CN101708455B
CN101708455B CN2009102318145A CN200910231814A CN101708455B CN 101708455 B CN101708455 B CN 101708455B CN 2009102318145 A CN2009102318145 A CN 2009102318145A CN 200910231814 A CN200910231814 A CN 200910231814A CN 101708455 B CN101708455 B CN 101708455B
Authority
CN
China
Prior art keywords
oil
purifying agent
attapulgite
suction
concave
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009102318145A
Other languages
English (en)
Other versions
CN101708455A (zh
Inventor
许庆华
袁长兵
许盛英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Fulunli New Material Co., Ltd.
Original Assignee
许庆华
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 许庆华 filed Critical 许庆华
Priority to CN2009102318145A priority Critical patent/CN101708455B/zh
Publication of CN101708455A publication Critical patent/CN101708455A/zh
Application granted granted Critical
Publication of CN101708455B publication Critical patent/CN101708455B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Solid-Sorbent Or Filter-Aiding Compositions (AREA)

Abstract

本发明公开了一种凹凸棒吸油净化剂,其技术方案的要点是,凹凸棒吸油净化剂由颗粒活性凹凸棒石粘土、高吸油树脂、高吸水树脂和改性羧甲基羟丙基纤维素组成。凹凸棒吸油净化剂的生产方法是将凹凸棒吸油净化剂的配料输入混料机中,混合均匀后包装为凹凸棒吸油净化剂;将凹凸棒吸油净化剂加入抽油烟机内的集油盒中,不但能将抽入油烟机内的有害气体进行吸附,而且能将落入抽油烟机内集油盒中的油水混合物从液体状态迅速吸收膨胀转化为凝胶状物体,将会凝结在颗粒活性凹凸棒石粘土上形成一个柔软的块状物,可以阻止细菌的滋生和避免产生霉变,并有利于在清洗抽油烟机时将其取出,凹凸棒吸油净化剂适用于吸附集油盒中的油水混合物。

