CN103146368A CN2013100664296A CN201310066429A CN103146368A CN 103146368 A CN103146368 A CN 103146368A CN 2013100664296 A CN2013100664296 A CN 2013100664296A CN 201310066429 A CN201310066429 A CN 201310066429A CN 103146368 A CN103146368 A CN 103146368A
Authority
CN
China
Prior art keywords
cement
agent
elasticity
fluid loss
well cementation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013100664296A
Other languages
English (en)
Inventor
王志伟
王峰
耿春香
安慧
赵朝成
赵东风
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China University of Petroleum East China
Original Assignee
China University of Petroleum East China
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China University of Petroleum East China filed Critical China University of Petroleum East China
Priority to CN2013100664296A priority Critical patent/CN103146368A/zh
Publication of CN103146368A publication Critical patent/CN103146368A/zh
Pending legal-status Critical Current

Links

Images

Landscapes

  • Curing Cements, Concrete, And Artificial Stone (AREA)
  • Preparation Of Clay, And Manufacture Of Mixtures Containing Clay Or Cement (AREA)

Abstract

本发明公开了一种弹性固井水泥浆及其制备方法,该弹性固井水泥浆各组分重量百分比以100%的水泥的重量为基准,降滤失剂1~2%,弹性材料4~12%,分散剂0.5~1.5%,增韧剂0.5~2%,消泡剂0.4~1%,缓凝剂0.5~2%,密度调节剂0~50%,淡水35~50%;制备该弹性固井水泥浆时,先将弹性材料、增韧剂、密度调节剂、水泥干混混合均匀备用;再将降滤失剂、分散剂、消泡剂、缓凝剂与淡水湿混混合均匀;最后在搅拌条件下,将干混的添加剂加入到湿混的材料中,搅拌均匀即得弹性固井水泥浆;该弹性固井水泥浆增加了水泥石弹性,降低了杨氏模量,水泥环具有较高的抗冲击性和韧性,减小了井下作业对水泥环的损坏。

