CN101597442B - Ink water-tight additive and preparation method and application thereof - Google Patents

Ink water-tight additive and preparation method and application thereof Download PDF

Info

Publication number
CN101597442B
CN101597442B CN 200910133796 CN200910133796A CN101597442B CN 101597442 B CN101597442 B CN 101597442B CN 200910133796 CN200910133796 CN 200910133796 CN 200910133796 A CN200910133796 A CN 200910133796A CN 101597442 B CN101597442 B CN 101597442B
Authority
CN
China
Prior art keywords
ink
water
additive
tight
milliliters
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200910133796
Other languages
Chinese (zh)
Other versions
CN101597442A (en
Inventor
张一鲜
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200910133796 priority Critical patent/CN101597442B/en
Publication of CN101597442A publication Critical patent/CN101597442A/en
Application granted granted Critical
Publication of CN101597442B publication Critical patent/CN101597442B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to an ink water-tight additive and a preparation method and application thereof, wherein the additive comprises the following raw materials in proportion by weight: 400 to 600 milliliters of 75 percent alcohol, 40 to 60 grams of wintergreen barberry root, 40 to 60 grams of folium onychii, and 400 to 600 milliliters of water. The method for preparing the ink water-tight additive comprises the following steps: crushing the wintergreen barberry root and the folium onychii; soaking the mixture with the 75 percent alcohol; filtering the mixture, washing the residues with the water, and then filtering the mixture; collecting filtrates; and combining the filtrates and mixing the mixture evenly to obtain the finished product. The ink water-tight additive is added into an inkin proportion so that a pen point is not dried, the water does not leak, the ink is even and smooth during writing, and handwritings are clear with a deep color, are not intolerance of light and damp, and can be preserved for a long time. The ink water-tight additive has the advantages of simple preparation method, low cost and easy industrial production.

Description

A kind of ink water-tight additive and its production and application
Technical field
The present invention relates to a kind of ink water-tight additive and its production and application.
Background technology
Pen is one of conventional book writing tools of China, but in use there is certain defective in traditional pen, and is inhomogeneous as water outlet; the phenomenon that occurs " having loose bowels " (leaking) or dry brush point through regular meeting; cause and write not smoothly, writing is unintelligible, has also reduced the work-ing life of pen simultaneously.In addition, also there is photophobia in the writing of writing, be afraid of tide, fugitive color, problem such as can not preserve for a long time, causes and is ready to use the people of pen fewer and feweri in the last few years.This just means pen and the Chinese hard-tipped pen calligraphical works that has passed on more than 2,000 year, will face the danger that steps down from the stage of history, so that the tomography of unluckily Chinese calligraphy occurs.
At present, some ink manufacturer has been noted that the problems referred to above, and attaching when selling every bottle of ink has several stump paper.But this method has just made things convenient for the user to a certain extent, fundamentally do not solve lettering pen leak, write not smooth, dry brush is sharp, writing is unintelligible, photophobia, fearness tide, fugitive color, problem such as can not preserve for a long time.
Technical problem to be solved by this invention be to overcome lettering pen in the prior art " have loose bowels " (leaking), dry brush point, draw paper, write not smooth, writing is unintelligible, fugitive color, defective such as can not preserve for a long time, and a kind of ink additive and its production and application of " not having loose bowels " is provided.
The present invention at first provides a kind of ink additive of " not having loose bowels ", and the raw material of described additive comprises 75% alcohol, Mahonia shenii Chun, FOLIUM ONYCHII and water, the ratio of each component is: 400~600 milliliters of 75% alcohol; Mahonia shenii Chun 40~60 grams; FOLIUM ONYCHII 40~60 grams; 400~600 milliliters in water.
The preparation method that the present invention also provides above-mentioned ink " not have loose bowels " additive:, Mahonia shenii Chun and FOLIUM ONYCHII are pulverized, with 75% alcohol-pickled 5-9 days according to the proportioning of each feed composition, filter, after washing residue with water, refilter, mix after gained filtrate is merged.
The present invention also provides the above-mentioned ink Application of Additives of " not having loose bowels ", and additive is joined in the ink, and the volume ratio of additive and ink is 1: 15~25.
Technique scheme provided by the invention has overcome that lettering pen in the prior art " is had loose bowels ", the dry brush point, write not smooth, draw defective such as paper, after adding additive provided by the invention in the ink, lettering pen " do not have loose bowels " (water-tight), not dry brush point, fluent writing, do not draw paper, prolonged the work-ing life of lettering pen simultaneously; And the writing of writing is evenly clear, not photophobia, be not afraid of tide, still clear as new after long-time the preservation, bring great convenience and joyful experience to the user." the do not have loose bowels " preparation method of additive of ink provided by the invention is simple, with low cost, is easy to suitability for industrialized production.
Embodiment
Below describe technical scheme of the present invention in detail by specific embodiment.
Embodiment 1
Each 50 gram of FOLIUM ONYCHII and Mahonia shenii Chun are pulverized.Soaked 7 days for 500 milliliters with 75% alcohol, use absorbent cotton and funnel to filter twice; Then, with 500 ml tap waters washing residue and filtration; Mix after gained filtrate merges invention product 1.
Embodiment 2
FOLIUM ONYCHII 40 grams, Mahonia shenii Chun 50 grams are pulverized.Soaked 9 days for 400 milliliters with 75% alcohol, use filter paper and Bu Shi funnel to filter; Then, with 400 ml distilled waters washing residue and filtration; Mixing after gained filtrate merges is this one-tenth invention product 2.
Embodiment 3
FOLIUM ONYCHII 60 grams, Mahonia shenii Chun 60 grams are pulverized.Soaked 5 days for 600 milliliters with 75% alcohol, use absorbent cotton and funnel to filter; Then, with 600 milliliters of pure water washing residues and filtration; Mix after gained filtrate merges invention product 3.
Embodiment 4
FOLIUM ONYCHII 50 grams, Mahonia shenii Chun 40 grams are pulverized.Soaked 7 days for 500 milliliters with 75% alcohol, use sand core funnel to filter; Then, add 500 milliliters in tap water, the residue after the washing and filtering; Mix after gained filtrate merges invention product 4.
Result of use is estimated
Get specification and be 60 milliliters/bottle 300 bottles of fountain pen inks, wherein, 100 bottles of blue-black inks add 2.5 milliliters of the present invention's product 1 for every bottle; 100 bottles of burnt black inks add 3 milliliters of invention product 2 for every bottle in addition; 100 bottles of remaining ethereal blue inks, 50 bottles of inks add every bottle of 3,50 bottles of ink of 3.5 milliliters of invention product for every bottle and add 4.0 milliliters of invention product 4.
With the above-mentioned ink thorough mixing that is added with additive evenly after, pour into pen and write, " do not have loose bowels " all the time (water-tight), dry brush point, fluent writing, writing are evenly not clear, color is dark, it is still clear as newly to preserve after 2 years.
The present invention includes but be not limited to above embodiment.More than cited embodiment only be used to understand essence of the present invention, to the change that does not break away from flesh and blood of the present invention that the present invention makes, still belong to protection scope of the present invention according to prior art.
The applicant used for four years, and shared 5800 bottle 60 milliliter/bottle ink is tested, and makes the whatsoever ink and the lettering pen of brand, in writing process, occur no longer all that " having loose bowels " leaks, the dry brush point, write not smooth, draw problem such as paper.This additive also can make ink color deepen, and writing is evenly clear, and photophobia is not afraid of tide, can preserve for a long time, prolongs the work-ing life of lettering pen simultaneously.
China is the big country of 1,300,000,000 populations, and at present, " the do not have loose bowels " market outlook of additive of ink provided by the invention are wide.According to investigations, existing 1.4 hundred million pupils, middle school student 6,000 ten thousand.National Development and Reform Commission's statistics in 2007: Colleges and Universities of China university student and postgraduate are respectively 1738.8 ten thousand and 110.5 ten thousand people, and the number of participating in college entrance examination in 2009 just has 1,000 ten thousand people.If per 3 months everyone with 1 bottle of fountain pen ink, then the sales volume in 1 year of manufacturer will be greatly surprising.
In today of scientific-technical progress, if adapt to modern demand, add the ink provided by the invention additive of " not having loose bowels ", not only solved lettering pen " have loose bowels " (leaking), dry brush point, write not smooth, draw problem such as paper, and the writing of writing is evenly clear, not photophobia, be not afraid of tide, still clear as new after long-time the preservation, also prolonged simultaneously the work-ing life of lettering pen, also bring the writer convenient and joyful experience, improved temperament and interest that the human consumer writes simultaneously and to the hobby of calligraphy, and then the sale of promotion ink, form benign cycle.
From economic angle, some ink manufacturer is the human consumer for convenience, and every bottle provides 5~6 stump paper (about 0.09 yuan of cost), the usefulness that in fact is nowhere near (about 23~25 ability are enough).Produce 1,000,000 bottles if producer is annual, then cost is annual increases by 90,000 yuan.As seen the use of stump paper not only can't resolve the root problem that ink exists, and has also increased the production cost of producer.In today that the economic benefit of ink factory go fromes bad to worse, if meeting the market requirement adds the ink provided by the invention additive of " not having loose bowels " in ink, can not only create very high economic benefit, can also bring good social benefit.