Description

凹凸棒吸油净化剂
技术领域
本发明涉及净化剂,具体涉及一种凹凸棒吸油净化剂。
背景技术
抽油烟机又称吸油烟机,是一种净化厨房环境的家用电器,能将炉灶燃烧的废物和烹饪过程中产生的的部份油烟和水蒸汽抽走,排出室外,减少污染,净化空气;但是人们在做饭或炒菜时,会产生大量的水蒸汽,水蒸汽和部份油烟混合在一起,很容易沾粘在在抽油烟机内的内壁和风机叶轮上,风机叶轮沾粘了水蒸汽和油烟混合物后,会使风机转动逐渐失去了动平衡,造成抽吸效果就越来越差,其机械噪音也就越来越大,同时也增加了抽油烟机的耗电量。
在抽油烟机内设有集油罩和集油盒,集油盒内的油水混合物呈液体状态,很容易形成细菌大量滋生和产生霉变。由于没有有效的净化手段,致使风机及机器内腔大量积油,清洗非常困难,需要专业人员才能完成,有时清洗后效果反而更差,费时又费力。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种凹凸棒吸油净化剂。
凹凸棒吸油净化剂由颗粒活性凹凸棒石粘土、高吸油树脂、高吸水树脂和改性羧甲基羟丙基纤维素组成。
颗粒活性凹凸棒石粘土,是用硫酸加入凹凸棒石粘土原矿中进行酸化,再经过高温焙烧为颗粒活性凹凸棒石粘土,凹凸棒石粘土酸化改性处理后,不但具有较好的吸附和脱色性能,还具有很强的吸水性,本发明选用的颗粒活性凹凸棒石粘土的颗粒细度控制在0.5~3毫米。
高吸油树脂具有吸油能力强、可吸油种类多、热稳定性和保油性能好的特点,有利于方便回收油污,用于本发明能将抽油烟机内集油盒中的污油迅速吸收膨胀转化为凝胶状物体,本发明选用的高吸油树脂的颗粒细度控制在0.5~3毫米。
高吸水树脂的吸水量大,可达自身质量的数百倍甚至上千倍。吸水速度可在数秒内生成凝胶,并且保水性强,即使在低温、加压条件下也不易失水,对光、热、冷和酸碱的稳定性好,具有良好的生物降解性能,用于本发明能将抽油烟机内集油盒中的水迅速吸收膨胀转化为凝胶状物体,本发明选用的高吸水树脂的颗粒细度控制在0.2~1毫米。
改性羧甲基羟丙基纤维素能迅速溶解于冷水或热水,具有良好的触变性性能,耐盐性和耐酸性性能优越,粘度高,增稠剂效果好,用于本发明有利于增加凝胶状物体的粘结性能,本发明选用的改性羧甲基羟丙基纤维素的颗粒细度控制在0.2~1毫米。
本发明通过下述技术方案予以实现:
凹凸棒吸油净化剂的配料按重量百分比由下列组分组成:颗粒活性凹凸棒石粘土80~90%、高吸油树脂0.1~10%、高吸水树脂0.1~5%和改性羧甲基羟丙基纤维素0.1~5%;
凹凸棒吸油净化剂的生产方法:将凹凸棒吸油净化剂的配料输入混料机中,混合均匀后包装为凹凸棒吸油净化剂成品;
所述颗粒活性凹凸棒石粘土的生产方法:①稀硫酸的配制,按重量百分比由下列组分组成:浓度98%的硫酸1~5%,水95~99%;②酸化处理的配料,按重量百分比由下列组分组成:凹凸棒石粘土原矿55~65%,稀硫酸35~45%,将稀硫酸缓慢加入凹凸棒石粘土原矿中进行酸化处理;③将酸化后的凹凸棒石粘土,通过挤压机进行挤压为片状物,片状物的厚度≤3毫米;④将凹凸棒石粘土的片状物输送到焙烧炉内进行焙烧,焙烧时间为1.5~3小时,焙烧温度控制在320~450℃;⑤将焙烧后的的片状物输入粉碎机中进行粉碎和筛分,颗粒细度控制在0.5~3毫米,包装为颗粒活性凹凸棒石粘土备用。
将凹凸棒吸油净化剂加入抽油烟机内的集油盒中,凹凸棒吸油净化剂不但能将抽入油烟机内的有害气体进行吸附,而且能将落入抽油烟机内集油盒中的油水混合物从液体状态迅速吸收膨胀转化为凝胶状物体。
由于凹凸棒吸油净化剂内的原料颗粒细度不同,高吸水树脂和改性羧甲基羟丙基纤维素分布在集油盒的中下层,有利于吸收集油盒内的水溶液,颗粒活性凹凸棒石粘土和高吸油树脂分布在集油盒的中上层,有利于吸附油烟机内的有害气体和吸收集油盒内的油污。
当集油盒内的凹凸棒吸油净化剂吸附饱和后,吸附油水混合物后的凝胶状物体,将会凝结在颗粒活性凹凸棒石粘土上形成一个柔软的块状物,可以阻止细菌的滋生和避免产生霉变,并有利于在清洗抽油烟机时将其取出。
凹凸棒吸油净化剂生产成本低廉,使用方便,没有环境污染。
凹凸棒吸油净化剂适用于吸附集油盒中的油水混合物,也适用于放置在各种需要进行油水混合物处理的装置内。
具体实施方式
下面结合实施例对本发明作进一步的描述:
凹凸棒吸油净化剂的配料按重量百分比由下列组分组成:颗粒活性凹凸棒石粘土92%、高吸油树脂6%、高吸水树脂1.5%和改性羧甲基羟丙基纤维素0.5%。
凹凸棒吸油净化剂的生产方法:将凹凸棒吸油净化剂的配料输入混料机中,混合均匀后包装为凹凸棒吸油净化剂;
所述颗粒活性凹凸棒石粘土的生产方法:①稀硫酸的配制,按重量百分比由下列组分组成:浓度98%的硫酸3%,水97%;②酸化处理的配料,按重量百分比由下列组分组成:凹凸棒石粘土原矿62%,稀硫酸38%,将稀硫酸缓慢加入凹凸棒石粘土原矿中进行酸化处理;③将酸化后的凹凸棒石粘土,通过挤压机进行挤压为片状物,片状物的厚度≤3毫米;④将凹凸棒石粘土的片状物输送到焙烧炉内进行焙烧,焙烧时间为2小时,焙烧温度控制在320~350℃;⑤将焙烧后的的片状物输入粉碎机中进行粉碎和筛分,颗粒细度控制在0.5~3毫米,包装为颗粒活性凹凸棒石粘土备用。

