CN101654337A - Method for processing hollow glass with lined aluminum plate - Google Patents
Method for processing hollow glass with lined aluminum plate Download PDFInfo
- Publication number
- CN101654337A CN101654337A CN200910027355A CN200910027355A CN101654337A CN 101654337 A CN101654337 A CN 101654337A CN 200910027355 A CN200910027355 A CN 200910027355A CN 200910027355 A CN200910027355 A CN 200910027355A CN 101654337 A CN101654337 A CN 101654337A
- Authority
- CN
- China
- Prior art keywords
- aluminum frame
- hollow aluminum
- sheet
- glass
- sheet glass
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for processing hollow glass of a lined aluminum plate, which comprises the steps of: selecting a piece of glass, and cutting the glass into glass sheets for edging, cleaning and toughening; placing the glass sheets into a coating chamber for coating; removing edge films of the coated glass sheets, cleaning the same and then putting the same into a sheet-combining chamber; gluing a hollow aluminum frame for the first time, and putting hollow aluminum frame/the same over the glass sheets for positioning; filling the hollow aluminum frame with driers; adhering double sided adhesive tapes along four internal frames of the hollow aluminum frame, and pasting an aluminum plate with the hollow aluminum frame; gluing the hollow aluminum frame for the second time, putting the second piece of coated sheet sequentially into a cleaner, the sheet-combining chamber for positioning, and a sheet presser for combination; drilling a small hole in the upper and lower edgeparts of the hollow aluminum frame, respectively, for inflation; rubberizing the butyl rubber around the hollow aluminum frame for the final sealing. The processing method has the advantages of accurate location for mounting, no scratch on film surfaces and resource saving.
Description
Technical field:
The present invention relates to a kind of working method of lined aluminum plate double glazing.
Background technology:
At present, general double glazing presses together two coated glasses exactly by the hollow aluminum frame, in order to meet requirement of client, need in the middle of two coated glasses, to add aluminium sheet, generally be that butyl rubber is coated on the aluminium sheet two sides, sticking mutually obedient with two coated glasses respectively again, can make the position of installation inaccurate like this, can be shifted easily, and face is caused scuffing, simultaneously, large-area like this gluing is also wasted resource.
Summary of the invention:
The objective of the invention is provides a kind of installation site accurate in order to overcome above deficiency, can not cause scuffing to face, saves the working method of the lined aluminum plate double glazing of resource.
Purpose of the present invention is achieved through the following technical solutions: the working method of lined aluminum plate double glazing may further comprise the steps:
A: select the thick glass of 3~15mm, cut into sheet glass by predetermined size, sheet glass is carried out edging, sheet glass is cleaned, again sheet glass is carried out tempering with cleaning machine with edge polisher with cutting machine;
B: the sheet glass behind the tempering is sent into plated film in the coating chamber;
C: the glass trimming film with plated film, clean with 4 meters/minute speed, entering after cleaning closed the sheet chamber;
D: the hollow aluminum frame after the bending is carried out the gluing first time, glue-coated hollow aluminum frame was placed on the sheet glass of limit film, and positions;
E: desiccant-filled in the hollow aluminum frame;
F: inboard four frames along the hollow aluminum frame stick double faced adhesive tape, with the sticking mutually card of aluminium sheet and hollow aluminum frame;
G: the hollow aluminum frame is carried out the gluing second time, second coated glass sheet entered cleaning machine, enter again and close the sheet chamber, position, enter tabletting machine, carry out pressing by 4~6kg pressure;
H: each makes a call to an aperture up and down in hollow aluminum edge portion, inflates by 2~3kg pressure with injection needles, and gas is rare gas element;
I: around the hollow aluminum frame, stamp the wide butyl rubber of 6~8mm, carry out last sealing.
The present invention compared with prior art has the following advantages: the installation site is accurate, can not cause scuffing to face, saves resource.
Embodiment:
In order to deepen the understanding of the present invention, the invention will be further described below in conjunction with embodiment, and this embodiment only is used to explain the present invention, do not constitute the qualification to protection domain of the present invention.
