CN102847743A - Manufacture method of pipe different in wall thickness - Google Patents

Manufacture method of pipe different in wall thickness Download PDF

Info

Publication number
CN102847743A
CN102847743A CN2012103535767A CN201210353576A CN102847743A CN 102847743 A CN102847743 A CN 102847743A CN 2012103535767 A CN2012103535767 A CN 2012103535767A CN 201210353576 A CN201210353576 A CN 201210353576A CN 102847743 A CN102847743 A CN 102847743A
Authority
CN
China
Prior art keywords
wall thickness
wait
thickness tube
pipe different
manufacture method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012103535767A
Other languages
Chinese (zh)
Inventor
蔡昌友
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Heda Auto Accessory Co Ltd
Original Assignee
Shanghai Heda Auto Accessory Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Heda Auto Accessory Co Ltd filed Critical Shanghai Heda Auto Accessory Co Ltd
Priority to CN2012103535767A priority Critical patent/CN102847743A/en
Publication of CN102847743A publication Critical patent/CN102847743A/en
Pending legal-status Critical Current

Abstract

The invention discloses a manufacture method of a pipe different in wall thickness. The manufacture method comprises the following steps: manufacturing an opening component of the pipe different in wall thickness through a die, and then rolling the opening component of the pipe different in wall thickness, thus forming the pipe different in wall thickness. The manufacture method disclosed by the invention has relatively low cost, and the prepared pipe different in wall thickness can meet the strength of a car body, so that the weight of the car body can be reduced as far as possible, and the oil consumption is reduced.

Description

A kind of preparation method that does not wait wall thickness tube
Technical field
The present invention relates to a kind of preparation method of pipe fitting, relate in particular to a kind of preparation method that does not wait wall thickness tube.
Background technology
The present main pipe fitting of being made by high-strength plate that adopts of the raw material of panel board for car bodies beam main pipe, body structure processing (such as the B post etc.), and high-strength plate is because yield strength is large, moulding is difficult, a lot of enterprises adopt the increase structure for reaching intensity, guarantee its intensity, so that tare increases.
In the research of body lightening, a kind of lightweight research for product is arranged---do not wait wall thickness tube.So-called do not wait wall thickness tube to refer to two or more different wall thickness occur at a pipe, and wherein one section be progressive thickness.
Have at present the report about unequal thickness plate, this unequal thickness plate can be used as the raw material that do not wait wall thickness tube, need to compress moulding to inner and outer plates during the roll moulding in the conventional roll extrusion tube-making process, but because not wait the pipe thickness of wall thickness tube be gradual change, the operation that inner and outer plates compresses moulding can cause damage to not waiting tube wall of wall thickness tube, this shows, does not wait wall thickness tube can not adopt conventional roll extrusion tube-making process.
Therefore, a kind of wall thickness tube preparation method that do not wait for unequal thickness plate of development is that those skilled in the art are devoted to one of direction of studying and solving.
Summary of the invention
The object of the invention is to overcome the defective of prior art and a kind of preparation method that does not wait wall thickness tube is provided.
The object of the present invention is achieved like this:
A kind of preparation method that does not wait wall thickness tube of the present invention may further comprise the steps:
S1: being that axial cross section is rounded with unequal thickness plate by mould molding does not ringently wait the wall thickness tube opening member, and its opened gap≤7mm;
S2: will not wait the wall thickness tube opening member by behind the four-pass roll at least, what obtain opened gap≤0.1mm, linearity requirement≤0.5mm does not wait the wall thickness tube semi-finished product;
S3: by gas laser, according to 2 m/mins speeds of welding the wall thickness tube semi-finished product that do not wait that step S2 obtains are welded;
S4: the product after above-mentioned welding finished obtains final products again by correcting wheel and material discharging wheel effect.
The inventive method adopts first mould molding to make and does not wait the wall thickness tube opening member, do not wait wall thickness tube will not waiting wall thickness tube opening member further can make by roll forming, the inventive method cost is lower, and what make does not wait wall thickness tube when satisfying bus body strength, can reduce tare as far as possible, reduce oil consumption.
The specific embodiment
Below in conjunction with embodiment, the invention will be further described.
The present invention does not wait the preparation method of wall thickness tube, may further comprise the steps:
S1: being that axial cross section is rounded with unequal thickness plate by mould molding does not ringently wait the wall thickness tube opening member, and its opened gap≤7mm;
S2: will not wait the wall thickness tube opening member by behind the four-pass roll at least, what obtain opened gap≤0.1mm, linearity requirement≤0.5mm does not wait the wall thickness tube semi-finished product;
S3: by gas laser, according to 2 m/mins speeds of welding the wall thickness tube semi-finished product that do not wait that step S2 obtains are welded;
S4: the product after above-mentioned welding finished obtains final products again by correcting wheel and material discharging wheel effect.
Above embodiment is only for explanation the present invention's, but not limitation of the present invention, person skilled in the relevant technique, in the situation that do not break away from the spirit and scope of the present invention, can also make various conversion or modification, therefore all technical schemes that are equal to also should belong to category of the present invention, should be limited by each claim.

Claims (1)

1. preparation method that does not wait wall thickness tube may further comprise the steps:
S1: being that axial cross section is rounded with unequal thickness plate by mould molding does not ringently wait the wall thickness tube opening member, and its opened gap≤7mm;
S2: will not wait the wall thickness tube opening member by behind the four-pass roll at least, what obtain opened gap≤0.1mm, linearity requirement≤0.5mm does not wait the wall thickness tube semi-finished product;
S3: by gas laser, according to 2 m/mins speeds of welding the wall thickness tube semi-finished product that do not wait that step S2 obtains are welded;
S4: the product after above-mentioned welding finished obtains final products again by correcting wheel and material discharging wheel effect.
CN2012103535767A 2012-09-20 2012-09-20 Manufacture method of pipe different in wall thickness Pending CN102847743A (en)