Claims (1)

1.一种凹凸棒吸油净化剂,其特征在于,凹凸棒吸油净化剂的配料按重量百分比由下列组分组成:颗粒活性凹凸棒石粘土80~90%、高吸油树脂0.1~10%、高吸水树脂0.1~5%和改性羧甲基羟丙基纤维素0.1~5%;
所述颗粒活性凹凸棒石粘土的生产方法:①稀硫酸的配制,按重量百分比由下列组分组成:浓度98%的硫酸1~5%,水95~99%;②酸化处理的配料,按重量百分比由下列组分组成:凹凸棒石粘土原矿55~65%,稀硫酸35~45%,将稀硫酸缓慢加入凹凸棒石粘土原矿中进行酸化处理;③将酸化后的凹凸棒石粘土,通过挤压机进行挤压为片状物,片状物的厚度≤3毫米;④将凹凸棒石粘土的片状物输送到焙烧炉内进行焙烧,焙烧时间为1.5~3小时,焙烧温度控制在320~450℃;⑤将焙烧后的的片状物输入粉碎机中进行粉碎和筛分,颗粒细度控制在0.5~3毫米,包装为颗粒活性凹凸棒石粘土备用;
所述高吸油树脂的颗粒细度控制在0.5~3毫米;
所述高吸水树脂的颗粒细度控制在0.2~1毫米;
所述改性羧甲基羟丙基纤维素的颗粒细度控制在0.2~1毫米;
所述凹凸棒吸油净化剂的生产方法,将凹凸棒吸油净化剂的配料输入混料机中,混合均匀后包装为凹凸棒吸油净化剂成品。
CN2009102318145A 2009-12-08 2009-12-08 凹凸棒吸油净化剂 Expired - Fee Related CN101708455B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2009102318145A CN101708455B (zh) 2009-12-08 2009-12-08 凹凸棒吸油净化剂

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2009102318145A CN101708455B (zh) 2009-12-08 2009-12-08 凹凸棒吸油净化剂

Publications (2)

Publication Number Publication Date
CN101708455A CN101708455A (zh) 2010-05-19
CN101708455B true CN101708455B (zh) 2011-10-26

Family

ID=42401275

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2009102318145A Expired - Fee Related CN101708455B (zh) 2009-12-08 2009-12-08 凹凸棒吸油净化剂

Country Status (1)

Country Link
CN (1) CN101708455B (zh)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104140110B (zh) * 2014-07-27 2015-12-02 甘肃华晨非金属应用科技有限公司 酸化后的黄土
CN106925218A (zh) * 2017-04-11 2017-07-07 安徽博硕科技有限公司 一种厨房油污吸附剂及其制备方法
CN106925230A (zh) * 2017-05-03 2017-07-07 明光市飞洲新材料有限公司 一种凹凸棒土高效油污吸附剂及其制备方法

