Histidine-lysine combination strengthening method of rotten silk fabrics Download PDFInfo
- Publication number
- CN102433737A CN102433737A CN2011102378764A CN201110237876A CN102433737A CN 102433737 A CN102433737 A CN 102433737A CN 2011102378764 A CN2011102378764 A CN 2011102378764A CN 201110237876 A CN201110237876 A CN 201110237876A CN 102433737 A CN102433737 A CN 102433737A
- Authority
- CN
- China
- Prior art keywords
- histidine
- lysine
- aqueous solution
- rotten
- silk goods
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a histidine-lysine combination strengthening method of rotten silk fabrics, comprising the following steps: A), flatting a rotten silk fabric, then uniformly spraying a histidine aqueous solution having a concentration of 0.5-2 wt% on the surface of the rotten silk fabric until the silk fabric is uniformly drenched through with the histidine aqueous solution to drip; B), at 10 min after completing the step A), spraying a lysine aqueous solution having a concentration of 0.5-2 wt% on the surface of the silk fabric until the silk fabric is uniformly drenched through with the lysine aqueous solution, naturally drying to strengthen the rotten silk fabric. Compared with the prior art, the invention has the advantage of convenient operation; because of no need of other chemical auxiliaries except for histidine and lysine, the strength of the fabrics can be effectively increased, and the original characteristics of the fabrics are not affected.
Description
Technical field
The present invention relates to a kind of silk historical relic's protection method, particularly a kind of histidine-lysine composite reinforcement method of poor rotten silk goods.
Background technology
At present; Both at home and abroad the reinforcement means to poor rotten silk goods mainly contain chucking method, mount the holder method, resin method for strengthening, silk gum method for strengthening, Pai Lalun Vacuum Coating method, grafting copolymerization process etc.; But all there is certain defective in these methods, and it is used and has also received great restriction.Silk-fibroin reinforcing project by Institutes Of Technology Of Zhejiang cooperates with the China Silk Museum has been developed the research that fibroin albumen is reinforced fragile silk; But cumbersome and difficult storage of the preparation of silk fibroin protein solution and transportation, people's expectation simultaneously has the reinforcement means without other chemical assistant.
Summary of the invention
The object of the present invention is to provide a kind of histidine-lysine composite reinforcement method of poor rotten silk goods, is a kind of reinforcement means efficiently that has easily and effectively, and this reinforcement means is simple to operate, and is low to environment requirement, and room temperature condition gets final product down.It is reinforcement material that the present invention selects the hydrolysate amino acid of protein for use, at ambient temperature the silk historical relic is reinforced, and through experimental study repeatedly, the compound of L-histidine and L-lysine has significant consolidation effect.The present invention does not need other chemical assistant except that histidine-lysine, the ultimate strength and the elongation at break of the fragile silk behind this composite reinforcement of process all are significantly improved, and to the almost not influence of silk goods primary characteristic.A kind of histidine-lysine composite reinforcement method of poor rotten silk goods is characterized in that adopting following steps:
A) will be pickled with grains or in wine after rotten silk goods divide, evenly spray mass percentage concentration on its surface and be 0.5%~2% the histidine aqueous solution, evenly drenched by the histidine aqueous solution and till dripping to silk goods;
B) completing steps A) behind the 10min, the sprinkling mass percentage concentration is 0.5%~2% lysine solution on fabric, and is evenly drenched by lysine solution to silk goods, air dry, and poor rotten silk goods obtain to reinforce.
Compared with prior art, advantage of the present invention has: 1) easy to operate; 2) the present invention does not need other chemical assistant except that histidine lysine, can effectively improve fabric intensity, to the almost not influence of silk goods primary characteristic.
The specific embodiment
Embodiment 1:
A kind of histidine-lysine composite reinforcement method of poor rotten silk goods is characterized in that adopting following steps:
A) will be pickled with grains or in wine after rotten silk goods divide, evenly spray mass percentage concentration on its surface and be 0.5% the histidine aqueous solution, evenly drenched by the histidine aqueous solution and till dripping to silk goods;
B) completing steps A) behind the 10min, the sprinkling mass percentage concentration is 2% lysine solution on fabric, and is evenly drenched by lysine solution to silk goods, air dry, and poor rotten silk goods obtain to reinforce.
Embodiment 2:
A kind of histidine-lysine composite reinforcement method of poor rotten silk goods is characterized in that adopting following steps:
A) will be pickled with grains or in wine after rotten silk goods divide, evenly spray mass percentage concentration on its surface and be 2% the histidine aqueous solution, evenly drenched by the histidine aqueous solution and till dripping to silk goods;
B) completing steps A) behind the 10min, the sprinkling mass percentage concentration is 0.5% lysine solution on fabric, and is evenly drenched by lysine solution to silk goods, air dry, and poor rotten silk goods obtain to reinforce.
Embodiment 3:
A kind of histidine-lysine composite reinforcement method of poor rotten silk goods is characterized in that adopting following steps:
A) will be pickled with grains or in wine after rotten silk goods divide, evenly spray mass percentage concentration on its surface and be 1.3% the histidine aqueous solution, evenly drenched by the histidine aqueous solution and till dripping to silk goods;
B) completing steps A) behind the 10min, the sprinkling mass percentage concentration is 1.3% lysine solution on fabric, and is evenly drenched by lysine solution to silk goods, air dry, and poor rotten silk goods obtain to reinforce.
Claims (1)
1. histidine-lysine composite reinforcement the method for poor rotten silk goods is characterized in that adopting following steps:
A) will be pickled with grains or in wine after rotten silk goods divide, evenly spray mass percentage concentration on its surface and be 0.5%~2% the histidine aqueous solution, evenly drenched by the histidine aqueous solution and till dripping to silk goods;
B) completing steps A) behind the 10min, the sprinkling mass percentage concentration is 0.5%~2% lysine solution on fabric, and is evenly drenched by lysine solution to silk goods, air dry, and poor rotten silk goods obtain to reinforce.