CN103227351A - 一种延长vrla电池使用寿命的脉冲充电方法 - Google Patents

一种延长vrla电池使用寿命的脉冲充电方法 Download PDF

Info

Publication number
CN103227351A
CN103227351A CN2013101491947A CN201310149194A CN103227351A CN 103227351 A CN103227351 A CN 103227351A CN 2013101491947 A CN2013101491947 A CN 2013101491947A CN 201310149194 A CN201310149194 A CN 201310149194A CN 103227351 A CN103227351 A CN 103227351A
Authority
CN
China
Prior art keywords
charging
voltage
section
current
battery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2013101491947A
Other languages
English (en)
Other versions
CN103227351B (zh
Inventor
周忠永
金新伟
余鋆
裘道林
严辉强
钱立峰
徐井华
章萍
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hangzhou Youlian New Energy Technology Co ltd
Original Assignee
HANGZHOU SINOCOM HIGH-TECH Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HANGZHOU SINOCOM HIGH-TECH Co Ltd filed Critical HANGZHOU SINOCOM HIGH-TECH Co Ltd
Priority to CN201310149194.7A priority Critical patent/CN103227351B/zh
Publication of CN103227351A publication Critical patent/CN103227351A/zh
Application granted granted Critical
Publication of CN103227351B publication Critical patent/CN103227351B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种延长VRLA电池使用寿命的脉冲充电方法。本发明的目的是提供一种延长VRLA电池使用寿命的脉冲充电方法,以延长阀控铅酸蓄电池使用寿命。本发明的技术方案是:一种延长VRLA电池使用寿命的脉冲充电方法,VRLA电池输出电压U、容量C,其特征在于:该方法分A、B、C三段进行,其中A段以充电限流电流I恒流充电;B段以限流电流I恒流与第二充电电压U2恒压周期性变化充电;C段以第一充电电压U1恒压与第二充电电压U2恒压周期性变化充电;所述A段中电池电压上升至U1后转入B段,B段中电池充电至接近满容量时转入C段。本发明适用于蓄电池充电器领域。

