CN102020929A - Metal anticorrosion gel - Google Patents

Metal anticorrosion gel Download PDF

Info

Publication number
CN102020929A
CN102020929A CN2009101829410A CN200910182941A CN102020929A CN 102020929 A CN102020929 A CN 102020929A CN 2009101829410 A CN2009101829410 A CN 2009101829410A CN 200910182941 A CN200910182941 A CN 200910182941A CN 102020929 A CN102020929 A CN 102020929A
Authority
CN
China
Prior art keywords
corrosion
zinc oxide
water glass
metal anticorrosion
percentage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2009101829410A
Other languages
Chinese (zh)
Inventor
付小建
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009101829410A priority Critical patent/CN102020929A/en
Publication of CN102020929A publication Critical patent/CN102020929A/en
Pending legal-status Critical Current

Abstract

The invention discloses metal anticorrosion gel, which is prepared by mixing silica sol, methyltrimethylsilane, zinc oxide and potash water glass. The metal anticorrosion gel has reasonable formula, good working effect and low production cost.

Description

Anti-corrosion of metal glue
Technical field:
The present invention relates to a kind of anti-corrosion of metal glue.
Background technology:
Generally there is certain shortcoming in existing anti-corrosion of metal glue on the work effect, production cost is also higher.
Summary of the invention:
The object of the present invention is to provide a kind of prescription reasonable, the anti-corrosion of metal glue of good working effect.
Technical solution of the present invention is:
A kind of anti-corrosion of metal glue is characterized in that: mixed by following component in percentage by weight and form:
Silicon sol 20~40%
Methyl trimethoxy base silane 1~5%
Zinc oxide 5~10%
The potash water glass surplus.
Described anti-corrosion of metal glue, form by following component in percentage by weight mixing:
Silicon sol 26%
Methyl trimethoxy base silane 4%
Zinc oxide 7%
The potash water glass surplus.
Described anti-corrosion of metal glue, form by following component in percentage by weight mixing:
Silicon sol 36%
Methyl trimethoxy base silane 2%
Zinc oxide 8%
The potash water glass surplus.
The present invention fills a prescription rationally, good working effect, and production cost is low.
The invention will be further described below in conjunction with embodiment.
Embodiment:
Embodiment 1:
A kind of anti-corrosion of metal glue, form by following component in percentage by weight mixing:
Silicon sol 26%
Methyl trimethoxy base silane 4%
Zinc oxide 7%
The potash water glass surplus.
Embodiment 2:
A kind of anti-corrosion of metal glue, form by following component in percentage by weight mixing:
Silicon sol 36%
Methyl trimethoxy base silane 2%
Zinc oxide 8%
The potash water glass surplus.

Claims (3)

1. anti-corrosion of metal glue is characterized in that: mixed by following component in percentage by weight and form:
Silicon sol 20~40%
Methyl trimethoxy base silane 1~5%
Zinc oxide 5~10%
The potash water glass surplus.
2. anti-corrosion of metal glue according to claim 1 is characterized in that: mixed by following component in percentage by weight and form:
Silicon sol 26%
Methyl trimethoxy base silane 4%
Zinc oxide 7%
The potash water glass surplus.
3. anti-corrosion of metal glue according to claim 1 is characterized in that: mixed by following component in percentage by weight and form:
Silicon sol 36%
Methyl trimethoxy base silane 2%
Zinc oxide 8%
The potash water glass surplus.
CN2009101829410A 2009-09-11 2009-09-11 Metal anticorrosion gel Pending CN102020929A (en)