CN101824952A - Welding-spot free hollow mosaic glass and assembling method thereof - Google Patents

Welding-spot free hollow mosaic glass and assembling method thereof Download PDF

Info

Publication number
CN101824952A
CN101824952A CN201010169245A CN201010169245A CN101824952A CN 101824952 A CN101824952 A CN 101824952A CN 201010169245 A CN201010169245 A CN 201010169245A CN 201010169245 A CN201010169245 A CN 201010169245A CN 101824952 A CN101824952 A CN 101824952A
Authority
CN
China
Prior art keywords
glass
mosaic
glass layer
mosaic glass
filler rod
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010169245A
Other languages
Chinese (zh)
Inventor
王卫东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHANGSHU ZHONGXIN BUILDING MATERIALS Co Ltd
Original Assignee
CHANGSHU ZHONGXIN BUILDING MATERIALS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGSHU ZHONGXIN BUILDING MATERIALS Co Ltd filed Critical CHANGSHU ZHONGXIN BUILDING MATERIALS Co Ltd
Priority to CN201010169245A priority Critical patent/CN101824952A/en
Publication of CN101824952A publication Critical patent/CN101824952A/en
Pending legal-status Critical Current

Abstract

The invention discloses welding-spot free hollow mosaic glass, which is formed by overlapping one mosaic glass layer and sealing glass layers arranged on two sides of the mosaic glass layer. A sealing strip is arranged on the peripheral edge part between the mosaic glass layer and the sealing glass layers, so that an air-sealed cavity is formed between the mosaic glass layer and the sealing glass layers; the mosaic glass layer comprises an aluminum alloy frame, at least two pieces of glass and spliced insertion strips; the glass is spliced into a whole through the spliced insertion strips, positioned on the same plane and fixed on the aluminum alloy frame. The invention has the following effects of directly mounting without welding, having the advantages of convenient mounting, energy saving and environmental protection and thoroughly solving the thickness problem of the hollow mosaic glass. The invention also discloses an assembling method of the welding-spot free hollow mosaic glass.

