CN102848660A - 一种复合轧花无纺布 - Google Patents
一种复合轧花无纺布 Download PDFInfo
- Publication number
- CN102848660A CN102848660A CN2012103142448A CN201210314244A CN102848660A CN 102848660 A CN102848660 A CN 102848660A CN 2012103142448 A CN2012103142448 A CN 2012103142448A CN 201210314244 A CN201210314244 A CN 201210314244A CN 102848660 A CN102848660 A CN 102848660A
- Authority
- CN
- China
- Prior art keywords
- low
- pressure membrane
- nonwoven
- hot pressing
- epe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了一种复合轧花无纺布,先由珍珠棉和低压膜经轧花机在热压温度为110~120℃,压辊转速为800~1200RPM下直接热压,再与无纺布经胶粘剂和低密度聚乙烯树脂粒子的混合物的涂覆层流延复合而成,上层是低压膜,中层是珍珠棉,下层是无纺布,其中低密度聚乙烯树脂粒子的使用量占涂覆料重量的20~40%,铝膜的厚度为8~25微米,由于低密度聚乙烯树脂粒子的价格低于胶粘剂,本发明的复合轧花无纺布在保证了无纺布和珍珠棉、低压膜的复合质量的同时降低了生产成本,也通过热压温度和压辊转速的控制提高了低压膜和珍珠棉的粘结强度,更加的牢固。
Description
技术领域
本发明属于包装材料技术领域,涉及无纺布复合材料,具体涉及一种复合轧花无纺布。
背景技术
EPE珍珠棉是一种新型环保的包装材料,由低密度聚乙烯经物理发泡产生无数的独立气泡构成。克服了普通发泡胶易碎、变形、回复性差的缺点,具有隔水防潮、防震、隔音、保温、可塑性能佳、韧性强、循环再造、环保、抗撞力强等诸多优点,亦具有很好的抗化学性能,是传统包装材料的理想替代品,广泛应用于电子电器、仪器仪表、电脑、音响、医疗器械、工控机箱、五金灯饰、工艺品、玻璃、陶瓷、家电、喷涂、家俱家私、酒类及树脂等高档易碎礼品包装、五金制品、玩具、瓜果、皮鞋的内包装、日用品等多种产品的包装。
PE低压膜以HDPE为基料,经挤出、吹塑成型,具有无毒无味强度高、透明度高、环保等特点。广泛应用于日常生活用品、电子行业、农业、商业、食品等包装领域。
无纺布(英文名:Non Woven)又称不织布,是由定向的或随机的纤维而构成,是新一代环保材料,具有防潮、透气、柔韧、质轻、不助燃、容易分解、无毒无刺激性、色彩丰富、价格低廉、可循环再用等特点。如多采用聚丙烯(pp材质)粒料为原料,经高温熔融、喷丝、铺纲、热压卷取连续一步法生产而成。无纺布制品色彩丰富、鲜艳明快、时尚环保、用途广泛、美观大方,图案和款式都多样,且质轻、环保、可循环再用,被国际公认为保护地球生态的环保产品。适用于农用薄膜、制鞋、制革、床垫、子母被、装饰、化工、印刷、汽车、建材,家具等行业,及服装衬布,医疗卫生一次性手术衣,口罩,帽,床单,酒店一次性台布,美容,桑拿乃至当今时尚的礼品袋,精品袋,购物袋,广告袋等等。环保产品,用途广泛,经济实惠。
单一的无纺布限制了其应用领域,需要和其他材料复合使用,低压膜、珍珠棉和无纺布的复合得到了广泛的使用,复合轧花无纺布在流延复合的过程中需要使用胶粘剂等涂覆料,由于胶粘剂的价格较高,使得复合轧花无纺布的成本相对较高。
发明内容
为了克服现有技术的不足,本发明在不损失其性能的基础上,提供了一种成本相对低廉且更加牢固的复合轧花无纺布。
