Prior art keywords
dislocation
electrode frame
bar
pile
battery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010101084190A
Other languages
English (en)
Inventor
高素军
张华民
刘景开
韩希
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dalian Rongke Power Co Ltd
Original Assignee
Dalian Rongke Power Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dalian Rongke Power Co Ltd filed Critical Dalian Rongke Power Co Ltd
Priority to CN2010101084190A priority Critical patent/CN102148389A/zh
Publication of CN102148389A publication Critical patent/CN102148389A/zh
Pending legal-status Critical Current

Links

Images

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/30Hydrogen technology
    • Y02E60/50Fuel cells

Landscapes

  • Fuel Cell (AREA)

Abstract

本发明涉及化学电源储能技术领域,特别涉及一种氧化还原液流电池的结构。本发明的特征是,通过在电池的端板上布置了一系列的限制电极框错位的杆,穿过电池(电堆),可以有效地防止电极框在运行过程中出现参差不齐现象的发生。解决了电堆长期运行过程中由于框的错位引起的渗漏和共用管道流经截面变化等问题,延长电池(堆)的寿命。

Description

一种氧化还原液流电池的结构
技术领域
本发明涉及储能电池的结构,特别涉及一种氧化还原液流电池的结构。
背景技术
为了人类免受气候变暖的威胁,《联合国气候变化框架公约》对各国二氧化碳排放进行指标性限制,为此许多国家逐步把能源发展战略转向可再生能源上,如风能,太阳能,潮汐能等。为了解决可再生能源的供需间矛盾,规模储能的发展势在必行。同时,规模电能存储在电能管理、电网辅助服务、电压控制、大型不间断电源等方面有着重要作用,若规模电能与大型火力发电联合,可降低电站峰值容量、降低发电成本以及减小污染。由于液流储能电池的具有功率与容量分离的特点,易于设计,操作方便,逐渐成为最有前途地规模电力存储的首选之一。其中,全钒氧化还原液流电池备受青睐。
液流储能电池(堆)的是氧化还原液流电池储能系统核心部件,其结构的合理性直接关系到系统效率以及运行的可靠性。目前电堆结构,存在一些弊端,特别是运行一段时间后,电堆的电极框出现层次不齐的现象,严重时可引起外漏,双极板塌陷等严重问题,直接威胁到电堆/系统的运行安全。
发明内容
为了解决上述液流电池结构上存在问题,特别是电堆的电极框出现层次不齐的现象,本发明通过在电池的端板上布置了一系列的限制电极框错位的杆,穿过电池(电堆),可以有效的防止电极框在运行过程中出现参差不齐的现象的发生,解决了电堆的长期运行过程由于框的错位引起的渗漏和共用管道流经截面变化等问题,延长电池(堆)的寿命。
为达到上述目的,本发明采用的技术方案为:
一种氧化还原液流电池的结构,包括液流电池或电堆(液流电池或电堆组件中包括端板和电极框),在液流电池或电堆的端板和电极框的四周对应位置处开设有防错位孔,在防错位孔内穿置有限制电极框错位的杆。
所述限制电极框错位的杆为空心的管或实心的杆。所述防错位孔和限制电极框错位的杆数量为≥2个,它们于端板和电极框的四周均匀分布设置。
于所述液流电池或电堆的集流板或双极板的四周对应位置处同样开设有防错位孔,限制电极框错位的杆从集流板或双极板的防错位孔穿过。
所述端板为用于补强的夹板、进液板或分布板;所述限制电极框错位的杆为钢性的金属杆、非金属杆、或外表面包覆有非金属材料的金属杆;所述外表面包覆有非金属材料的金属杆是指金属杆外直接套插有非金属管,或是金属杆外表面涂非金属涂层。
本发明的优点在于:
1.结构简单合理,装配方便快捷。
2.附加成本低,易于实现工业化。
附图说明
图1为本发明液流电池的结构图;
1限制电极框错位的杆,2为端板和集流板,3为双极板,4为密封垫,5为电极,6电极框7为离子交换膜,8为限制框错位的孔。
具体实施方式
实施例1
电池结构如图1所示,用于由4根限制电极框错位的杆穿过端板和电极框,位置在电极框的长边侧。限制电极框错位的杆由Φ4不锈钢杆外套Φ6×1尼龙管构成,对应的限制电极框错位的孔为Φ6.5。
电极面积:225cm2,单电池数:13个。
连续运行2000小时,电极框没有发生明显的错位。电池效率没有衰减,保持在86~89%,90.5~92.4%,能量效率大于80%
实施例2
电池结构如图1所示,用于由6根限制电极框错位的杆穿过端板和电极框,其中4根电极框的长边侧,2根在短边侧。限制电极框错位的杆采用Φ6×1不锈钢管,对应的限制电极框错位的孔为Φ6.5。
其中电极面积:460cm2,单电池数:20个。
连续运行1500小时,电极框没有发生明显的错位。电池效率没有衰减,保持在85~89%,90.2~91.0%,能量效率大于78%。

Claims (7)