Description

一种弹性固井水泥浆及其制备方法
技术领域
本发明属于水泥浆制备技术领域,尤其涉及一种弹性固井水泥浆及其制备方法。
背景技术
普通固井用水泥浆弹性小,脆性大,在射孔、压裂等作业产生的冲击载荷作用下产生裂纹,随着应力的发展产生裂缝,容易造成油气层的窜槽,给射孔开发和改造挖潜等增产措施带来极大地困难。
发明内容
本发明提供了一种弹性固井水泥浆及其制备方法,旨在解决普通固井用水泥浆弹性小,脆性大,在射孔、压裂等作业产生的冲击载荷作用下产生裂纹,随着应力的发展产生裂缝,容易造成油气层的窜槽,给射孔开发和改造挖潜等增产措施带来极大地困难的问题。
本发明的目的在于提供一种弹性固井水泥浆,该弹性固井水泥浆各组分重量百分比以100%的水泥的重量为基准,各添加剂占水泥重量的百分比为:降滤失剂:1~2%,弹性材料:4~12%,分散剂:0.5~1.5%,增韧剂:0.5~2%,消泡剂:0.4~1%,缓凝剂:0.5~2%,密度调节剂:0~50%,淡水:35~50%。
进一步,降滤失剂SWJ-3、弹性材料WF-1、分散剂SWJZ-1、增韧剂SWZR-1、消泡剂SWX-1、缓凝剂SWH-1、密度调节剂。
本发明的另一目的在于提供一种弹性固井水泥浆的制备方法,该制备方法包括:
步骤一,按比例称取水泥、降滤失剂、弹性材料、分散剂、增韧剂、消泡剂、缓凝剂、密度调节剂、淡水;
步骤二,将弹性材料、增韧剂、密度调节剂、水泥干混混合均匀备用;
步骤三,将降滤失剂、分散剂、消泡剂、缓凝剂与淡水湿混混合均匀;
步骤四,在搅拌条件下,将步骤二获得的干混的添加剂加入到步骤三获得的湿混的材料中,搅拌均匀即得到弹性固井水泥浆。
本发明提供的弹性固井水泥浆及其制备方法,该弹性固井水泥浆各组分重量百分比以100%的水泥的重量为基准,各添加剂占水泥重量的百分比为:降滤失剂:1~2%,弹性材料:4~12%,分散剂:0.5~1.5%,增韧剂:0.5~2%,消泡剂:0.4~1%,缓凝剂:0.5~2%,密度调节剂:0~50%,淡水:35~50%;制备该弹性固井水泥浆时,首先将弹性材料、增韧剂、密度调节剂、水泥干混混合均匀备用;然后将降滤失剂、分散剂、消泡剂、缓凝剂与淡水湿混混合均匀;最后在搅拌条件下,将获得的干混的添加剂加入到获得的湿混的材料中,搅拌均匀即得到弹性固井水泥浆;该弹性固井水泥浆有效地增加了水泥石的弹性,降低了杨氏模量,水泥环具有较高的抗冲击性和韧性,减小了井下作业对水泥环的损坏,降低并节约了修井费用,延长了油气井的寿命,提高了油气采收率,具有较强的推广与应用价值。
附图说明
图1是本发明实施例提供的弹性固井水泥浆的制备方法的实现流程图。
具体实施方式
为了使本发明的目的、技术方案及优点更加清楚明白,以下结合附图及实施例,对本发明进行进一步的详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本发明,并不用于限定发明。
本发明的目的在于提供一种弹性固井水泥浆,该弹性固井水泥浆各组分重量百分比以100%的水泥的重量为基准,各添加剂占水泥重量的百分比为:降滤失剂:1~2%,弹性材料:4~12%,分散剂:0.5~1.5%,增韧剂:0.5~2%,消泡剂:0.4~1%,缓凝剂:0.5~2%,密度调节剂:0~50%,淡水:35~50%。
在本发明实施例中,降滤失剂SWJ-3、弹性材料WF-1、分散剂SWJZ-1、增韧剂SWZR-1、消泡剂SWX-1、缓凝剂SWH-1、密度调节剂。
图1示出了本发明实施例提供的弹性固井水泥浆的制备方法的实现流程。
该制备方法包括以下步骤:
步骤S101,按比例称取水泥、降滤失剂、弹性材料、分散剂、增韧剂、消泡剂、缓凝剂、密度调节剂、淡水;
步骤S102,将弹性材料、增韧剂、密度调节剂、水泥干混混合均匀备用;
步骤S103,将降滤失剂、分散剂、消泡剂、缓凝剂与淡水湿混混合均匀;
步骤S104,在搅拌条件下,将步骤S102获得的干混的添加剂加入到步骤S103获得的湿混的材料中,搅拌均匀即得到弹性固井水泥浆。
下面结合附图及具体实施例对本发明的应用原理作进一步描述。
本发明涉及一种弹性固井水泥浆,各组分的重量百分比以100%的水泥的重量为基准,各添加剂占水泥重量的百分比为:降滤失剂:1~2%;弹性材料:4~12%;分散剂:0.5~1.5%;增韧剂:0.5~2%;消泡剂:0.4~1%;缓凝剂:0.5~2%;密度调节剂:0~50%;淡水:35~50%;制备该弹性固井水泥浆时,将上述材料按比例称取,将弹性材料、增韧剂、加重剂、水泥干混混合均匀备用;将其他添加剂与水湿混混合均匀,在搅拌下将干混的添加剂加入到湿混的材料中,搅拌均匀即得到本发明。本发明解决了普通固井水泥石弹性小,脆性大,在冲击载荷作用下易产生裂纹的缺点,弹性水泥浆能增加水泥石的弹性,杨氏模量大大降低,水泥环具有较高的抗冲击性和韧性,可减小井下作业对水泥环的损坏,降低、节约修井费用,延长油气井的寿命,提高采收率。
本发明实施例提供的弹性固井水泥浆及其制备方法,该弹性固井水泥浆各组分重量百分比以100%的水泥的重量为基准,各添加剂占水泥重量的百分比为:降滤失剂:1~2%,弹性材料:4~12%,分散剂:0.5~1.5%,增韧剂:0.5~2%,消泡剂:0.4~1%,缓凝剂:0.5~2%,密度调节剂:0~50%,淡水:35~50%;制备该弹性固井水泥浆时,首先将弹性材料、增韧剂、密度调节剂、水泥干混混合均匀备用;然后将降滤失剂、分散剂、消泡剂、缓凝剂与淡水湿混混合均匀;最后在搅拌条件下,将获得的干混的添加剂加入到获得的湿混的材料中,搅拌均匀即得到弹性固井水泥浆;该弹性固井水泥浆有效地增加了水泥石的弹性,降低了杨氏模量,水泥环具有较高的抗冲击性和韧性,减小了井下作业对水泥环的损坏,降低并节约了修井费用,延长了油气井的寿命,提高了油气采收率,具有较强的推广与应用价值。
以上所述仅为本发明的较佳实施例而已,并不用以限制本发明,凡在本发明的精神和原则之内所作的任何修改、等同替换和改进等,均应包含在本发明的保护范围之内。

Claims (3)

