Prior art keywords
smelting
ring body
electrode part
closed
ring bodies
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2008101115986A
Other languages
Chinese (zh)
Other versions
CN101604602A (en
Inventor
邱鸿智
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2008101115986A priority Critical patent/CN101604602B/en
Publication of CN101604602A publication Critical patent/CN101604602A/en
Application granted granted Critical
Publication of CN101604602B publication Critical patent/CN101604602B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Abstract

The invention relates to a micro-fuse which comprises a melting part, two electrode parts, a seat body and a cover body, wherein the melting part is provided with a column body surrounding a melting wire body to form a surrounding melting wire; one end of the electrode parts is provided with two ring bodies with closed end parts and bearing and fixing surfaces; the seat body is provided with through holes for the two electrode parts to pass through, the upper end of the seat body is provided with a bearing platform, sides of the seat body are provided with buckling rings, the lower end of the seat body is provided with a positioning block; and the cover body is buckled on the seat body to form a close space. The invention also relates to a fabricating method of the micro-fuse, which comprises the following steps: providing the seat body, arranging the two electrode parts in a penetrating way; forming planes and the bearing and fixing surfaces at the end parts of the two electrode parts, and bending through hole grooves to form the two ring bodies, wherein the inner ring body is pressed and fixedly connected to the inner side of the melting part, the outer ring body is welded and fixedly connected to the end part of the melting part; bearing the melting part by the bearing platform at the upper end of the seat body; and forming the close space by the cover body correspondingly covering the seat body. The micro-fuse has high yield, high quality and high safety.