本发明的复合轧花无纺布先由珍珠棉和低压膜经轧花机直接热压,再与无纺布经涂覆层流延复合而成,上层是低压膜,中层是珍珠棉,下层是无纺布,所述的涂覆层的涂覆料为胶粘剂和低密度聚乙烯树脂粒子的混合物。
优选涂覆料含有20~40wt%的低密度聚乙烯树脂粒子。
所述的低压膜层厚度为8~25微米,优选12~20微米。
珍珠棉覆低压膜复合材料在热压温度为110~120℃,压辊转速为800~1200RPM下压制制得,优选压辊转速为1000RPM。
由于低密度聚乙烯树脂粒子的价格低于胶粘剂,本发明的复合轧花无纺布在保证了无纺布和珍珠棉、低压膜的复合质量的同时降低了生产成本,也通过热压温度和压辊转速的控制提高了低压膜和珍珠棉的粘结强度,更加的牢固。
附图说明
附图1为本发明的复合轧花无纺布的结构示意图。
具体实施方式
下面结合附图1和实施例对本发明的复合轧花无纺布进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
参照附图1,本发明的复合轧花无纺布首先由低压膜和珍珠棉经轧花机直接热压,再与无纺布经涂覆层流延复合而成,上层是低压膜1,中层是珍珠棉2,下层是无纺布3,采用的涂覆料为胶粘剂和低密度聚乙烯树脂粒子的混合物,二者在液态下易于流延复合,选用不同混合比例的涂覆料和不同厚度的铝膜层以及不同的热压温度和压辊转速进行了对比试验。
实施例1
首先将上层低压膜和中层珍珠棉经轧花机在热压温度110℃下,压辊转速800RPM直接热压,由80wt%的胶粘剂和20wt%的低密度聚乙烯树脂粒子混合而成作为涂覆层,将下层无纺布和热压而成的低压膜和珍珠棉在240℃下流延复合而成,铝膜厚度为8微米。
实施例2
首先将上层低压膜和中层珍珠棉经轧花机在热压温度110℃下,压辊转速1200RPM直接热压,由60wt%的胶粘剂和40wt%的低密度聚乙烯树脂粒子混合而成作为涂覆层,将下层无纺布和热压而成的低压膜和珍珠棉在280℃下流延复合而成,铝膜厚度为25微米。
实施例3
首先将上层低压膜和中层珍珠棉经轧花机在热压温度110℃下,压辊转速1000RPM直接热压,由70wt%的胶粘剂和30wt%的低密度聚乙烯树脂粒子混合而成作为涂覆层,将下层无纺布和热压而成的低压膜和珍珠棉在260℃下流延复合而成,铝膜厚度为15微米。
实施例4
首先将上层低压膜和中层珍珠棉经轧花机在热压温度120℃下,压辊转速1000RPM直接热压,由70wt%的胶粘剂和30wt%的低密度聚乙烯树脂粒子混合而成作为涂覆层,将下层无纺布和热压而成的低压膜和珍珠棉在260℃下流延复合而成,铝膜厚度为12微米。
实施例5
首先将上层低压膜和中层珍珠棉经轧花机在热压温度120℃下,压辊转速1000RPM直接热压,由70wt%的胶粘剂和30wt%的低密度聚乙烯树脂粒子混合而成作为涂覆层,将下层无纺布和热压而成的低压膜和珍珠棉在260℃下流延复合而成,铝膜厚度为20微米。
上述实施例不以任何方式限制本发明,凡是采用等同替换或等效变换的方式获得的技术方案均落在本发明的保护范围内。
Claims (7)
1.一种复合轧花无纺布,其特征在于:先由低压膜和珍珠棉经轧花机直接热压,再与无纺布经涂覆层流延复合而成,上层是低压膜(1),中层是珍珠棉(2),下层是无纺布(3)。
2.根据权利要求1所述的复合轧花无纺布,其特征在于:所述的涂覆层涂覆料为胶粘剂和低密度聚乙烯树脂粒子的混合物。
3.根据权利要求2所述的复合轧花无纺布,其特征在于:所述的涂覆料中低密度聚乙烯树脂粒子的用量为20~40wt%。
4.根据权利要求1所述的复合轧花无纺布,其特征在于:所述的铝膜(1)厚度为8~25微米。
5.根据权利要求1或4所述的复合轧花无纺布,其特征在于:所述的铝膜(1)厚度为12~20微米。
6.根据权利要求1所述的复合轧花无纺布,其特征在于:低压膜和珍珠棉在热压温度110~120℃,压辊转速800~1200RPM下直接压制。
7.根据权利要求6所述的复合轧花无纺布,其特征在于:所述的压辊转速为1000RPM。