CN102078948A - 一种电脉冲孕育连续铸钢浇注装置 - Google Patents

一种电脉冲孕育连续铸钢浇注装置 Download PDF

Info

Publication number
CN102078948A
CN102078948A CN 201110031260 CN201110031260A CN102078948A CN 102078948 A CN102078948 A CN 102078948A CN 201110031260 CN201110031260 CN 201110031260 CN 201110031260 A CN201110031260 A CN 201110031260A CN 102078948 A CN102078948 A CN 102078948A
Authority
CN
China
Prior art keywords
river
mouth
electrode
electro
continuous casting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 201110031260
Other languages
English (en)
Other versions
CN102078948B (zh
Inventor
于树金
边仁杰
任勇
白金成
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinan Iron And Steel Group Co ltd
Original Assignee
HEBEI WENFENG IRON AND STEEL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HEBEI WENFENG IRON AND STEEL CO Ltd filed Critical HEBEI WENFENG IRON AND STEEL CO Ltd
Priority to CN201110031260A priority Critical patent/CN102078948B/zh
Publication of CN102078948A publication Critical patent/CN102078948A/zh
Application granted granted Critical
Publication of CN102078948B publication Critical patent/CN102078948B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开一种电脉冲孕育连续铸钢浇注装置,包括中间罐、塞棒、水口、浸入水口和结晶器,在水口上设置有水口电脉冲孕育装置。其优点是金属液孕育后直接进入结晶器,克服了金属液孕育衰退的缺陷,孕育效果好,能够达到稳定生产的目的。

