CN101870183A - Antiseize scald knife - Google Patents
Antiseize scald knife Download PDFInfo
- Publication number
- CN101870183A CN101870183A CN201010212133A CN201010212133A CN101870183A CN 101870183 A CN101870183 A CN 101870183A CN 201010212133 A CN201010212133 A CN 201010212133A CN 201010212133 A CN201010212133 A CN 201010212133A CN 101870183 A CN101870183 A CN 101870183A
- Authority
- CN
- China
- Prior art keywords
- antiseize
- knife
- scald
- teflon
- edge
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an antiseize scald knife comprising a knife body, wherein a teflon antiseize layer is coated on the outside of a blade of the knife body. The antiseize scald knife has simple structure, easy manufacture, favorable high-temperature resistant performance and antiseize performance and smooth film feeding, and the prepared product has no blur or damage and has low fraction defective.
Description
Technical field
The present invention relates to the boiling hot cutter on the Bag Making Machine, particularly, is a kind of Antiseize scald knife.
Background technology
Boiling hot cutter is one of critical component of Bag Making Machine, and its material of main part is generally brass, works under 260 ℃~300 ℃ the temperature of being everlasting; Coking can take place because plastic sheeting is subjected to the influence of high-temperature factor, therefore after work a period of time, the plastic sheeting that always has part generation coking sticks on the edge of a knife, and cumulative trend arranged, this will have a strong impact on the sharpness that scalds the edge of a knife and cause film feeding to have some setbacks, and then the product burr that makes is increased even breakage can not be used, i.e. the fraction defective height of product.
Summary of the invention
The object of the present invention is to provide a kind of Antiseize scald knife, it has the good temperature resistance energy, can avoid the residue due to the film Yin Gaowen to stick on the edge of a knife effectively.
Concrete technical scheme of the present invention is:
A kind of Antiseize scald knife comprises cutter hub, and the edge of a knife of described cutter hub is externally coated with the Teflon adherent layer.
Described Teflon adherent layer is coated on edge of a knife outside by Teflon coating and forms.Teflon can tolerate 350 ℃~400 ℃ high temperature, be far longer than the normal working temperature (260 ℃~300 ℃) of scalding cutter, Teflon also has excellent chemical inertness, insulation stability and low frictional properties simultaneously, thereby the plastic sheeting residue that can avoid Yin Gaowen that carbonization takes place effectively sticks on the edge of a knife, even thereby guaranteed that boiling hot cutter still has preferably sharpness after working long hours and can guarantee that film feeding is smooth and easy, i.e. operate as normal for a long time, making the product that makes not have burr does not have breakage, and the fraction defective of product is low.
Antiseize scald knife of the present invention has following beneficial effect: 1. simple structure, make easily, and with low cost; 2. have good temperature resistance energy and anti-adhesion performance, can effectively avoid the bonding of thin film residue; 3. film feeding is smooth and easy, and the product that makes does not have burr and do not have breakage, good product quality; 4. the product fraction defective is low, and the loss in the production process is lower than 3%, and cost is saved greatly.
Description of drawings
With embodiment the present invention is described in further detail with reference to the accompanying drawings below.
Fig. 1 is a structural representation of the present invention.
Among the figure: 1, cutter hub; 2, the edge of a knife; 3, Teflon adherent layer.
The specific embodiment
As shown in Figure 1, provided an embodiment of the present invention.Antiseize scald knife comprises the cutter hub 1 that brass is made into, and the edge of a knife 2 of cutter hub 1 is externally coated with Teflon adherent layer 3.Teflon can tolerate 350 ℃~400 ℃ high temperature, be far longer than the normal working temperature (260 ℃~300 ℃) of scalding cutter, Teflon also has excellent chemical inertness, insulation stability and low frictional properties simultaneously, thereby the plastic sheeting residue that can avoid Yin Gaowen that carbonization takes place effectively sticks on the edge of a knife, even thereby guaranteed that boiling hot cutter still has preferably sharpness after working long hours and can guarantee that film feeding is smooth and easy, making the product that makes not have burr does not have breakage, and the product fraction defective reduces greatly.
Claims (1)
1. an Antiseize scald knife comprises cutter hub, it is characterized in that: the edge of a knife of described cutter hub is externally coated with the Teflon adherent layer.