CN101649239B - Composite coal-saving agent - Google Patents

Composite coal-saving agent Download PDF

Info

Publication number
CN101649239B
CN101649239B CN200910176493A CN200910176493A CN101649239B CN 101649239 B CN101649239 B CN 101649239B CN 200910176493 A CN200910176493 A CN 200910176493A CN 200910176493 A CN200910176493 A CN 200910176493A CN 101649239 B CN101649239 B CN 101649239B
Authority
CN
China
Prior art keywords
coal
saving agent
saving
iron
sodium
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200910176493A
Other languages
Chinese (zh)
Other versions
CN101649239A (en
Inventor
于江善
于晴
于跃海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shandong Juxian Jiangshan Technology Co., Ltd.
Original Assignee
于江善
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 于江善 filed Critical 于江善
Priority to CN200910176493A priority Critical patent/CN101649239B/en
Publication of CN101649239A publication Critical patent/CN101649239A/en
Application granted granted Critical
Publication of CN101649239B publication Critical patent/CN101649239B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a composite coal-saving agent in order to improve the thermal efficiency of coal and achieve the aims of energy saving and emission reduction. The coal-saving agent is prepared by the following components: charcoal powder, strontium nitrate, sodium nitrate, sodium nitrite, nitrate, calcium oxide, sodium carbonate, potassium chloride, ammonium perchlorate, ferric chloride, ferric oxide and lead hydroxide, bentonite, boric acid and high-sodium chlorate.

