CN101586022A - Preparing method of silicon viscosity reducer for drilling fluid - Google Patents

Preparing method of silicon viscosity reducer for drilling fluid Download PDF

Info

Publication number
CN101586022A
CN101586022A CNA2009100334374A CN200910033437A CN101586022A CN 101586022 A CN101586022 A CN 101586022A CN A2009100334374 A CNA2009100334374 A CN A2009100334374A CN 200910033437 A CN200910033437 A CN 200910033437A CN 101586022 A CN101586022 A CN 101586022A
Authority
CN
China
Prior art keywords
drilling fluid
viscosity reducer
silicon
equal
silicon viscosity
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2009100334374A
Other languages
Chinese (zh)
Inventor
陆明富
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA2009100334374A priority Critical patent/CN101586022A/en
Publication of CN101586022A publication Critical patent/CN101586022A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparing method of a silicon viscosity reducer for the drilling fluid, comprising steps: step one, adding proper water in a reactor, then feeding methyl chlorosilane, stirring and reacting for generating mixed solution, cooling the mixed solution; step two, adding aqueous alkali into the cooled reaction solution for complete reaction, feeding aluminium sulphate solution, stirring and reacting for a period, forming the silicon viscosity reducer for the drilling fluid. The prepared viscosity reducer has strong high-temperature (more than 240 DEG C) resistance and high compatibility with the other substances, good mud stream rheological property, dilution, viscosity reduction property and lubricating property. The working substance content is higher or equal to 16%; the chloride content is lower or equal to 10% and the viscosity reduction ratio is higher or equal to 80% at the room temperature and the viscosity reduction ratio at 220 DEG C for 16 hours is higher than or equal to 70%.

Description

A kind of preparation method of silicon viscosity reducer for drilling fluid
Technical field
The present invention relates to a kind of preparation method of silicon viscosity reducer for drilling fluid.
Background technology
The high-temperature resistance of present silicon viscosity reducer is more weak, and poor with the compatibleness of other products.
Summary of the invention
The invention provides a kind of preparation method of silicon viscosity reducer for drilling fluid, the viscosity-depression agent that it makes not only high-temperature resistance is strong, and has good viscosity-reducing performance.
The present invention has adopted following technical scheme: a kind of preparation method of silicon viscosity reducer for drilling fluid, it may further comprise the steps: step 1, an amount of water is added in the reactor, and then adding methyl chlorosilane, carry out again generating mixing solutions behind the stirring reaction, after question response finishes mixing solutions is cooled off; Step 2; In cooling afterreaction solution, add alkaline solution and fully react, after adding alum liquor stirring reaction for some time again after the reaction, form silicon viscosity reducer for drilling fluid.
Adding the time of alum liquor stirring reaction time in the step 2 of the present invention is 4 hours.The silicon viscosity reducer for drilling fluid that makes in the step 2 of the present invention is water white transparency or weak yellow liquid, and its pH value is 13-14, and proportion is 1.1-1.3.
The present invention has following beneficial effect: the viscosity-depression agent that adopts above method to make has very strong high-temperature resistance, high temperature resistance can reach more than 240 ℃, and it is strong with the compatibility ability of other materials, the good stability of while drilling fluid rheology and high temperature resistance thereof, have good dilution, viscosity reduction and lubricity, the content of its working substance 〉=16%, muriatic content≤10%, its viscosity break ratio at ambient temperature 〉=80%, 16 hours viscosity break ratio 〉=70% under 220 ℃ condition.
Embodiment
The invention discloses a kind of preparation method of silicon viscosity reducer for drilling fluid, it may further comprise the steps: step 1 adds an amount of water in the reactor, and then adds methyl chlorosilane, carry out again generating mixing solutions behind the stirring reaction, after question response finishes mixing solutions is cooled off; Step 2; Adding alkaline solution in cooling afterreaction solution fully reacts, form silicon viscosity reducer for drilling fluid after 4 hours adding the alum liquor stirring reaction after the reaction again, silicon viscosity reducer for drilling fluid is water white transparency or weak yellow liquid, and its pH value is 13-14, and proportion is 1.1-1.3.

Claims (3)

1, a kind of preparation method of silicon viscosity reducer for drilling fluid, it may further comprise the steps:
Step 1 adds an amount of water in the reactor, and then adds methyl chlorosilane, carries out generating mixing solutions behind the stirring reaction again, after question response finishes mixing solutions is cooled off;
Step 2; In cooling afterreaction solution, add alkaline solution and fully react, after adding alum liquor stirring reaction for some time again after the reaction, form silicon viscosity reducer for drilling fluid.
2, the preparation method of silicon viscosity reducer for drilling fluid according to claim 1 is characterized in that adding the time of alum liquor stirring reaction time in the step 2 is 4 hours.
3, the preparation method of silicon viscosity reducer for drilling fluid according to claim 1 is characterized in that the silicon viscosity reducer for drilling fluid that makes in the step 2 is water white transparency or weak yellow liquid, and its pH value is 13-14, and proportion is 1.1-1.3.
CNA2009100334374A 2009-06-22 2009-06-22 Preparing method of silicon viscosity reducer for drilling fluid Pending CN101586022A (en)