CN102537541A - 一种圆管骨架式大口径波纹管及制作方法 - Google Patents

一种圆管骨架式大口径波纹管及制作方法 Download PDF

Info

Publication number
CN102537541A
CN102537541A CN2012100040546A CN201210004054A CN102537541A CN 102537541 A CN102537541 A CN 102537541A CN 2012100040546 A CN2012100040546 A CN 2012100040546A CN 201210004054 A CN201210004054 A CN 201210004054A CN 102537541 A CN102537541 A CN 102537541A
Authority
CN
China
Prior art keywords
pipe
wall
bellows
heavy caliber
fomale
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012100040546A
Other languages
English (en)
Inventor
施经东
洪建坤
谈刚强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHEJIANG SHUANGLIN ELECTROMECHANICAL TECHNOLOGY Co Ltd
Original Assignee
ZHEJIANG SHUANGLIN ELECTROMECHANICAL TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHEJIANG SHUANGLIN ELECTROMECHANICAL TECHNOLOGY Co Ltd filed Critical ZHEJIANG SHUANGLIN ELECTROMECHANICAL TECHNOLOGY Co Ltd
Priority to CN2012100040546A priority Critical patent/CN102537541A/zh
Publication of CN102537541A publication Critical patent/CN102537541A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种不仅能有效地提高大口径波纹管强度,而且能使大口径波纹管的弹性得到根本性提高的一种圆管骨架式大口径波纹管及制作方法,它包括内管,螺旋缠绕在内管管身上的圆管内外壁面呈凹凸状结构,塑料层复合在圆管内壁上,或外壁上,或内壁和外壁上,且与内壁或外壁或内壁和外壁呈凹凸不平的非纯平面结合。优点:一是金属圆管犹如拱形桥结构,不仅承载力大、抗压,而且极大提高了内管的支撑强度和承压能力;二是圆管面为凹凸结构,就犹如塑料层有了塑料楔,形成的是塑料层与圆管壁间楔嵌复合,复合强度高,不会发生分层现象。