Claims (7)

1. ink water-tight additive, it is characterized in that: the raw material of described additive comprises 75% alcohol, Mahonia shenii Chun, FOLIUM ONYCHII and water, the ratio of each component is: 400~600 milliliters of 75% alcohol; Mahonia shenii Chun 40~60 grams; FOLIUM ONYCHII 40~60 grams; 400~600 milliliters in water;
The preparation method is as follows: according to the proportioning of each feed composition, Mahonia shenii Chun and FOLIUM ONYCHII are pulverized, with 75% alcohol-pickled 5~9 days, filtered, wash residue with water and filter, will mix after the merging of gained filtrate.
2. ink water-tight additive according to claim 1 is characterized in that: the ratio of each component is: 75% alcohol, 450~550 milliliters; Mahonia shenii Chun 45~55 grams; FOLIUM ONYCHII 45~55 grams; 450~550 milliliters in water.
3. ink water-tight additive according to claim 1 is characterized in that: the proportioning of each component is as follows: 75% alcohol, 500 milliliters; Mahonia shenii Chun 50 grams; FOLIUM ONYCHII 50 grams; 500 milliliters in water.
4. according to the described ink water-tight additive of claim 1, it is characterized in that: described preparation method is: according to the proportioning of each feed composition, Mahonia shenii Chun and FOLIUM ONYCHII are pulverized, with 75% alcohol-pickled 7 days, filter, wash residue and filtration with water, will mix after the merging of gained filtrate.
5. the application of each described ink water-tight additive of claim 1~4 is characterized in that: additive is joined in the ink, and the volume ratio of additive and ink is 1: 15~25.
6. the application of ink water-tight additive according to claim 5 is characterized in that: additive is joined in the ink volume ratio of additive and ink 1: 18~22.
7. the application of ink water-tight additive according to claim 6 is characterized in that: additive is joined in the ink, and the volume ratio of additive and ink is 1: 20.
CN 200910133796 2009-04-17 2009-04-17 Ink water-tight additive and preparation method and application thereof Expired - Fee Related CN101597442B (en)