Description

A kind of welding-spot free hollow mosaic glass and assemble method
Technical field
The present invention relates to a kind of welding-spot free hollow mosaic glass, belong to the glass door and window technical field, the invention still further relates to a kind of assemble method of this kind hollow mosaic glass simultaneously.
Background technology
Hollow glass is a kind of good heat insulation, sound insulation, and can reduce the New Building Materials of building deadweight, it is with two (or multi-disc) glass, use high strength high-air-tightness compound binding agent, with sheet glass and the aluminum alloy frame bonding that includes desiccant, the high-effect sound-insulating and heat-insulating glass of making.The multiple performance of hollow glass is superior to ordinary double-layer glass, has therefore obtained the approval of countries in the world, and hollow glass is with two or multi-disc glass evenly separates with effective support and the perimeter bond sealing, makes the glass product that is formed with the dry gas space between glassy layer.Its main material is glass, aluminium spacer bar, bent angle bolt, butyl rubber, poly-sulphur glue, desiccant.
Mosaic glass makes materials such as utilizing various rules, fluid sealant with tempered glass, float glass and stained glass, and through engraving, grinding is milled, welding, the high-grade art glass that technologies such as cleaning-drying sealing manufacture.Mosaic glass can embody the variation of home room, be have randomness in the ornamental glass a kind of, glass, clear exquisitely carved glass that it can be dim with glass, the cloudy surface of multicolour pattern make up arbitrarily, reasonably collocation " intention ", present different aesthetic feelings, make us intoxicated more.
In the prior art, the glass building material manufacturer is for advantage heat insulation in conjunction with hollow glass, sound insulation, the advantage elegant in appearance with mosaic glass, develop a kind of hollow mosaic glass, its rule of this kind mosaic glass is to be fixed on the bezel by the mode of welding, therefore then a mosaic glass and two seal glass are installed and fixed by weather strip, have heat-insulating sound-insulating, advantage elegant in appearance.But because rule is fixed by the mode of welding, solder joint itself has thickness significantly, if polylith glass carries out composite assembly, directly causes the increase greatly of product thickness, is unfavorable for marketing; And by welding manner fixing metal filler rod, its complex process is loaded down with trivial details, and cost is higher; And, can produce poisonous zinc chloride gas during owing to welding, bigger to human body harm, do not meet environmental requirement.
Therefore, there is following shortcoming at least in prior art: the thickness of hollow mosaic glass itself is big, technology for making glass is complicated, manufacturing cost is higher, and does not meet the energy-conserving and environment-protective requirement.
Summary of the invention
The objective of the invention is to overcome above-mentioned shortcoming of the prior art, the hollow mosaic glass of a kind of superior performance, cheap for manufacturing cost, manufacturing process environmental protection is provided.
A kind of welding-spot free hollow mosaic glass, it was formed by one deck mosaic glass layer and seal glass stacked the adding that is arranged at mosaic glass layer both sides, surrounding edge is provided with weather strip between mosaic glass layer and the seal glass layer, make the cavity that forms a hermetic seal between mosaic glass layer and the seal glass layer, described mosaic glass layer comprises aluminum alloy frame, at least two blocks of glass and grafting filler rod, described glass splices in aggregates by the grafting filler rod and is positioned at same plane, and is fixed on the aluminum alloy frame.
In a preferred embodiment of the invention, the two ends of described grafting filler rod are provided with contact, make between grafting filler rod and the adjacent grafting filler rod by this node to interconnect, or interconnect between grafting filler rod and the adjacent aluminum alloy frame.
In a preferred embodiment of the invention, the contact of described grafting filler rod is a tenon, and correspondingly, the upper and lower end face of described grafting filler rod forms first embedding groove that is complementary with tenon, and correspondingly, described aluminum alloy frame forms second embedding groove that is complementary with tenon.
In a preferred embodiment of the invention, the tenon of described grafting filler rod forms by the mode cutting of milling.
In a preferred embodiment of the invention, described cavity is a vacuum.
In a preferred embodiment of the invention, described cavity is filled with dry gas.
In a preferred embodiment of the invention, the groove width and the thickness of glass of described first and second embedding groove are complementary.
In a preferred embodiment of the invention, offer guiding groove in described first and second embedding groove.
Another object of the present invention is to, a kind of assemble method of welding-spot free hollow mosaic glass is provided, because this method need not any welding, contact is smoothly consistent, has advantage easy for installation, elegant in appearance.
A kind of assemble method of welding-spot free hollow mosaic glass, described hollow mosaic glass was formed by one deck mosaic glass layer and seal glass stacked the adding that is arranged at mosaic glass layer both sides, surrounding edge is provided with weather strip between mosaic glass layer and the seal glass layer, make the cavity that forms a hermetic seal between mosaic glass layer and the seal glass layer, described mosaic glass layer comprises aluminum alloy frame, at least two blocks of glass and grafting filler rod, described glass splices in aggregates by the grafting filler rod and is positioned at same plane, and be fixed on the aluminum alloy frame, it is characterized in that, comprise the steps:
A, the grafting filler rod is assembled on the aluminum alloy frame;
B, assemble, thereby finish the assembling of mosaic glass by the sequencing of grafting filler rod and glass;
C, the surrounding edge of the mosaic glass layer that assembles is installed weather strip,
D, with the seal glass layer be installed on the both sides of mosaic glass layer, make the cavity of a hermetic seal of formation between mosaic glass layer and the seal glass layer.
In a preferred embodiment of the invention, described b step also comprises, glass is assembled to the grafting filler rod goes forward, and earlier applies glue on the filler rod patching.
A kind of welding-spot free hollow mosaic glass that the present invention discloses has following effect with respect to prior art: need not welding can directly install, and has advantages easy for installation, energy-conserving and environment-protective; And, fundamentally solved the thickness problem of hollow mosaic glass.
Description of drawings
Fig. 1 is the hollow mosaic glass lateral view of the preferred embodiment of the present invention;
Fig. 2 is the structure for inlaying glass schematic diagram of the preferred embodiment of the present invention;
Fig. 3 be the preferred embodiment of the invention patch the inlay strip structure schematic diagram;
Fig. 4 be the preferred embodiment of the invention patch the filler rod lateral view;
Fig. 5 is the assemble method of the hollow mosaic glass of the preferred embodiment of the invention;
Among the figure, 1000 is that hollow mosaic glass, 1100 is that mosaic glass layer, 1200 is that weather strip, 1300 is that seal glass layer, 1110 is that aluminum alloy frame, 1120 is that glass, 1130 grafting filler rods, 1111 are that second embedding groove, 1112 is that sliver, 1113 guide grooves, 1131 are that tenon, 1132 is that first embedding groove, 1133 is that guiding groove, 1134 is the protruding wing.
