CN102587199B - Wallpaper paint and manufacturing method thereof - Google Patents

Wallpaper paint and manufacturing method thereof Download PDF

Info

Publication number
CN102587199B
CN102587199B CN201210008322.1A CN201210008322A CN102587199B CN 102587199 B CN102587199 B CN 102587199B CN 201210008322 A CN201210008322 A CN 201210008322A CN 102587199 B CN102587199 B CN 102587199B
Authority
CN
China
Prior art keywords
parts
paint
calculating
wallpaper
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201210008322.1A
Other languages
Chinese (zh)
Other versions
CN102587199A (en
Inventor
胡学强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201210008322.1A priority Critical patent/CN102587199B/en
Publication of CN102587199A publication Critical patent/CN102587199A/en
Application granted granted Critical
Publication of CN102587199B publication Critical patent/CN102587199B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses wallpaper paint and a manufacturing method thereof. The wallpaper paint comprises the following components in part by weight: 300 parts of base paint, 18 parts of film formation aid, 177 parts of water, 1 part of fungicide, 10 parts of propylene glycol, 1 part of antifoaming agent, 1.5 parts of alkali swelling association thickener and 500 parts of color particles. By the invention, the problem of poor adhesion effect of the wallpaper paint is effectively solved, chromatic aberration is relatively avoided after spraying operation is finished, a texture effect of the wallpaper paint is fully achieved, and preferable proportion is obtained. By adoption of the manufacturing method, compared with the like products, the wallpaper paint is higher in adhesion and longer in adhesion life.