Description

一种延长VRLA电池使用寿命的脉冲充电方法
技术领域
本发明涉及通信用阀控铅酸蓄电池充电电源的充电方法,尤其是一种延长阀控铅酸蓄电池使用寿命的充电方法。适用于蓄电池充电器领域。
背景技术
在通信电源领域,VRLA电池的设计寿命可达5~10年,有的甚至可达到10~15年。但在实际使用过程中,大多数厂家的产品在使用中均存在早期失效现象,有的3年甚至不到3年就放不出电。尤其是在移动通信的户外基站使用时,大部分只能使用1~2年就失效,存在维护工作量大、维护费用高的问题,对通信的正常进行产生了严重的影响。
充电模式是伴随电池的使用寿命全过程的,很大程度上决定了电池的运行状态和工作寿命。普遍认为,太高的浮充电压会加速腐蚀和增加水损;而过低的浮充电压又将导致负极板的自放电及硫酸盐化。
目前,通信行业VRLA电池的充电方式普遍采用恒压限流充电模式,大量实践证明,对频繁放电的通信用、深循环用的多个电池串联的VRLA电池组采用这种充电模式是不合适的。这种充电模式给电池造成以下故障:一是由于长期充电不足,正负极表面沉积大量大体积、不活性的PbS04结晶和其包覆下的活性差的Pb02,表现为充电时,该电池电压很快升到控制的终止电压。放电时又很快跌落到终止电压,电池有容量但放不出电。二是反复过充电和长期浮充,电池析出大量的气体导致电解液损失加快,内阻增大。三是电池组中各电池性能的差异性,在多次循环之后表现非常明显。
国内外学者针对以上问题,进行了相关的研制,提出了多种能改进电池使用寿命的充电方法,有普通固定降电流脉冲充电、普通固定恒电流脉冲充电。   
中国专利“一种自适应定流间歇脉冲限时充电方法”,专利号200510134746.2,针对以上几种方法提出了各自的缺点,同时提出了一种自适应定流间歇脉冲限时充电方法。图1为该方法的电流电压变化曲线图,先以第一充电电流I1恒流充电至第一充电电压U1,再以第一充电电流I1进行自适应间歇限时脉冲充电,充电时间限定为第一充电时间T1,最后以第二充电电压U2进行浮充充电。以第一充电电流I1进行自适应间歇限时脉冲充电过程中,充电的电流第一充电电流I1保持不变,充电脉冲的宽度和间歇的时间根据蓄电池本身的电压而变化。但在该方法中,第一阶段时间长达4~6H,充电电压高达14.4V,第二阶段,充电电压也达13.9V,而时间根据蓄电池本身的电压而变化,是一种自适应脉冲充电,但恢复充电的电压高达13.8V,此种方法不能解决由于充电电压过高引起的水解反应,析气现象依旧存在,影响电池使用寿命。
文献(文章编号: 1002~ 087 X(2008)01~ 0056~ 03 Design of fast charger with slow pulse for VRLA battery TANG Xiu~fen1, MI Chen2,WEI Feng~lan3)提出了一种慢脉冲快速充电方法:如图2所示,在恒流恒压二段充电方式中,慢脉冲充电以0.5~1.5C 的高幅值大电流充电3 min,再以0.02 C 的低幅值小电流充电0.5 min,大小电流交替贯穿于恒流充电阶段, 在恒压阶段中以恒定电压充电3 min,再以小电流0.02 C 充电0.5min,两者也交替贯穿于恒压充电阶段。在整个充电过程中, 慢脉冲的重复周期固定在3.5 min。但是,该方法存在以下问题:初期恒流充电时,有0.5 min时间是以0.02 C 的低幅值小电流进行充电,影响充电效率;在后期恒压充电时,以恒定电压充电3 min, 再以小电流0.02 C 充电0.5min,这种方法如果恒压电压过高,依然会让电池电压高于水解电压、析气严重,而恒压电压过低的话,电池又会处于充电不满状态。
综上所述,以上方法在一定程度上能有效加快蓄电池的充电速度、延长蓄电池的循环使用寿命,但由于存在充电效率较低、充电模式转化复杂、充电电压限值存在偏差等原因,并不能最大程度地消除在充电过程中因过充导致的电池内部电解水反应引起的电池析气问题,从而影响到电池的使用寿命。
发明内容
本发明要解决的技术问题是:针对上述存在的问题,提供一种延长VRLA电池使用寿命的脉冲充电方法,以克服充电效率低、失水量大、充电转换复杂、电池组容易不均衡产生落后蓄电池的缺陷,延长阀控铅酸蓄电池使用寿命。
本发明所采用的技术方案是:一种延长VRLA电池使用寿命的脉冲充电方法,VRLA电池输出电压U、容量C,其特征在于:该方法分A、B、C三段进行,其中A段以充电限流电流I恒流充电;B段以限流电流I恒流与第二充电电压U2恒压周期性变化充电;C段以第一充电电压U1恒压与第二充电电压U2恒压周期性变化充电;所述A段中电池电压上升至U1后转入B段,B段中电池充电至接近满容量时转入C段;
其中限流电流I为0.1~1C;B段中限流电流I持续时间为T1 500ms~1.5s,以2V单体电池为基准,第二充电电压U2为2.15-2.22V,持续时间T2 1~5s;C段中第一充电电压U1为2.267-2.4V,持续时间为T1,第二充电电压U2持续时间为T2。
所述限流电流I优选0.2~0.5C。所述持续时间T2优选2s。
所述VRLA电池上并联负载。 
本发明的有益效果是:在设定周期内,第一充电电压U1较高,TI时间内,由于每次充电脉冲的电流较大,大电流充电有利于形成更紧凑的正极活性物质骨架,对正极活性物质和表面的结构有良好影响;大电流充电形成的正极活性物质由于来不及生长从而形成活性物质的颗粒尺寸较小,活性物质之间的连接较紧凑,使得正极板的孔率较大,从而有利于循环寿命的延长;同时这种脉冲对蓄电池又有很好的修复激活作用,可以消除“极板硫化”,能有效地防止电池组间的不均衡现象发生。而第二充电电压U2较低,当电池接近充满时,在T2时间内,电池停止充电,电池的欧姆极化、浓差极化和电化学极化消除,蓄电池端电压会降低,充电效率会大大增加,可以减少析气量,最终减少失水。较大的电流限值设置,使得电池初期充电速度加快,后期因限压起作用,又可以防止过充电,对蓄电池有良好的保护作用,不会出现发热变形等故障。该充电方法可以防止蓄电池早期衰减,大大延长电池的循环使用寿命。 
附图说明
图1为现有技术中自适应定流间歇脉冲限时充电方法的电流电压变化曲线。
图2为现有技术中慢脉冲快速充电方法的电流-时间曲线。
图3是本发明提出的充电方法的电压时间设置曲线。
图4为本发明的电流电压变化曲线。
图5为本发明充电方法具体实现的系统框图。
具体实施方式
本实施例提出了一种能延长通信电源用VRLA电池使用寿命的脉冲充电方法。如图4所示,该方法将充电过程分为A、B、C三段进行,其中A段以充电限流电流I恒流充电;B段以限流电流I恒流与第二充电电压U2恒压周期性变化充电;C段以第一充电电压U1恒压与第二充电电压U2恒压周期性变化充电。在按图3设定的充电电压-时间曲线时,A段中电池容量从接近0开始充电,电池电压逐渐提高,当电压上升至U1后转入B段;B段中恒流和恒压交替充电,直至电池充电接近满容量时转入C段。     
本例中VRLA电池作为通信设备用电源,一般电池组直接挂接有负载,C段中T1时段内补充进的能量在转入T2时段时通过负载予以释放,最终达到脉冲平衡充放电。
本实施例以48V/100AH电池组作为实施实例,此时第一充电电压U1为54.4~57.6V,T1为500ms~1.5S,第二充电电压U2为51.6~53.2V ,T2为在1~5S之间,典型值为2S,充电限流电流I设为10-100A之间,优选20-50A。
      图5是本实施例一种延长VRLA电池使用寿命的充电方法具体实现的系统框图。系统由具有稳压稳流功能的开关电源组成,开关电源的最高稳压电压满足负载和电池充电电压要求,输出电流应能满足负载所需最大功率时电流和充电时最大脉冲充电电流之和。该系统具有智能控制功能,能通过自身或外部的监控单元完成对蓄电池组进行按上述程序的充电。系统具有电池电压检测电路,将检测到的电池组电压,和设定的电压进行比较后,调节电源的输出电压,以达到所需脉冲电压限压控制的目的,同时,系统还具有检测电池电流电路,电池电流检测到的电流和设定的充电限流电流进行比较,通过控制电源的输出电压达到限流充电的目的。 

