CN102145414A - 一种多孔攻芽方法 - Google Patents
一种多孔攻芽方法 Download PDFInfo
- Publication number
- CN102145414A CN102145414A CN 201110071599 CN201110071599A CN102145414A CN 102145414 A CN102145414 A CN 102145414A CN 201110071599 CN201110071599 CN 201110071599 CN 201110071599 A CN201110071599 A CN 201110071599A CN 102145414 A CN102145414 A CN 102145414A
- Authority
- CN
- China
- Prior art keywords
- bud
- substrate
- workpiece
- tapping
- attack
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种多孔攻芽方法,其特征在于,包括以下步骤:(
1
)基板的制作:采用绝缘板或其他可以不划伤待加工工件的材料割一个与工件外形相同的基板;(
2
)打孔:在所述基板上与待加工工件上要攻的芽相对应的位置打孔,不同的芽用不同形状的孔表示;(
3
)连线:将相同形状的孔用最短的连接线连接起来;(
4
)攻芽,将基板与工件重叠,依照步骤(
3
)所述的连接线依次攻芽。本发明减少漏攻芽和错攻芽事件的发生,提高钳工操作人员的攻芽准确率,减少批量全检情况的发生,从而提高了工作效率降低了成本。
Description
技术领域
本发明涉及钣金领域,尤其是一种多孔攻芽方法。
背景技术
攻芽是指对孔内壁进行螺纹加工;其作用就是制造螺纹,使对应的螺栓或螺丝能与之连接。很多产品需要攻芽的种类和数量均比较多,此时完全靠操作工的来保证完成的质量,是不可能的,数量比较少时还好,但大批生产时,操作人员就无法完成如此繁重的任务。经常会出现漏芽和攻错芽的事情,因此需要对产品进行全检,浪费大量的人力和时间。
发明内容
本发明目的是:提供一种可以提高工作效率,帮助操作人员避免漏攻芽和错攻芽事件的发生的多孔攻芽方法。
本发明的技术方案是:一种多孔攻芽方法,其特征在于,包括以下步骤:
(1)基板的制作:采用绝缘板或其他可以不划伤待加工工件的材料割一个与工件外形相同的基板;
(2)打孔:在所述基板上与待加工工件上要攻的芽相对应的位置打孔,不同的芽用不同形状的孔表示;
(3)连线:将相同形状的孔用最短的连接线连接起来;
(4)攻芽,将基板与工件重叠,依照步骤(3)所述的连接线依次攻芽。
进一步的,所述不同孔之间的连接线采用不同的颜色。
进一步的,所述连接线上还有用于标识攻芽顺序的箭头。
本发明的优点是:
减少漏攻芽和错攻芽事件的发生,提高钳工操作人员的攻芽准确率,减少批量全检情况的发生,从而提高了工作效率降低了成本。
附图说明
下面结合附图及实施例对本发明作进一步描述:
图1为待攻芽工件的示意图。
图2为基板的示意图。
图3为基板的示意图。
具体实施方式
实施例1:如图1所示的671mm*571mm的工件,需要在上面切削攻芽,图中h表示切削攻芽36-M3,底孔为Φ2.50mm;m表示切削攻芽12-M4,底孔为Φ3.30mm。首先用绝缘板(或其他材料,只要不划伤产品均可)割一个类似产品的外形的基板,用圆孔表示M3,用方孔表示M4(也可用三角形或者其他形状表示),如图2所示;将此基板上的圆孔和方孔用最短的线段将他们各自连接起来,如图3所示;将此基板与工件重叠,操作人员只需要按照线路依次攻芽,简单明了,省时省力,不会出现漏攻或攻错的现象。生产完毕后,经工装做保存处理,下批再次使用。
实施例2:如图1所示的671mm*571mm的工件,需要在上面切削攻芽,图中h表示切削攻芽36-M3,底孔为Φ2.50mm;m表示切削攻芽12-M4,底孔为Φ3.30mm。首先用绝缘板(或其他材料,只要不划伤产品均可)割一个类似产品的外形的基板,用圆孔表示M3,用方孔表示M4(也可用三角形或者其他形状表示),如图2所示;将此基板上的圆孔和方孔用最短的线段将他们各自连接起来,连接圆孔的线采用红色的线,连接方孔的采用蓝色的线(也可以采用其他的颜色);将此基板与工件重叠,操作人员只需要按照线路依次攻芽,做完一种颜色的线继续做下一种颜色的,简单明了,省时省力,不会出现漏攻或攻错的现象。生产完毕后,经工装做保存处理,下批再次使用。
实施例3:如图1所示的671mm*571mm的工件,需要在上面切削攻芽,图中h表示切削攻芽36-M3,底孔为Φ2.50mm;m表示切削攻芽12-M4,底孔为Φ3.30mm。首先用绝缘板割一个类似产品的外形的基板,用圆孔表示M3,用方孔表示M4,如图2所示;将此基板上的圆孔和方孔用最短的线段将他们各自连接起来,连接圆孔的线采用红色的线,连接方孔的采用蓝色的线,线路上标有指示箭头;将此基板与工件重叠,操作人员只需要按照指示箭头指示的线路依次攻芽,做完一种颜色的线继续做下一种颜色的,简单明了,省时省力,不会出现漏攻或攻错的现象。生产完毕后,经工装做保存处理,下批再次使用。
以上实施例仅为本发明其中的一种实施方式,其描述较为具体和详细,但并不能因此而理解为对本发明专利范围的限制。应当指出的是,对于本领域的普通技术人员来说,在不脱离本发明构思的前提下,还可以做出若干变形和改进,这些都属于本发明的保护范围。因此,本发明专利的保护范围应以所附权利要求为准。
Claims (3)
1.一种多孔攻芽方法,其特征在于,包括以下步骤:
(1)基板的制作:采用绝缘板或其他可以不划伤待加工工件的材料割一个与工件外形相同的基板; (2)打孔:在所述基板上与待加工工件上要攻的芽相对应的位置打孔,不同的芽用不同形状的孔表示;
(3)连线:将相同形状的孔用最短的连接线连接起来;
(4)攻芽,将基板与工件重叠,依照步骤(3)所述的连接线依次攻芽。
2.根据权利要求1所述的多孔攻芽方法,其特征在于,所述不同孔之间的连接线采用不同的颜色。
3.根据权利要求1所述的多孔攻芽方法,其特征在于,所述连接线上还有用于标识攻芽顺序的箭头。