Description

Mini-insurance yarn production method and finished product
Technical field
The present invention provides a kind of mini-insurance yarn production method and finished product, relates in particular to finished electrode portion, and the one of which end is set as two ring bodies of closed-end, and is provided with the solid face that holds; In addition its manufacturing approach comprises: the position on its electrode part plane, form the open-work groove end that the end links to each other, and make the melting welding can be more effectively firm.
Background technology
The traditional insurance silk generally is used for electronic product, via through fuse pass through electric current excessive, danger such as thermal ignition took place in order to avoid circuit in smelting part thereby fusing, purpose is protecting people and equipment not to damage because of overcurrent, even breaking out of fire.
Moreover along with electric equipment is compact, function becomes increasingly complex at present, and the part that needs is more and more; Circuit and electronic component on the circuit board are also more and more intensive, so the circuit of circuit substrate trends towards miniaturization, electronic component is microminiaturized; Be the normality method for using, it can make the part of circuit board can be comparatively intensive, and greater functionality is placed on the printed circuit board (PCB) of same area; Yet general mini-insurance yarn production method uses the direct joining of scolding tin to connect pin and the manufacture that melts white silk portion; Do not have the good location design again, make it form unsettled protective effect, so its product stability is not good; Make difficulty, cost is high again, uses waste material and produce fraction defective high.
Again, general electronic circuit is the one side that part is placed in circuit board, and the fuse pin is welded on the another side; The solder joint operation of this kind processing pin lets and between this microfuze pin and the molten white silk portion small peeling off takes place easily, because outward appearance is normal; Be not easy to check out the small of inner smelting part and pin to peel off, cause secondary melting welding, so let and pass through greater than the maximum electric current that uses of normal rating and produce localized hyperthermia; Make it be not sure of the maximum electric current that uses of normal rating; And make expensive device impaired, burn, injury or peril etc., so protection not exclusively, can not be satisfied the demand on the market.
Therefore prior art summary has following shortcoming:
1, the microfuze of prior art, no good location design, the product stability is not good, and it is high again to make difficult cost, uses waste material and produce fraction defective high.
2, the microfuze of prior art when the solder joint operation of processing pin, is easy to generate localized hyperthermia and causes secondary melting welding, and protection not exclusively can not be satisfied the demand on the market.
3, the microfuze of prior art is not sure of the maximum electric current that uses of normal rating during use, protective circuit safety, and make expensive device impaired, burn, injury or peril.
4, prior art when small peeling off taken place, because outward appearance is normal, has the problem that is not easy to check out inner disappearance.
In view of this, how above-mentioned disappearance is forgone, be the place of the technical difficulties of this case inventor institute desire solution.So; This case inventor is based on the experience of being engaged in the Related product design for many years, and thoughts on the inconvenience of above-mentioned traditional articles for use, warp is taken great pains to attain one's goal for many years and concentrated on studies; Study improvement; Finally the many shortcomings of commonly using microfuze of can forgoing are are successfully researched and developed completion this case, make the present invention be able to be born, and to promote effect.
Summary of the invention
The objective of the invention is to: a kind of microfuze and manufacturing approach thereof are provided,, make melting welding can be more effectively firm to overcome the shortcoming of above-mentioned prior art.When its smelting part end and two electrode part melting welding, tin liquor can wrong not invaded smelting part, or rotates because of two electrode part slippages when using and influence smelting part, causes the danger that ensures electric current mistake standard, and makes microfuze have high yield, high-quality, high security.
For realizing the purpose of foregoing invention, the technical scheme that the present invention adopted is: a kind of microfuze is provided, and it comprises:
One smelting part is provided with cylinder and reaches the melting filament around said cylinder; Two electrode part; One end of each electrode part is set as two ring bodies of closed-end, and wherein, inner ring body is pressed to establish and is fixed in said smelting part inboard; Outer ring body melting welding is fixed in said smelting part end; Two ring body necks of this closed-end form closure, and are provided with the solid face that holds, and slippage takes place when preventing that this two electrode part free end from passing through the pedestal open-work rotate; One pedestal has open-work and passes through for two electrode part, and its upper end is provided with cushion cap firmly to accept smelting part, and side is provided with and fastens ring to fasten with lid, and the lower end is provided with the locating piece provider to the location; And a lid, having the ring of cooperation, corresponding buckling base body forms airtight connection.
The present invention also provides a kind of manufacturing approach of microfuze, and it may further comprise the steps:
(A) pedestal is provided, in this pedestal, passes through two electrode part are set;
(B) said two electrode part ends are formed the plane with impact style, and this rear, plane is formed the solid face that holds;
(C) in the position on said two electrode part planes with punching out or drag for the groove mode, make to form the open-work groove that the end links to each other;
(D) put in the open-work groove end of said two electrode part and establish smelting part, and make the two crooked ring bodies that form closed-end, said smelting part is vertical with the maintenance of two electrode part free ends;
(E) with two crooked ring body neck bendings, make this two crooked ring body become two ring bodies of closed-end, said ring body and two electrode part free ends are positioned at same vertical plane;
(F) for two ring bodies of closed-end, wherein the inner ring body extrusion is fixed in the smelting part inboard;
(G) for two ring bodies of closed-end, wherein outer ring body melting welding is fixed in the smelting part end;
(H) in the pedestal upper end cushion cap is set, firmly accepts smelting part;
(I) form with a lid buckling base body airtight, with the protection smelting part.
In another aspect of the present invention, the manufacturing approach of this microfuze comprises that further wherein this step (G) has following substep:
(G-1), be stained with sticking tin point at smelting part end and outer ring body melting welding fixing position;
(G-2) with noncontact mode of heatings such as flame, high frequency or hot blasts, that outer ring body and the melting welding of smelting part end is affixed.