Also Published As

Publication number Publication date
CN101708455A (zh) 2010-05-19

Similar Documents

Publication Publication Date Title
CN110100746A (zh) 一种无尘除臭膨润土猫砂及其制备方法
CN104475038A (zh) 一种汽车用环保型空气净化剂及其制备方法
CN107349901A (zh) 一种介孔氮化碳吸附材料及其制备方法和应用
CN101708455B (zh) 凹凸棒吸油净化剂
CN104709904B (zh) 吸附pm2.5及防辐射用稻麦秸秆活性炭生态建筑材料制作方法
CN100497236C (zh) 一种具有释放负离子性能的水泥基地面材料
CN107552027A (zh) 一种利用生物质废弃料制备碳材料的方法及其制备的碳材料的应用
CN104351253A (zh) 一种天然抗菌吸附超细粉体及其制备方法
CN106242633A (zh) 一种多功能硅藻土陶粒的制备方法
CN102874803A (zh) 一种用于活性炭板材的活性炭的制备工艺
CN108620020A (zh) 一种含有贝壳粉的新型复合空气净化材料
CN103418344A (zh) 纳米氧化锌蜂窝型净化活性炭及其制备方法
CN105087016B (zh) 富含海洋物质的土壤调理剂
CN103418343B (zh) 竹酢蜂窝型净化活性炭及其制备方法
CN106745880A (zh) 应用于城市污水的污水处理方法
CN106423110A (zh) 以文冠果壳为原料制备高效脱除多环芳烃的磁性吸附剂
CN105056894A (zh) 一种新型吸附剂
CN103432991B (zh) 纳米银蜂窝型净化活性炭及其制备方法
CN104841367A (zh) 一种添加坚果壳以及山葵的复合活性炭过滤材料及其制备方法
CN106925218A (zh) 一种厨房油污吸附剂及其制备方法
CN107494634A (zh) 家用空调过滤网的杀菌剂及其制备方法
CN105597130A (zh) 一种油气脱臭环保工艺
CN105251443A (zh) 一种脱臭碳质吸附剂的制备方法
CN102091338A (zh) 一种麦饭石冰箱、居室除臭剂及其制备方法
CN105271492A (zh) 一种净水处理剂

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: JIANGSU BAITENG TECHNOLOGY CO., LTD.

Free format text: FORMER OWNER: XU QINGHUA

Effective date: 20120719

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 211700 HUAIAN, JIANGSU PROVINCE TO: 213164 CHANGZHOU, JIANGSU PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20120719

Address after: 213164 building four, block B, building 1, Changzhou science and Education City, Jiangsu

Patentee after: Jiangsu 5ipatent Technology Co.,Ltd.

Address before: 211700 Huaian City, Jiangsu province Xuyi County Xu town of Stonebridge Road No. 40

Patentee before: Xu Qinghua

ASS Succession or assignment of patent right

Owner name: NANTONG TONGZHOU DISTRICT PRODUCTIVITY PROMOTION C

Free format text: FORMER OWNER: JIANGSU BAITENG TECHNOLOGY CO., LTD.

Effective date: 20130904

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 213164 CHANGZHOU, JIANGSU PROVINCE TO: 226300 NANTONG, JIANGSU PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20130904

Address after: 226300, six floor, Xianghe Road, Jinsha Road, Jinsha Town, Nantong, Jiangsu, Tongzhou District

Patentee after: Tongzhou District Nantong Productivity Promotion Center

Address before: 213164 building four, block B, building 1, Changzhou science and Education City, Jiangsu

Patentee before: Jiangsu 5ipatent Technology Co.,Ltd.

ASS Succession or assignment of patent right

Owner name: NANTONG FULUNLI NEW MATERIAL CO., LTD.?

Free format text: FORMER OWNER: NANTONG TONGZHOU DISTRICT PRODUCTIVITY PROMOTION CENTER

Effective date: 20150521

C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20150521

Address after: 226300 No. 788 Century Avenue, hi tech Zone, Jiangsu, Nantong

Patentee after: Nantong Fulunli New Material Co., Ltd.

Address before: 226300, six floor, Xianghe Road, Jinsha Road, Jinsha Town, Nantong, Jiangsu, Tongzhou District

Patentee before: Tongzhou District Nantong Productivity Promotion Center

CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20111026

Termination date: 20181208

CF01 Termination of patent right due to non-payment of annual fee