CN103275432A - 一种聚氯乙烯塑料制软管 - Google Patents
一种聚氯乙烯塑料制软管 Download PDFInfo
- Publication number
- CN103275432A CN103275432A CN2013102465456A CN201310246545A CN103275432A CN 103275432 A CN103275432 A CN 103275432A CN 2013102465456 A CN2013102465456 A CN 2013102465456A CN 201310246545 A CN201310246545 A CN 201310246545A CN 103275432 A CN103275432 A CN 103275432A
- Authority
- CN
- China
- Prior art keywords
- flexible pipe
- polyvinyl chloride
- igelite
- cadmium
- pipe processed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种聚氯乙烯塑料制软管,以质量百分比计,其原料组成为:聚氯乙烯65-82%、环氧增塑剂4-12%、有机锡稳定剂4-7%、己二酸二辛脂7-12%、镉液体稳定剂4-6%、硬脂酸镉3-5%。通过上述方式,本发明提供的一种聚氯乙烯塑料制软管,所述软管具有重量轻、强度好等优点,对周围环境中的酸碱腐蚀物有很强的耐受性,长时间使用内部不结垢,有很长的使用寿命,不需要经常更换,极大的节省了更换软管所造成的人工费用和损失,可以保证建筑物的使用安全。
Description
技术领域
本发明涉及塑料管材领域,特别是涉及一种聚氯乙烯塑料制软管。
背景技术
塑料为合成的高分子化合物,又可称为高分子或巨分子。塑料可以自由改变形体样式,是一种利用单体原料以合成或缩合反应聚合而成的材料,由合成树脂及填料、增塑剂、稳定剂、润滑剂、色料等添加剂组成的。塑料的基本性能主要决定于树脂的本性,但添加剂也起着重要作用。有些塑料基本上是由合成树脂所组成,不含或少含添加剂,如有机玻璃、聚苯乙烯等。
聚氯乙烯塑料可以用于制成软管,但目前使用的软管容易受周围环境中酸碱性物质的腐蚀,长时间使用容易发生漏水现象,对建筑物的安全有极大的影响,频繁更换软管也会造成人力资源和物力资源的浪费。
发明内容
本发明主要解决的技术问题是提供一种聚氯乙烯塑料制软管,该软管具有重量轻、强度好等优点。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种聚氯乙烯塑料制软管,以质量百分比计,其原料组成为:
聚氯乙烯 65-82%
环氧增塑剂 4-12%
有机锡稳定剂 4-7%
己二酸二辛脂 7-12%
镉液体稳定剂 4-6%
硬脂酸镉 3-5%。
在本发明一个较佳实施例中,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 75%
环氧增塑剂 6%
有机锡稳定剂 4%
己二酸二辛脂 7%
镉液体稳定剂 5%
硬脂酸镉 3%。
在本发明一个较佳实施例中,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 65%
环氧增塑剂 10%
有机锡稳定剂 7%
己二酸二辛脂 7%
镉液体稳定剂 6%
硬脂酸镉 5%。
在本发明一个较佳实施例中,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 70%
环氧增塑剂 7%
有机锡稳定剂 6%
己二酸二辛脂 10%
镉液体稳定剂 4%
硬脂酸镉 3%。
本发明的有益效果是:本发明的聚氯乙烯塑料制软管,所述软管具有重量轻、强度好等优点,对周围环境中的酸碱腐蚀物有很强的耐受性,长时间使用内部不结垢,有很长的使用寿命,不需要经常更换,极大的节省了更换软管所造成的人工费用和损失,可以保证建筑物的使用安全。
具体实施方式
下面对本发明的较佳实施例进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
实施例一:
提供一种聚氯乙烯塑料制软管,以质量百分比计,其原料组成为:
聚氯乙烯 75%
环氧增塑剂 6%
有机锡稳定剂 4%
己二酸二辛脂 7%
镉液体稳定剂 5%
硬脂酸镉 3%。
实施例二:
提供一种聚氯乙烯塑料制软管,以质量百分比计,其原料组成为:
聚氯乙烯 65%
环氧增塑剂 10%
有机锡稳定剂 7%
己二酸二辛脂 7%
镉液体稳定剂 6%
硬脂酸镉 5%。
实施例三:
提供一种聚氯乙烯塑料制软管,以质量百分比计,其原料组成为:
聚氯乙烯 70%
环氧增塑剂 7%
有机锡稳定剂 6%
己二酸二辛脂 10%
镉液体稳定剂 4%
硬脂酸镉 3%。
本发明揭示的聚氯乙烯塑料制软管,所述软管具有重量轻、强度好等优点,对周围环境中的酸碱腐蚀物有很强的耐受性,长时间使用内部不结垢,有很长的使用寿命,不需要经常更换,极大的节省了更换软管所造成的人工费用和损失,可以保证建筑物的使用安全。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其他相关的技术领域,均同理包括在本发明的专利保护范围内。
Claims (4)
1.一种聚氯乙烯塑料制软管,其特征在于,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 65-82%
环氧增塑剂 4-12%
有机锡稳定剂 4-7%
己二酸二辛脂 7-12%
镉液体稳定剂 4-6%
硬脂酸镉 3-5%。
2.根据权利要求1所述的聚氯乙烯塑料制软管,其特征在于,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 75%
环氧增塑剂 6%
有机锡稳定剂 4%
己二酸二辛脂 7%
镉液体稳定剂 5%
硬脂酸镉 3%。
3.根据权利要求1所述的聚氯乙烯塑料制软管,其特征在于,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 65%
环氧增塑剂 10%
有机锡稳定剂 7%
己二酸二辛脂 7%
镉液体稳定剂 6%
硬脂酸镉 5%。
4.根据权利要求1所述的聚氯乙烯塑料制软管,其特征在于,以质量百分比计,所述聚氯乙烯塑料制软管的原料组成为:
聚氯乙烯 70%
环氧增塑剂 7%
有机锡稳定剂 6%
己二酸二辛脂 10%
镉液体稳定剂 4%
硬脂酸镉 3%。