Beneficial effect of the present invention is that microfuze of the present invention has this good location design of two ring bodies of closed-end, and the product stability is good, and waste material and production yield are not high.When the solder joint operation of processing pin, be not easy to take place localized hyperthermia and cause secondary melting welding, protection can be satisfied the demand on the market fully.The inner ring body extrusion is fixed in the smelting part inboard, prevents scolding tin intrusion smelting part, and stay in grade during use can confirm to ensure the maximum electric current that uses of normal rating.The present invention has and holds solid face, avoided small peeling off takes place, but protective circuit safety, and make expensive device do not have impaired, burn, injury or peril.Can satisfy value and actual required on business circles and the industrial circle.
Simultaneously, the present invention has well solved microfuze, the problem of high-quality, high yield, high safety, make microfuze can safe relieved use in electrical appliance, reach and can economize the purpose that can, subtract carbon, practiced thrift cost greatly.By this, kept microfuze quality function originally simultaneously, reached the effect of not destroying the quality of electrical appliance really, the user is provided safety guarantee.
Description of drawings
Fig. 1 is the present invention's a stereoscopic combination sketch map;
Fig. 2 is a part section schematic perspective view of the present invention;
Fig. 3 is a preferred embodiment manufacturing approach schematic flow sheet of the present invention;
Fig. 4 is the thin schematic flow sheet of preferred embodiment of the present invention.
Description of reference numerals:
The 1-microfuze; The 2-smelting part; The 21-cylinder; 22-melting filament; 23-tin point; 3-two electrode part; 31-two ring bodies; The 311-inner ring body; The 312-outer ring body; The 313-heating; The 32-neck; 33-holds solid face; The 34-free end; The 35-plane; 36-open-work groove; 37-two crooked ring bodies; The 4-pedestal; The 41-open-work; The 42-cushion cap; 43-fastens ring; The 44-locating piece; The 5-lid; 51-cooperates ring.
Embodiment
Below in conjunction with accompanying drawing the above-mentioned feature and advantage with other of the present invention are elaborated.
At first see also Fig. 1 and shown in Figure 2, it is respectively the present invention's stereoscopic combination sketch map and part section schematic perspective view of the present invention; A kind of microfuze 1 of the present invention wherein, its characteristic includes:
One smelting part 2 is provided with cylinder 21 and around the melting filament 22 on it, its both ends are installed with two electrode part;
Two electrode part 3; During rectifying, one of each electrode part 3 vertically is provided with two ring bodies 31 of closed-end; The inner ring body 311 of two ring bodies 31 is pressed to establish and is fixed in smelting part 2 inboards, and ring body 312 melting welding are fixed in smelting part 2 ends outside two ring bodies 31, and the neck 32 of two ring bodies 31 of this closed-end forms closed; And be provided with and hold solid face 33, slippage takes place when passing through pedestal 4 open-works 41 and rotates in the free end 34 that prevents this two electrode part 3;
One pedestal 4, having open-work 41 provides two electrode part 3 to pass through, and its upper end is provided with cushion cap 42 and can firmly accepts smelting part 2, and side is provided with fastening ring 43 can fasten lid 5, and the lower end is provided with locating piece 44 providers to the location; And
One lid 5 has the ring of cooperation 51, can correspondingly fasten pedestal 4 and form airtight protection;
Other sees also Fig. 3 and shown in Figure 4, is the thin schematic flow sheet of preferred embodiment manufacturing approach schematic flow sheet of the present invention and preferred embodiment of the present invention; The manufacturing approach of a kind of microfuze of the present invention wherein, it may further comprise the steps:
(A) pedestal 4 is provided, the open-work 41 in this pedestal 4 passes through two electrode part 3 is set;
(B) two electrode part, 3 ends are formed plane 35 with impact style, and this position, 35 rear, plane is formed the solid face 33 that holds;
(C) in the position on two electrode part, 3 formation planes 35 with punching out or drag for the groove mode, make to form the open-work groove 36 that the end links to each other;
(D) at open-work groove 36 ends of this two electrode part, put and establish smelting part 2, and make the two crooked ring bodies 37 that form closed-end, and make smelting part 2 keep vertical with two electrode part, 3 free ends 34;
(E), form two ring bodies 31 of closed-end, and keep center vertical (being the circular center of circle, straight-line pass said ring body place at said free end 34 places) with two electrode part, 3 free ends 34 with 32 bendings of two crooked ring body 37 necks;
(F) for two ring bodies 31 of closed-end, wherein inner ring body 311 extrusions are fixed in smelting part 2 inboards;
(G) for two ring bodies 31 of closed-end, wherein outer ring body 312 melting welding are fixed in smelting part 2 ends;
(H) in pedestal 4 upper ends cushion cap 42 is set, firmly to accept smelting part 2;
(I) with a lid 5, corresponding fastening pedestal 4 forms airtight, with protection smelting part 2.
In manufacturing approach of the present invention, wherein this step (G) has following substep:
(G-1), be stained with sticking tin point 23 at smelting part 2 ends and outer ring body 312 melting welding fixing positions;
(G-2) heat 313 modes with noncontacts such as flame, high frequency or hot blasts, outer ring body 312 is affixed with the tin point melting welding of smelting part 2 end fixing positions.
Be noted that; Above embodiment is merely the preferred embodiment of the present invention/utility model; Its description of this invention is illustrative, and nonrestrictive, and those skilled in the art is understood; Within spirit that claim limits and scope, can carry out many modifications, variation or equivalence, but they will fall in protection scope of the present invention all to it.
For making the present invention show its progressive and practicality more, now its advantage is listed below:
1. microfuze of the present invention, this good location design of two ring bodies with closed-end, the product stability is good, and waste material and production yield are not high.
2. microfuze of the present invention when the solder joint operation of processing pin, is not easy to take place localized hyperthermia and causes secondary melting welding, and protection can be satisfied the demand on the market fully.
3. microfuze of the present invention, the inner ring body extrusion is fixed in the smelting part inboard, prevents scolding tin intrusion smelting part, and stay in grade during use can confirm to ensure the maximum electric current that uses of normal rating.
4. the present invention has and holds solid face, avoided small peeling off takes place, but protective circuit safety, and make expensive device do not have impaired, burn, injury or peril.
5. have on business circles and the industrial circle value with actual required.
In sum, the present invention is breaking through under the previous technical pattern, has reached the effect that institute's desire is promoted really, and the easy full of beard of also non-those skilled in the art institute reaches; Moreover not open before the application of the present invention, the creativeness of its tool, practicality show the application important document that has met patent of invention, propose the invention application in accordance with the law.