1.一种氧化还原液流电池的结构,包括液流电池或电堆,其特征在于:在液流电池或电堆的端板和电极框的四周对应位置处开设有防错位孔,在防错位孔内穿置有限制电极框错位的杆。
2.如权利要求1所述的结构,其特征在于:所述限制电极框错位的杆为空心的管或实心的杆。
3.如权利要求1所述的结构,其特征在于:所述防错位孔和限制电极框错位的杆数量为≥2个,它们于端板和电极框的四周均匀分布设置。
4.如权利要求1所述的结构,其特征在于:于所述液流电池或电堆的集流板或双极板的四周对应位置处同样开设有防错位孔,限制电极框错位的杆从集流板或双极板的防错位孔穿过。
5.如权利要求1所述的结构,其特征在于:所述端板为用于补强的夹板、进液板或分布板。
6.如权利要求1所述的结构,其特征在于:所述限制电极框错位的杆为钢性的金属杆、非金属杆、或外表面包覆有非金属材料的金属杆。
7.如权利要求1所述的结构,其特征在于:所述外表面包覆有非金属材料的金属杆是指金属杆外直接套插有非金属管,或是金属杆外表面涂非金属涂层。
CN2010101084190A 2010-02-10 2010-02-10 一种氧化还原液流电池的结构 Pending CN102148389A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010101084190A CN102148389A (zh) 2010-02-10 2010-02-10 一种氧化还原液流电池的结构

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010101084190A CN102148389A (zh) 2010-02-10 2010-02-10 一种氧化还原液流电池的结构

Publications (1)

Publication Number Publication Date
CN102148389A true CN102148389A (zh) 2011-08-10

Family

ID=44422487

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010101084190A Pending CN102148389A (zh) 2010-02-10 2010-02-10 一种氧化还原液流电池的结构

Country Status (1)

Country Link
CN (1) CN102148389A (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103022544A (zh) * 2012-12-29 2013-04-03 大连融科储能技术发展有限公司 一种液流电池用电堆
CN104409761A (zh) * 2014-11-28 2015-03-11 中国科学院金属研究所 一种新型液流电池堆及其压紧方法
CN110061261A (zh) * 2019-05-28 2019-07-26 乐山伟力得能源有限公司 一种电堆结构

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH04319254A (ja) * 1991-04-17 1992-11-10 Sumitomo Electric Ind Ltd 電池構造
JP2002175829A (ja) * 2000-12-07 2002-06-21 Sumitomo Electric Ind Ltd 全バナジウムレドックスフロー電池および全バナジウムレドックスフロー電池の運転方法
US20030087156A1 (en) * 2001-04-12 2003-05-08 Squirrel Holdings Ltd. Porous mat electrodes for electrochemical reactor having electrolyte solution distribution channels
CN201266642Y (zh) * 2008-07-31 2009-07-01 比亚迪股份有限公司 一种液流电池的电堆结构

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH04319254A (ja) * 1991-04-17 1992-11-10 Sumitomo Electric Ind Ltd 電池構造
JP2002175829A (ja) * 2000-12-07 2002-06-21 Sumitomo Electric Ind Ltd 全バナジウムレドックスフロー電池および全バナジウムレドックスフロー電池の運転方法
US20030087156A1 (en) * 2001-04-12 2003-05-08 Squirrel Holdings Ltd. Porous mat electrodes for electrochemical reactor having electrolyte solution distribution channels
CN201266642Y (zh) * 2008-07-31 2009-07-01 比亚迪股份有限公司 一种液流电池的电堆结构

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103022544A (zh) * 2012-12-29 2013-04-03 大连融科储能技术发展有限公司 一种液流电池用电堆
CN104409761A (zh) * 2014-11-28 2015-03-11 中国科学院金属研究所 一种新型液流电池堆及其压紧方法
CN110061261A (zh) * 2019-05-28 2019-07-26 乐山伟力得能源有限公司 一种电堆结构

Similar Documents

Publication Publication Date Title
CN103579658B (zh) 一种液流电池堆
Bhattarai et al. Vanadium redox flow battery with slotted porous electrodes and automatic rebalancing demonstrated on a 1 kW system level
CN100578849C (zh) 大功率氧化还原液流储能电堆模块化结构及其群组模式
CN201845830U (zh) 一种液流电池电堆
JP2018186014A (ja) フロー電池、フロー電池システム及び発電システム
CN103137986A (zh) 一种锌溴单液流电池
WO2018198252A1 (ja) 二次電池、二次電池システム及び発電システム
CN203644856U (zh) 电解液存储装置和液流电池系统
CN101847724A (zh) 一种液流电池的双极板框和电堆
CN109037725B (zh) 一种提高电解液分布均匀性的液流电池及电极结构和方法
CN101562257B (zh) 一种全钒离子氧化还原液流的电池结构
CN102148389A (zh) 一种氧化还原液流电池的结构
KR101402948B1 (ko) 레독스 흐름전지
CN202268450U (zh) 一种液流电池的电极框
CN204011565U (zh) 全钒液流电池储能系统
CN204947013U (zh) 一种液流电池电堆进液板、电堆结构及电堆和液流电池系统
CN203659985U (zh) 一种液流电池用极板结构及全钒液流电池
CN202888323U (zh) 一种不易泄漏液流电池的电堆结构
CN207426029U (zh) 一种提高电解液利用率的液流电池脉冲式充放电系统
CN202888318U (zh) 一种分配管外置的液流电池堆
CN219180554U (zh) 一种提高电池性能的新型液流电池装置
CN204596879U (zh) 一种结构优化的全钒液流电池用液流框装置
CN106611863B (zh) 一种液流电池电堆中防止双极板腐蚀的结构
CN201444489U (zh) 一种全钒离子氧化还原液流的新型电池结构
CN104733747B (zh) 一种液流电池系统泄漏的快速自动报警装置

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
WD01 Invention patent application deemed withdrawn after publication
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20110810