Description

A kind of wallpaper paint and manufacture method thereof
Technical field
The present invention relates to a kind of wallpaper paint and manufacture method thereof.
Background technology
Wallpaper paint is as a kind of artistic decoration coating, and the color that overcome emulsion paint is single, easy to change without stereovision and wallpaper, alice, bubble, have seam, short problem of life-span, because decorative effect is well favored by consumer.But current wallpaper paint exists the poor problem of adhesiving effect, to such an extent as to that spraying operation completes the pattern adhesion time that back wall surface forms is short, not washability.
Summary of the invention
The technical problem to be solved in the present invention is to provide a kind of wallpaper paint and manufacture method thereof, can effectively solve the poor problem of adhesiving effect that wallpaper paint exists.
For solving the problems of the technologies described above, the technical solution used in the present invention is that described a kind of wallpaper paint comprises the following component of calculating with weight ratio: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle.Wallpaper paint is imitated strong sense of reality, and relative no color differnece after spraying operation completes fully shows wallpaper paint texture effect, and more excellent proportion scale has obtained compared with the better adhesiveness of like product the present invention, adheres to the life-span longer.
As a kind of improvement, described base paint comprises the component of calculating with weight ratio as follows: 427 parts of water, 5 parts of ammonium salt dispersants, 1 part of defoamer, 1 part of bactericide, 12 parts of pearl essences, 5 parts of crosslinking agents, 5 parts of hydroxyethylcelluloses, 280 parts of elastic emulsions, 20 parts of propylene glycol, 2 parts of thick slurry defoamers, 3 parts of anionic wetting agents, 1.5 parts of alkali swelling associative thickeners and 120 parts of colloidal solution.More excellent proportioning, base paint dissolves better effects if.
As a kind of improvement, described colored particle comprises the component of calculating with weight ratio as follows: 100 parts of colloidal solution, 200 parts of colored paints.Add colored paint, strengthen the storage stability of coating.
As a kind of improvement; described colloidal solution comprises following percentage by weight component: described colloidal solution comprises the following component of calculating by weight percentage: water 90.5%-92.5%; HG-1 protection rubber powder 5%-7.5%, setting agent 0.2%-0.3%, crosslinked stabilizing agent 2%-3%.
The present invention also provides a kind of method of manufacturing above-mentioned wallpaper paint, and a kind of described method of manufacturing wallpaper paint comprises the following steps: 1) prepare colloidal solution, 2) prepare base paint, 3) granulation son, 4) prepare finished product paint.
As a kind of improvement; the described colloidal solution step of preparing is: to adding the following component of calculating by weight percentage in container: water 90.5%-92.5%; water is stirred and slowly adds HG-1 protection rubber powder 5%-7.5% simultaneously; then add setting agent 0.2%-0.3% and crosslinked stabilizing agent 2%-3% to form mixed solution I; mixed solution I is disperseed; paint granule is done again to the technique that dispersion and fining is processed; first low speed disperses 10-15 minute; then high speed dispersion 10-20 minute, makes colloidal solution.
As a kind of improvement, the described base paint step of preparing is: first in backward container, add the component of calculating with weight ratio as follows: 427 parts of water, 5 parts of ammonium salt dispersants, 1 part of defoamer, 1 part of bactericide, 120 parts of pearl essences form mixed solution I I, then described mixed solution I I high speed dispersion 25-35 minute to its solution fineness is reached to 35UM, then in container, add crosslinking agent, disperse in backward container, to add hydroxyethylcellulose in five minutes, adjust pH value to 8-9, then in container, add elastic emulsion, propylene glycol and thick slurry defoamer, then in container, add anion wetting agent to stir 3-5 minute, slowly after adding colloidal solution to stir in container, fill into again anion wetting agent, then add for adjusting the alkali swelling associative thickener of solution concentration, then base paint is made in discharging, described crosslinking agent, hydroxyethylcellulose, elastic emulsion, propylene glycol, magma defoamer, anionic wetting agent, colloid emulsion, the weight ratio of alkali swelling associative thickener is 5, 5, 280, 20, 2, 6, 120, 1.5, wherein add for the first time the weight of anion wetting agent and fill into being for the second time equal in weight of anion wetting agent, improved technique, dissolve better effects if.
As a kind of improvement, described granulation refers to the colored paint for preparing to import in colloidal solution, rinses respectively that net, 20 orders are rinsed net, 30 orders are rinsed net and are evenly cut into colored particle according to particle size by 10 orders.Paint particle refinement is even, and color is more well-balanced; Colored paint increases working viscosity, and adhesion effect is better.
As a kind of improvement; the described finished product paint step of preparing is for successively adding container by the following component of calculating by weight percentage: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle are mixed into mixed solution I II; described mixed solution I II stirring at low speed is adjusted to its solution viscosity to 80-85KU, then finished product paint is made in discharging simultaneously.Finished product paint adhesion effect is better.
The present invention adopts above-mentioned formula and manufacturing technique, its beneficial effect is: efficiently solve the poor problem of wallpaper paint adhesiving effect, relative no color differnece after spraying operation completes, fully show wallpaper paint texture effect, more excellent proportion scale, coordinate the manufacture method adopting in the present invention that the present invention has been obtained compared with the better adhesiveness of like product, adhere to the life-span longer.
The specific embodiment
In the present embodiment, described a kind of wallpaper paint, comprises the component of following weight ratio: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle.
In the present embodiment, described base paint comprises the component of calculating with weight ratio as follows: 427 parts of water, 5 parts of ammonium salt dispersants, 1 part of defoamer, 1 part of bactericide, 12 parts of pearl essences, 5 parts of crosslinking agents, 5 parts of hydroxyethylcelluloses, 280 parts of elastic emulsions, 20 parts of propylene glycol, 2 parts of thick slurry defoamers, 3 parts of anionic wetting agents, 1.5 parts of alkali swelling associative thickeners and 120 parts of colloidal solution, each component of described base paint must add successively by listed order.Described colored particle comprises the component of calculating with weight ratio as follows: 100 parts of colloidal solution, and 200 parts of colored paints, colored paint is given and being filmed with color, and can stop that light sees through, and strengthens mechanical performance and the chemical property of filming.Described colloidal solution comprises the following component of calculating by weight percentage: water 90.5%-92.5%, HG-1 protection rubber powder 5%-7.5%, setting agent 0.2%-0.3%, crosslinked stabilizing agent 2%-3%.
The present embodiment also comprises a kind of method of manufacturing above-mentioned wallpaper paint, a kind of described method of manufacturing wallpaper paint comprises the following steps: 1) prepare colloidal solution, 2) prepare base paint, 3) granulation, 4) prepare finished product paint, step 2 wherein) and step 3) order can carry out simultaneously, or hocket, step 1) and step 4) sequencing is constant.
In the present embodiment; the described colloidal solution step of preparing is: to adding the following component of calculating by weight percentage in container: water 90.5%-92.5%; water is stirred and slowly adds HG-1 protection rubber powder 5%-7.5% simultaneously; then add setting agent 0.2%-0.3% and crosslinked stabilizing agent 2%-3% to form mixed solution I; mixed solution I is disperseed; paint granule is done again to dispersion and fining to be processed; first low speed disperses 10-15 minute; then high speed dispersion 10-20 minute, makes colloidal solution.The described base paint step of preparing is: first in backward container, add the component of calculating with weight ratio as follows: 427 parts of water, 5 parts of ammonium salt dispersants, 1 part of defoamer, 1 part of bactericide, 120 parts of pearl essences form mixed solution I I, then described mixed solution I I high speed dispersion 25-35 minute to its solution fineness is reached to 35UM, then in container, add crosslinking agent, disperse in backward container, to add hydroxyethylcellulose in five minutes, adjust pH value to 8-9, then in container, add elastic emulsion, propylene glycol and thick slurry defoamer, then in container, add anion wetting agent to stir 3-5 minute, slowly after adding colloidal solution to stir in container, fill into again anion wetting agent, then add for adjusting the alkali swelling associative thickener of solution concentration, then base paint is made in discharging, described crosslinking agent, hydroxyethylcellulose, elastic emulsion, propylene glycol, magma defoamer, anionic wetting agent, colloid emulsion, the weight ratio of alkali swelling associative thickener is 5, 5, 280, 20, 2, 6, 120, 1.5, wherein add for the first time the weight of anion wetting agent and fill into being for the second time equal in weight of anion wetting agent.Described granulation refers to the colored paint for preparing to import in colloidal solution, rinses respectively that net, 20 orders are rinsed net, 30 orders are rinsed net and are evenly cut into colored particle according to particle size by 10 orders.The described finished product paint step of preparing is for successively adding container by the following component of calculating by weight percentage: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle are mixed into mixed solution I II; described mixed solution I II stirring at low speed is adjusted to its solution viscosity to 80-85KU simultaneously; then finished product paint is made in discharging; more excellent material selection and proportioning process, make that finished product paint dissolves better effects if, adhesiveness is better.
Except above preferred embodiment, the present invention also has other embodiment, and those skilled in the art can make according to the present invention various changes and distortion, only otherwise depart from spirit of the present invention, all should belong to the defined scope of claims of the present invention.

