CN102698939A - Leveling method for sealant of electric porcelain electrical appliance - Google Patents
Leveling method for sealant of electric porcelain electrical appliance Download PDFInfo
- Publication number
- CN102698939A CN102698939A CN2012101799050A CN201210179905A CN102698939A CN 102698939 A CN102698939 A CN 102698939A CN 2012101799050 A CN2012101799050 A CN 2012101799050A CN 201210179905 A CN201210179905 A CN 201210179905A CN 102698939 A CN102698939 A CN 102698939A
- Authority
- CN
- China
- Prior art keywords
- fluid sealant
- potato
- sealant
- floating
- softening
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to the technical field of high-voltage electric porcelain, in particular to a leveling method for a sealant of an electric porcelain electrical appliance. The leveling method comprises the following steps of: a. cutting potatoes into slices; b. softening potato slices in the step a for standby application; and c. leveling the surface of the sealant by using the softened potato slices. The leveling method for the sealant of the electric porcelain electrical appliance has the advantages of good leveling effect, simple construction and low cost.
Description
Technical field
The present invention relates to the high tension insulator production technical field, specifically establish the flatening method that relates to a kind of electroceramics electrical equipment fluid sealant.
Background technology
Electroceramics electrical equipment need be smeared fluid sealant, for example installed part junction of the junction of the flange of insulator and porcelain body, electrical equipment etc. in order to reach water-tight, insulation, requirement such as smooth at some positions.Irregular phenomenons such as glue tuft after smearing, electroceramics electrical equipment fluid sealant are arranged; In the prior art; In order to make its surfacing; The technical scheme that adopts: have plenty of that Polypropylence Sheet with gloves floating, the employing that has be floating with criticizing cutter, these methods all have easy adhesion, can not effectively guarantee to smear shortcomings such as smooth, that effect is not satisfactory.
Summary of the invention
The object of the invention is exactly to above-mentioned shortcoming, and a kind of flatening method of floating effective, the simple electroceramics electrical equipment fluid sealant of construction is provided.
Technical scheme of the present invention is achieved in that the flatening method of electroceramics electrical equipment fluid sealant, may further comprise the steps: a, potato is thinly sliced; B, the potato chips among the method a is softening subsequent use; The surface of the floating fluid sealant in plane of the potato chips that c, usefulness are softened gets final product.
The invention has the beneficial effects as follows: the floating electroceramics electrical equipment of such method fluid sealant has floating effective, the advantage simple, that cost is low of constructing.
The specific embodiment
Below in conjunction with embodiment the present invention is done further description.
Embodiment 1
A, the fresh potato of buying on the market is cut into the thin slice of 2 millimeters thick; B, with the potato thin slice among the method a in 45 degree water 2 minutes softening, take out in the warm water that is placed on 20 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating process is completion in smearing fluid sealant 10 minutes.
The aforesaid operations effect has good, the simple to operate effect of surface smoothness.
Embodiment 2
A, the fresh potato of buying on the market is cut into the thin slice of 3 millimeters thick; B, with the potato thin slice among the method a in 55 degree water 1.5 minutes softening, take out in the warm water that is placed on 25 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating process is completion in smearing fluid sealant 5 minutes.
The aforesaid operations effect has good, the simple to operate effect of surface smoothness.
Embodiment 3
A, the fresh potato of buying on the market is cut into the thin slice of 3.3 millimeters thick; B, with the potato thin slice among the method a 25 degree, contain in 10% saline solution 10 minutes softening, take out in the warm water that is placed on 25 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating process is completion in smearing fluid sealant 20 minutes.
The aforesaid operations effect has good, the simple to operate effect of surface smoothness.
Embodiment 4
A, the fresh potato of buying on the market is cut into the thin slice of 2.8 millimeters thick; B, with the potato thin slice among the method a 25 degree, contain in 8% saline solution 15 minutes softening, take out in the warm water that is placed on 22 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating process is completion in smearing fluid sealant 7 minutes.
The aforesaid operations effect has good, the simple to operate effect of surface smoothness.
Embodiment 5
A, the fresh potato of buying on the market is cut into the thin slice of 3.5 millimeters thick; The airing under the situation of temperature 25 degree, humidity 80% of potato thin slice among the method a was softened in 1 hour, take out in the warm water that is placed on 25 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating is completion in smearing fluid sealant 15 minutes.
The aforesaid operations effect has good, the simple to operate effect of surface smoothness.
Embodiment 6
A, the fresh potato of buying on the market is cut into the thin slice of 2.5 millimeters thick; The airing under the situation of temperature 30 degree, humidity 85% of potato thin slice among the method a was softened in 2 hours, take out in the warm water that is placed on 22 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating is completion in smearing fluid sealant 12 minutes.
The aforesaid operations effect has good, the simple to operate effect of surface smoothness.
Above potato chips can repeatedly use.
Embodiment 7
A, the fresh potato of buying on the market is cut into the thin slice of 5 millimeters thick; The airing under the situation of temperature 30 degree, humidity 85% of potato thin slice among the method a was softened in 2 hours, take out in the warm water that is placed on 22 degree subsequent use; C, get final product with the surface of the floating fluid sealant in plane of softening potato chips, floating is completion in smearing fluid sealant 35 minutes.
The aforesaid operations effect has the relatively poor shortcoming of surface smoothness.This is because potato chips is too thick, lacks softly, and the gluing overlong time has solidification phenomenon in addition, influence leveling effect.
More than used electroceramics electrical equipment fluid sealant be the product of Jiangyin City long-range auxiliary agent Co., Ltd, use Shenzhen pure prosperous silicon rubber Co., Ltd instead and have same technique effect.
Potato has alkalescent, also contains starch, and potato chips and fluid sealant are not stained with knot, uses potato chips to have above technique effect.
Claims (4)
1. the flatening method of electroceramics electrical equipment fluid sealant may further comprise the steps: a, potato is thinly sliced; B, the potato chips among the method a is softening subsequent use; The surface of the floating fluid sealant in plane of the potato chips that c, usefulness are softened gets final product.
2. flatening method according to claim 1 is characterized in that: the thickness of described potato thin slice is the 2-3.5 millimeter.
3. flatening method according to claim 1 is characterized in that: described softening is to place in airing, saline sook or the warm water.
4. according to claim 1,2 or 3 described flatening methods, it is characterized in that floating process will be smeared in back 20 minutes at fluid sealant to accomplish.