The specific embodiment
Below in conjunction with accompanying drawing preferred embodiment of the present invention is described in detail, thereby protection scope of the present invention is made more explicit defining so that advantages and features of the invention can be easier to be it will be appreciated by those skilled in the art that.
As shown in Figure 1, in the preferred embodiment of the present invention, hollow mosaic glass 1000 comprises one deck mosaic glass layer 1100, is installed on the seal glass layer 1300 of mosaic glass layer 1100 both sides, the sealing layer can be the tempered glass layer, it also can be the doubling glass layer, even can also be mosaic glass layer 1100, as a preferential embodiment of the embodiment of the invention, the applicant adopts tempered glass as the seal glass layer; Mosaic glass layer 1100 is provided with weather strip 1200 with tempered glass layer surrounding edge, make the bubble-tight cavity of formation between mosaic glass layer and the tempered glass layer by weather strip 1200, this bubble-tight cavity can be the vacuum setting, as everyone knows, under vacuum state, has splendid heat-insulating sound-insulating effect; Be apparently, this tightness cavity also can charge into dry gas, has moistureproof heat insulation effect.
Please continue to consult Fig. 1, and in conjunction with Fig. 2, the structure for inlaying glass schematic diagram of Fig. 2 preferred embodiment of the present invention, among the figure, the main part of mosaic glass is made of aluminum alloy frame 1110, also comprise some blocks of glass 1120 and plug-in unit filler rod 1130, aluminum alloy frame 1110 herein is formed by connecting by four skeletal fixation, can certainly adopt integrated mode to process, the inner side edge of aluminum alloy frame 1110 forms second embedding groove 1111, this embedding groove is used to install glass 1120 and grafting filler rod 1130, the outer side edges of aluminum alloy frame 1110 is provided with guide groove 1113 equally, extended sliver 1112 in guide groove 1113 bottoms in addition, by cooperating of this guide groove 1113 and sliver 1112 and weather strip, realize the hermetic seal of mosaic glass 1120 and firmization glass, specifically, sliver 1112 inserts in the slot of weather strip 1200, the raised line of weather strip 1200 inserts in the guide groove 1113 of aluminum alloy frame 1110, thereby realize both hermetic seals, owing to realize that by weather strip 1200 hermetic seal of hollow glass belongs to the known technology of this area, this technology does not also belong to innovation part of the present invention simultaneously, so the concrete structure of this part is not shown in the drawings.
Please again in conjunction with shown in Figure 3, Fig. 3 patches the inlay strip structure schematic diagram for the preferred embodiment of the invention, grafting filler rod 1130 shown in Fig. 2 comprises horizontal two and vertical one, in embodiments of the present invention, patch filler rod 1130, two ends are provided with tenon 1131, and, the upper and lower end face is provided with first embedding groove 1132, tenon 1131 matches with adjacent first embedding groove 1132 that patches filler rod, and in other words, the insertion that tenon 1131 can mate is adjacent to patch in first Inlaid strip 1132 of filler rod, in addition, because second Inlaid strip 1111 is identical with first Inlaid strip, 1132 shapes, so in insertion second embedding groove 1111 that tenon 1131 also can mate, therefore, match with adjacent first embedding groove and second embedding groove that patches filler rod by the tenon 1131 that patches filler rod, realized the installation of the rule of mosaic glass.In addition,, therefore can make things convenient for the installation of glass,, make polylith glass be in same plane so first, second embedding groove also is used for the installation of glass 1120 except interconnecting with tenon 1131 because the width of first and second embedding groove and thickness of glass are thought coupling.
In a preferential embodiment of the present invention, tenon 1131 forms by the mode cutting of milling, therefore, tenon 1131 both sides also are formed with along the protruding wing 1134 of arc that patches the filler rod length direction, this to the protruding wing 1134 of arc can with patch matching of filler rod 1130 surfaces with arc section, thereby can further improve the installation firmness that patches filler rod 1130.
In an optimum embodiment of the present invention, as shown in Figure 4, offer guiding groove 1133 in first embedding groove 1111, because in order further to improve the firmness that glass 1120 is installed, the applicant squeezes into glass cement in this guiding groove 1133 before glass 1120 is installed, thereby glass 1120 can be patched on the filler rod 1130 with firm being installed on.
Fig. 5 is the assemble method of welding-spot free hollow mosaic glass of the present invention, is example with mosaic glass shown in Figure 2 still, may further comprise the steps:
S01 is assembled to the grafting filler rod on the aluminum alloy frame;
Specifically, will patch filler rod 1130 earlier longitudinally inserts in second embedding groove of aluminum alloy frame 1110.
S02 assembles by the sequencing of grafting filler rod and glass, thereby finishes the assembling of mosaic glass;
Specifically, again two blocks of glass 1120 are inserted along embedding groove, and then insert horizontal two downwards and patch filler rod, first embedding groove 1132 that patches filler rod is connected with glassy phase, by that analogy, with all glass with patch filler rod and install.
S03 installs weather strip with the surrounding edge of the mosaic glass layer that assembles;
Specifically, sliver 1112 is inserted in the slot of weather strip 1200, the raised line of weather strip 1200 inserts in the guide groove 1113 of aluminum alloy frame 1110.
S04 with the seal glass layer be installed on the both sides of mosaic glass layer,
Specifically, seal glass is laminated in the mounted weather strip, makes the seal glass layer be arranged at the both sides of mosaic glass layer, thereby make the cavity that forms a hermetic seal between mosaic glass layer and the seal glass layer.
A preferential embodiment as welding-spot free hollow mosaic glass mounting method of the present invention is assembled to grafting filler rod 1130 with glass 1120 and goes forward, and earlier applies glue patching on the filler rod 1130, improves glass 1120 firmness are installed.
As an optimum embodiment of welding-spot free hollow mosaic glass mounting method of the present invention, before glass 1120 is installed, glass cement is squeezed in this guiding groove 1133, thereby glass 1120 can be patched on the filler rod 1130 with firm being installed on.
A kind of welding-spot free hollow mosaic glass that the present invention discloses has following effect with respect to prior art: need not welding can directly install, and has advantages easy for installation, energy-conserving and environment-protective; And, fundamentally solved the thickness problem of hollow mosaic glass.
The above; it only is the specific embodiment of the present invention; but protection scope of the present invention is not limited thereto; any those of ordinary skill in the art are in the disclosed technical scope of the present invention; variation or the replacement that can expect without creative work all should be encompassed within protection scope of the present invention.Therefore, protection scope of the present invention should be as the criterion with the protection domain that claims were limited.