Description

一种电脉冲孕育连续铸钢浇注装置
技术领域
本发明涉及一种水口,尤其是一种电脉冲孕育连续铸钢浇注装置。
背景技术
申请号为98100543.8的金属液脉冲孕育处理方法的发明申请,公开了一种将电极插入冶金金属罐的钢液面下进行电脉冲孕育的方法。众所周知,冶金液体金属电脉冲孕育处理效果与处理后到结晶时间长短成反比关系。上述电脉冲孕育方法所处理好的金属液再浇注到结晶器内,所经历的时间比较长,由于孕育衰退的原因,很难在实际生产中起到满意的孕育效果。因此,设计一种金属液孕育后直接进入结晶器的电脉冲孕育连续铸钢浇注装置,是目前需要解决的技术问题。
发明内容
本发明所要解决的技术问题是提供一种金属液孕育后直接进入结晶器的电脉冲孕育连续铸钢浇注装置。
本发明解决其技术问题的技术方案是:
一种电脉冲孕育连续铸钢浇注装置,包括中间罐、塞棒、水口、浸入水口和结晶器,在水口上设置有水口电脉冲孕育装置。
本发明解决其技术问题的技术方案还可以是:
本发明在浸入水口上设置有浸入水口电脉冲孕育装置。
本发明所述的水口电脉冲孕育装置为镶嵌在水口上的两个电极对,所述的浸入水口电脉冲孕育装置为镶嵌在浸入水口上的两个电极对,镶嵌在水口上的两个电极对和镶嵌在浸入水口上的两个电极对均通过电连接件与电脉冲发生器电连接。
本发明所述的塞棒为电极式塞棒,电极式塞棒也与电脉冲发生器电连接,电极式塞棒与镶嵌在水口上的两个电极对中的任意一个电极均构成电极对。
本发明所述的结晶器与也与电脉冲发生器电连接,结晶器与浸入水口上的两个电极对中的任意一个电极均构成电极对。
本发明镶嵌在水口上的电极对与镶嵌在浸入水口上的电极的结构相同,电极为由两部分组合而成的复合电极,复合电极的其中一部分为一端为锥体的柱状石墨,复合电极的另一部分为以ZrO2为主要成分的柱体,ZrO2为主要成分的柱体与柱状石墨的平面端连接,复合电极被包裹在绝缘套内,复合电极的ZrO2端略伸出绝缘套,复合电极的石墨锥体部分完全伸出绝缘套,复合电极的ZrO2端为放电端,复合电极的石墨锥体端为受电端。
本发明所述的电连接件为两个绝缘体块,在每个绝缘体块上均嵌装由两个球缺形导体,嵌装在绝缘体块上的球缺形导体在绝缘体块的嵌装窝内可自由转动,在球缺形导体的平面上设置有与石墨锥体的锥面匹配的锥形凹槽,每个绝缘体块上均嵌装的两个球缺形导体之间的距离与镶嵌在水口上的两个电极对和镶嵌在浸入水口上的两个电极对之间的距离相等,在每个球缺形导体上引出的导线与电脉冲发生器电连接,两个绝缘体块通过活动夹紧装置夹紧。
本发明所述的活动夹紧装置由与其中一个绝缘体块固定连接的导杆、固定导杆上的电控伸缩装置、套装在导杆上的滑套和两端分别与滑套和另一个绝缘体块固定连接的曲杆构成,滑套与导杆滑动配合,在滑套上设置有两块带导向孔的导向板,电控伸缩装置的伸缩杆穿装在导向板的导向孔内,电控伸缩装置的伸缩杆与导向板的导向孔滑动配合,在两块导向板之间的伸缩杆上固定有弹簧挂板,在弹簧挂板与电控伸缩装置一侧的导向板之间固定有压缩弹簧。
本发明所述的塞棒的棒体为中空管体,在棒体的下端部连接有以ZrO2为主要成分的塞头,在中空管体的孔内穿装有与塞头连接的导电石墨体,在导电石墨体的上端固定连接有导线,导线穿出中空管体后与电脉冲发生器电连接,在塞棒悬臂的固定孔内镶有塞棒绝缘体,塞棒悬臂通过塞棒绝缘体与塞棒的中空螺杆绝缘。
本发明在浸入水口的内腔底部设置有以ZrO2为主要成分的内孔上小下大的缓冲环,在浸入水口的下端部设置有直径小于浸入水口内径且上小下大的垂直孔,缓冲环的内孔与垂直孔的内孔光滑过渡。
与现有技术相比,本发明将金属液孕育后直接进入结晶器,克服了金属液孕育衰退的缺陷,孕育效果好,能够达到稳定生产的目的。
附图说明
图1是本发明的系统结构示意图。
图2是本发明复合电极结构示意图。
图3是图1中件3的结构示意图(电极组装后)。
图4是图1中件6的结构示意图(电极组装后)。
图5是图4中A-A向剖视图。
图6是图1中件1的结构示意图。
图7是图4中B-B向剖视图。
图8是图4中C-C向剖视图。
具体实施方式
如图所示,一种电脉冲孕育连续铸钢浇注装置,包括中间罐2、塞棒1、水口3、浸入水口6和结晶器7,在水口2上设置有水口电脉冲孕育装置4。在浸入水口6上设置有浸入水口电脉冲孕育装置5。所述的水口电脉冲孕育装置4为镶嵌在水口3上的两个电极对,所述的浸入水口电脉冲孕育装置5为镶嵌在浸入水口6上的两个电极对,镶嵌在水口3上的两个电极对和镶嵌在浸入水口6上的两个电极对均通过电连接件与电脉冲发生器电连接。所述的塞棒1为电极式塞棒,电极式塞棒也与电脉冲发生器电连接,电极式塞棒与镶嵌在水口3上的两个电极对中的任意一个电极均构成电极对。所述的结晶器7与也与电脉冲发生器电连接,结晶器7与浸入水口6上的两个电极对中的任意一个电极均构成电极对。镶嵌在水口3上的电极对与镶嵌在浸入水口6上的电极的结构相同,电极为由两部分组合而成的复合电极,复合电极的其中一部分为一端为锥体的柱状石墨8,复合电极的另一部分为以ZrO2为主要成分的柱体9,ZrO2为主要成分的柱体9与柱状石墨8的平面端连接,复合电极被包裹在绝缘套10内,复合电极的ZrO2端略伸出绝缘套10,复合电极的石墨锥体部分完全伸出绝缘套10,复合电极的ZrO2端为放电端,复合电极的石墨锥体端为受电端。所述的电连接件为两个绝缘体块11、12,在每个绝缘体块上均嵌装由两个球缺形导体,嵌装在绝缘体块上的球缺形导体在绝缘体块的嵌装窝内可自由转动,在球缺形导体的平面上设置有与石墨锥体的锥面匹配的锥形凹槽,每个绝缘体块上均嵌装的两个球缺形导体之间的距离与镶嵌在水口3上的两个电极对和镶嵌在浸入水口6上的两个电极对之间的距离相等,在每个球缺形导体上引出的导线与电脉冲发生器电连接,两个绝缘体块通过活动夹紧装置夹紧。所述的活动夹紧装置由与其中一个绝缘体块11固定连接的导杆13、固定导杆13上的电控伸缩装置16、套装在导杆13上的滑套17和两端分别与滑套17和另一个绝缘体块12固定连接的曲杆18构成,滑套17与导杆13滑动配合,在滑套17上设置有两块带导向孔的导向板,电控伸缩装置16的伸缩杆15穿装在导向板的导向孔内,电控伸缩装置16的伸缩杆15与导向板的导向孔滑动配合,在两块导向板之间的伸缩杆上固定有弹簧挂板,在弹簧挂板与电控伸缩装置16一侧的导向板之间固定有压缩弹簧14。所述的塞棒1的棒体为中空管体,在棒体的下端部连接有以ZrO2为主要成分的塞头19,在中空管体的孔内穿装有与塞头19连接的导电石墨体20,在导电石墨体20的上端固定连接有导线21,导线21穿出中空管体后与电脉冲发生器电连接,在塞棒悬臂22的固定孔内镶有塞棒绝缘体23,塞棒悬臂22通过塞棒绝缘体23与塞棒的中空螺杆24绝缘。在浸入水口6的内腔底部设置有以ZrO2为主要成分的内孔上小下大的缓冲环27,在浸入水口6的下端部设置有直径小于浸入水口内径且上小下大的垂直孔26,缓冲环27的内孔与垂直孔26的内孔光滑过渡。

