CN102372881A - 一种新型防腐塑料涂布地板 - Google Patents
一种新型防腐塑料涂布地板 Download PDFInfo
- Publication number
- CN102372881A CN102372881A CN2010102483041A CN201010248304A CN102372881A CN 102372881 A CN102372881 A CN 102372881A CN 2010102483041 A CN2010102483041 A CN 2010102483041A CN 201010248304 A CN201010248304 A CN 201010248304A CN 102372881 A CN102372881 A CN 102372881A
- Authority
- CN
- China
- Prior art keywords
- plastic coating
- floor
- novel anti
- coating floor
- corrosion plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明属于PVC地板,特别涉及一种新型防腐塑料涂布地板。一种新型防腐塑料涂布地板,其特征在于由如下配方组成,按重量份数其配方为:聚氯乙烯树脂100-120份,纳米级石英砂50-100份,稀土稳定剂R108A 8-10份,双季戊四醇25-30份。本发明提供一种新型防腐塑料涂布地板,具有防腐,耐磨等优点。
Description
技术领域
本发明属于PVC地板,特别涉及一种新型防腐塑料涂布地板。
背景技术
塑料涂布地板是由合成树脂、填料、颜料等组成的,在现场施工的一种新型的塑料地面材料。它有如下特点:1.施工简便。由于它可以在施工现场用手工配料,用一般的泥工工具涂布,技术要求不高,所以施工简便、速度快。2.能形成无接缝的地面,整体性好。这一点对工业建筑中的防腐蚀要求特别重要。某些现场铺设的块状防腐蚀地面往往会由于接缝处的泄漏而被破坏。3.与基层的附着力强,不易起壳、剥离。根据以上特点,塑料涂布地板很适宜用在化工厂、轧钢厂热处理车间、电池室、电子管厂加汞车回等场合。用来铺设塑料涂布地板的合成树脂的种类有好几种。如环氧树脂,不饱和聚醋、聚氨醋、聚醋酸乙烯乳液、丙烯酸类树脂乳液等。本发明提供一种新型防腐塑料涂布地板,具有防腐,耐磨等优点。
发明内容
发明目的
本发明提供一种新型防腐塑料涂布地板,具有防腐,耐磨等优点。
技术方案
一种新型防腐塑料涂布地板,其特征在于由如下配方组成,按重量份数其配方为:聚氯乙烯树脂100-120份,纳米级石英砂50-100份,稀土稳定剂R108A8-10份,双季戊四醇25-30份。
一种新型防腐塑料涂布地板的制备工艺:
A、混料将上述配方混合;
B、混炼:在两辊炼塑机上将Pvc塑化均匀,拉片;温度为140-160左右;
C、压片:温度140-160左右,压力180-200kg/cm2;
D、成品。
有益效果
1、目前,由于树脂的价格较高,所以塑料涂布地板的成本较高,虽然成本较高,但对化工厂等有特殊防腐蚀要求的地面,仍有的使用价值。
具体实施方式
实施例1
一种新型防腐塑料涂布地板,其特征在于由如下配方组成,按重量份数其配方为:聚氯乙烯树脂100kg,纳米级石英砂50kg,稀土稳定剂R108A 8kg,双季戊四醇25kg。
一种新型防腐塑料涂布地板的制备工艺:
A、混料将上述配方混合;
B、混炼:在两辊炼塑机上将Pvc塑化均匀,拉片;温度为140-160左右;
C、压片:温度140-160左右,压力180-200kg/cm2;
D、成品。
实施例2
一种新型防腐塑料涂布地板,其特征在于由如下配方组成,按重量份数其配方为:聚氯乙烯树脂120kg,纳米级石英砂100kg,稀土稳定剂R108A 10kg,双季戊四醇30kg。
一种新型防腐塑料涂布地板的制备工艺:
A、混料将上述配方混合;
B、混炼:在两辊炼塑机上将Pvc塑化均匀,拉片;温度为140-160左右;
C、压片:温度140-160左右,压力180-200kg/cm2;
D、成品。
Claims (1)
1.一种新型防腐塑料涂布地板,其特征在于由如下配方组成,按重量份数其配方为:聚氯乙烯树脂100-120份,纳米级石英砂50-100份,稀土稳定剂R108A8-10份,双季戊四醇25-30份。