CN101527177A - 环氧少胶单面聚酯薄膜粉云母带 - Google Patents
环氧少胶单面聚酯薄膜粉云母带 Download PDFInfo
- Publication number
- CN101527177A CN101527177A CN200810034189A CN200810034189A CN101527177A CN 101527177 A CN101527177 A CN 101527177A CN 200810034189 A CN200810034189 A CN 200810034189A CN 200810034189 A CN200810034189 A CN 200810034189A CN 101527177 A CN101527177 A CN 101527177A
- Authority
- CN
- China
- Prior art keywords
- polyester film
- mica tape
- supporting material
- mica
- epoxy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种环氧少胶单面聚酯薄膜粉云母带,包括:云母纸(1);还包括:补强材料(3);所述的云母纸(1)和补强材料(3)之间通过改性环氧粘合剂(2)连接;本发明的有益效果是:能满足线圈制造工艺,加快生产速度,降低成本,粘结强度高,不分层,不掉粉的环氧少胶云母带。由于采用聚酯薄膜为补强材料,大大提高了绝缘性能,使绝缘厚度减薄成为可能。减少了电机的尺寸,降低了成本。
Description
技术领域
本发明涉及一种云母带,尤其涉及该云母带的结构。
背景技术
现有技术中交流高压电机主绝缘有多胶粉云母带模压绝缘、中胶粉云母带VPI绝缘和少胶云母带VPI绝缘等几种体系。从综合性能与长远发展来看,少胶云母带VPI绝缘无疑是高压电机绝缘制造技术的发展方向。
与前两种绝缘体系相比,少胶云母带VPI绝缘中的云母含量显著提高,绝缘内无气隙,整体性能好,有利于提高绝缘的电气性能,耐电晕性与耐电寿命,从而提高了电机的技术指标、运行寿命及运行可靠性,同时大大简化了线圈制造工艺,不但可缩短生产周期,降低制造成本,而且有利于提高线圈绝缘质量。
在以前的研制样品中,少胶云母带极不稳定,有飞粉、分层等问题,不能满足机械绕包线圈工艺要求,无法进行批量生产,满足不了电机行业的需求。
发明内容
本发明需要解决的技术问题是提供了一种环氧少胶单面聚酯薄膜粉云母带,旨在解决上述的问题。
为了解决上述技术问题,本发明是通过以下技术方案实现的:
本发明包括:云母纸;还包括:补强材料;所述的云母纸和补强材料之间通过改性环氧粘合剂连接。
与现有技术相比,本发明的有益效果是:能满足线圈制造工艺,加快生产速度,降低成本,粘结强度高,不分层,不掉粉的环氧少胶云母带。由于采用聚酯薄膜为补强材料,大大提高了绝缘性能,使绝缘厚度减薄成为可能。减少了电机的尺寸,降低了成本。
附图说明
图1是本发明的结构图;
具体实施方式
下面结合附图与具体实施方式对本发明作进一步详细描述:
由图1可见:本发明包括:云母纸1;还包括:补强材料3;所述的云母纸1和补强材料3之间通过改性环氧粘合剂2连接;
所述的云母纸1是大鳞片云母纸;
所述的补强材料3是单面介电强度很高的聚酯薄膜。
本发明由补强材料、改性环氧粘合剂和大鳞片云母纸组成。经复合、烘焙、收卷、切割而成。
补强材料是聚酯薄膜。聚酯薄膜介电击穿强度很高,使用以后可以减薄线圈的绝缘厚度。由于采用改性环氧粘合剂,胶含量低于11%,云母带柔软,不掉粉,粘结强度高,不分层。适于高速绕包,可大批量应用于高压电机的线圈绕包,大大减薄了绝缘厚度,提高了线圈的绝缘质量,缩短了周期,大大降低了生产成本。
本发明适用于电动机、风力发电机线圈、引线和端部绕包绝缘。采用大鳞片云母带使云母带具有更好的渗透性,提高了电机线圈的整体性能,提高了电气、耐电晕、耐电寿命。改性环氧胶粘剂具有很高的粘接强度,同时又与现有的绝缘浸渍树脂有较高的相溶性,使少胶云母带批量生产成为可能。
Claims (3)
1.一种环氧少胶单面聚酯薄膜粉云母带,包括:云母纸(1);其特征在于:还包括:补强材料(3);所述的云母纸(1)和补强材料(3)之间通过改性环氧粘合剂(2)连接。
2.根据权利要求1所述的环氧少胶单面聚酯薄膜粉云母带,其特征在于:所述的云母纸(1)是大鳞片云母纸。
3.根据权利要求1或2所述的环氧少胶单面聚酯薄膜粉云母带,其特征在于:所述的补强材料(3)是单面介电强度很高的聚酯薄膜。