CN102798948B - 单模光纤尾纤的毛细管封装结构 - Google Patents
单模光纤尾纤的毛细管封装结构 Download PDFInfo
- Publication number
- CN102798948B CN102798948B CN201210275350.XA CN201210275350A CN102798948B CN 102798948 B CN102798948 B CN 102798948B CN 201210275350 A CN201210275350 A CN 201210275350A CN 102798948 B CN102798948 B CN 102798948B
- Authority
- CN
- China
- Prior art keywords
- capillary tube
- glue
- optical fiber
- kapillary
- mode optical
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明提供一种单模光纤尾纤的毛细管封装结构,包括单模光纤以及毛细管;所述单模光纤从毛细管的尾锥孔处贯穿所述毛细管,所述毛细管和单模光纤之间的腔体内充满353ND胶水,所述毛细管的尾锥孔开口处填充有353NDT胶水。本发明在毛细管内填充353ND胶水的基础上,在毛细管的尾锥孔开口处补充353NDT胶水,避免了因353ND胶水在固化过程中释放过多的应力导致毛细管玻璃裂开的问题,提高了产品的合格率和可靠性。
Description
技术领域
本发明涉及光纤通讯器件,特别涉及一种基于353ND胶水和353NDT胶水的单模光纤尾纤的毛细管封装结构。
背景技术
近年来,随着光纤通讯网络的急速发展,必须要求大量的高性能,并且低价格的光学器件。特别地,将光纤封装在毛细管中是最常用的封装方法。目前单模光纤尾纤的封装方式是将剥好的250um单模光纤直接从充满353ND胶水的毛细管的尾锥孔处穿入,并从毛细管的另一端锥孔处穿出,然后进行高温固化制作完成。毛细管的尾锥孔的直径比另一端锥孔的直径大。由于操作环境和操作人员的微小差异,制作完成的单模光纤在毛细管尾锥孔处经常会出现裂纹。
发明内容
本发明的目的在于提供一种对操作环境以及操作人员要求较低的,可提高产品的合格率和可靠性的单模光纤尾纤的毛细管封装结构。
本发明的技术方案如下:
一种单模光纤尾纤的毛细管封装结构,包括单模光纤以及毛细管;所述单模光纤从毛细管的尾锥孔处贯穿所述毛细管,所述毛细管和单模光纤之间的腔体内充满353ND胶水,所述毛细管的尾锥孔开口处填充有353NDT胶水。
本发明的有益技术效果是:
本发明结构合理,在毛细管内填充353ND胶水的基础上,在毛细管的尾锥孔开口处补充353NDT胶水。353NDT胶水内所含有的石英粉可改善热膨胀系数,避免了因353ND胶水在固化过程中释放过多的应力导致毛细管玻璃裂开的问题,提高了产品的合格率和可靠性。
附图说明
图1是本发明的结构示意图。
具体实施方式
下面结合附图对本发明的具体实施方式做进一步说明。
如图1所示,本发明包括剥好的250um单模光纤1和毛细管2;剥好的250um单模光纤1从毛细管2的尾锥孔处贯穿而过,毛细管2和剥好的250um单模光纤1之间的毛细管2腔体内充满有353ND胶水3,毛细管2的尾锥孔开口处填充有353NDT胶水4。
本发明的封装步骤如下:将353ND胶水3注入到毛细管2中,使353ND胶水3充满毛细管2。然后将剥好的250um单模光纤1从充满353ND胶水3的毛细管2的尾锥孔处穿入,并从毛细管2的另一端锥孔处穿出,从而贯穿毛细管2,并进行高温固化。最后在毛细管2的尾锥孔开口处用353NDT胶水4密封,再进行高温固化。(注:毛细管2的另一端锥孔开口处不用填充353NDT胶水4。)
所述353ND胶水和353NDT胶水均为市售商品。其中,所述353NDT胶水是在353ND胶水中加入石英粉而形成的混合胶水。
以上所述的仅是本发明的优选实施方式,本发明不限于以上实施例。可以理解,本领域技术人员在不脱离本发明的基本构思的前提下直接导出或联想到的其他改进和变化,均应认为包含在本发明的保护范围之内。
Claims (2)
1.一种单模光纤尾纤的毛细管封装结构,包括单模光纤(1)以及毛细管(2);所述单模光纤(1)从毛细管(2)的尾锥孔处贯穿所述毛细管(2),其特征在于:所述毛细管(2)和单模光纤(1)之间的腔体内充满353ND胶水(3),所述毛细管(2)的尾锥孔开口处填充有353NDT胶水(4)。
2.根据权利要求1所述单模光纤尾纤的毛细管封装结构,其特征在于:所述单模光纤(1)为剥好的250um单模光纤。