CN103242004A - Method for manufacturing reinforced bricks from construction wastes - Google Patents
Method for manufacturing reinforced bricks from construction wastes Download PDFInfo
- Publication number
- CN103242004A CN103242004A CN2013101765580A CN201310176558A CN103242004A CN 103242004 A CN103242004 A CN 103242004A CN 2013101765580 A CN2013101765580 A CN 2013101765580A CN 201310176558 A CN201310176558 A CN 201310176558A CN 103242004 A CN103242004 A CN 103242004A
- Authority
- CN
- China
- Prior art keywords
- bricks
- percent
- construction wastes
- building waste
- mud
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for manufacturing reinforced bricks from construction wastes. The reinforced bricks comprise 20 percent of construction wastes, 50 percent of red clay, 5 percent of coquina, 10 percent of yellow sand, 12 percent of cement and 3 percent of cooked glutinous rice mud. The method comprises the steps of adding water and mud to all the components to manufacture green bricks, and then drying and sintering the green bricks to obtain the reinforced bricks. The bricks produced by the method are high in hardness; and as being made from the construction wastes, the reinforced bricks are economical and low in cost and can beautify the environment.
Description
Technical field the present invention relates to utilize building waste system to strengthen the method for brick.
Building waste in the background technology municipal wastes accounts for greatly, huddles disorderly contaminate environment, and the present invention utilizes brick-making technology exactly, and building waste is turned waste into wealth, and has both beautified environment, has improved economic benefit again.
Summary of the invention the objective of the invention is to utilize building waste system to strengthen the method for brick.
The following scheme of present method is achieved:
Building waste is stirred into mud, and glutinous rice boils smashes into mud.
Building waste 20%, red clay 50%, shell-lime 5%, yellow sand 10%, cement 12%, ripe glutinous rice mud 3% with all component Jia Shui and mud, removes the caking residue, makes adobe, and drying bakes bricks gets final product.
Embodiment
Embodiment 1:
Building waste 30%, red clay 40%, shell-lime 5%, yellow sand 10%, cement 12%, ripe glutinous rice mud 3% is general by this proportioning brick output hardness.
Embodiment 2:
Building waste 20%, red clay 50%, shell-lime 5%, yellow sand 10%, cement 12%, ripe glutinous rice mud 3% is by this proportioning brick output hardness height.
Claims (2)
1. method of utilizing building waste system to strengthen brick, building waste 30%, red clay 40%, shell-lime 5%, yellow sand 10%, cement 12%, ripe glutinous rice mud 3% is general by this proportioning brick output hardness.
2. the above-mentioned method of utilizing building waste system to strengthen brick according to claim 1 is characterized in that:
Building waste 20%, red clay 50%, shell-lime 5%, yellow sand 10%, cement 12%, ripe glutinous rice mud 3% is by this proportioning brick output hardness height.