CN102249586A CN 201110123585 CN201110123585A CN102249586A CN 102249586 A CN102249586 A CN 102249586A CN 201110123585 CN201110123585 CN 201110123585 CN 201110123585 A CN201110123585 A CN 201110123585A CN 102249586 A CN102249586 A CN 102249586A
Authority
CN
China
Prior art keywords
grinding
reinforcing agent
slag
mineral powder
grinding aid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201110123585
Other languages
Chinese (zh)
Inventor
白文利
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
LYOYANG WANSHUN BUILDING MATERIALS CO Ltd
Original Assignee
LYOYANG WANSHUN BUILDING MATERIALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by LYOYANG WANSHUN BUILDING MATERIALS CO Ltd filed Critical LYOYANG WANSHUN BUILDING MATERIALS CO Ltd
Priority to CN 201110123585 priority Critical patent/CN102249586A/en
Publication of CN102249586A publication Critical patent/CN102249586A/en
Pending legal-status Critical Current

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C04CEMENTS; CONCRETE; ARTIFICIAL STONE; CERAMICS; REFRACTORIES
    • C04BLIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE; CERAMICS; REFRACTORIES; TREATMENT OF NATURAL STONE
    • C04B40/00Processes, in general, for influencing or modifying the properties of mortars, concrete or artificial stone compositions, e.g. their setting or hardening ability
    • C04B40/0028Aspects relating to the mixing step of the mortar preparation
    • C04B40/0039Premixtures of ingredients

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Ceramic Engineering (AREA)
  • Materials Engineering (AREA)
  • Structural Engineering (AREA)
  • Organic Chemistry (AREA)
  • Curing Cements, Concrete, And Artificial Stone (AREA)

Abstract

The invention relates to a grinding-assistant reinforcing agent for mineral powder. The grinding-assistant reinforcing agent is mainly composed of molasses, triethanolamine, triisopropanolamine, mixed dibasic alcohol, sodium acetate, sodium hydroxide and water. By the adoption of the grinding-assistant reinforcing agent for mineral powder, which is disclosed by the invention, powder grinding efficiency can be improved, grinding machine yield is improved by 10-15%, the specific surface area of mineral powder is improved, and the activity index of the mineral powder is improved.