1.一种弹性固井水泥浆,其特征在于,该弹性固井水泥浆各组分重量百分比以100%的水泥的重量为基准,各添加剂占水泥重量的百分比为:降滤失剂:1~2%,弹性材料:4~12%,分散剂:0.5~1.5%,增韧剂:0.5~2%,消泡剂:0.4~1%,缓凝剂:0.5~2%,密度调节剂:0~50%,淡水:35~50%。
2.如权利要求1所述的制备方法,其特征在于,降滤失剂SWJ-3、弹性材料WF-1、分散剂SWJZ-1、增韧剂SWZR-1、消泡剂SWX-1、缓凝剂SWH-1、密度调节剂。
3.一种弹性固井水泥浆的制备方法,其特征在于,该制备方法包括:
步骤一,按比例称取水泥、降滤失剂、弹性材料、分散剂、增韧剂、消泡剂、缓凝剂、密度调节剂、淡水;
步骤二,将弹性材料、增韧剂、密度调节剂、水泥干混混合均匀备用;
步骤三,将降滤失剂、分散剂、消泡剂、缓凝剂与淡水湿混混合均匀;
步骤四,在搅拌条件下,将步骤二获得的干混的添加剂加入到步骤三获得的湿混的材料中,搅拌均匀即得到弹性固井水泥浆。
CN2013100664296A 2013-03-01 2013-03-01 一种弹性固井水泥浆及其制备方法 Pending CN103146368A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2013100664296A CN103146368A (zh) 2013-03-01 2013-03-01 一种弹性固井水泥浆及其制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2013100664296A CN103146368A (zh) 2013-03-01 2013-03-01 一种弹性固井水泥浆及其制备方法

Publications (1)

Publication Number Publication Date
CN103146368A true CN103146368A (zh) 2013-06-12

Family

ID=48544698

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2013100664296A Pending CN103146368A (zh) 2013-03-01 2013-03-01 一种弹性固井水泥浆及其制备方法

Country Status (1)

Country Link
CN (1) CN103146368A (zh)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103320107A (zh) * 2013-06-19 2013-09-25 西南石油大学 一种用于实体膨胀管固井的韧性防气窜水泥浆
CN103361041A (zh) * 2013-08-09 2013-10-23 卫辉市化工有限公司 一种高密度防气窜固井水泥浆的制备方法
CN103923628A (zh) * 2014-04-17 2014-07-16 中国海洋石油总公司 一种小井眼单通道固井用低粘柔性水泥浆
CN104610949A (zh) * 2015-02-02 2015-05-13 中国海洋石油总公司 一种过饱和氯化钾固井水泥浆
CN105784482A (zh) * 2016-03-31 2016-07-20 西南石油大学 一种评价油井水泥石弹性的方法
CN105778876A (zh) * 2016-04-08 2016-07-20 陕西省石油化工研究设计院 一种适用于热采水泥的抗高温强度衰退剂
CN107056158A (zh) * 2017-05-02 2017-08-18 成都西油奥星石油技术有限公司 用于易漏失小井眼或窄间隙环空井固井的封堵防气窜水泥浆

Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2008084200A2 (en) * 2007-01-11 2008-07-17 Halliburton Energy Services, Inc Compositions comprising quaternary material and sorel cements and methods of servicing a wellbore with the same
CN101338183A (zh) * 2007-07-04 2009-01-07 中国石油集团工程技术研究院 一种抗盐高密度水泥浆
CN102250596A (zh) * 2011-05-25 2011-11-23 天津中油渤星工程科技有限公司 一种新型固井用水泥浆
CN102492404A (zh) * 2011-12-13 2012-06-13 四川嘉华企业(集团)股份有限公司 一种防窜用水泥浆
CN102516965A (zh) * 2011-12-06 2012-06-27 中国石油集团渤海钻探工程有限公司 高温高密度韧性固井水泥浆
CN102604610A (zh) * 2012-02-10 2012-07-25 成都欧美科石油科技股份有限公司 一种弹塑性固井水泥浆及其制备方法
CN102604614A (zh) * 2012-02-15 2012-07-25 成都欧美科石油科技股份有限公司 防窜固井水泥浆
WO2012143687A1 (en) * 2011-04-21 2012-10-26 Fumi Minerals Limited Weighting agent for use in subterranean wells

Patent Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2008084200A2 (en) * 2007-01-11 2008-07-17 Halliburton Energy Services, Inc Compositions comprising quaternary material and sorel cements and methods of servicing a wellbore with the same
CN101338183A (zh) * 2007-07-04 2009-01-07 中国石油集团工程技术研究院 一种抗盐高密度水泥浆
WO2012143687A1 (en) * 2011-04-21 2012-10-26 Fumi Minerals Limited Weighting agent for use in subterranean wells
CN102250596A (zh) * 2011-05-25 2011-11-23 天津中油渤星工程科技有限公司 一种新型固井用水泥浆
CN102516965A (zh) * 2011-12-06 2012-06-27 中国石油集团渤海钻探工程有限公司 高温高密度韧性固井水泥浆
CN102492404A (zh) * 2011-12-13 2012-06-13 四川嘉华企业(集团)股份有限公司 一种防窜用水泥浆
CN102604610A (zh) * 2012-02-10 2012-07-25 成都欧美科石油科技股份有限公司 一种弹塑性固井水泥浆及其制备方法
CN102604614A (zh) * 2012-02-15 2012-07-25 成都欧美科石油科技股份有限公司 防窜固井水泥浆