A kind of embodiment of the working method of lined aluminum plate double glazing of the present invention is: may further comprise the steps:
A: select 6mm glass, cut into sheet glass with cutting machine by predetermined size, with edge polisher sheet glass is carried out edging, with cleaning machine sheet glass is cleaned, again sheet glass is carried out tempering, when sheet glass is carried out tempering, need be warmed to 700 ℃, by changing but slow cool down again of the first chilling of blast size, reach 50 ℃ again up to temperature;
B: the sheet glass behind the tempering is sent into plated film in the coating chamber;
C: the sheet glass trimming film with plated film, clean with 4 meters/minute speed, entering after cleaning closed the sheet chamber, the room temperature of closing the sheet chamber is 24 ℃, relative humidity 30%;
D: the hollow aluminum frame after the bending is carried out being coated with the first time butyl rubber, glue-coated hollow aluminum frame was placed on the sheet glass of limit film, and positions;
E: desiccant-filled in the hollow aluminum frame;
F: inboard four frames along the hollow aluminum frame stick double faced adhesive tape, with the sticking mutually card of aluminium sheet and hollow aluminum frame;
G: the hollow aluminum frame is carried out being coated with the second time butyl rubber, second coated glass sheet entered cleaning machine, enter again and close sheet chamber (room temperature with relative humidity with above-mentioned the same), position, enter tabletting machine, carry out pressing by 4kg pressure;
H: each makes a call to an aperture up and down in hollow aluminum edge portion, inflates by 2kg pressure with injection needles, and gas is rare gas element;
I: around the hollow aluminum frame, stamp the wide butyl rubber of 6mm, carry out last sealing.
Embodiment two:
A: select 9mm glass, cut into sheet glass with cutting machine by predetermined size, with edge polisher sheet glass is carried out edging, with cleaning machine sheet glass is cleaned, again sheet glass is carried out tempering, when sheet glass is carried out tempering, need be warmed to 720 ℃, by changing but slow cool down again of the first chilling of blast size, reach 40 ℃ again up to temperature;
B: the sheet glass behind the tempering is sent into plated film in the coating chamber;
C: the sheet glass trimming film with plated film, clean with 4 meters/minute speed, entering after cleaning closed the sheet chamber, the room temperature of closing the sheet chamber is 26 ℃, relative humidity 28%;
D: the hollow aluminum frame after the bending is carried out being coated with the first time butyl rubber, glue-coated hollow aluminum frame was placed on the sheet glass of limit film, and positions;
E: desiccant-filled in the hollow aluminum frame;
F: inboard four frames along the hollow aluminum frame stick double faced adhesive tape, with the sticking mutually card of aluminium sheet and hollow aluminum frame;
G: the hollow aluminum frame is carried out being coated with the second time butyl rubber, second coated glass sheet entered cleaning machine, enter again and close sheet chamber (room temperature with relative humidity with above-mentioned the same), position, enter tabletting machine, carry out pressing by 6kg pressure;
H: each makes a call to an aperture up and down in hollow aluminum edge portion, inflates by 3kg pressure with injection needles, and gas is rare gas element;
I: around the hollow aluminum frame, stamp the wide butyl rubber of 8mm, carry out last sealing.
It is accurate that the present invention has the installation site, can not cause scuffing to face, the advantage of saving resource.
Claims (4)
1, a kind of working method of lined aluminum plate double glazing is characterized in that: may further comprise the steps:
A: select the thick glass of 3~15mm, cut into sheet glass by predetermined size, sheet glass is carried out edging, sheet glass is cleaned, again sheet glass is carried out tempering with cleaning machine with edge polisher with cutting machine;
B: the sheet glass behind the tempering is sent into plated film in the coating chamber;
C: the sheet glass trimming film with plated film, clean with 4 meters/minute speed, the sheet glass after cleaning is entered close the sheet chamber;
D: the hollow aluminum frame after the bending is carried out the gluing first time, glue-coated hollow aluminum frame was placed on the sheet glass of limit film, and positions bonding;
E: desiccant-filled in the hollow aluminum frame;
F: inboard four frames along the hollow aluminum frame stick double faced adhesive tape, with the sticking mutually card of aluminium sheet and hollow aluminum frame;
G: the hollow aluminum frame is carried out the gluing second time, second coated glass sheet entered cleaning machine, enter again and close the sheet chamber, position, enter tabletting machine, carry out pressing by 4~6kg pressure;
H: each makes a call to an aperture up and down in hollow aluminum edge portion, inflates by 2~3kg pressure with injection needles, and described gas is rare gas element;
I: around the hollow aluminum frame, stamp the wide butyl rubber of 6~8mm, carry out last sealing.
2, according to the working method of the described lined aluminum plate double glazing of claim 1, it is characterized in that: in the described steps A, when sheet glass is carried out tempering, need be warmed to 680 ℃~720 ℃, by changing but slow cool down again of the first chilling of blast size, reach 40 ℃~50 ℃ again up to temperature.
3, according to the working method of the described lined aluminum plate double glazing of claim 1, it is characterized in that: among described step C and the G, the room temperature of closing the sheet chamber is 24 ℃~26 ℃, relative humidity 28%~30%.
4, according to the working method of the described lined aluminum plate double glazing of claim 1, it is characterized in that: among described step D and the G, the glue that gluing is used is butyl rubber.