Description

A kind of breeze grinding aid reinforcing agent
 
Technical field
The present invention relates to a kind of breeze grinding aid reinforcing agent of blast-furnace cinder micro-powder manufacture field, belong to grinding aid field in cement and the slag micropowder processing.
Background technology
Slag is the byproduct when smelting the pig iron, has higher lateral reactivity, and the annual slag output of China has more than 100,000,000 ton, if these slags can not get effective utilization, will inevitably cause pollution difficult to the appraisal to environment, also will cause huge energy dissipation.At present, slag is as the blended material of cement with in order to outside the operating mine slag cement, and particularly ground slag has become one of requisite component of preparation high performance concrete as mineral admixture.Slag micropowder has become produces one of high-quality cement, configuration high-performance, large volume, concrete first-selected material of long lifetime.The concrete that is mixed with slag micropowder has that hydration heat is low, corrosion-resistant, good fluidity, later strength height, anti-micro, can make characteristics such as concrete interface adhesive property improvement, is defined as one of ten new technologies of construction industry by nation-building portion.Owing to scoriaceous vitreous structure reason, common grinding aid joins in the slag milling process, though can remove the agglomeration around the slag particle, can not improve the grindability of slag particle itself, so grinding-aid effect is often not good.
But slag in use exists grindability poor, and early strength is on the low side, has restricted scoriaceous applying.Can improve mill efficiency though prolong the grinding time, but increased power consumption, increased the grinding cost, in scoriaceous grinding process,, produce the difference of electron density in grinding process simultaneously because material is subjected to the influence of various power to cause the electrovalent bond of granule interior to rupture, form a series of staggered active sites in the section both sides, they attract each other, make surface of fracture trend towards compound and material is reunited, thereby grinding output and quality are descended significantly.
For reducing the grinding energy consumption, stop the healing of slag surface of fracture and reducing agglomeration, using grinding aid is the most simple way, uses suitable grinding aid can improve mill efficiency about 10%.
Research on cement additive and use abroad just begin as far back as the thirties in last century, carried out extensive work, many patents have been applied for, domesticly just study and use from the fifties, the most value of the grinding aid of studying and using both at home and abroad are expensive at present, the source shortage, and not remarkable to the slag grinding-aid effect, to slag properties do not have improve or the improvement effect little, thereby generally apply and be restricted.
CN100357214C adopts glycol ether, trolamine, dispersing agent NNO, pearlstone, Sodium sulfate anhydrous.min(99), Tai-Ace S 150 to obtain powder slag cement toughener, and addition is 0.5%, and this product is mainly used in slag cement.
A kind of slag composite activated grinding aids of CN100404456C invention adopts trolamine, polycarboxylate water-reducer and compound with the calcium hydroxide saturated solution, forms through magnetization.This product adopts that trolamine reaches 40%, polycarboxylate water-reducer 20%, saturated aqua calcis 40%.On the one hand cost is too high, and calcium hydroxide has only 0.17% in the saturated on the other hand aqua calcis, is difficult to play the effect of calcium hydroxide, and the magnetization product iron ware of packing into, the magnetic easily dissolved.
The disclosed blast furnace slag liquid grinding aid of CN101597655A, form by glycol ether, sucrose slag waste liquid, sorbyl alcohol, glycerine, tripoly phosphate sodium STPP, yellow soda ash and water, each constituent mass per-cent: glycol ether 10%~20%, sucrose slag waste liquid 10%~15%, sorbyl alcohol 10~20%, glycerine 10-20%, tripoly phosphate sodium STPP 1~5%, yellow soda ash 1~10%, surplus are water.But when using the slag grinding aid, guarantee ore grinding slag water content between 0.5~1.0% as far as possible, moisturely all can influence scoriaceous mill efficiency too greatly or too little.In actual production process, go into to grind scoriaceous moisture and be difficult to be controlled in 0.5% scope.
The technical scheme that CN101781690A adopts is: comprising: trolamine 15~20%, wooden calcium 10~15%, modulus are 1.75~2.1 water glass 15~20%, water 45~55%.When adding other composition in the water glass, can condense usually, form similar cotton globular precipitate, cause and to use.
Summary of the invention
In order to improve mill grinding efficiency, increase the activity index of slag micropowder, adopt raw material easily to purchase and cheaply, it is few to have volume simultaneously, and liquid meter adds characteristics such as convenient, and a kind of breeze grinding aid reinforcing agent of the present invention is adsorbed on particle surface shielding particulate surface residual electric charge, prevent the coalescent of powder, stop section to overlap, reduced agglomeration, thereby helped improving the fineness of slag powders; Simultaneously, can excite the activity of breeze, improve the hydration rate of slag cement, promote further densification of hardened cement paste.Therefore, a kind of breeze grinding aid reinforcing agent of the present invention can grinding aid improve output, can improve ore powder granularity again, increases the breeze activity.
A kind of breeze grinding aid reinforcing agent of the present invention is made up of molasses, trolamine, tri-isopropanolamine, mixing dibasic alcohol, sodium-acetate, sodium hydroxide and water.Consist of by mass percentage: molasses 3-8%, trolamine 5-10%, tri-isopropanolamine 3-5%, mixing dibasic alcohol 30-40%, sodium-acetate 3-8%, sodium hydroxide 1-2%, water surplus, preferred mass percent consists of, molasses 5%, trolamine 8%, tri-isopropanolamine 4%, mixing dibasic alcohol 32%, sodium-acetate 5%, sodium hydroxide 1%, water 45%.
A kind of breeze grinding aid reinforcing agent advantage of the present invention is:
1, adopts the mixing dibasic alcohol, mix dibasic alcohol and mainly form, make ethylene glycol and glycol ether play synergy by ethylene glycol and glycol ether.
2, adopt low-cost byproduct molasses, both reduced cost, product performance are improved.
3, the consumption of trolamine, tri-isopropanolamine reduces significantly, product cost is reduced greatly, and product performance is enhanced.
Embodiment
EmbodimentWith 50 kilograms in molasses, 80 kilograms of trolamines, 40 kilograms of tri-isopropanolamines, 320 kilograms of dibasic alcohol of mixing, 50 kilograms of sodium-acetates, 10 kilograms in sodium hydroxide, 450 kilograms in water, join in the stirred reactor, after mixing, filter barrelling, obtain 1000 kilograms of breeze grinding aid reinforcing agents of the present invention.
Breeze grinding aid reinforcing agent of the present invention is produced the user and is used data as follows:
1, is applied in φ 3.2 * 13m open circuit mill
Numbering Unit-hour output (T/h) Grinding aid add-on (g/ T) Specific surface area (m2/Kg)
1 28 ---- 420
2 30.5 220 433
2, be applied in the closed circuit mill of φ 3.8 * 13m (p.s42.5)
Figure 945760DEST_PATH_IMAGE001

