方法,其特征在于将各原料成分混合,加热至90-98℃,高速分散搅拌反应1-2小时,即得。
CN201310271187.4A 2013-07-01 2013-07-01 羽绒防蛀护理剂及其制备方法 Active CN103352370B (zh)