Claims (6)

1. a wallpaper paint, it is characterized in that: comprise the following component of calculating with weight ratio: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle, described base paint comprises the component of calculating with weight ratio as follows: 427 parts of water, 5 parts of ammonium salt dispersants, 1 part of defoamer, 1 part of bactericide, 12 parts of pearl essences, 5 parts of crosslinking agents, 5 parts of hydroxyethylcelluloses, 280 parts of elastic emulsions, 20 parts of propylene glycol, 2 parts of thick slurry defoamers, 3 parts of anionic wetting agents, 1.5 parts of alkali swelling associative thickeners and 120 parts of colloidal solution.
2. a wallpaper paint, it is characterized in that: comprise the following component of calculating with weight ratio: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle, described colored particle comprises the component of calculating with weight ratio as follows: 100 parts of colloidal solution, 200 parts of colored paints.
3. a kind of wallpaper paint according to claim 1 and 2, is characterized in that: described colloidal solution comprises the following component of calculating by weight percentage: water 90.5%-92.5%, HG-1 protection rubber powder 5%-7.5%, setting agent 0.2%-0.3%, crosslinked stabilizing agent 2%-3%.
4. a method of manufacturing a kind of wallpaper paint described in claim 1 or 2, it is characterized in that: comprise the following steps: 1) prepare colloidal solution, 2) prepare base paint, 3) granulation, 4) prepare finished product paint, the described colloidal solution step of preparing is: to adding the following component of calculating by weight percentage in container: water 90.5%-92.5%, water is stirred and slowly adds HG-1 protection rubber powder 5%-7.5% simultaneously, then add setting agent 0.2%-0.3% and crosslinked stabilizing agent 2%-3% to form mixed solution I, mixed solution I is disperseed, first low speed disperses 10-15 minute, then high speed dispersion 10-20 minute, make colloidal solution.
5. the manufacture method of a kind of wallpaper paint according to claim 4, it is characterized in that: described granulation refers to the colored paint for preparing to import in colloidal solution, according to particle size, by 10 orders, rinse respectively that net, 20 orders are rinsed net, 30 orders are rinsed net and are evenly cut into colored particle.
6. the manufacture method of a kind of wallpaper paint according to claim 4; it is characterized in that: the described finished product paint step of preparing is for successively adding container by the following component of calculating by weight percentage: 300 parts of base paints, 18 parts of coalescents, 177 parts of water, 1 part of bactericide, 10 parts of propylene glycol, 1 part of defoamer, 1.5 parts of alkali swelling association thickeners and 500 parts of colored particle are mixed into mixed solution I II; described mixed solution I II stirring at low speed is adjusted to its solution viscosity to 80-85KU, then finished product paint is made in discharging simultaneously.
CN201210008322.1A 2012-01-12 2012-01-12 Wallpaper paint and manufacturing method thereof Expired - Fee Related CN102587199B (en)