Claims (3)

1. microfuze, it comprises:
One smelting part is provided with cylinder and reaches the melting filament around said cylinder;
Two electrode part, an end of each electrode part is set as two ring bodies of closed-end, and two ring bodies of described closed-end are meant that the free end of the open-work groove that forms this two ring body is what seal; Wherein, Inner ring body is pressed to establish and is fixed in said smelting part inboard, and outer ring body melting welding is fixed in said smelting part end, and two ring body necks of this closed-end form closure; And be provided with the solid face that holds, slippage taking place when preventing that this two electrode part free end from passing through the pedestal open-work rotates;
One pedestal has open-work and passes through for two electrode part, and its upper end is provided with cushion cap firmly to accept smelting part, and side is provided with and fastens ring to fasten with lid, and the lower end is provided with the locating piece provider to the location; And
One lid has the ring of cooperation, and corresponding buckling base body forms airtight connection.
2. the manufacturing approach of a microfuze, it may further comprise the steps:
(A) pedestal is provided, in this pedestal, passes through two electrode part are set;
(B) said two electrode part ends are formed the plane with impact style, and this rear, plane is formed the solid face that holds;
(C) in the position on said two electrode part planes with punching out or drag for the groove mode, make to form the open-work groove that the end links to each other;
(D) in the open-work groove end of said two electrode part smelting part is set; And make the two crooked ring bodies that form closed-end; Two crooked ring bodies of described closed-end are meant the free end of the open-work groove that forms this two crooked ring body for what seal, and said smelting part keeps vertical with two electrode part free ends;
(E) with two crooked ring body neck bendings, make this two crooked ring body become two ring bodies of closed-end, two ring bodies of described closed-end are meant that the end of said two ring bodies and neck form closure, and said two ring bodies and two electrode part free ends are positioned at same vertical plane;
(F) for two ring bodies of closed-end, wherein the inner ring body extrusion is fixed in the smelting part inboard;
(G) for two ring bodies of closed-end, wherein outer ring body melting welding is fixed in the smelting part end;
(H) in the pedestal upper end cushion cap is set, firmly accepts smelting part;
(I) form with a lid buckling base body airtight, with the protection smelting part.
3. the manufacturing approach of microfuze according to claim 2 is characterized in that, this step (G) has following substep:
(G-1), be stained with sticking tin point at smelting part end and outer ring body melting welding fixing position;
(G-2) with flame, high frequency or hot blast or other noncontact mode of heating, that outer ring body and the melting welding of smelting part end is affixed.
CN2008101115986A 2008-06-10 2008-06-10 Manufacturing method and finished product of micro-fuse Expired - Fee Related CN101604602B (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2008101115986A CN101604602B (en) 2008-06-10 2008-06-10 Manufacturing method and finished product of micro-fuse