Claims (10)

1.一种电脉冲孕育连续铸钢浇注装置,包括中间罐(2)、塞棒(1)、水口(3)、浸入水口(6)和结晶器(7),其特征在于:在水口(2)上设置有水口电脉冲孕育装置(4)。
2.根据权利要求1所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:在浸入水口(6)上设置有浸入水口电脉冲孕育装置(5)。
3.根据权利要求1或2所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:所述的水口电脉冲孕育装置(4)为镶嵌在水口(3)上的两个电极对,所述的浸入水口电脉冲孕育装置(5)为镶嵌在浸入水口(6)上的两个电极对,镶嵌在水口(3)上的两个电极对和镶嵌在浸入水口(6)上的两个电极对均通过电连接件与电脉冲发生器电连接。
4.根据权利要求3所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:所述的塞棒(1)为电极式塞棒,电极式塞棒也与电脉冲发生器电连接,电极式塞棒与镶嵌在水口(3)上的两个电极对中的任意一个电极均构成电极对。
5.根据权利要求4所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:所述的结晶器(7)与也与电脉冲发生器电连接,结晶器(7)与浸入水口(6)上的两个电极对中的任意一个电极均构成电极对。
6.根据权利要求3所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:镶嵌在水口(3)上的电极对与镶嵌在浸入水口(6)上的电极的结构相同,电极为由两部分组合而成的复合电极,复合电极的其中一部分为一端为锥体的柱状石墨(8),复合电极的另一部分为以ZrO2为主要成分的柱体(9),ZrO2为主要成分的柱体(9)与柱状石墨(8)的平面端连接,复合电极被包裹在绝缘套(10)内,复合电极的ZrO2端略伸出绝缘套(10),复合电极的石墨锥体部分完全伸出绝缘套(10),复合电极的ZrO2端为放电端,复合电极的石墨锥体端为受电端。
7.根据权利要求6所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:所述的电连接件为两个绝缘体块(11、12),在每个绝缘体块上均嵌装由两个球缺形导体,嵌装在绝缘体块上的球缺形导体在绝缘体块的嵌装窝内可自由转动,在球缺形导体的平面上设置有与石墨锥体的锥面匹配的锥形凹槽,每个绝缘体块上均嵌装的两个球缺形导体之间的距离与镶嵌在水口(3)上的两个电极对和镶嵌在浸入水口(6)上的两个电极对之间的距离相等,在每个球缺形导体上引出的导线与电脉冲发生器电连接,两个绝缘体块通过活动夹紧装置夹紧。
8.根据权利要求7所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:所述的活动夹紧装置由与其中一个绝缘体块(11)固定连接的导杆(13)、固定导杆(13)上的电控伸缩装置(16)、套装在导杆(13)上的滑套(17)和两端分别与滑套(17)和另一个绝缘体块(12)固定连接的曲杆(18)构成,滑套(17)与导杆(13)滑动配合,在滑套(17)上设置有两块带导向孔的导向板,电控伸缩装置(16)的伸缩杆(15)穿装在导向板的导向孔内,电控伸缩装置(16)的伸缩杆(15)与导向板的导向孔滑动配合,在两块导向板之间的伸缩杆上固定有弹簧挂板,在弹簧挂板与电控伸缩装置(16)一侧的导向板之间固定有压缩弹簧(14)。
9.根据权利要求8所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:所述的塞棒(1)的棒体为中空管体,在棒体的下端部连接有以ZrO2为主要成分的塞头(19),在中空管体的孔内穿装有与塞头(19)连接的导电石墨体(20),在导电石墨体(20)的上端固定连接有导线(21),导线(21)穿出中空管体后与电脉冲发生器电连接,在塞棒悬臂(22)的固定孔内镶有塞棒绝缘体(23),塞棒悬臂(22)通过塞棒绝缘体(23)与塞棒的中空螺杆(24)绝缘。
10.根据权利要求1所述的一种电脉冲孕育连续铸钢浇注装置,其特征在于:在浸入水口(6)的内腔底部设置有以ZrO2为主要成分的内孔上小下大的缓冲环(27),在浸入水口(6)的下端部设置有直径小于浸入水口内径且上小下大的垂直孔(26),缓冲环(27)的内孔与垂直孔(26)的内孔光滑过渡。
CN201110031260A 2011-01-28 2011-01-28 一种电脉冲孕育连续铸钢浇注装置 Active CN102078948B (zh)