CN101935149A - Stabilizing device for tin bath hot-end glass strip - Google Patents

Stabilizing device for tin bath hot-end glass strip Download PDF

Info

Publication number
CN101935149A
CN101935149A CN 201010142211 CN201010142211A CN101935149A CN 101935149 A CN101935149 A CN 101935149A CN 201010142211 CN201010142211 CN 201010142211 CN 201010142211 A CN201010142211 A CN 201010142211A CN 101935149 A CN101935149 A CN 101935149A
Authority
CN
China
Prior art keywords
tin bath
glass ribbon
molten tin
hot junction
glass strip
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 201010142211
Other languages
Chinese (zh)
Other versions
CN101935149B (en
Inventor
李兆廷
陈发伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beijing Yuanda Xinda Technology Co Ltd
Original Assignee
HEBEI DONGXU INVESTMENT Corp CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HEBEI DONGXU INVESTMENT Corp CO Ltd filed Critical HEBEI DONGXU INVESTMENT Corp CO Ltd
Priority to CN2010101422110A priority Critical patent/CN101935149B/en
Publication of CN101935149A publication Critical patent/CN101935149A/en
Application granted granted Critical
Publication of CN101935149B publication Critical patent/CN101935149B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a stabilizing device for a tin bath hot-end glass strip, solves the problem of poor transverse stability of the glass strip in the prior art, overcomes the disadvantages of the stabilizing device for the tin bath hot-end glass strip without regional adjustment, reduces accidents, such as loosing of edge of the glass strip and the like and improves the production quality. The adopted technical scheme is that: the structure comprises a base at a lower layer and a graphite device, wherein the graphite device is fixed on the base through a connecting bolt and provided with a groove for holding tin-lead mixed melt; and a cooling device is arranged in the groove of the graphite device. By effectively adjusting the contact condition of the stabilizing device and the tin bath hot-end glass strip, the stability of the tin bath hot-end glass strip is obviously improved, the accidents, such as loosing of edge of the glass strip and the like, are greatly reduced, and the production quality of ultra-thin glass is greatly improved. The stabilizing device has the advantages of simple structure, high practicability and good stabilizing effect.

