CN102709631A - 氮化铝陶瓷基板30瓦13dB衰减片 - Google Patents

氮化铝陶瓷基板30瓦13dB衰减片 Download PDF

Info

Publication number
CN102709631A
CN102709631A CN2012102158805A CN201210215880A CN102709631A CN 102709631 A CN102709631 A CN 102709631A CN 2012102158805 A CN2012102158805 A CN 2012102158805A CN 201210215880 A CN201210215880 A CN 201210215880A CN 102709631 A CN102709631 A CN 102709631A
Authority
CN
China
Prior art keywords
aluminium nitride
aluminum nitride
resistance
substrate
printed
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012102158805A
Other languages
English (en)
Inventor
陈建良
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou New Chengshi Electronic Co Ltd
Original Assignee
Suzhou New Chengshi Electronic Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou New Chengshi Electronic Co Ltd filed Critical Suzhou New Chengshi Electronic Co Ltd
Priority to CN2012102158805A priority Critical patent/CN102709631A/zh
Publication of CN102709631A publication Critical patent/CN102709631A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种氮化铝陶瓷基板30瓦13dB衰减片,是一种能量损耗性射频/微波元件,其包括一高导热氮化铝基板,所述氮化铝基板的背面印刷有背导层,所述氮化铝基板的正面印刷有导线,所述导线间印刷有3个膜状电阻,所述3个膜状电阻有两个电阻值相同,所述膜状电阻通过串并联电路对电信号起到衰减作用,通过控制所述膜状电阻的电阻值,得到需要的衰减值。该衰减片体积小,成本低,低插损,驻波比小,衰减精度高,频率使用范围广,与大规模集成电路生产工艺兼容,适合大批量生产。

Description

氮化铝陶瓷基板30瓦13dB衰减片
技术领域
本发明涉及一种氮化铝陶瓷基板衰减片,特别涉及一种氮化铝陶瓷基板30瓦13dB的衰减片。
背景技术
目前大多数通讯基站都是应用大功率陶瓷负载片来吸收通信部件中反向输入功率,大功率陶瓷负载片则只能单纯地消耗吸收多余的功率,而无法对基站的工作状况做实时的监控,当基站工作发生故障时无法及时地作出判断,对设备没有保护作用。集合了三种电阻设计的衰减片不但能在通信基站中可吸收通信部件中反向输入的功率并在高频电路上调整功率电平,去耦,对相关设备起到了保护作用。
由于氮化铝陶瓷仍然属于新兴行业,故在产品线上没有呈现多样化的格局。同时市场上存在的衰减片其衰减精度大多只能做到1G频率以内,少数能做到2G,且衰减精度和设备配备的VSWR较难控制。而市场对衰减精度的要求很高,我们希望的衰减器是一个功率消耗元件,不能对两端电路有影响,也就是说,与两端电路都是匹配的。当衰减精度或VSWR达不到要求时,输出端得到的信号不符合实际要求。目前市场上的衰减片当使用频段高于2G时,其衰减精度达不到要求,回波损耗变大,满足不了2G以上的频段应用要求。
发明内容
针对上述现有技术的不足,本发明要解决的技术问题是提供一种阻抗满足50±1.5Ω,在3G频段以内衰减精度为13±0.8dB,驻波要求输入端在1.2以内,输出端在1.25以内,能够满足目前3G网络的应用要求的氮化铝陶瓷基板30瓦13dB衰减片。
为解决上述技术问题,本发明采用如下技术方案:
一种氮化铝陶瓷基板30瓦13dB衰减片,其包括一高导热氮化铝基板,所述氮化铝基板的背面印刷有背导层,所述氮化铝基板的正面印刷有导线,所述导线间印刷有3个膜状电阻,所述3个膜状电阻有两个电阻值相同,所述膜状电阻通过串并联电路对电信号起到衰减作用,通过控制所述膜状电阻的电阻值,得到需要的衰减值。
优选的,所述衰减电路沿所述氮化铝基板的中心线对称。
优选的,所述电路采用5*5*1mm小尺寸的高导热氮化铝陶瓷基板。
上述技术方案具有如下有益效果:该氮化铝陶瓷基板30瓦13dB衰减片体积小,成本低,低插损,驻波比小,衰减精度高,频率使用范围广,与大规模集成电路生产工艺兼容,适合大批量生产可广泛应用于航空、航天、雷达、电台、广播通讯等设备领域隔离器、环形器等微波产品的生产。
上述说明仅是本发明技术方案的概述,为了能够更清楚了解本发明的技术手段,并可依照说明书的内容予以实施,以下以本发明的较佳实施例并配合附图详细说明如后。本发明的具体实施方式由以下实施例及其附图详细给出。
附图说明
图1为本发明实施例的结构示意图。
具体实施方式
下面结合附图对本发明的优选实施例进行详细介绍。
如图1所示,该氮化铝陶瓷基板30瓦13dB衰减片包括一5*5*1MM的氮化铝基板1,氮化铝基板1的背面印刷有背导层,氮化铝基板1的正面印刷有导线2及电阻R1、R2、R3,电阻R1、R2、R3通过导线连接形成衰减电路,衰减电路通过银浆与背导层电连接,从而使衰减电路接地导通。该衰减电路沿氮化铝基板的中心线对称,衰减电路的输出端与一焊盘5连接,输入端与一焊盘6连接,两个焊盘5、6沿氮化铝基板的中心线对称。电阻R1、R2、R3上印刷有玻璃保护膜3,导线2及玻璃保护膜3的上表面还印刷有一层黑色保护膜4,这样可对导线2及电阻R1、R2、R3形成保护。
该氮化铝陶瓷基板30瓦13dB衰减片要求输入端和接地的阻抗为50±1.5Ω,输出端和接地端的阻抗为50±1.5Ω。信号输入端进入衰减片,经过电阻R1、R3、R2对功率的逐步吸收,从输出端输出实际所需要的信号,
该氮化铝陶瓷基板30瓦13dB衰减片体积小,成本低,低插损,驻波比小,衰减精度高,频率使用范围广,与大规模集成电路生产工艺兼容,适合大批量生产可广泛应用于航空、航天、雷达、电台、广播通讯等设备领域隔离器、环形器等微波产品的生产。
以上对本发明实施例所提供的一种氮化铝陶瓷基板30瓦13dB衰减片进行了详细介绍,对于本领域的一般技术人员,依据本发明实施例的思想,在具体实施方式及应用范围上均会有改变之处,综上所述,本说明书内容不应理解为对本发明的限制,凡依本发明设计思想所做的任何改变都在本发明的保护范围之内。

Claims (3)

1.一种氮化铝陶瓷基板30瓦13dB衰减片,其特征在于:其包括一高导热氮化铝基板,所述氮化铝基板的背面印刷有背导层,所述氮化铝基板的正面印刷有导线,所述导线间印刷有3个膜状电阻,所述3个膜状电阻有两个电阻值相同,所述膜状电阻通过串并联电路对电信号起到衰减作用,通过控制所述膜状电阻的电阻值,得到需要的衰减值。
2.根据权利要求1所述的氮化铝陶瓷基板30瓦13dB衰减片,其特征在于:所述衰减电路沿所述氮化铝基板的中心线对称。
3.根据权利要求1所述的氮化铝陶瓷基板30瓦13dB衰减片,其特征在于:所述电路采用5*5*1mm小尺寸的高导热氮化铝陶瓷基板。
CN2012102158805A 2012-06-28 2012-06-28 氮化铝陶瓷基板30瓦13dB衰减片 Pending CN102709631A (zh)