Claims (3)

1. a breeze grinding aid reinforcing agent product is characterized in that: be made up of molasses, trolamine, tri-isopropanolamine, mixing dibasic alcohol, sodium-acetate, sodium hydroxide and water.
2. a kind of breeze grinding aid reinforcing agent according to claim 1, it is characterized in that: consist of molasses 3-8%, trolamine 5-10%, tri-isopropanolamine 3-5%, mixing dibasic alcohol 30-40%, sodium-acetate 3-8%, sodium hydroxide 1-2%, water surplus by mass percentage.
3. a kind of breeze grinding aid reinforcing agent according to claim 1 is characterized in that: consist of molasses 5%, trolamine 8%, tri-isopropanolamine 4%, mixing dibasic alcohol 32%, sodium-acetate 5%, sodium hydroxide 1%, water 45% by mass percentage.
CN 201110123585 2011-05-13 2011-05-13 Grinding-assistant reinforcing agent for mineral powder Pending CN102249586A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201110123585 CN102249586A (en) 2011-05-13 2011-05-13 Grinding-assistant reinforcing agent for mineral powder

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201110123585 CN102249586A (en) 2011-05-13 2011-05-13 Grinding-assistant reinforcing agent for mineral powder

Publications (1)

Publication Number Publication Date
CN102249586A true CN102249586A (en) 2011-11-23

Family

ID=44977211

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201110123585 Pending CN102249586A (en) 2011-05-13 2011-05-13 Grinding-assistant reinforcing agent for mineral powder

Country Status (1)

Country Link
CN (1) CN102249586A (en)