Description

The stabilizing deyice of a kind of molten tin bath hot junction glass ribbon
Technical field
The present invention relates to a kind of modifying device of float shaping, when particularly producing super-thin electronic glass such as PDP, the device of the stability of control molten tin bath hot junction glass ribbon.
Background technology
When using float glass production, particularly produce extraordinary ultra-thin glass, if during glass such as PDP, STN,, increased the transverse temperature difference of whole molding space because the drawing amount is little, cause glass ribbon lateral stability variation; Because the high-quality requirement of extraordinary ultra-thin glass has been introduced the equipment of adjustment tin such as line motor to flow in the molten tin bath hot junction, more increased and caused the unstable of glass ribbon simultaneously in zone, molten tin bath hot junction; It is very thin to add extraordinary ultra-thin glass itself, be subjected to the outer room condition influence clearly, only wait the stability of adjusting molten tin bath hot junction glass ribbon traditionally, and do not have a kind of specific equipment that is adapted under this district's environment that the stability of glass ribbon is regulated by angle, speed, compression distance and undercut amount to edge machine.
On certain 300 tons of/day ultra-thin float glass line of electronic-grade, actual drawing amount when it produces electronic glass has been reduced to 100 tons/day, because the reduction significantly of drawing amount, the heat of being brought in the molten tin bath by glass metal also obviously reduces, the transverse temperature difference of tin liquor has had tangible increase in the whole molten tin bath, cause the stable also remarkable variation of glass ribbon in the molten tin bath hot junction, poor for improving the molten tin bath transverse temperature, this line has been opened the electric heater of limit portion, also linear electric motors have been installed simultaneously, have been improved transverse temperature difference with this in zone, molten tin bath hot junction symmetry; Though the transverse temperature difference improves significantly, but, increased the labile factor of molten tin bath hot junction glass ribbon owing to adopted multiple measure, the vibration problems of hot junction glass ribbon takes place often, cause the accidents such as off-clip of glass ribbon when serious, can't ordinary production, bring bigger influence to yield and quality.
Summary of the invention
Poor in order to solve in the prior art glass ribbon lateral stability, remedy and do not have regional defective of regulating the stability devices of molten tin bath hot junction glass ribbon, reduce the generation of the accidents such as off-clip of glass ribbon, improve the quality of production, the present invention has designed a kind of this regional environment that is fit to fully, and the device that can effectively adjust the stability of glass ribbon in this zone.The technical scheme that adopts is: the stabilizing deyice of a kind of molten tin bath hot junction glass ribbon, be fixed on the inside of molten tin bath, include in the structure: the pedestal that is positioned at lower floor, be fixed on the graphite device that being provided with on the pedestal fills the plumbous consolute body of tin groove by joint bolt, be provided with refrigerating unit in the groove of graphite device.
The invention has the beneficial effects as follows: the present invention adopts sillimanite in the refractory materials as pedestal, the graphite device of special shape requirement is installed in the above, the bolt that graphite device and sillimanite are made with tungsten is connected and fixed, dug groove in the graphite device, the body cell body fills the consolute body of metallic lead and tin, in the consolute body, have one be connected with water coolant and and entire equipment together fixed U type water pipe pass through, the consolute body of water pipe cool metal lead and tin, the consolute body is given the suitable cooling of graphite, so just promptly slowed down the infringement of hot environment to the graphite device, increased rigidity again with the glass metal of graphite device contacts, this rigidity makes the glass ribbon can be with to a certain degree " dependence " graphite and do not swing, increase its stability, also reduce simultaneously the graphite material temperature too high and and glass ribbon adherent probability takes place.By the effective adjustment to the contact condition of this stabilizing deyice and molten tin bath hot junction glass ribbon, the stability of molten tin bath hot junction glass ribbon has obtained tangible improvement, accident such as off-clip takes place also significantly reduced, and the yield and quality of ultra-thin glass improves greatly.
The present invention is simple in structure, and is practical, and stabilising effect is good.
Description of drawings
Fig. 1 is a vertical view of the present invention.
Fig. 2 is the A-A sectional view of Fig. 1.
Fig. 3 is the B-B sectional view of Fig. 1
Among the figure, 1 is pedestal, and 2 is the graphite device, and 3 is joint bolt, and 4 is water-cooled tube, and 5 is upper surface, and 6 is holding bolt, and 7 is the thin slice firmware.
Embodiment
Referring to accompanying drawing, the technical solution used in the present invention is: the stabilizing deyice of a kind of molten tin bath hot junction glass ribbon, be fixed on the inside of molten tin bath, include in the structure: the pedestal 1 that is positioned at lower floor, be fixed on the graphite device 2 that being provided with on the pedestal 1 fills the plumbous consolute body of tin groove by joint bolt 3, be provided with refrigerating unit in the groove of graphite device 2.
In the technical scheme of the present invention, described refrigerating unit is a water-cooled tube 4, is arranged on the bottom of groove by means of being wrapped in outer field tungsten thin slice firmware 7 and holding bolt 6, and water-cooled tube 4 is connected with supporting cold feed device.
In the technical scheme of the present invention, described water-cooled tube 4 adopts the U-shaped loop vertically to be arranged in the groove of graphite device 2.
In the technical scheme of the present invention, the material of described pedestal 1 adopts the sillimanite of refractory materials.
In the technical scheme of the present invention, upper surface 5 two ends of described graphite device 2 are that circular-arc middle portion is a rectangle.
In the technical scheme of the present invention, the circular-arc arc diameter of described upper surface 5 is 5000-5090mm, and the length of rectangular edges is 70-90mm.
In the technical scheme of the present invention, the material of described joint bolt 3 is a tungsten.
In the technical scheme of the present invention, the material of described water-cooled tube 4 adopt high temperature resistance and not with the plumbous consolute body of the tin metal material that reacts, for example: 1Cr18N, 9Ti.
The present invention adopts sillimanite pedestal 1, under the condition of high temperature that can reach in the molten tin bath hot junction, its still can keep enough strength support above it graphite device 2 and the metal slicker solder consolute body in the groove in the graphite device 2, structures such as water bag, and itself shaking property of heat resistanceheat resistant is very good, is not easy damaging than great fluctuation process of Yin Wendu in regular job; Because of refractory materials sillimanite and glass ribbon adhere to easily, and do not make a difference, also do not have what influence with the bottom land brick, so whole sillimanite pedestal 1 needs suitable height and is immersed in the tin liquor fully with tin liquor almost; The chain connecting bolt material of pedestal 1 and graphite device 2 is a tungsten, and its fusing point height has higher intensity in the molten tin bath hot junction, and with metallic tin, refractory materials physics and chemical reaction does not take place, is very suitable material.
The present invention it adopt sillimanite in the refractory materials as pedestal 1, the graphite device 2 of special shape requirement is installed in the above, the joint bolt 3 that graphite device 2 and pedestal 1 usefulness tungsten are made is fixing, dug cell body in the graphite device 2, cell body fills the consolute body of metallic lead and tin, in the consolute body, have one be connected with water coolant and and entire equipment together fixed U type water-cooled tube 4 pass through, the consolute body of water-cooled tube 4 cool metals lead and tin, the consolute body is given the suitable cooling of graphite, so just promptly slowed down the infringement of hot environment to graphite body, increased the rigidity of the glass metal that contacts with graphite again, this rigidity makes the glass ribbon can be with to a certain degree " dependence " graphite and do not swing, increase its stability, also reduce simultaneously the graphite material temperature too high and and glass ribbon adherent probability takes place.By the effective adjustment to the contact condition of this stabilizing deyice and molten tin bath hot junction glass ribbon, the stability of molten tin bath hot junction glass ribbon has obtained tangible improvement, accident such as off-clip takes place also significantly reduced, and the yield and quality of ultra-thin glass improves greatly.

