CN102654429A - 高强度铝合金复杂孔系集成板的气密性检验方法 - Google Patents
高强度铝合金复杂孔系集成板的气密性检验方法 Download PDFInfo
- Publication number
- CN102654429A CN102654429A CN2011100517137A CN201110051713A CN102654429A CN 102654429 A CN102654429 A CN 102654429A CN 2011100517137 A CN2011100517137 A CN 2011100517137A CN 201110051713 A CN201110051713 A CN 201110051713A CN 102654429 A CN102654429 A CN 102654429A
- Authority
- CN
- China
- Prior art keywords
- aluminum alloy
- strength aluminum
- test method
- sealing
- integrated plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种高强度铝合金复杂孔系集成板的气密性检验方法,适用于金属内部复杂孔系集成板气密性的检验,属于流体密封检测技术。本发明按系集成板尺寸确定上下模板的尺寸,且制作封闭面四周,从而制成测试模。把测试模淹入水中打开冲气阀开关,当压力表达到15公斤时关气,观察压力表变化。从压力表的变化检测到集成板是否合格。本发明具有设备投入低,测试方法简单、迅速,便于大批量检测等优点。
Description
技术领域
本发明涉及一种高强度铝合金复杂孔系集成板的气密性检验方法,适用于金属内部复杂孔系集成板气密性的检验,属于流体密封检测技术。
背景技术
由于经济及技术的飞速发展,采用先进气动控制的行业及设备越来越多。大量高强度铝合金复杂孔系集成极需要科学有效的检测手段。特别是金属内部设有的大量气路且与外部相连接的集成式组合件,其密封性关系到工作设备的安全和正常工作的问题。
发明内容
本发明的目的在于提供一种高强度铝合金复杂孔系集成板的气密性检验方法。它能有效地检测出气路板的密封性。
为了实现上述目的,本发明采用技术方案包括:
1、按高强度铝合金复杂孔系集成板尺寸确定上下模板的尺寸,上模加工进气口,四周每隔30毫米,加工锁紧螺孔,
2、根据不同的高强度铝合金复杂孔系集成板外形制作封闭面四周厚度>3毫米、宽约50毫米密封垫,如果边缘50毫米内遇到气孔,去除密封条堵塞部分,
3、用密封螺堵塞住高强度铝合金复杂孔系集成板四周边的气孔,
4、下模面按高强度铝合金复杂孔系集成板外形设置密封垫,放上工件,在工件上放上密封垫,再放上模。锁紧测试模四周螺丝,
5、把测试模淹入水中打开冲气阀开关,当压力表达到15公斤时关气,观察压力表变化。
本发明具有设备投入低,测试方法简单、迅速,便于大批量检测等优点。
具体实施方式
根据集成板尺寸确定上下模板的尺寸,如长为27cm、宽为25cm、厚为2.5cm的高强度铝合金复杂孔系集成板,制作出对应尺寸的上、下模,即锁紧测试模。且在上模上加工进气口,四周每隔30毫米,加工锁紧螺孔,再制作封闭面四周厚度>3毫米、宽约50毫米密封垫,然后去除密封条堵塞部分,密封螺堵塞四周边的气孔,在下模面设置密封垫,在密封垫上设置放上工件,工件上方放上置上模面,且在上模面与工件之间设置密封垫,锁紧测试模四周螺丝。把测试模淹入水中打开冲气阀开关,当压力表达到15公斤时关气,观察压力表变化。按照上述方法,一般情况下(客户或设计另有要求除外)如果压力表半小时之内平稳不动,则高强度铝合金复杂孔系集成板气密性、功能性达到要求。如果压力表有较大变化,则首先应检查测试模的密封性,排除该问题后,若压力表仍有较大变化则该高强度铝合金复杂孔系集成板不合格。
Claims (1)
1.一种高强度铝合金复杂孔系集成板的气密性检验方法,其特征在于
(1)、按高强度铝合金复杂孔系集成板尺寸确定上下模板的尺寸,上模加工进气口,四周每隔30毫米,加工锁紧螺孔,
(2)、根据不同的高强度铝合金复杂孔系集成板外形制作封闭面四周厚度>3毫米、宽约50毫米密封垫,如果边缘50毫米内遇到气孔,去除密封条堵塞部分,
(3)、用密封螺堵塞住高强度铝合金复杂孔系集成板四周边的气孔,
(4)、下模面按高强度铝合金复杂孔系集成板外形设置密封垫,放上工件,在工件上放上密封垫,再放上模。锁紧测试模四周螺丝,
(5)、把测试模淹入水中打开冲气阀开关,当压力表达到15公斤时关气,观察压力表变化。