Description

Composite coal-saving agent
Technical field
The invention belongs to the additive for fire coal field, relate in particular to a kind of composite coal-saving agent.
Background technology
For the protection environment, make full use of the energy, the scientific worker of countries in the world is in the correlative study of constantly carrying out power-saving technology.Coal-saving agent also is born thus.Coal-saving agent mainly is made into by multiple industrial chemicals such as oxygenation agent, properties-correcting agent, catalyzer, ignition dope, smoke suppressor, swelling agent, sulphur-fixing agents, is used to improve the thermo-efficiency of coal, reaches the purpose of energy-saving and emission-reduction.
Summary of the invention
Main purpose of the present invention is to disclose a kind of coal-saving agent, to improve the thermo-efficiency of coal, reaches the purpose of energy-saving and emission-reduction.
Coal-saving agent disclosed by the invention is processed by following component: powdered carbon, strontium nitrate, SODIUMNITRATE, Sodium Nitrite, nitre, quicklime, yellow soda ash, Repone K, ammoniumper chlorate, iron(ic)chloride, red oxide of iron, Potassium peroxide 85, wilkinite, boric acid and sodium perchlorate.
Wherein, The optimal components ratio of said components is: powdered carbon 15%: strontium nitrate 12%: SODIUMNITRATE 11%: Sodium Nitrite 9%: nitre 8%: quicklime 7%, yellow soda ash 6%: Repone K 5%: ammoniumper chlorate 5%: iron(ic)chloride 4%: red oxide of iron 4%: Potassium peroxide 85 4%: wilkinite 4%: boric acid 3%: sodium perchlorate 3%.
The coal saving rate of coal-saving agent disclosed by the invention can reach more than 20%, and this coal-saving agent is mixed in the raw material in 5/10000ths ratio, possibly make gas emissions and smoke discharge amount in the cement in vertical kiln reduce by 60%~80%, and output when significantly improving; This coal-saving agent is mixed in the raw coal that boiler uses with 3/1000ths ratio, can make carbon content in the slag when not adding be reduced to more than 14% after the interpolation below 2%, Gu sulphur, solid dirt rate reach more than 50%, discharge of harmful gases reduces more than 60%.
Specific embodiment
The present invention discloses a kind of composite coal-saving agent, and is composed of the following components:
Powdered carbon, strontium nitrate, SODIUMNITRATE, Sodium Nitrite, nitre, quicklime, yellow soda ash, Repone K, ammoniumper chlorate, iron(ic)chloride, red oxide of iron, Potassium peroxide 85, boric acid and sodium perchlorate.
Said components on the one hand, increases concentration of oxygen through the use strong oxidizer in combustion processes, utilization " microexplosion " and collision mechanism make interior temperature of burner hearth and oxygen distribution more even, and makes rapid, the fully burning of combustiblematerials in the fire coal; And generation IX combustion reactions under the effect of catalyzer, properties-correcting agent; Make traditional coal (or vertical kiln raw material) change into from combustion system from outward appearance to inner essence inside and outside together the burning; Improve the burn-out degree of coal burning, reduced the thermosteresis that chemical incomplete combustion coal-fired in the kiln is taken away.On the other hand, the sulfurous gas that utilizes sulphur-fixing agent (quicklime, yellow soda ash) to produce when making coal burning is solidificated in the cinder, generates the vitriol solids, has reduced the discharge of harmful gases amount.Thus, this coal-saving agent has improved the efficiency of combustion of coal, has reached the effect of energy-saving and emission-reduction; Can make nonflammable low grade coal reach the combustion efficacy of fat coal, can produce the excellent usefulness of smut, the excellent coal economic benefit of usefulness less.
Embodiment one
Choose raw material,, prepare burden in following ratio then putting in storage after raw material pulverizing, the oven dry:
Powdered carbon 15%: strontium nitrate 12%: SODIUMNITRATE 11%: Sodium Nitrite 9%: nitre 8%: quicklime 7%, yellow soda ash 6%: Repone K 5%: ammoniumper chlorate 5%: iron(ic)chloride 4%: red oxide of iron 4%: Potassium peroxide 85 4%: wilkinite 4%: boric acid 3%: sodium perchlorate 3%.
The proportioning of above-mentioned raw materials is an optimal components ratio of the present invention.Above-mentioned batching after grinding, homogenizing are handled, is packaged into finished product and sells.
Application example one
Coal-saving agent among the embodiment one is mixed in 5/10000ths ratio in the raw material of shaft kiln and boiler of cement manufacturing usefulness.This coal-saving agent can make gas emissions and the smoke discharge amount in the cement in vertical kiln reduce by 60%~80%, and coal saving rate can reach more than 20%, and significantly improves the time output of cement, and coal saving rate can reach more than 20%.
Embodiment two
Choose raw material,, prepare burden in following ratio then putting in storage after raw material pulverizing, the oven dry:
Powdered carbon 13%: strontium nitrate 12%: SODIUMNITRATE 11%: Sodium Nitrite 8%: nitre 9%: quicklime 7%, yellow soda ash 6%: Repone K 5%: ammoniumper chlorate 3%: iron(ic)chloride 6%: red oxide of iron 4%: Potassium peroxide 85 4%: wilkinite 6%: boric acid 3%: sodium perchlorate 3%.
Above-mentioned batching after grinding, homogenizing are handled, is packaged into finished product and sells.
Application example two
Coal-saving agent among the embodiment two is mixed in the raw coal that boiler uses with 3/1000ths ratio; Make carbon content in the slag when not adding be reduced to more than 14% after the interpolation below 2%; Gu sulphur, solid dirt rate reach more than 50%; Discharge of harmful gases reduces more than 60%, and coal saving rate can reach more than 20%.
More than; Be merely preferred embodiment of the present invention, but protection scope of the present invention is not limited thereto, any technician who is familiar with the present technique field is in the technical scope that the present invention discloses; The variation that can expect easily or replacement all should be encompassed within protection scope of the present invention.Therefore, protection scope of the present invention should be as the criterion with the protection domain that claim was defined.

Claims (2)

1. a composite coal-saving agent is characterized in that, the proportioning of said component is following:
Powdered carbon 15%: strontium nitrate 12%: SODIUMNITRATE 11%: Sodium Nitrite 9%: nitre 8%: quicklime 7%: yellow soda ash 6%: Repone K 5%: ammoniumper chlorate 5%: iron(ic)chloride 4%: red oxide of iron 4%: Potassium peroxide 85 4%: wilkinite 4%: boric acid 3%: sodium perchlorate 3%.
2. a composite coal-saving agent is characterized in that, the proportioning of said component is following:
Powdered carbon 13%: strontium nitrate 12%: SODIUMNITRATE 11%: Sodium Nitrite 8%: nitre 9%: quicklime 7%, yellow soda ash 6%: Repone K 5%: ammoniumper chlorate 3%: iron(ic)chloride 6%: red oxide of iron 4%: Potassium peroxide 85 4%: wilkinite 6%: boric acid 3%: sodium perchlorate 3%.
CN200910176493A 2009-09-17 2009-09-17 Composite coal-saving agent Expired - Fee Related CN101649239B (en)