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2008101115986A CN101604602B (en) 2008-06-10 2008-06-10 Manufacturing method and finished product of micro-fuse

Publications (2)

Publication Number Publication Date
CN101604602A CN101604602A (en) 2009-12-16
CN101604602B true CN101604602B (en) 2012-05-16

Family

ID=41470281

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2008101115986A Expired - Fee Related CN101604602B (en) 2008-06-10 2008-06-10 Manufacturing method and finished product of micro-fuse

Country Status (1)

Country Link
CN (1) CN101604602B (en)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP6175256B2 (en) * 2013-03-21 2017-08-02 矢崎総業株式会社 fuse
CN107610988B (en) 2017-10-30 2021-01-01 Aem科技(苏州)股份有限公司 Miniature super surface-mounted fuse and manufacturing method thereof

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1469410A (en) * 2002-07-16 2004-01-21 邱鸿智 Manufacture of miniature industrial fuse
CN2874759Y (en) * 2006-01-11 2007-02-28 厦门宁利电子有限公司 Micro fuse
CN200993949Y (en) * 2006-12-29 2007-12-19 颜琼章 Fuse melt wire joint structure

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1469410A (en) * 2002-07-16 2004-01-21 邱鸿智 Manufacture of miniature industrial fuse
CN2874759Y (en) * 2006-01-11 2007-02-28 厦门宁利电子有限公司 Micro fuse
CN200993949Y (en) * 2006-12-29 2007-12-19 颜琼章 Fuse melt wire joint structure

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
JP特开平9-204871A 1997.08.05

Also Published As

Publication number Publication date
CN101604602A (en) 2009-12-16

Similar Documents

Publication Publication Date Title
CN101685734B (en) Explosion proof fuse with energy saving and environmental protection as well as manufacturing method thereof
CN101604602B (en) Manufacturing method and finished product of micro-fuse
CN109037509B (en) Secondary battery top cover assembly, secondary battery containing same and assembling method
CN102263466A (en) Electric machine rotor bar and method of making same
JP6090155B2 (en) Induction heating heating element and induction heating container
CN102741963A (en) Fuse unit
CN104520956B (en) Can melt back welding circuit protection device
CN201702484U (en) Soldering bit
CN101763982B (en) Thin temperature fuse with cushion layer structure and preparation method thereof
CN205508751U (en) Thermal fuse
US20130186867A1 (en) Spot Welding Clamp and A Spot Welding Process
JP2008159351A (en) Battery device
CN205264765U (en) Battery pack
CN101894716A (en) Metal-jointed high voltage fuse structure and manufacturing method thereof
CN103531401B (en) A kind of magnetic switch structure of Split type welding and assemble method thereof
CN201307574Y (en) Metal tube cap structure of fuse
CN205621694U (en) Fusible body structure of fuse
TWI345256B (en)
CN106813117A (en) LED straight lamps
KR101026132B1 (en) Method for manufacturing cooking vessel for induction range and the cooking vessle thereby
CN206226892U (en) A kind of circuit board assemblies and cooking apparatus
CN107978450A (en) A kind of explosion-proof block of capacitor
CN208284547U (en) Battery module and its connection sheet
CN207475898U (en) A kind of planar heat producing body connects insulated terminal
CN206596042U (en) A kind of mobile device and its housing

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20120516

Termination date: 20210610