Claims (8)

1. the stabilizing deyice of a molten tin bath hot junction glass ribbon, be fixed on the inside of molten tin bath, it is characterized in that: include in the structure: the pedestal (1) that is positioned at lower floor, be fixed on the graphite device (2) that being provided with on the pedestal (1) fills the plumbous consolute body of tin groove by joint bolt (3), be provided with refrigerating unit in the groove of graphite device (2).
2. the stabilizing deyice of a kind of molten tin bath according to claim 1 hot junction glass ribbon, it is characterized in that: described refrigerating unit is water-cooled tube (4), be arranged on the bottom of groove by means of being wrapped in outer field tungsten thin slice firmware (7) and holding bolt (6), water-cooled tube (4) is connected with supporting cold feed device.
3. the stabilizing deyice of a kind of molten tin bath according to claim 2 hot junction glass ribbon is characterized in that: described water-cooled tube (4) adopts the U-shaped loop vertically to be arranged in the groove of graphite device (2).
4. the stabilizing deyice of a kind of molten tin bath according to claim 1 hot junction glass ribbon is characterized in that: the material of described pedestal (1) adopts the sillimanite of refractory materials.
5. the stabilizing deyice of a kind of molten tin bath according to claim 1 hot junction glass ribbon is characterized in that: upper surface (5) two ends of described graphite device (2) are that circular-arc middle portion is a rectangle.
6. the stabilizing deyice of a kind of molten tin bath according to claim 5 hot junction glass ribbon is characterized in that: the circular-arc arc diameter of described upper surface (5) is 5000-5090mm, and the length of rectangular edges is 70-90mm.
7. the stabilizing deyice of a kind of molten tin bath according to claim 1 hot junction glass ribbon, it is characterized in that: the material of described joint bolt (3) is a tungsten.
8. the stabilizing deyice of a kind of molten tin bath according to claim 2 hot junction glass ribbon is characterized in that: the material of described water-cooled tube (4) adopt high temperature resistance and not with the plumbous consolute body of the tin metal material that reacts, for example: 1Cr18N, 9Ti.
CN2010101422110A 2010-04-09 2010-04-09 Stabilizing device for tin bath hot-end glass strip Active CN101935149B (en)