CN102757575B - Method for bonding rubber component - Google Patents

Method for bonding rubber component Download PDF

Info

Publication number
CN102757575B
CN102757575B CN201210268920.2A CN201210268920A CN102757575B CN 102757575 B CN102757575 B CN 102757575B CN 201210268920 A CN201210268920 A CN 201210268920A CN 102757575 B CN102757575 B CN 102757575B
Authority
CN
China
Prior art keywords
rubber
neoprene
bonding
pressure
rubber assembly
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210268920.2A
Other languages
Chinese (zh)
Other versions
CN102757575A (en
Inventor
何燕春
石红
崔景新
曲亮
喻少英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
AVIC No 631 Research Institute
Original Assignee
AVIC No 631 Research Institute
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by AVIC No 631 Research Institute filed Critical AVIC No 631 Research Institute
Priority to CN201210268920.2A priority Critical patent/CN102757575B/en
Publication of CN102757575A publication Critical patent/CN102757575A/en
Application granted granted Critical
Publication of CN102757575B publication Critical patent/CN102757575B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a method for bonding a rubber component. The method comprises the following steps of: carrying out surface treatment on the rubber component; cleaning a bonding surface of the rubber component by using a solvent; infiltrating the rubber surface by using a neoprene-phenolic aldehyde adhesive; and placing the rubber component until the surface of the rubber component is semi-cured, etc. The invention provides the method for bonding the rubber component, which solves a technical problem that rubber shortage or rubber overflow is easy to generate by singly using a curing adhesive or the bonding force is insufficient by singly using a pressure sensitive adhesive film. Through the adoption of the method provided by the invention, a neoprene-phenolic aldehyde adhesive infiltrated rubber adhesive film is formed on the surface of the rubber component, so that the rubber surface energy is increased, coarseness is reduced, the bonding area of the rubber film is increased, and rubber shortage or rubber overflow is avoided after semi-curing.