Claims (4)

1.一种延长VRLA电池使用寿命的脉冲充电方法,VRLA电池输出电压U、容量C,其特征在于:该方法分A、B、C三段进行,其中A段以充电限流电流I恒流充电;B段以限流电流I恒流与第二充电电压U2恒压周期性变化充电;C段以第一充电电压U1恒压与第二充电电压U2恒压周期性变化充电;所述A段中电池电压上升至U1后转入B段,B段中电池充电至接近满容量时转入C段;
其中限流电流I为0.1~1C;B段中限流电流I持续时间为T1 500ms~1.5s,以2V单体电池为基准,第二充电电压U2为2.15-2.22V,持续时间T2 1~5s;C段中第一充电电压U1为2.267-2.4V,持续时间为T1,第二充电电压U2持续时间为T2。
2.根据权利要求1所述的延长VRLA电池使用寿命的脉冲充电方法,其特征在于:所述限流电流I优选0.2~0.5C。
3.根据权利要求1或2所述的延长VRLA电池使用寿命的脉冲充电方法,其特征在于:所述持续时间T2优选2s。
4.根据权利要求1所述的延长VRLA电池使用寿命的脉冲充电方法,其特征在于:所述VRLA电池上并联负载。
CN201310149194.7A 2013-04-26 2013-04-26 一种延长vrla电池使用寿命的脉冲充电方法 Active CN103227351B (zh)