CN102505446A - Formaldehyde-free suit fabric - Google Patents

Formaldehyde-free suit fabric Download PDF

Info

Publication number
CN102505446A
CN102505446A CN201110333931XA CN201110333931A CN102505446A CN 102505446 A CN102505446 A CN 102505446A CN 201110333931X A CN201110333931X A CN 201110333931XA CN 201110333931 A CN201110333931 A CN 201110333931A CN 102505446 A CN102505446 A CN 102505446A
Authority
CN
China
Prior art keywords
dyeing
formaldehyde
free
finishing
formaldehydeless
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201110333931XA
Other languages
Chinese (zh)
Inventor
王养飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG KE'ER TEXTILE AND GARMENTS CO Ltd
Original Assignee
NANTONG KE'ER TEXTILE AND GARMENTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG KE'ER TEXTILE AND GARMENTS CO Ltd filed Critical NANTONG KE'ER TEXTILE AND GARMENTS CO Ltd
Priority to CN201110333931XA priority Critical patent/CN102505446A/en
Publication of CN102505446A publication Critical patent/CN102505446A/en
Pending legal-status Critical Current

Abstract

The invention discloses formaldehyde-free suit fabric. The manufacture technology of the suit fabric comprises a dyeing process and a finishing process. The dyeing process includes steps of oxygen bleaching, liquid wax coating and package yarn drying. The finishing process includes steps of desizing and washing. In the dyeing process, hot water at the temperature ranging from 75 to 85 DEG C is added after oxygen bleaching to wash the fabric for 15 to 25 minutes, hot water at the temperature ranging from 60 to 70 DEG C is added before liquid wax coating to wash the fabric for 15 to 25 minutes, and temperature of the package yarn drying ranges from 110 to 120 DEG C. After desizing, spraying water temperature of each washing tank is controlled to range from 55 to 65 DEG C, and cloth feeding speed ranges from 55 to 65 m/minute. The formaldehyde-free suit fabric is free of formaldehyde pollution, and on the basis of using dyeing and finishing auxiliaries free of the formaldehyde during production, requirements of multi-functional and top grade formaldehyde-free products in the market are met by improving dyeing and finishing technology of textiles.

Description

Formaldehydeless suit facing material
Technical field
The present invention relates to a kind of suit facing material, is a kind of suit facing material of formaldehydeless pollution.
Background technology
Existing suit facing material; Owing in the lining process, use the dyeing and finishing agent that contains formaldehyde; Its inevitable residual a part of formaldehyde; Have in the prior art to listen and use formaldehydeless dyeing and finishing auxiliaries to realize formaldehydeless purpose, but no matter present formaldehydeless dyeing and finishing auxiliaries is the demand that kind or aspect of performance all can't satisfy multi-functional and expensive goods.
Summary of the invention
The object of the present invention is to provide a kind of formaldehydeless suit facing material that does not have formaldehyde to pollute.
Technical solution of the present invention is:
A kind of formaldehydeless suit facing material; The manufacture craft of suit facing material comprises dyeing process and arranging process, comprises in the dyeing process that oxygen floats, goes up liquid wax, tube yarn baking step, comprises destarch, water-washing step in the arranging process; It is characterized in that: in the said dyeing process; Add 75 ~ 85 ℃ hot water wash 15 ~ 25 minutes after oxygen floats one time, before last liquid wax, add 60 ~ 70 ℃ hot water wash 15 ~ 25 minutes one time, a tube yarn bake out temperature is 110 ~ 120 ℃; After the destarch, each rinsing bowl shower water temperature control is at 55 ~ 65 ℃, and advancing the cloth speed of a motor vehicle is 55 ~ 65 meters/minute.
Adopt formaldehydeless dyeing and finishing auxiliaries in dyeing and the arranging process.
The formaldehydeless pollution of product of the present invention does not contain on the dyeing and finishing auxiliaries basis of formaldehyde in use during production, through improving the dyeing and finishing technology of textiles, satisfies market to multi-functional, high-grade formaldehydeless product demand.
Below in conjunction with embodiment the present invention is described further.
The specific embodiment
A kind of formaldehydeless suit facing material; The manufacture craft of suit facing material comprises dyeing process and arranging process, comprises in the dyeing process that oxygen floats, goes up liquid wax, tube yarn baking step, comprises destarch, water-washing step in the arranging process; In the said dyeing process; Add 75 ~ 85 ℃ hot water wash 15 ~ 25 minutes after oxygen floats one time, before last liquid wax, add 60 ~ 70 ℃ hot water wash 15 ~ 25 minutes one time, a tube yarn bake out temperature is 110 ~ 120 ℃; After the destarch, each rinsing bowl shower water temperature control is at 55 ~ 65 ℃, and advancing the cloth speed of a motor vehicle is 55 ~ 65 meters/minute.Adopt formaldehydeless dyeing and finishing auxiliaries in dyeing and the arranging process.

Claims (2)

1. formaldehydeless suit facing material; The manufacture craft of suit facing material comprises dyeing process and arranging process, comprises in the dyeing process that oxygen floats, goes up liquid wax, tube yarn baking step, comprises destarch, water-washing step in the arranging process; It is characterized in that: in the said dyeing process; Add 75 ~ 85 ℃ hot water wash 15 ~ 25 minutes after oxygen floats one time, before last liquid wax, add 60 ~ 70 ℃ hot water wash 15 ~ 25 minutes one time, a tube yarn bake out temperature is 110 ~ 120 ℃; After the destarch, each rinsing bowl shower water temperature control is at 55 ~ 65 ℃, and advancing the cloth speed of a motor vehicle is 55 ~ 65 meters/minute.
2. formaldehydeless suit facing material according to claim 1 is characterized in that: adopt formaldehydeless dyeing and finishing auxiliaries in dyeing and the arranging process.
CN201110333931XA 2011-10-28 2011-10-28 Formaldehyde-free suit fabric Pending CN102505446A (en)