CN101928522A - Leather finishing agent - Google Patents
Leather finishing agent Download PDFInfo
- Publication number
- CN101928522A CN101928522A CN2009101523034A CN200910152303A CN101928522A CN 101928522 A CN101928522 A CN 101928522A CN 2009101523034 A CN2009101523034 A CN 2009101523034A CN 200910152303 A CN200910152303 A CN 200910152303A CN 101928522 A CN101928522 A CN 101928522A
- Authority
- CN
- China
- Prior art keywords
- grams
- stirring
- finishing agent
- leather
- pcp
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a leather finishing agent, which consists of 500 grams of castor oil, 500 grams of sodium carbonate, 500 grams of hydrogen peroxide, 600 grams of gasoline, 600 grams of ozocerite, 500 grams of oxidized microcrystalline wax, 300 grams of sodium pentachlorophenol (PCP-Na), 600 grams of formaldehyde, 100 grams of camphor oil, 300 grams of essence, 200 grams of isopropyl alcohol and 5,000 grams of lithopone. The leather finishing agent is prepared by blending the castor oil, the hydrogen peroxide, the ozocerite and the oxidized microcrystalline wax together according to a ratio, adding the gasoline into the mixed material, heating and stirring to obtain emulsified liquid; adding the sodium carbonate and the PCP-Na into 95 DEG C water, and stirring to obtain the emulsified liquid; mixing the two parts of emulsified liquid, keeping temperature at 55 DEG C, uniformly blending and stirring to obtain the emulsified liquid, adding the camphor oil into the emulsified liquid and continuously stirring, adding the formaldehyde, the essence, the isopropyl alcohol and the lithopone into the mixed solution, uniformly blending and stirring the materials in rest water to obtain emulsion; and spraying the emulsion into a pot.
Description
Technical field
The present invention relates to a kind of finishing agent, particularly a kind of leather finishing agent.Belong to the daily-use chemical industry technical field.
Background technology
The raw material of process hides is an animal skin, though we the life in modal be pigskin, ox-hide, sheepskin, in fact most of animal skin may be used to process hides.Just the quality of ox-hide, pigskin and sheepskin is good and output is big, is the main raw material of process hides.
At present, when the greasy dirt of people on removing leather, grease spot, dirt, all use article such as washing powder, sanitising agent to clean generally speaking, because people do not understand the smooth, pliable and tough etc. of leather cortex, though the effect of play decontamination, deoiling, but after leather is subjected to washing away of washing powder, sanitising agent, water, easily cause the cortex decolouring of leather surface, withered, shattered crack, make smooth, pliable and tough, the bright function of leather be subjected to serious destruction, and reduce work-ing life of leather fast, cause very big waste.
Summary of the invention
The objective of the invention is to provide a kind of: result of use is good, and is with low cost, decontamination, degreasing, decontamination dirt, the spot that deoils, a kind of leather finishing agent that the mildew performance is good.Having overcome article such as use washing powder, sanitising agent cleans, though the effect of play decontamination, deoiling, but after leather is subjected to washing away of washing powder, sanitising agent, water, easily cause the cortex decolouring of leather surface, withered, shattered crack, make smooth, pliable and tough, the bright function of leather be subjected to serious destruction, and reduce work-ing life of leather fast, cause the defective of very big waste.
Solving the scheme that its technical problem takes is: a kind of leather finishing agent, it by: Viscotrol C 500 grams, soda ash 500 grams, hydrogen peroxide 500 grams, gasoline 600 grams, ceresine 600 grams, oxidized microcrystalline wax 500 grams, PCP-sodium 300 grams, formaldehyde 600 grams, white oil of camphor 100 grams, essence 300 grams, Virahol 200 grams, zinc sulfide white 5000 grams are formed.
In proportion Viscotrol C, hydrogen peroxide, ceresine, oxidized microcrystalline wax all are mixed, add gasoline, heated and stirred becomes emulsion liquid.Soda ash, PCP-sodium are added 95 ℃ water, stir into emulsion liquid.Then both are mixed, and keep 55 ℃ of temperature, thorough mixing stirs after stirring into the oil that camphorates behind the emulsion liquid, adds formaldehyde, essence, Virahol, zinc sulfide white again, and the remainder water thorough mixing stirs into emulsion liquid and injects and spray jar.
Beneficial effect: owing to adopted such scheme; raw material in the prescription all adopts nontoxic; free of contamination batching; the method that adds easy handling then is made; material is easily got; prescription and compound method are simple; it is good that the leather gloss agent that makes has a cleaning performance; remove various dirts; greasy dirt; oil mark; mildew; dirt effect performance is strong; make leather keep light as new; smooth; snappiness reaches good luminance brightness well; and effectively prevented leather cortex decolouring; withered; the phenomenon of shattered crack; effectively increase the work-ing life and the defencive function of leather, reached purpose of the present invention.This formula compatibility is simple, and result of use is good, and is with low cost, and decontamination, degreasing, decontamination dirt, the spot that deoils, mildew performance are good, has effectively solved to use that cleaning such as washing powder, brightening agent easily cause the cortex decolouring, dry up, the defective of shattered crack.
Embodiment
Embodiment 1: Viscotrol C 500 grams, soda ash 500 grams, hydrogen peroxide 500 grams, gasoline 600 grams, ceresine 600 grams, oxidized microcrystalline wax 500 grams, PCP-sodium 300 grams, formaldehyde 600 grams, white oil of camphor 100 grams, essence 300 grams, Virahol 200 grams, zinc sulfide white 5000 grams are formed.
Compound method: in proportion Viscotrol C, hydrogen peroxide, ceresine, oxidized microcrystalline wax all are mixed, add gasoline, heated and stirred becomes emulsion liquid.Soda ash, PCP-sodium are added 95 ℃ water, stir into emulsion liquid.Then both are mixed, and keep 55 ℃ of temperature, thorough mixing stirs after stirring into the oil that camphorates behind the emulsion liquid, adds formaldehyde, essence, Virahol, zinc sulfide white again, and the remainder water thorough mixing stirs into emulsion liquid and injects and spray jar.
Using method: the leather gloss agent of preparation is extruded a little, can accomplish to remove various dirts, greasy dirt, oil mark, mildew, and can produce effects such as smooth, pliable and tough, waterproof, glazing to leather, keep leather polishing as newly.
Viscotrol C in this prescription, soda ash, hydrogen peroxide, gasoline, ceresine, oxidized microcrystalline wax, PCP-sodium, formaldehyde, white oil of camphor, essence, Virahol, zinc sulfide white are all buied from market.
Claims (2)
1. a leather finishing agent is characterized in that: be made up of Viscotrol C 500 grams, soda ash 500 grams, hydrogen peroxide 500 grams, gasoline 600 grams, ceresine 600 grams, oxidized microcrystalline wax 500 grams, PCP-sodium 300 grams, formaldehyde 600 grams, white oil of camphor 100 grams, essence 300 grams, Virahol 200 grams, zinc sulfide white 5000 grams.
2. a kind of leather finishing agent according to claim 1 is characterized in that: in proportion Viscotrol C, hydrogen peroxide, ceresine, oxidized microcrystalline wax all are mixed, add gasoline, heated and stirred becomes emulsion liquid.Soda ash, PCP-sodium are added 95 ℃ water, stir into emulsion liquid.Then both are mixed, and keep 55 ℃ of temperature, thorough mixing stirs after stirring into the oil that camphorates behind the emulsion liquid, adds formaldehyde, essence, Virahol, zinc sulfide white again, and the remainder water thorough mixing stirs into emulsion liquid and injects and spray jar.