Description

A kind of method of adhesive rubber assembly
Technical field
The invention belongs to Hardening Technique of Computer field, relate to rubber assembly bonding.
Background technology
In computer realm, often metalwork and rubber parts need to be bondd, but rubber assembly belongs to low-surface-energy material, the bonding difficulty of metal and elastomeric material, at present, general employing curing type adhesive carries out bonding, and in gluing assembling, inevitable overflow glue or the starved phenomenon of occurring, not only affects the visual appearance of product but also can bring unpredictable hidden danger of quality.Also there is part to adopt pressure-sensitive adhesive film adhesive rubber assembly, but can show glued membrane bonding force deficiency.
Summary of the invention
Be prone to starved or excessive glue for fear of independent use curing type adhesive, or use separately the bonding hypodynamic technical problem of pressure-sensitive adhesive film, the invention provides a kind of method of adhesive rubber assembly, in this bonding system, combine and used neoprene-modified phenolic adhesive and acrylic pressure sensitive glued membrane.
Technical solution of the present invention:
A method for adhesive rubber assembly, its special character is: comprise the following steps:
1] rubber assembly surface is cleaned:
Use solvent to carry out clean to rubber assembly bonding plane;
2] rubber assembly after clean is carried out to surface treatment:
Use neoprene-phenol formaldehyde tackifier to infiltrate rubber assembly surface, and be placed to neoprene-phenol formaldehyde tackifier semicure, form neoprene-phenolic tacky film on rubber assembly surface;
3] adhesive rubber assembly:
3.1] pressure-sensitive adhesive film of acrylic acid or the like is bonded in by bonded assembly, forms the pressure-sensitive adhesive film of acrylic acid or the like on by bonded assembly;
3.2] by bonding the bonded assembly that infiltrated the rubber assembly of neoprene-phenol formaldehyde tackifier and the pressure-sensitive adhesive film of surface adhesion acrylic acid or the like, the pressure-sensitive adhesive film of acrylic acid or the like is bonded in neoprene-phenolic tacky film, add after the pressure of 2Kg~15Kg and wait for and solidifying.
Above-mentioned neoprene-phenol formaldehyde tackifier is neoprene-modified phenolic adhesive 801.
The pressure-sensitive adhesive film of aforesaid propylene acids is acrylic pressure sensitive glued membrane W-2174-CI or acrylic pressure sensitive glued membrane 9473.
The present invention has advantages of:
1, the method for adhesive rubber assembly provided by the present invention is easy to operate, quick, without using new tool, new installation.
2, method provided by the present invention has overcome curing type adhesive and in gluing assembling process, has occurred uncontrollable excessive glue and starved phenomenon, has eliminated the hidden danger of quality of product, improves the quality of product.
3, method provided by the present invention has overcome the bonding hypodynamic problem of pressure-sensitive adhesive film.
4, method bonding strength provided by the present invention is higher than using separately the bonding bonding strength of pressure-sensitive adhesive film.
5, the method bonding strength provided by the present invention is higher than the bonding bonding strength of curing type adhesive of independent neoprene-phenolic.
Accompanying drawing explanation
Fig. 1 is the schema of the method for adhesive rubber assembly of the present invention;
Fig. 2 be rubber assembly of the present invention with bonding by bonded assembly after structural representation;
Fig. 3 is the A-A schematic diagram of Fig. 2;
Wherein Reference numeral is: 1-rubber assembly, 2-is by bonded assembly, 3-neoprene-phenolic tacky film, the pressure-sensitive adhesive film of 4-acrylic acid or the like.
Embodiment
The adhering method of combined type rubber assembly of the present invention is mainly to combine to have used the curing type adhesive of neoprene-phenolic and the pressure-sensitive adhesive film adhesive rubber assembly of acrylic acid or the like, and as shown in Figure 1, operating process is as follows for its flow process:
First, rubber assembly is carried out to surface treatment, use solvent to carry out clean to rubber assembly bonding plane; Use neoprene-phenol formaldehyde tackifier to infiltrate rubber surface, be placed to surperficial semicure, form neoprene-phenol formaldehyde tackifier on rubber assembly surface and infiltrate rubber mucous membrane 3, this processes rear rubber surface and can improve, roughness reduces, glued membrane bond area improves, and the glue starved phenomenon of overflowing does not occur after semicure.
Then, use the pressure-sensitive adhesive film of acrylic acid or the like bonding, the pressure-sensitive adhesive film of acrylic acid or the like is bonded in by bonded assembly 2, again that the pressure-sensitive adhesive film of acrylic acid or the like 4 is bonding with the rubber assembly being infiltrated, rubber assembly 1 is bonded on the pressure-sensitive adhesive film 4 of acrylic acid or the like, adds after the pressure of 2Kg~15Kg and wait for and solidifying.
Embodiment:
Embodiment mono-: adhesive rubber plate on the aluminum component of electric conductive oxidation, tackiness agent is neoprene-modified phenolic adhesive 801 and acrylic pressure sensitive glued membrane 9473, its bonding strength is independent 2 times of using 801 glue after tested, is independent 4 times of using 9473 glued membranes, and the excessive glue starved phenomenon of the bonding rear nothing of product.
Embodiment bis-: adhesive rubber circle on the aluminum component of hard anodized, tackiness agent is neoprene-modified phenolic adhesive 801 and acrylic pressure sensitive glued membrane W-2174-CII, its bonding strength is independent 2 times of using 801 glue after tested, to use separately 4 times of W-2174-CII glued membrane, and the bonding rear nothing of the product glue starved phenomenon of overflowing.

Claims (3)

1. a method for adhesive rubber assembly, is characterized in that: comprise the following steps:
1] rubber assembly surface is cleaned:
Use solvent to carry out clean to rubber assembly bonding plane;
2] rubber assembly after clean is carried out to surface treatment:
Use neoprene-phenol formaldehyde tackifier to infiltrate rubber assembly surface, and be placed to neoprene-phenol formaldehyde tackifier semicure, form neoprene-phenolic tacky film on rubber assembly surface;
3] adhesive rubber assembly:
3.1] pressure-sensitive adhesive film of acrylic acid or the like is bonded in by bonded assembly, forms the pressure-sensitive adhesive film of acrylic acid or the like on by bonded assembly, described is metalwork by bonded assembly;
3.2] will infiltrate the rubber assembly of neoprene-phenol formaldehyde tackifier and the bonded assembly of surface adhesion is bonding, the pressure-sensitive adhesive film of acrylic acid or the like is bonded in neoprene-phenolic tacky film, and added after the pressure of 2Kg~15Kg and wait for and solidifying.
2. the method for adhesive rubber assembly according to claim 1, is characterized in that: described neoprene-phenol formaldehyde tackifier is neoprene-modified phenolic adhesive 801.
3. the method for adhesive rubber assembly according to claim 1 and 2, is characterized in that: the pressure-sensitive adhesive film of described acrylic acid or the like is acrylic pressure sensitive glued membrane W-2174-CI or acrylic pressure sensitive glued membrane 9473.
CN201210268920.2A 2012-07-30 2012-07-30 Method for bonding rubber component Active CN102757575B (en)