Non-Patent Citations (2)

* Cited by examiner, † Cited by third party
Title
刁胜贤等: "盐探2井固井水泥浆技术", 《钻井液与完井液》 *
赖金荣: "SDJR胶乳水泥浆体系研究", 《钻井液与完井液》 *

Cited By (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103320107A (zh) * 2013-06-19 2013-09-25 西南石油大学 一种用于实体膨胀管固井的韧性防气窜水泥浆
CN103361041A (zh) * 2013-08-09 2013-10-23 卫辉市化工有限公司 一种高密度防气窜固井水泥浆的制备方法
CN103361041B (zh) * 2013-08-09 2015-10-21 卫辉市化工有限公司 一种高密度防气窜固井水泥浆的制备方法
CN103923628A (zh) * 2014-04-17 2014-07-16 中国海洋石油总公司 一种小井眼单通道固井用低粘柔性水泥浆
CN104610949A (zh) * 2015-02-02 2015-05-13 中国海洋石油总公司 一种过饱和氯化钾固井水泥浆
CN105784482A (zh) * 2016-03-31 2016-07-20 西南石油大学 一种评价油井水泥石弹性的方法
CN105784482B (zh) * 2016-03-31 2018-07-24 西南石油大学 一种评价油井水泥石弹性的方法
CN105778876A (zh) * 2016-04-08 2016-07-20 陕西省石油化工研究设计院 一种适用于热采水泥的抗高温强度衰退剂
CN105778876B (zh) * 2016-04-08 2018-07-17 陕西省石油化工研究设计院 一种适用于热采水泥的抗高温强度衰退剂
CN107056158A (zh) * 2017-05-02 2017-08-18 成都西油奥星石油技术有限公司 用于易漏失小井眼或窄间隙环空井固井的封堵防气窜水泥浆
CN107056158B (zh) * 2017-05-02 2020-11-24 四川宝鑫石油科技有限公司 用于易漏失小井眼或窄间隙环空井固井的封堵防气窜水泥浆

Similar Documents

Publication Publication Date Title
CN103146368A (zh) 一种弹性固井水泥浆及其制备方法
CN103320107B (zh) 一种用于实体膨胀管固井的韧性防气窜水泥浆
CN103555304A (zh) 一种高效油基冲洗隔离液及其制备方法
CN102504775A (zh) 深井长封固段固井用大温差水泥浆及其制备方法
CN102492404A (zh) 一种防窜用水泥浆
CN103642476A (zh) 一种页岩气开发油基钻井液固井前置液
CN103274650B (zh) 高压富水岩溶区隧道堵水用注浆材料及其制备方法
CN103074045B (zh) 一种用于小间隙环空水平井固井的增韧防气窜水泥浆
CN102250596A (zh) 一种新型固井用水泥浆
CN103666420A (zh) 用于页岩气开发油基钻井液固井工艺的水泥浆
CN103102128A (zh) 用于地下结构堵水的注浆材料及其制备方法
CN103910511A (zh) 一种全程无收缩超高强钢筋套筒连接用灌浆材料
CN106966648A (zh) 一种防co2、h2s腐蚀固井水泥浆
CN103923628A (zh) 一种小井眼单通道固井用低粘柔性水泥浆
CN105505350A (zh) 一种基于温敏形状记忆聚合物的弹韧性固井水泥浆体系及制备方法
EP2880002A1 (en) Cement compositions for cementing in confined locales and methods for use thereof
CN103740352A (zh) 具有抗温性能的膨胀油井水泥
CN103980871A (zh) 一种低弹性模量的抗温韧性油井水泥
CN106995687A (zh) 一种干热岩用高温固井水泥浆及其制备方法
CN101962530B (zh) 一种油气田区域探井固井水泥二级浆工艺
CN105778876A (zh) 一种适用于热采水泥的抗高温强度衰退剂
CN104291733A (zh) 水泥用增韧防窜剂及页岩气水平井固井用增韧水泥
CN102533235B (zh) 一种油井水泥中高温早强剂
CN101338184B (zh) 一种可水分散油井水泥加重剂
CN106753294A (zh) 一种堵漏水泥浆

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130612