CN102002230A - Environmentally-friendly luminous nylon 12 material - Google Patents
Environmentally-friendly luminous nylon 12 material Download PDFInfo
- Publication number
- CN102002230A CN102002230A CN 201010528715 CN201010528715A CN102002230A CN 102002230 A CN102002230 A CN 102002230A CN 201010528715 CN201010528715 CN 201010528715 CN 201010528715 A CN201010528715 A CN 201010528715A CN 102002230 A CN102002230 A CN 102002230A
- Authority
- CN
- China
- Prior art keywords
- nylon
- percent
- environmental protection
- environmentally
- lubricant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an environmentally-friendly luminous nylon 12 material. The material is characterized by consisting of the following components in percentage by weight: 77.5 to 96 percent of nylon, 1.0 to 5.0 percent of luminous agent, 0.1 to 2.0 percent of antioxidant, 0.1 to 2.0 percent of lubricant and 1.3 to 20.5 percent of other aids. The environmentally-friendly luminous nylon 12 material of the invention can automatically release light ray energy absorbed in the presence of light rays for automatic lightening without any support of any external energy source in the absence of light ray irradiation and the brightness is easy to recognize clearly; a product is attractive, convenient for injection molding and extrusion processing and convenient to produce and purchase, and has high comprehensive mechanical and physical performance and high production efficiency; simultaneously, the product meets all environmental requirements, so that product competitiveness is enhanced comprehensively.
Description
Technical field
The present invention relates to a kind of organic polymer composite, more particularly, relate to a kind of noctilucence nylon 12 materials.The invention still further relates to the method for making this noctilucence nylon 12 materials.
Background technology
Nylon is used one of maximum several engineering plastics at present, his amide group has polarity, has well-set hydrogen bond in his structure, and fusing point is higher, have good physical and mechanical property and wear resistance and self lubricity, these comprehensive characteristics are that other plastics are not available.Nylon 12 is except the characteristic with general nylon, be a kind of of relative density minimum in the existing industrialization nylon product, have the advantages that water-absorbent is low, snappiness good, wear resistance is good, be suitable for producing flexible products, its forming process is good, and product size is good, and is good with the cementability of metal, can injection moulding and extrusion moulding processing, be suitable for producing electric precise part, and various flexible pipe, flexible pipe, sheath, sheet material, film, also can make the metallic surface powder coating.
Current social is very high for energy-saving and emission-reduction, low-carbon economy cry, and the Chinese government promotes energetically.The physical and mechanical properties of nylon 12 materials own is good, and gloss is splendid, if possess the noctilucence feature again, is convenient to injection moulding and extrudes processing processing, will play good social agency, creates good economic worth simultaneously.
Summary of the invention
The objective of the invention is to, provide a kind of light ray energy that is absorbed when being released in light automatically and luminous automatically, its light is easy to environmental protection noctilucence nylon 12 materials of clear identification and environmental protection.
In order to achieve the above object, technical scheme provided by the invention is as follows: form nylon 12:77.5-96% by weight by following composition; Luminous agent: 1.0-5.0%; Oxidation inhibitor: 0.1-2.0%; Lubricant: 0.1-2.0%; Other auxiliary agents: 1.3-20.5%.
Environmental protection noctilucence nylon 12 preparation methods of the present invention, comprise the steps: earlier with nylon 12 and oxidation inhibitor, luminous agent, lubricant, other auxiliary agents proportionally after the weighing in mixer low speed mixing 10 minutes, after more in time through parallel parallel dual-screw extruding machine under the screw combinations situation that certain intensity is sheared, keeping under the good vacuum state, extrude with certain screw speed is mixing, the pelletizing of water-cooled tie rod makes environmental protection noctilucence nylon 12 materials through screening and dewatering.
Environmental protection noctilucence nylon 12 materials of the present invention, under the dull thread radiation situation, do not need external any energy support, the light ray energy that is absorbed in the time of can being released in light automatically and luminous automatically, its light is easy to clear identification, product appearance is attractive in appearance, and comprehensive physical is good, is convenient to injection moulding and extrudes processing, the production efficiency height, and production procurement is convenient, also meets all environmental requirements, comprehensive like this product competitiveness that improved simultaneously.
Embodiment
Below be the embodiment of environmental protection noctilucence nylon 12 materials of the present invention, therefore do not limit protection scope of the present invention.
Embodiment one, and a kind of environmental protection noctilucence nylon 12 materials are provided, and forms nylon 12:88.8% by weight by following composition; Luminous agent: 3.2%; Oxidation inhibitor: 1.0%, lubricant: 0.3%; Other auxiliary agents: 6.7%.
Concrete steps of the present invention are as follows: earlier with nylon 12 and oxidation inhibitor, luminous agent, lubricant, other auxiliary agents proportionally after the weighing in mixer low speed mixing 10 minutes, mixer adopts low speed mixing, stainless steel, paddle should with the barrel gap less than 0.5 centimetre, the supplementary material mixed effect should visual various particles and powder even substantially, do not have obvious agglomerate or gather, and then in time through parallel parallel dual-screw extruding machine under the screw combinations situation that certain intensity is sheared, twin screw extruder uses 36 length-to-diameter ratios, keeping under the good vacuum state, extrude with certain screw speed is mixing, the pelletizing of water-cooled tie rod makes environmental protection noctilucence nylon 12 materials through screening and dewatering.
The above; it only is the specific embodiment of the present invention; but protection scope of the present invention is not limited thereto; any those of ordinary skill in the art are in the disclosed technical scope of the present invention; variation or the replacement that can expect without creative work all should be encompassed within protection scope of the present invention.Therefore, protection scope of the present invention should be as the criterion with the protection domain that claims were limited.
Claims (2)
1. environmental protection noctilucence nylon 12 materials is characterized in that, it forms nylon by weight by following composition: 77.5-96%; Luminous agent: 1.0-5.0%; Oxidation inhibitor: 0.1-2.0%; Lubricant: 0.1-2.0%; Other auxiliary agents: 1.3-20.5%.
2. environmental protection noctilucence nylon 12 preparation methods, it is characterized in that, comprise the steps: earlier with nylon 12 and oxidation inhibitor, luminous agent, lubricant, other auxiliary agents proportionally after the weighing in mixer low speed mixing 10 minutes, after more in time through parallel parallel dual-screw extruding machine under the screw combinations situation that certain intensity is sheared, keeping under the good vacuum state, extrude with certain screw speed is mixing, the pelletizing of water-cooled tie rod makes environmental protection noctilucence nylon 12 materials through screening and dewatering.