Description

一种圆管骨架式大口径波纹管及制作方法
技术领域
本发明涉及一种不仅能有效地提高大口径波纹管强度,而且能使大口径波纹管的弹性得到根本性提高的一种圆管骨架式大口径波纹管及制作方法,属波纹管制造领域。
背景技术
CN201078525Y、名称“承插电熔连接式钢带增强聚乙烯螺旋波纹管”, 其用于解决钢带增强聚乙烯螺旋波纹管连接接口容易渗漏和可靠性差的问题。承插电熔连接式钢带增强聚乙烯螺旋波纹管,是用外层聚乙烯将缠绕的金属骨架固定在内层聚乙烯上,特别是波纹管的一端设有插口,波纹管的另一端设有承口,承口内壁上埋入一圈电热元件组成。采用这种承插电熔连接式钢带增强聚乙烯螺旋波纹管,可广泛地应用于塑料管材的连接施工。其不足之处:一是金属骨架呈外扒结构,与内层聚乙烯形成的是线面接触,而不是面接触,不仅复合性差,而且在外力的作用下,金属骨架易外扒移动,造成对内层聚乙烯破坏,直接影管质的质量,甚至造成内层聚乙烯破损;二是支撑强度低,由于金属骨架呈外扒结构,外压其金属骨架两侧向外移动,不仅造成金属骨架与内层聚乙烯的分层,而且导致内层聚乙烯强度的直接降低;三是由于外层聚乙烯与金属骨架系两种不同的材料,受温度的影响其热胀冷缩的系数各不相同,因此在使用中不可避免地发生分层现象,导致波纹管强度急剧下降,波纹管坍塌。
发明内容
设计目的:避免背景技术中的不足之处,设计一种不仅能有效地提高大口径波纹管强度,而且能使大口径波纹管的弹性得到根本性提高的一种圆管骨架式大口径波纹管及制作方法。
设计方案:为了实现上述设计目的。螺旋缠绕在内管管身上的圆管内外壁面呈凹凸状结构的设计,是本发明的主要技术特征。这样做的目的在于:圆管的壁面凹凸状结构中的凸起和凹进,犹如加强筋,既提高了圆管壁的强度,又使熔融塑料与圆管壁面的粘接更粘固,更重要的是这些凹凸面,相互制约了温度变化时伸缩系数,使其更适应于塑料层的温度变化,从而有效地避免了分层现象的出现。
技术方案1:一种圆管骨架式大口径波纹管,它包括内管,螺旋缠绕在内管管身上的圆管内外壁面呈凹凸状结构,塑料层复合在圆管内壁上,或外壁上,或内壁和外壁上,且与内壁或外壁或内壁和外壁呈凹凸不平的非纯平面结合。
技术方案2:一种圆管骨架式大口径波纹管的制作方法,将非纯平面钢带通滚压设备中的凹凸模,挤压成凹凸面,然通过卷管机将凹凸面的钢带卷成圆管,对圆管表面进行洁净处理后,采用申请人所制造的大口径聚烯烃缠绕增长管生产线在制作波纹管内管过程中,一边制作波纹管内管、一边将内外壁面呈凹凸面的圆管缠绕在波纹管上且采用申请人所制造的大口径聚烯烃缠绕增长管生产线将熔融塑料复合在凹凸面的圆管壁上。
本发明与背景技术相比,一是金属圆管犹如拱形桥结构,不仅承载力大、抗压,而且极大提高了内管的支撑强度和承压能力;二是圆管面为凹凸结构,就犹如塑料层有了塑料楔,形成的是塑料层与圆管壁间楔嵌复合,复合强度高,不会发生分层现象。
附图说明
图1是圆管骨架式大口径波纹管的结构示意图。
图2是图1中圆管内外壁复塑料层的截面结构示意图。
图3是图1中圆管外壁复塑料层的截面结构示意图。
图4是图1中圆管内壁复塑料层的截面结构示意图。
具体实施方式
实施例1:参照附图1-2。一种圆管骨架式大口径波纹管,它包括内管1,螺旋缠绕在内管1管身上的圆管2内外壁面呈凹凸状结构,塑料层3复合在圆管2内壁、塑料层4复合在圆管2外壁上且与内壁或外壁或内壁和外壁呈凹凸不平的非纯平面结合。所述凹凸状结构的圆管2内外壁的面为非纯平面,目的提高两者之间的粘接力。
实施例2:参照附图1和3。在实施例1的基础上,塑料层4复合在圆管2外壁上。
实施例3:参照附图1和4。在实施例1的基础上,塑料层3复合在圆管2内壁上。
实施例4:在实施例1-3的基础上,一种圆管骨架式大口径波纹管的制作方法,将非纯平面钢带通滚压设备中的凹凸模,挤压成凹凸面,然通过卷管机将凹凸面的钢带卷成圆管,对圆管表面进行洁净处理后,采用申请人所制造的大口径聚烯烃缠绕增长管生产线在制作波纹管内管过程中,一边制作波纹管内管、一边将内外壁面呈凹凸面的圆管缠绕在波纹管上且采用申请人所制造的大口径聚烯烃缠绕增长管生产线将熔融塑料复合在凹凸面的圆管壁上。将熔融塑料复合在凹凸面的圆管的内壁上或外壁上或内壁和外壁上。
需要理解到的是:上述虽然对本发明的设计思路作了比较详细的文字描述,但是这些文字描述,只是对本发明设计思路的简单文字描述,而不是对本发明设计思路的限制,任柯不超过本发明设计思路的组合,增加和修改,均落入本发明的保护范围内。

Claims (4)

1.一种圆管骨架式大口径波纹管,它包括内管,其特征是:螺旋缠绕在内管管身上的圆管内外壁面呈凹凸状结构,塑料层复合在圆管内壁上,或外壁上,或内壁和外壁上,且与内壁或外壁或内壁和外壁呈凹凸不平的非纯平面结合。
2.根据权利要求1所述的圆管骨架式大口径波纹管,其特征是:所述凹凸状结构的圆管内外壁的面为非纯平面。
3.一种圆管骨架式大口径波纹管的制作方法,其特征是:将非纯平面钢带通滚压设备中的凹凸模,挤压成凹凸面,然通过卷管机将凹凸面的钢带卷成圆管,对圆管表面进行洁净处理后,采用申请人所制造的大口径聚烯烃缠绕增长管生产线在制作波纹管内管过程中,一边制作波纹管内管、一边将内外壁面呈凹凸面的圆管缠绕在波纹管上且采用申请人所制造的大口径聚烯烃缠绕增长管生产线将熔融塑料复合在凹凸面的圆管壁上。
4.根据权利要求3所述的圆管骨架式大口径波纹管的制作方法,其特征是:将熔融塑料复合在凹凸面的圆管的内壁上或外壁上或内壁和外壁上。
CN2012100040546A 2012-01-09 2012-01-09 一种圆管骨架式大口径波纹管及制作方法 Pending CN102537541A (zh)