Cited By (19)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102923982A (en) * 2012-11-06 2013-02-13 沈阳建筑大学 Liquid composite grinding aid for granulated blast-furnace slag and preparation method thereof
CN102992694A (en) * 2012-12-17 2013-03-27 桂林理工大学 Preparation method of composite portland cement additive
CN103570269A (en) * 2013-10-23 2014-02-12 沈阳建筑大学 Mineral waste residue liquid composite grinding aid and preparation method thereof
CN104045255A (en) * 2014-04-29 2014-09-17 镇江市振发水泥外加剂有限公司 Cement grinding aid
CN104072006A (en) * 2014-06-13 2014-10-01 山东联合王晁水泥有限公司 Efficient liquid grinding aid for cement
CN104230198A (en) * 2014-09-12 2014-12-24 北京工业大学 Admixture for increasing activity index of air cooling slag and preparation method thereof
CN104478276A (en) * 2014-11-19 2015-04-01 沈阳建筑大学 Granulated blast furnace slag liquid composite grinding aid
CN104591557A (en) * 2015-02-05 2015-05-06 廊坊天盛环保建材科技有限公司 Slag synergist and application thereof
CN104743599A (en) * 2015-03-20 2015-07-01 溧阳市同鑫新材料科技有限公司 Production additive capable of increasing and improving yield and quality of calcium carbonate powder and use method of production additive
CN104926180A (en) * 2015-06-17 2015-09-23 廖德仲 Mineral powder liquid grinding aid and production method thereof
CN105110672A (en) * 2015-07-31 2015-12-02 武汉理工大学 Method for homogeneously modifying pulverized coal ash by vapor deposition process
CN105669054A (en) * 2016-01-28 2016-06-15 桂林华越环保科技有限公司 Special composite liquid grinding aid for blast furnace slag and preparation method of special composite liquid grinding aid
CN106396454A (en) * 2016-09-26 2017-02-15 同济大学 Slag grinding aid and preparation method and application thereof
CN106565122A (en) * 2016-10-19 2017-04-19 同济大学 Polymeric grinding aid, and preparation method and application thereof
CN109553322A (en) * 2019-01-23 2019-04-02 济南大学 A kind of early-strength miberal powder activator
CN110171939A (en) * 2019-04-11 2019-08-27 武汉理工大学 A kind of sial phase chaotropic agent and its preparation method and application
CN114163162A (en) * 2021-12-24 2022-03-11 常州坚鹏建材有限公司 Mineral powder hardening grinding aid and grinding-aid process thereof
CN115321871A (en) * 2022-06-27 2022-11-11 武汉源锦建材科技有限公司 Grinding-aid exciting agent for mineral admixture and preparation method and application thereof
CN115368085A (en) * 2022-09-22 2022-11-22 浙江交工金筑交通建设有限公司 Modified mineral powder doped steaming-free ultrahigh-performance concrete and preparation method thereof

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101575185A (en) * 2009-06-19 2009-11-11 徐彬 High-efficiency compound slag-grinding aid of beet waste mash compound and production method thereof
CN101665338A (en) * 2009-09-08 2010-03-10 南京筑基节能科技有限公司 Chlorine-free powdery cement grinding aid and preparation method thereof

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101575185A (en) * 2009-06-19 2009-11-11 徐彬 High-efficiency compound slag-grinding aid of beet waste mash compound and production method thereof
CN101665338A (en) * 2009-09-08 2010-03-10 南京筑基节能科技有限公司 Chlorine-free powdery cement grinding aid and preparation method thereof

