CN103350288A - 新型低合金钢焊条 - Google Patents

新型低合金钢焊条 Download PDF

Info

Publication number
CN103350288A
CN103350288A CN2013103309065A CN201310330906A CN103350288A CN 103350288 A CN103350288 A CN 103350288A CN 2013103309065 A CN2013103309065 A CN 2013103309065A CN 201310330906 A CN201310330906 A CN 201310330906A CN 103350288 A CN103350288 A CN 103350288A
Authority
CN
China
Prior art keywords
welding rod
alloy steel
low alloy
core wire
welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN2013103309065A
Other languages
English (en)
Inventor
吴厚余
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG HONEST MACHINERY Co Ltd
Original Assignee
NANTONG HONEST MACHINERY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG HONEST MACHINERY Co Ltd filed Critical NANTONG HONEST MACHINERY Co Ltd
Priority to CN2013103309065A priority Critical patent/CN103350288A/zh
Publication of CN103350288A publication Critical patent/CN103350288A/zh
Withdrawn legal-status Critical Current

Abstract

本发明涉及焊接技术领域,具体涉及新型低合金钢焊条,包括两段焊条本体以及设于所述两段焊条本体之间的夹持部,所述焊条本体由焊芯和药皮组成,所述药皮均匀包裹焊芯,所述焊芯为低合金钢焊芯。本发明采用上述结构,在使用时,在将两段焊条使用完后,才将夹持部丢弃,避免造成浪费现象,并提高利用率;同时采用低合金钢焊芯,有效提高了焊接质量和性能。另外,本发明具有设计合理、结构简单、使用方便等特点,主要用于海洋平台、船舶压力容器、耐候的铁路机车辆等焊接。

Description

新型低合金钢焊条
技术领域
本发明涉及焊接技术领域,具体涉及新型低合金钢焊条。
背景技术
现有的焊条包括焊芯和焊药,除焊芯的一端为焊药包裹位于焊芯,未包裹焊药的焊芯一端即是焊钳夹持部,当使用焊条时,焊钳夹住所述夹持部,从而不可避免的造成了浪费。另外,焊条种类不同,即焊芯不同,从而也直接影响了焊接质量。
发明内容
本发明的目的是提供一种设计合理、结构简单、避免造成浪费现象、并有效提高焊接质量的新型低合金钢焊条。
为了解决背景技术所存在的问题,本发明是采用以下技术方案:新型低合金钢焊条,包括两段焊条本体以及设于所述两段焊条本体之间的夹持部,所述焊条本体由焊芯和药皮组成,所述药皮均匀包裹焊芯,所述焊芯为低合金钢焊芯。
进一步地,所述药皮为钛钙型药皮。
本发明具有以下有益效果:本发明所述的新型低合金钢焊条,主要包括两段焊条本体以及设于两段焊条本体之间的夹持部,其中,焊条本体由焊芯和药皮组成,药皮均匀包裹焊芯,且焊芯为低合金钢焊芯;本发明采用上述结构,在使用时,在将两段焊条使用完后,才将夹持部丢弃,避免造成浪费现象,并提高利用率;同时采用低合金钢焊芯,有效提高了焊接质量和性能。另外,本发明具有设计合理、结构简单、使用方便等特点,主要用于海洋平台、船舶压力容器、耐候的铁路机车辆等焊接。
附图说明
图1为本发明的结构示意图。
具体实施方式
下面结合附图对本发明做进一步详细的说明。
如图1所示,新型低合金钢焊条,包括两段焊条本体1以及设于所述两段焊条本体1之间的夹持部2,所述焊条本体1由焊芯3和药皮4组成,所述药皮4均匀包裹焊芯3,所述焊芯3为低合金钢焊芯;本实施例中,使用用,在将两段焊条本体使用完后才将夹持部丢弃,避免造成浪费现象,提高利用率;同时采用低合金钢焊芯的作用在于,一方面是含合金钢低时钢丝塑性好,焊丝拉拔比较容易;另一方面可降低还原性气体CO含量,减少飞溅或气孔,并可增高焊缝金属凝固时的温度,对仰焊有利。其中,现两段焊条本体的端部的药皮45度左右的倒角,这是便于在焊接时引弧;另外,焊芯在焊接时有两个作用,一是传导焊接电流,产生电弧把电能转换成热能,二是焊芯本身熔化作为填充金属与液体母材金属熔合形成焊缝。
其中,所述药皮4为钛钙型药皮,这样设计,其焊条工艺性能良好,熔渣流动性好,熔深一般,电弧稳定,焊缝美观,脱渣方便,适用于全位置焊接。
最后说明的是,以上实施例仅用以说明本发明的技术方案而非限制,本领域普通技术人员对本发明的技术方案所做的其他修改或者等同替换,只要不脱离本发明技术方案的精神和范围,均应涵盖在本发明的权利要求范围当中。

Claims (2)

1.新型低合金钢焊条,其特征在于,包括两段焊条本体(1)以及设于所述两段焊条本体(1)之间的夹持部(2),所述焊条本体(1)由焊芯(3)和药皮(4)组成,所述药皮(4)均匀包裹焊芯(3),所述焊芯(3)为低合金钢焊芯。
2.根据权利要求1所述的新型低合金钢焊条,其特征在于,所述药皮(4)为钛钙型药皮。
CN2013103309065A 2013-08-01 2013-08-01 新型低合金钢焊条 Withdrawn CN103350288A (zh)