Claims (10)

1. welding-spot free hollow mosaic glass, it is characterized in that, it was formed by one deck mosaic glass layer and seal glass stacked the adding that is arranged at mosaic glass layer both sides, surrounding edge is provided with weather strip between mosaic glass layer and the seal glass layer, make the cavity that forms a hermetic seal between mosaic glass layer and the seal glass layer, described mosaic glass layer comprises aluminum alloy frame, at least two blocks of glass and grafting filler rod, described glass splices in aggregates by the grafting filler rod and is positioned at same plane, and is fixed on the aluminum alloy frame.
2. welding-spot free hollow mosaic glass according to claim 1, it is characterized in that, the two ends of described grafting filler rod are provided with contact, make between grafting filler rod and the adjacent grafting filler rod by this node to interconnect, or interconnect between grafting filler rod and the adjacent aluminum alloy frame.
3. welding-spot free hollow mosaic glass according to claim 2, it is characterized in that, the contact of described grafting filler rod is a tenon, correspondingly, the upper and lower end face of described grafting filler rod forms first embedding groove that is complementary with tenon, and correspondingly, described aluminum alloy frame forms second embedding groove that is complementary with tenon.
4. welding-spot free hollow mosaic glass according to claim 3 is characterized in that the tenon of described grafting filler rod forms by the mode cutting of milling.
5. welding-spot free hollow mosaic glass according to claim 4 is characterized in that, described cavity is a vacuum.
6. welding-spot free hollow mosaic glass according to claim 4 is characterized in that described cavity is filled with dry gas.
7. according to claim 5 or 6 described welding-spot free hollow mosaic glass, it is characterized in that the groove width and the thickness of glass of described first and second embedding groove are complementary.
8. welding-spot free hollow mosaic glass according to claim 7 is characterized in that, offers guiding groove in described first and second embedding groove.
9. the assemble method of a welding-spot free hollow mosaic glass, described hollow mosaic glass was formed by one deck mosaic glass layer and seal glass stacked the adding that is arranged at mosaic glass layer both sides, surrounding edge is provided with weather strip between mosaic glass layer and the seal glass layer, make the cavity that forms a hermetic seal between mosaic glass layer and the seal glass layer, described mosaic glass layer comprises aluminum alloy frame, at least two blocks of glass and grafting filler rod, described glass splices in aggregates by the grafting filler rod and is positioned at same plane, and be fixed on the aluminum alloy frame, it is characterized in that, comprise the steps:
A, the grafting filler rod is assembled on the aluminum alloy frame;
B, assemble, thereby finish the assembling of mosaic glass by the sequencing of grafting filler rod and glass;
C, the surrounding edge of the mosaic glass layer that assembles is installed weather strip;
D, with the seal glass layer be installed on the both sides of mosaic glass layer, make the cavity of a hermetic seal of formation between mosaic glass layer and the seal glass layer.
10. the assemble method of welding-spot free hollow mosaic glass according to claim 9 is characterized in that, described b step also comprises, glass is assembled to the grafting filler rod goes forward, and earlier applies glue on the filler rod patching.
CN201010169245A 2010-05-12 2010-05-12 Welding-spot free hollow mosaic glass and assembling method thereof Pending CN101824952A (en)