Cited By (24)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102923982A (en) * 2012-11-06 2013-02-13 沈阳建筑大学 Liquid composite grinding aid for granulated blast-furnace slag and preparation method thereof
CN102992694A (en) * 2012-12-17 2013-03-27 桂林理工大学 Preparation method of composite portland cement additive
CN103570269B (en) * 2013-10-23 2015-06-10 沈阳建筑大学 Mineral waste residue liquid composite grinding aid and preparation method thereof
CN103570269A (en) * 2013-10-23 2014-02-12 沈阳建筑大学 Mineral waste residue liquid composite grinding aid and preparation method thereof
CN104045255A (en) * 2014-04-29 2014-09-17 镇江市振发水泥外加剂有限公司 Cement grinding aid
CN104072006A (en) * 2014-06-13 2014-10-01 山东联合王晁水泥有限公司 Efficient liquid grinding aid for cement
CN104230198A (en) * 2014-09-12 2014-12-24 北京工业大学 Admixture for increasing activity index of air cooling slag and preparation method thereof
CN104230198B (en) * 2014-09-12 2016-04-20 北京工业大学 A kind ofly improve admixture of air-cooled slag reactivity index and preparation method thereof
CN104478276A (en) * 2014-11-19 2015-04-01 沈阳建筑大学 Granulated blast furnace slag liquid composite grinding aid
CN104591557A (en) * 2015-02-05 2015-05-06 廊坊天盛环保建材科技有限公司 Slag synergist and application thereof
CN104743599A (en) * 2015-03-20 2015-07-01 溧阳市同鑫新材料科技有限公司 Production additive capable of increasing and improving yield and quality of calcium carbonate powder and use method of production additive
CN104926180A (en) * 2015-06-17 2015-09-23 廖德仲 Mineral powder liquid grinding aid and production method thereof
CN105110672A (en) * 2015-07-31 2015-12-02 武汉理工大学 Method for homogeneously modifying pulverized coal ash by vapor deposition process
CN105669054A (en) * 2016-01-28 2016-06-15 桂林华越环保科技有限公司 Special composite liquid grinding aid for blast furnace slag and preparation method of special composite liquid grinding aid
CN106396454A (en) * 2016-09-26 2017-02-15 同济大学 Slag grinding aid and preparation method and application thereof
CN106565122A (en) * 2016-10-19 2017-04-19 同济大学 Polymeric grinding aid, and preparation method and application thereof
CN106565122B (en) * 2016-10-19 2018-12-18 同济大学 Mcromolecular grinding aid and its preparation method and application
CN109553322A (en) * 2019-01-23 2019-04-02 济南大学 A kind of early-strength miberal powder activator
CN110171939A (en) * 2019-04-11 2019-08-27 武汉理工大学 A kind of sial phase chaotropic agent and its preparation method and application
CN110171939B (en) * 2019-04-11 2021-09-21 武汉理工大学 Silicon-aluminum phase promoter and preparation method and application thereof
CN114163162A (en) * 2021-12-24 2022-03-11 常州坚鹏建材有限公司 Mineral powder hardening grinding aid and grinding-aid process thereof
CN114163162B (en) * 2021-12-24 2022-08-09 常州坚鹏建材有限公司 Mineral powder hardening grinding aid and grinding-aid process thereof
CN115321871A (en) * 2022-06-27 2022-11-11 武汉源锦建材科技有限公司 Grinding-aid exciting agent for mineral admixture and preparation method and application thereof
CN115368085A (en) * 2022-09-22 2022-11-22 浙江交工金筑交通建设有限公司 Modified mineral powder doped steaming-free ultrahigh-performance concrete and preparation method thereof

Similar Documents

Publication Publication Date Title
CN102249586A (en) Grinding-assistant reinforcing agent for mineral powder
CN100404456C (en) Slag composite activated grinding aids, and preparation method
CN101428985B (en) Composite grinding aid, production method and uses thereof
CN112079589A (en) Modified lithium slag complex mineral admixture and preparation and application thereof
CN101182149A (en) Composite activated cement reinforced grinding aids containing polycarboxylic acid series and method for preparing the same
CN107010853B (en) A kind of method that microwave synergy is activated S95 grade slag powder
CN101337779B (en) Additive of composite portland cement and producing method thereof
CN105399349A (en) High-activity iron and steel slag powder and preparation method thereof
CN101372409A (en) Solid non-chlorate cement grinding aid
CN105399353A (en) Alkali-activated cement utilizing abandoned clay brick powder and preparation method thereof
CN106495583B (en) The early strong compound steelslag powder as additive of high-performance and its application in concrete batching
CN107746198A (en) A kind of scrap glass powder composite blend and preparation method thereof
CN101560578B (en) Performance adjustment material for activating steel slag at high temperature and application thereof
CN104478276A (en) Granulated blast furnace slag liquid composite grinding aid
CN113880486B (en) Composite admixture utilizing solid wastes of iron and steel plant and preparation method thereof
CN105621909B (en) It is a kind of to mix modified Desulphurization and the cement of rice hull ash again
CN114890744A (en) Green low-carbon concrete and preparation method thereof
KR20130087240A (en) Activator for high volume slag cement, high volume slag cement composition containing the activator and process of the cement
CN104449568A (en) High-yield energy-saving type slag grinding aid
CN102351446A (en) Preparation method of gangue active mixed material
CN101781111A (en) Cementing material for mine filling and preparation method thereof
CN112723762A (en) Cementing material for modifying bulk filling body and preparation method and application thereof
CN101343156B (en) Method for improving quality of fly ash concrete blending material
CN102838303A (en) Method for preparing cement by nickel-chromium residue
CN102976651A (en) Excitant for inferior lime-cement mixed material and preparation method thereof

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20111123